Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Abstracts archive – Issue 18 (2026)


1. EXPERIMENTAL STUDIES OF NANOPARTICLES, NANOSYSTEMS, AND NANOMATERIALS – page 7

Anofriev V.A., Antonov A.S., Semenova E.M., Afanasiev M.S., Sdobnyakov N.Yu.
Size effect in the formation of fractal nickel films – page 7
Abstract: In this paper, we examine the size effect to describe the patterns of fractal relief formation using nanoscale nickel films (50-100 nm thick). Two alternative imaging methods were employed: atomic force microscopy and scanning tunneling microscopy. By analyzing a series of images at a scale of 500 nm, which provides the best surface resolution and image quality for both methods, we obtained the size dependences of the fractal dimension on film thickness. We have described the formation of fractal relief depending on the location of the studied region on the film surface using both methods: varying the film thickness and selecting specific, statistically identical regions of the nickel film. The non-linear change in the fractal dimension for nickel films with increasing thickness can be explained by two parallel processes: the formation of a «new» fractal relief and the degradation of the «formed» fractal relief during the deposition process, which distinguishes this effect from some classical dimensional effects for nanoscale films, for example, the dependence of their melting temperature on thickness.
Keywords: size effect, degradation and growth, atomic force microscopy, scanning tunneling microscopy, fractal relief, nickel films.

Burtsev A.A., Bukharov D.N., Ionin V.V., Mikhalevsky V.A., Kiselev A.V., Nevzorov A.A., Eliseev N.N., Konnikova M.R., Lotin A.A.
Formation of fractal nanostructures of Ge2Sb2Te5 phase-change material by laser-induced transfer – page 21
Abstract: This work is devoted to the study of the synthesis of Ge2Sb2Te5 phase-change material nanoparticles via direct laser-induced forward transfer using sub-nanosecond pulses with durations of the order of hundreds of picoseconds. Thin Ge2Sb2Te5 films deposited by thermal vacuum evaporation onto silicon substrates were used as the initial targets. It is shown that the temperature regime, governed by the high melting temperature of the crystalline Ge2Sb2Te5 phases (approximately 600 °C) and their ability to rapidly recrystallize, plays a key role in determining the efficiency of the cluster formation and morphology of the resulting aggregates. These factors create specific conditions for nucleation and growth of particles from the molten material. A detailed morphological analysis of the synthesized nanoparticles and their aggregates was performed using scanning electron microscopy. It was found that depending on the laser pulse fluence and the initial film thickness, structures of varying complexity can be formed, ranging from isolated spherical particles to highly branched dendritic clusters. To quantitatively describe the aggregation processes, the diffusion-limited aggregation model was employed, which explains the observed morphological features in terms of random walks of particles in the gas phase and their subsequent adhesion to the substrate. It is demonstrated that by varying the experimental parameters (pulse energy and duration, film thickness, and target-to-substrate distance), clusters with tailored morphology and, consequently, controllable optical and electrical properties can be synthesized. This opens up the possibility of creating switchable elements based on Ge2Sb2Te5 nanoparticles with predictable characteristics, which could potentially replace conventional thin-film devices in a number of applications. The fractal dimension of the aggregates is identified as a key parameter correlating with their functional properties and can serve as a criterion for evaluating their performance.
Keywords: chalcogenides, phase change materials, nanoparticles, clustering, laser-induced transfer, fractal dimension.

Volodko S.S., Markova G.V., Kasimtsev A.V., Permyakova D.V., Gusev A.D.
Formation of the porous structure of the NiTi intermetallic compound during vacuum sintering of mechanically milled powder – page 31
Abstract: A study explores the feasibility of controlling the morphology and pore size of a NiTi intermetallic compound by mechanical processing the starting powder. The powder was pre-hydrogenated to induce embrittlement, processed in a planetary mill, and then vacuum sintered. It was found that intense shrinkage of the starting powder begins at temperatures of approximately 0,9 melting temperature, significantly narrowing the temperature range for porosity control. Mechanical processing reduces the average particle size from approximately 90 to 10 μm, while maintaining the powder’s phase composition and not significantly increasing crystal lattice microstrain. The use of milled powder promotes the formation of smaller, more uniformly distributed pores and enhances sintering compared to the starting powder. With comparable overall porosity, the specific length of pore-matrix boundaries increases by almost an order of magnitude for the milled powder. These results demonstrate the feasibility of controlling geometric characteristics of the NiTi pore space by varying the dispersion of the starting powder without the use of some additional pore-forming agents. The proposed approach can be used in the development of porous functional materials for which a developed pore-matrix interface and controlled pore morphology are essential.
Keywords: NiTi, porous materials, pore structure, mechanical milling, planetary mill, vacuum sintering.

Zezyanov I.T., Solnyshkin A.V., Sergeeva O.N., Sharofidinov Sh.Sh., Pronin I.P., Sharenkova N.V., Kaptelov E.Yu.., Staritsyn M.V.
Dielectric response in thin-film heterostructures with AlGaN nanolayers – page 44
Abstract: AlGaN-based heterostructures are functional materials for various applications in microelectronics and optics, owing to the preservation of their thermal and electrical properties over a wide temperature range. In this study, AlxGa1-xN thin-film multilayer structures were grown on SiC/Si substrates using hydride vapour phase epitaxy. Their microstructural characteristics were investigated using X-ray diffraction, phase analysis, and scanning electron microscopy. Microstructural analysis reveals that the thin-film structures under investigation are complex compounds containing AlGaN nanolayers of different composition. An analysis of the formation processes of the interlayers within the periodic AlGaN structure indicates that this structure results from the compositional self-organization and formation of a complex composite material. Studies of the dielectric response of AlGaN-based films have revealed that composites incorporating a multilayer structure exhibit dielectric permittivity dispersion; the magnitude of the permittivity increases significantly – particularly in the low-frequency range – due to enhanced ohmic conductivity. The complex behaviour of the dielectric loss tangent and the capacitance-voltage characteristics corroborates the conclusion that structures containing AlGaN layers possess significant electrical conductivity. In the high-frequency range, this dielectric response can be attributed to a space-charge polarization arising at the boundaries between AlGaN layers of different compositions, as well as at the AlGaN/SiC interface.
Keywords: silicon carbide-on-silicon substrates, chloride-hydride epitaxy, epitaxial AlGaN layers, dielectric permittivity dispersion, capacitance-voltage characteristics.

Kanametova O.Kh., Dyshekova F.F.
The influence of small additives of lithium on the surface tension of alloys based on bismuth – page 54
Abstract: The paper presents the results of an experimental study of the temperature and concentration dependences of the surface tension of bismuth and its alloys with small additives of lithium in a composition range containing up to 0,44 at.% Li. Surface tension measurements were carried out by the large drop method using an automated experimental setup and the «SigmaDrop» hardware and software complex in the temperature range of 570-700 K; the error was of approximately 2,5%. A specially developed solid-soldered measuring cell ensured identical alloy preparation conditions and reliable thermodynamic equilibrium of the surface of each alloy with its own saturated vapor. Our study demonstrated that the temperature dependence of the surface tension of all liquid alloys is strictly linear. The concentration dependence of the surface tension at a temperature of 600 K was plotted as a monotonic curve. Based on the obtained isotherms, it was concluded that lithium is a weak surface-inactive additive in the studied composition range. The obtained results are in agreement with the criteria for the surface activity of components in binary alloys, as well as with the literature data on the activity coefficient of lithium, which maintains a constant value in the concentration range of compositions with a low lithium content in melts with bismuth.
Keywords: lithium, bismuth, alloys, surface tension, large drop method.

Malyshkina O.V., Petrov R.A., Malysheva N.E.
Effects of calcium ions on the relaxation processes in ceramics based on barium titanate – page 62
Abstract: Comparative studies of experimental and calculated dielectric responses of barium-calcium titanate ceramic samples with different Ba/Ca. ratios based on a mathematical model were conducted. Based on mathematical modeling, it has been shown that for Ba1-xCaxTiO3 samples with a calcium concentration of x < 0,25, there are only two relaxation processes: high-frequency (with the most probable relaxation time of ~ 10-8s), corresponding to the thermal ionic polarization, and low-frequency (with the most probable relaxation time of ~ 1 s), corresponding to the migration polarization. The presence of individual grains of calcium titanate in the sample, which occurs at x > 0,25, leads to an increase in the number of low-frequency relaxation processes, as evidenced by the presence of not one, but several most probable relaxation times (with values from 10–2 to 1 s). Analysis using mathematical modeling revealed the absence of a contribution to the dielectric response of barium titanate-based ceramics from the low-frequency conductivity, which is present in sodium niobate-based ceramics, despite the fact that both materials have a perovskite-type structure.
Keywords: piezoelectric ceramics, lead-free materials, barium titanate ceramics, calcium titanate, dispersion of complex permittivity, relaxation processes, resonant polarization.

Misochenko A.A., Korolkov O.E.
Thermal phenomena induced by pulsed current in titanium during tensile deformation – page 72
Abstract: The study analyzes the thermal effect of pulsed current during tensile testing in Grade 2 and Grade 4 titanium in coarse‑grained and ultrafine‑grained states. The work demonstrates the determining role of the current duty cycle in the manifestation of electroplastic and thermal effects. It is shown that in the single‑pulse mode (duty cycle 5000-10000), there is a correspondence between the onset of the temperature peak and the yield stress jump. In the multi‑pulse current mode (duty cycle 10), the maximum temperatures increase linearly with increasing current density above 40 A/mm2 and can reach approximately 170°C at a current density of 100 A/mm2. When the duty cycle is below 5000, thermal effects become the dominant mechanisms. The results of comparing the electroplastic effect manifestation in coarse‑grained and ultrafine‑grained Grade 4 titanium are presented, demonstrating the structural sensitivity of the effect to grain size. A comparison was made of the reduction in the flow stress under the influence of current versus heating by an external source, demonstrating the presence of other contributions to the electroplastic effect besides the thermal one. At the same time, the thermal contribution of the current to the reduction of the flow stress in ultrafine‑grained titanium is smaller than in coarse‑grained titanium.
Keywords: electroplastic effect, tension, pulsed current, titanium, thermal effect of pulsed current.

Mustafayev G.A., Cherkesova N.V., Mustafayev A.G.
Charge transfer effects in Me-Al2O3-SiO2-Si structures – page 82
Abstract: The aim of the work is to experimentally study the effects of charge transfer and flat-band voltage shift in metal-Al2O3-SiO2-Si structures under high-temperature treatment and applied bias. It was found that a negative bias resulted in the formation of an «instantaneous» polarization component of the shift, while a positive bias additionally produced a thermally activated «slow» component with a delay time of ~10 min at 125°C. The dependence of the shift on applied voltage at 190°C is linear. It was determined that charge transfer from the metal-Al2O3 interface to the Si-SiO2 interface was caused by the thermal release of carriers from bulk traps with an activation energy of 1,2 eV. A correlation was found between aluminum oxide thickness and the stability of the structure’s parameters, with the minimum mobile charge density observed at a layer thickness of 70 nm. Practical significance is as follows: optimizing the Al2O3 layer thickness to 70 nm ensures maximum stability of the electrical characteristics of metal-insulator-semiconductor structures under combined thermal and electrical loads. The obtained patterns and physical model of charge transport can be used in the technological design of reliable microelectronic devices.
Keywords: metal-insulator-semiconductor-structures, flat-band voltage, capacitance-voltage characteristics, high-temperature processing, multilayer dielectric, charge traps, stability of parameters.

Nevzorov A.A., Mikhalevsky V.A., Burtsev A.A., Ionin V.V., Kiselev A.V., Eliseev N.N., Lotin A.A.
Temperature dependence of the ellipsometric parameters of thin films of the AIST phase-change chalcogenide – page 94
Abstract: This work is devoted to the study of the temperature dependences of the refractive index (n) and extinction coefficient (k) of thin films of the phase-change chalcogenide AIST (Ag5In5Sb60Te30) in the spectral range of 380-1000 nm. Using spectroscopic ellipsometry, a direct comparison of optical properties of the amorphous and crystalline phases was performed during heating from room temperature to 170°C. It was found that heating the amorphous film to 100°C leads to a decrease in n by 3,2% and an increase in k by 2,55% at a wavelength of 780 nm, as well as a decrease in n by 5,0% and a decrease in k by 4,2% at a wavelength of 910 nm. The observed behavior indicates a notable instability of both the amorphous and crystalline phases of the investigated AIST material. The quantitative data obtained provide a necessary experimental basis for accurate thermal and optical modeling of phase-change memory devices operating in the near-infrared range. The effective application of this material requires optimization and control of synthesis methods, thin-film properties, and the precise kinetics of phase transformations. Nevertheless, AIST can be recommended for applications where high switching speed is a priority, rather than requirements for stability and multilevel state storage.
Keywords: chalcogenides, phase change materials, thin films, crystallization, optical properties.

Ostroushko A.A., Permyakova A.E., Zhulanova T.Yu.
Dependence of sintering parameters for nanosized complex oxide powders on intensity of charge generation during synthesis from nitrate-organic precursors – page 102
Abstract: Parameters of the sintering process for compacted complex oxide powders based on lanthanum strontium manganite with a perovskite-type structure were studied: the temperature of intensive sintering and the achieved shrinkage of the workpiece. The studied complex oxide samples were obtained in the combustion reactions of nitrate-organic precursors (the so-called solution combustion method). During the synthesis, the composition of the precursors was varied: the nature of the organic component (polyvinyl alcohol, polyvinylpyrrolidone, glycine) and its relative content in relation to the stoichiometry of the combustion reaction with the formation of water vapor, molecular nitrogen and carbon dioxide as gaseous products. At the same time, positive or negative electric charges were generated in the precursors due to the formation and carry-over with the released gases of ionized molecular groups. The intensity of this process was monitored using an electrostatic field meter. The ground-precursor potential difference, depending on the composition of the initial composition, ranged from values close to zero to several tens of volts. With intensive generation due to the accumulation of the excess surface energy of mutually repulsive nanoparticles of the complex oxide, the temperature of intensive sintering decreased by 350 degrees compared to that (1050°C) for materials obtained from precursors with a low intensity of charge formation. The relative shrinkage of samples of the first type increased from 3 to 23%. The established correlation was universal and practically independent of the sign of the generated charge.
Keywords: nanosized powders, synthesis of nitrate-organic precursors in combustion reactions, charge generation, sintering, complex oxides, lanthanum-strontium manganite.

Pavlenko D.S., Bulanova A.L., Pavlenko A.V.
Dielectric properties of Pt/0,91NaNbO3-0,09SrZrO3/SrRuO3/MgO(001) antiferroelectric thin films – page 112
Abstract: In this work, 0,91NaNbO3-0,09SrZrO3 (NZNO-0,09) thin films were grown on SrRuO3/MgO(001) substrates using the high-frequency magnetron sputtering method in an O2 atmosphere. A comprehensive study of their crystal structure, dielectric response, and polarization characteristics was carried out using X-ray diffraction analysis, dielectric spectroscopy, and measurements of dielectric hysteresis loops. It was established that the obtained films are single-phase, impurity-free, and at room temperature they exist in the antiferroelectric phase. At the same time, in contrast to ceramics of the same composition, they exhibit relaxor behavior in terms of the temperature–frequency dependence of the relative permittivity ε and dielectric loss tangent tg δ. Analysis of the dispersion of ε and tan δ in the temperature range T = 305-460 K and frequency range f = 0,2-500 kHz revealed the presence of contributions from two relaxation processes associated with different polarization mechanisms. A model describing the observed spectra is proposed. The paper discusses the origins of the observed features in the formation of dielectric properties, as well as the high energy efficiency of the NZNO-0,09 films. The obtained results are important for understanding the mechanisms governing the property formation in antiferroelectric nanoscale thin films in view of their application in modern functional electronics.
Keywords: antiferroelectric, dielectric properties, thin films, polarization, high-frequency magnetron sputtering method.

Pustovoit V.N., Dolgachev Yu.V.
Ferromagnetic nanoclusters in austenite: nature, role, characteristics, and controllability – page 122
Abstract: This article examines the nature of magnetic inhomogeneities in austenite steels and their fundamental role in phase transformations. It is shown that austenite, being a paramagnetic phase, contains spontaneously emerging regions of short-range ferromagnetic order (ferromagnetic nanoclusters), the existence of which has been confirmed experimentally using neutron magnetic diffraction methods. The dependence of the magnetic susceptibility of austenite is described by the Langevin function for superparamagnets, which reflects the fluctuation nature of these magnetic inhomogeneities localized in nanometer-sized regions. The magnetic state of the initial phase crucially determines the nature of the γ→α transformation. Using computer simulation based on the Ising model, the effect of an external magnetic field on the characteristics of nanoclusters over a wide temperature range was studied. It has been established that a magnetic field of up to 2,4 MA/m can increase the average cluster size, their total number by two orders of magnitude (most effectively at low temperatures, where the increase reaches 1,4 nm), and increase the proportion of large clusters, as well as extend their stable existence by up to 25%. Experiments with quenching in a constant magnetic field for a range of steels demonstrated a significant reduction in the volume fraction of retained austenite, comparable to cold treatment, and an acceleration of the bainitic transformation kinetics by 1,5-1,8 times. The magnetic field enhances the magnetic heterogeneity of austenite, activates new nucleation centers, and stimulates the multiplicative mechanism of α-phase formation, providing a practical tool for targeted phase transition control during heat treatment of steels in a magnetic field.
Keywords: austenite, magnetic state, nanocluster, steel, hardening, external magnetic field.

Senkevich S.V., Pronin V.P., Ryzhov I.V., Staritsyn M.V., Dunkabash A.R., Kaptelov E.Yu., Pronin I.P.
Imprint effect in spherulitic lead zirconate titanate thin films – page 133
Abstract: We investigated the microstructure and imprint (internal field) of spherulitic lead zirconate titanate thin films formed via a two-stage radio frequency magnetron sputtering process on Pt/TiO2/SiO2/Si substrates at various perovskite phase crystallization temperatures (Tann = 580–650°C). The films were subjected to a thermal treatment and application of a strong external field, and prolonged aging. Microstructural analysis using scanning electron microscopy revealed that increasing Tann led to a sharp increase (by a factor of 5-10) in the crystal lattice rotation rate; this effect is attributed to the recrystallization of the perovskite phase, accompanied by an increase in its density. It was found that the magnitude and orientation of the internal field in the films, determined from dielectric hysteresis loops, depended on the «phase» state of the films. Long-term aging (~ 108 s) had little effect on the internal field in the loose phase. In the dense phase, aging led to a significant change in the magnitude and direction of the internal field vector. The observed changes are attributed to strong bending deformation of the crystal lattice and the resulting directed diffusion of charged oxygen vacancies toward the upper film interface. The study discusses the role of the electronic subsystem and charged oxygen vacancies in the formation of the imprint (internal field) and in charge redistribution across the film thickness under the influence of external factors and the passage of time.
Keywords: radio frequency magnetron sputtering, lead zirconate titanate thin films, spherulitic microstructure, oxygen vacancies, Gorsky effect.

Surkov I.A., Pasechnik L.A., Gyrdasova O.I.
Synthesis and physico-mechanical characteristics of functional Er2O3/ScSZ ceramics – page 144
Abstract: Solid solutions of the Er2O3/ScSZ system were synthesized by a sol-gel method using ethylene glycol as an organic component, which ensures high homogeneity of dopant distribution in the ZrO2 matrix. Thermolysis of the intermediate sol in air at 700 °C leads to the formation of Zr0,8Sc0,2-xErxO2 (x = 0-0,04) compositions based on the tetragonal t–ZrO2 phase. Ceramic samples with a relative density of 96-98% were obtained at 1500°C. According to X‑ray diffraction data, in the range x = 0-0,01 the sintered ceramics consist of a mixture of cubic (c–ZrO2) and rhombohedral (r–ZrO2) phases, whereas at x = 0,02-0,04 a single‑phase cubic structure is formed. Scanning electron microscopy reveals a well‑sintered microstructure with grains closely adhering to each other; pores are closed and have submicron dimensions. The microhardness ranges from 12,3 to 15,6 GPa, which is comparable to that of conventional technical ceramics based on ZrO2. Co-doping with erbium almost doubles the flexural strength, raising it from 81,2 MPa (undoped ScSZ) to 150,2 MPa for the composition Zr0,8Sc0,19Er0,01O2. This value exceeds the typical strength of unstabilized ZrO2 ceramics and demonstrates a pronounced strengthening effect of erbium. The observed strengthening is attributed to the transformation toughening mechanism, as well as to reduced porosity and microstructural optimization achieved through the sol‑gel synthesis. To ensure stability of thermomechanical and thermoelectric characteristics under long‑term and cyclic operating conditions, a co-doping level of 2-3 mol.% Er (x = 0,02-0,03) is preferable, which yields a single‑phase c–ZrO2 structure that prevents unwanted phase transitions in the working temperature range. Such doping provides the best combination of strength (~154 MPa) and microhardness (~14,5-15,0 GPa), thereby reducing the risk of property degradation. Thus, the developed Er2O3/ScSZ materials represent a promising alternative to conventional electrolytes for solid oxide fuel cells, offering high density, mechanical strength, and phase stability.
Keywords: scandium stabilized zirconium oxide, co-doping, erbium oxide, sol-gel synthesis, microhardness, bending strength.

Teplyakova N.A., Masloboeva S.M., Biryukova I.V.
Influence of the doping method on optical properties of LiNbO3:Y single crystals – page 155
Abstract: Using different doping methods (homogeneous and solid-phase) and the Czochralski method, LiNbO3:Y crystals with an yttrium concentration of 0,46 wt.% were grown. Optimal technological conditions for growing LiNbO3:Y crystals have been determined, including both the growth parameters and the melt preparation conditions. The optical and photorefractive properties of the obtained LiNbO3:Y single crystals have been studied using laser conoscopy and photoinduced light scattering methods. Comparative analysis of two LiNbO3:Y crystals showed a significant difference in their optical properties. In the LiNbO3:Y crystal grown from the homogeneous doping charge, the photorefractive effect is absent; in the LiNbO3:Y crystal grown from the solid-phase doping charge, a photorefractive response is present, and an almost instantaneous opening of the photoinduced light scattering indicatrix is observed. In addition, the homogeneously doped LiNbO3:Y crystal has a significantly higher optical homogeneity compared to the solid-phase doped LiNbO3:Y crystal. The obtained results indicate that the developed technological scheme for obtaining a single-phase lithium niobate charge doped with yttrium by the homogeneous doping method creates conditions for the growth of optically and compositionally homogeneous LiNbO3:Y single crystals, which are promising for use in electronic engineering as a nonlinear optical material with a low photorefraction effect.
Keywords: lithium niobate, single crystal, charge, homogeneous and direct doping, laser conoscopy, photoinduced light scattering.

Teplyakova N.A.
Processes of structural disordering in the solid solution Li0,015Na0,985Ta0,1Nb0,9O3 – page 164
Abstract: Temperature-induced changes in the Raman spectra of the Li0,015Na0,985Ta0,1Nb0,9O3 solid solution have been studied in the low-frequency region. This region encompasses the fully symmetric librations of the oxygen octahedra as a whole, vibrations of the Li and Na cations in the cuboctahedral voids, and vibrations of the Nb and Ta cations in the octahedral voids in the temperature range of 22-400°C. As the temperature increases, a significant broadening of the Raman spectrum bands appears. This indicates disordering of the solid solution structure. However, a “softening” (decrease in frequency) of the band in the 50-80 cm-1 region corresponding to the totally symmetric librations of the oxygen octahedra as a whole is also observed. This fact indicates a misorientation in the structure of the Li0,015Na0,985Ta0,1Nb0,9O3 solid solution of oxygen octahedra, while the possibilities for transport of Li ions at high temperatures increase. A predominant broadening (compared to other spectral bands) and a decrease in band intensity have been detected In the 110-160 cm-1 range. These bands correspond to vibrations of Na+ and Li+ cations in Li/NaO12 polyhedra. This indicates “melting” of the alkali metal sublattice. Such behavior of the Raman spectrum bands indicates the existence of a phase transition to a state with superionic conductivity in the studied Li0,015Na0,985Ta0,1Nb0,9O3 solid solutions.
Keywords: ceramic solid solutions; phase transition; superionic conductivity; Raman scattering.

Tonkushina M.O., Gagarin I.D., Sharadgah B.T.M.A.., Ostroushko A.A.
Formation of supramolecular particles of polyoxometalate {Mo72Fe30}-doxorubicin-biocompatible polymer: interaction of components and properties – page 171
Abstract: Polyoxometalate nanoclusters are capable of interacting with various compounds and forming multicomponent supramolecular systems. Fine-tuning the properties of such a system, based on the tasks of future practical application, can be carried out by selecting its components. In this work, three-component supramolecular systems of polyoxometalate {Mo72Fe30}-doxorubicin-biocompatible polymer, which form without the involvement of additional crosslinking reagents, were investigated. It was found that upon interaction with polyethylene glycol, the {Mo72Fe30}(doxorubicin)12 complex forms hydrogen bonds with the ether oxygen and terminal groups of the polymer, whereas in {Mo72Fe30}(doxorubicin)12-polyvinylpyrrolidone system, the nitrogen in the lactam ring of the polymer is electrostatically attracted to the negatively charged surface of the polyoxometalate. The presence of polymers does not affect the release rate of doxorubicin from the {Mo72Fe30}(doxorubicin)12 complex in a solution at pH 7,4 (blood pH). The difference in the nature of interaction of the two polymers with the polyoxometalate is manifested in the sizes of the particles formed in solution; specifically, in the system with polyethylene glycol, the particle size distribution did not differ from that of the solution in the absence of the polymer (average size 22 nm), whereas in the system with polyvinylpyrrolidone, a broad particle size distribution ranging from 30 nanometers to several micrometers was observed.
Keywords: {Mo72Fe30}, doxorubicin, polyethylene glycol, polyvinylpyrrolidone, particle size, supramolecular systems.

Torianik S.V., Ilina T.S., Skryleva E.A., Senatulin B.R., Voronova M.I., Pavlenko A.V., Kiselev D.A., Parkhomenko Yu.N.
The effect of NiO doping on the phase composition and ferroelectric properties of lead-free ceramics based on sodium and potassium niobate – page 185
Abstract: The development of lead-free piezoelectric materials capable of replacing toxic lead zirconate titanate is a priority in modern materials science due to stricter environmental regulations and growing demand for environmentally friendly high-temperature transducers. Potassium sodium niobate based ceramics offer potential as promising candidates due to their high Curie temperature; however, their practical application is limited by the difficulty of obtaining dense samples and insufficiently high electrophysical characteristics, which makes it relevant to study the influence of both substitutions in the A- and B-positions of the perovskite structure (ABO3) and additives that can improve sinterability and modify local ferroelectric properties. In this work, three compositions 0,94(Na0,54K0,46)(Nb0,9Ta0,1)O3 – 0,06LiSbO3 – xNiO (KNNT‑LS‑xNiO), where x = 0, 0,01 and 0,02, were investigated. A comprehensive characterization of the samples was carried out using complementary methods – X-ray phase analysis with Rietveld structure refinement, X-ray photoelectron spectroscopy, atomic force microscopy and piezoresponse force microscopy. It was established that in samples with x = 0 and x = 0,01 nonpolar secondary phases are present, whereas at x = 0,02 these phases are completely suppressed and coexistence of polar phases P1m1 and P4mm is observed. The highest content of ferroactive phases and the maximum relaxation time of the induced domain structure were recorded for the sample with the highest NiO content, which indicates a significant increase in the stability of residual polarization upon optimal doping. The obtained results demonstrate that a targeted combination of substitutions in the crystal lattice and NiO additive makes it possible to control the phase composition and relaxation functions of the induced domain structure, opening the way to the creation of lead-free ceramics with improved and reproducible ferroelectric phenomena.
Keywords: potassium-sodium niobate, lead-free ceramics, atomic force microscopy, X-ray photoelectron spectroscopy, X-ray phase analysis.

Yudin S.N., Kasimtsev A.V., Volodko S.S., Moskovskikh D.O.
Features of zirconium carbonitride formation under multistage reduction-carburization-nitridation of ZrO2 – page 197
Abstract: The nitridation of products obtained by calcium hydride reduction–carburization of ZrO2 at 1200°C was studied with the aim of synthesizing zirconium carbonitride ZrCxN1-x. The effect of nitriding duration (ranging from 1 to 12 hours) in a stationary nitrogen atmosphere at a pressure of 1,1 atm on the elemental and phase composition of the powders was investigated. Increasing the holding time did not result in a systematic increase in nitrogen content: the carbon and nitrogen concentrations were of approximately 40 and 6–8 at.%, respectively (C/N ≈ 5,5). X-ray diffraction analysis showed that, regardless of the nitridation time, a B1-type phase with the lattice parameter of 0,4691 nm was formed, corresponding to nearly pure ZrC. Energy-dispersive X-ray spectroscopy analysis indicated a local enrichment in nitrogen, predominantly at the protruding regions of the carbide particles. It was shown that at 1200°C nitridation of ZrC proceeds only to a limited extent and does not result in the formation of a homogeneous ZrCxN1-x carbonitride phase. It is suggested that the incompleteness of gas-phase (N2) nitriding processes is due to the formation of solid cyanamide (CaCN2), which physically blocks nitrogen access to the ZrC surface. It is shown that the nitriding products inherit the particle morphology of the synthesized ZrC carbide and are characterized by a nanodisperse structure.
Keywords: zirconium carbonitride, zirconium carbide, calcium hydride synthesis, reduction-carburization, nitridation, ZrO2.

2. THE THEORY OF NANOSYSTEMS – page 214

Akhmatov Z.A., Akhmatov Z.A.
On the possibility of using a graphene membrane as a mass sensor – page 214
Abstract: Detection of chemical and biological molecules with high sensitivity and selectivity is crucial in various fields of science and medicine. Highly sensitive mass sensors are used for environmental monitoring, detecting trace amounts of toxic substances or explosive gases. In addition, such sensors can be used to weigh individual protein, DNA, and RNA molecules to understand the mechanisms of their interactions. An important role of mass sensors is in monitoring the growth of thin films, nanowires, and fullerenes, where precision must be at the atomic level. With the development of nanotechnology, a new class of sensors based on the use of graphene and carbon nanotubes has been proposed. Graphene-based sensors are expected to have ultra-high sensitivity to adsorbed atoms and molecules. In this regard, this study examines the possibility of using edge-clamped graphene membrane as an ultra-sensitive mass sensor. A molecular dynamics simulation of oscillations of a free-standing rectangular graphene membrane and a rectangular graphene membrane loaded by iron nanodroplet was performed. The added mass was determined from obtained values of the fundamental frequencies of vibrations of the free and loaded membranes. It has been shown that the use of formulas for the vibrations of a classical membrane gives a difference in mass of more than 5 times. For thin carbon membranes such as graphene, bending stiffness must be taken into account to obtain a sufficiently accurate result when determining the load mass.
Keywords: graphene membrane, mass sensor, molecular dynamics simulation, vibrational mode, bending stiffness.

Greshnyakov V.A.
Structure and properties of a novel hexagonal C108 clathrate – page 223
Abstract: The structure and properties of a new clathrate variety of carbon (C108) have been studied for the first time using density functional theory with a generalized gradient approximation. The new nanostructured phase has a hexagonal crystal lattice belonging to the P6m2 space group, with parameters a = 6,813 Å and c = 18,07 Å, which can be considered intermediate between the lattices of type II carbon clathrate and the hexagonal C40 clathrate. The structure of the C108 clathrate consists of fullerene-like blocks C20, C24, C26, and C28, due to which its density is 13,8% lower than that of diamond. Since the total energy of the new clathrate is only 0,10 eV/atom higher than that of diamond, the proposed phase should stably exist under normal conditions. The hexagonal C108 clathrate is expected to be a wide-bandgap semiconductor with high mechanical properties: a bulk modulus of 384 GPa, the Young’s modulus of ~880-890 GPa, and a Vickers hardness of 81 GPa. It has also been established that the structure of the C108 clathrate should be stable under strong hydrostatic compression at least up to 70 GPa. Identification of the new phase is possible using X-ray diffraction methods.
Keywords: nanostructured compounds, carbon clathrate, mechanical properties, stability, first-principles calculations.

Grigoriev A.D., Boroznin S.V., Zaporotskova I.V.
Carbon nanotubes with impurity nitrogen atoms as promising filters for harmful gases – page 233
Abstract: Carbon nanotubes modified with nitrogen atoms are one of the promising materials for the development of electronic devices in the modern world. They are characterized by the presence of structural distortions and increased nucleophilicity, which significantly distinguishes them from primitive graphene structures. These facilities exhibit abnormally high stability in aggressive environments and low overvoltage. Their uniqueness lies in the synergy of the mechanical strength of the carbon backbone and the chemical activity of nitrogen-containing centers, which makes it possible to solve the problems of creating effective sorbents and heterogeneous catalysts. To study the interaction of nanotubes with harmful gases and obtain the energy characteristics of adsorption, some semi-empirical calculations using the Gaussian software package were used in the framework of the density functional theory using the B3LYP method with a 6-31G baseline set. The nanotube model was built using GaussView 6.0. Every second carbon atom of the nanotube was replaced by a nitrogen atom. To obtain the adsorption energy, the gas molecule approached the surface of the nanotube perpendicular to the axis of the nanotube with 0,2 nm increments. The energy was calculated at each step, which made it possible to build profiles of the potential energy of interaction of chlorine, fluorine and carbon dioxide. During the theoretical experiment, interaction energies were obtained for each step of the approach of Cl, F, and CO2. Based on the results, the potential energy interaction curves were constructed, which made it possible to determine the most effective distance for the sorption of harmful gases onto the surface of a carbon nanotube modified with nitrogen atoms. Sorption occurs at various distances. For chlorine, it is 1,4-1,8 Å, and for fluorine and carbon dioxide, it is 2-3 angstroms. The interaction graphs clearly demonstrate the possibility of sorption of hazardous gases by the nanocomposite. Fluorine forms a stable chemical bond with the carbon atom of the nanotube, while chlorine is physically sorbed onto the nitrogen atom, which indicates the high potential of the material under study for reusable filters. The experiments conducted demonstrate the possibility of using carbon nanotubes with substituting nitrogen atoms as filters. The assessment of the energy properties shows a high potential for application in microelectronic technology.
Keywords: carbon-nitrogen nanotubes, filters, density functional theory, gas adsorption, harmful gases.

Devitsky O.V.
Problems and strategies of epitaxial growth of III-V-Bi semiconductor thin films: a review – page 244
Abstract: This review article systematically summarizes fundamental and applied research concerning the epitaxy of metastable III-V–Bi solid solutions. The main challenge in obtaining thin films of III-V–Bi is their thermodynamic instability, which results from a wide miscibility gap and extremely low equilibrium solubility of bismuth in III-V compounds. It is demonstrated that overcoming these limitations is only possible through kinetic stabilization methods. Key strategies to enhance bismuth incorporation are identified, including lowering the substrate temperature to 200-350°C, manipulating surface stoichiometry by shifting to gallium-rich regimes, and employing surface reconstructions such as the 2×1 pattern. Additional approaches involve engineering tensile strain to increase bismuth solubility by up to 100 times and using high-index substrates like (115)A and (311)B, along with congruent transfer techniques. The paper also thoroughly discusses strategies for improving structural quality, such as suppressing bismuth droplet formation, implementing two-temperature growth procedures, and performing in-situ and post-growth annealing. A comparative analysis of molecular beam epitaxy, metal-organic vapor phase epitaxy, and pulsed laser deposition methods is presented within the context of producing high-quality III-V–Bi thin films. The review concludes that further progress in developing devices based on III-V–Bi requires shifting from empirical process optimization to precise control of surface kinetics and atomic-level defect management.
Keywords: GaAsBi, thin films, III-V-Bi, molecular beam epitaxy, metal-organic vapor phase epitaxy, pulsed laser deposition.

Magomedov R.A., Akhmedov E.N.
Calculation of P-ρ-T properties of noble gases using the fractal state equation in the temperature range from 500 to 3000 K – page 256
Abstract: This paper presents a calculation of the state equation isotherms for noble gases: neon, argon, krypton, and xenon in the temperature range from 500 to 3000 K. The calculation was performed using a mathematical model based on a fractal state equation, which has previously demonstrated high efficiency in calculating the P-ρ-T properties of other substances. The obtained results are in good agreement with literature reference data. The dependence of the fitting parameter α of the fractal state equation on density is determined for various temperatures. It is found that for neon, krypton, and xenon, the density dependence is small, but the temperature dependence is noticeable. For argon, the opposite is true: the density dependence is more pronounced, and the temperature dependence is almost absent. To evaluate the effectiveness of the fractal state equation, a comparative analysis of the calculation accuracy is performed and compared to the classical equation of state of a real gas. It is shown that the accuracy of the classical equation decreases with increasing pressure. The fractal equation has high calculation accuracy over the entire studied range of temperatures and pressures.
Keywords: mathematical modeling, fractal equation of state, thermophysical properties of inert gases, neon, argon, krypton, xenon, fractional integro-differentiation, software calculation module.

Malashenko V.V.
The effect of irradiation on the dynamic instability of dislocation slip in metals – page 264
Abstract: Within the framework of the theory of dynamic interaction of defects, the above-barrier motion of edge dislocations in an irradiated metal containing radiation point and nanoscale defects (prismatic dislocation loops) is analyzed. Intense external loads generate high strain rate deformation of irradiated metals. During high strain rate deformation, dislocations accelerate to high velocities, and their kinetic energy exceeds the height of potential barriers generated by structural defects. During above-barrier motion of dislocations, the energy of external loads is converted into the energy of dislocation oscillations. This dissipation mechanism differs significantly from the dissipation mechanism in the low-velocity region. The presence of a gap in the dislocation oscillation spectrum significantly affects the efficiency of this mechanism. This paper considers the case where the gap is generated by the collective interaction of radiation point defects. An analytical expression defining the rate dependence of the dynamic yield strength in irradiated metal is obtained. A new region of dynamic instability of dislocation motion was predicted, caused by a high concentration of prismatic dislocation loops. This dynamic instability is the cause of plastic deformation jumps. Some analytical expressions defining the boundaries of the dynamic instability region are obtained, and numerical estimates of the boundary values are performed.
Keywords: irradiated metals, dislocations, dislocation loops, radiation defects, high-speed deformation.

Mitinev E.S., Savina K.G., Polev O.V., Gostintsev M.G., Kolosov A.Yu., Sokolov D.N., Vzglyadov I.A., Dmitriev I.S., Ershov P.M., Sdobnyakov N.Yu.
Can the presence of a cavity alter the nature of structural transformations during a cycle of thermally induced treatment, taking Ag-Ni-Pd ternary nanoparticles as an example? – page 271
Abstract: A comparative molecular dynamics study was conducted on equiatomic Ag-Ni-Pd ternary nanoparticles with two types of initial configurations: a nanoparticle containing a central cavity and a nanoparticle without a hollow core. A cycle of thermally induced treatment (heating and cooling) was performed at a rate of 0,3 K/ps. Specific features of the structural behavior of these objects during heating and subsequent melting were identified. In particular, the fraction of atoms forming a local hcp structure is significantly higher for the nanoparticle with a hollow core in the temperature range from 660 K up to the melting point. The temperature dependencies of specific internal energy during cooling are virtually identical for the two initial configurations; however, the process of nickel core formation exhibits distinct characteristics regarding the number of nucleated clusters and their subsequent internal coalescence. Furthermore, polyhedral template matching analysis reveals differences between the two initial configurations regarding the formation of local fcc and hcp environments by the constituent elements (Ag, Ni, Pd) of the ternary alloy at the end of the thermal cycle (at 300 K). Thus, the presence of an artificially created cavity or bulk defect in equiatomic Ag-Ni-Pd ternary nanoparticles influences not only the parameters of phase transitions associated with melting and crystallization but, to a greater extent, the patterns of chemical and structural segregation.
Keywords: molecular dynamics method, MDSym, tight-binding potential, ternary nanoparticles, cavity, phase transition, segregation, local structure.

Tvardovskiy A.V.
Equation of polymolecular adsorption on a flat homogeneous surface of an adsorbent for a finite number of layers – page 282
Abstract: To date, a large number of different adsorption and absorption equations have been proposed, describing a variety of equilibrium situations on homogeneous and inhomogeneous surfaces of adsorbents as well as polymers, micro-, meso- and macroporous adsorbents. However, the most valuable works are those in which attempts are made to build a general theory of adsorption (and absorption). At least the well-known classical adsorption equations should follow from such a general equation as special cases. Such an equation was previously proposed, and it was shown that the classical Henry, Langmuir, and Brunauer – Emmett – Teller equations with constants having a clear physical meaning follow from the general equation as special cases. Thus, the constant in the Henry equation is determined by the temperature as well as by the specific surface of the adsorbent, the size of the adsorbate molecules, the molar mass of the adsorbate, and the isosteric heat of adsorption (the energy of interaction of the adsorbate molecules with the surface of the adsorbent). In the derived Brunauer – Emmett – Teller partial equation, in contrast to its classical version, a clear dependence of the equation constant on the specific physical characteristics of the adsorption system is provided for the first time. The dependence in question is determined by the concentration of adsorbate molecules in the liquid phase at the temperature under consideration, the concentration of adsorbate molecules during the formation of a dense monolayer on the surface of the adsorbent, and by the energy of interaction of adsorbate molecules with the surface of the adsorbent and the heat of condensation. The presented approach can serve as a basis for modeling a variety of adsorption and absorption phenomena, including adsorption on microporous and deformable adsorbents. In this paper, based on previous investigation, the equation of polymolecular adsorption on a flat homogeneous surface for a limited number of layers is derived.
Keywords: adsorption, adsorbent, absorption, thermodynamics of phase equilibria, Henry equation, Langmuir equation, Brunauer – Emmett – Teller equation, equation of polymolecular adsorption, flat homogeneous surface.

Shebzukhova I.G., Aref`eva L.P.
Modeling the thermal effect on the surface energy and electron work function of a monocrystal thallium – page 289
Abstract: The aim of this work was to carry out numerical modeling of thermal influence on energy and force characteristics of monocrystal thallium. The surface energies and work function of faces of thallium crystals are calculated using the electron-statistical method taking into account quantum corrections. The influence of polymorphic transformations and temperature on anisotropy of these properties is analyzed. The cohesive energy of α- and β- thallium has also been estimated based on the values of surface and interfacial energies, which include the average configuration energy and the energy of chemical interaction between two parts of the metal, and the temperature dependence of the chemical interaction energy has been investigated. The contact potential difference for pairs of close-packed faces has been calculated. Computer simulations of the mechanical properties have been performed using the Griffiths model, and the tensile strength of thallium has been obtained, which allows for the prediction of the material’s service life.
Keywords: surface energy, electron work function, anisotropy, polymorphic modifications of thallium, cohesive energy, crack resistance.

Shishulin A.V., Shishulina A.V.
Model of the diffusion process in a nanostructured system as a generator of pseudorandom sequences – page 296
Abstract: Complex random number generators that combine rapid pseudorandom sequence generation with hardware entropy sources have numerous practical applications in stochastic process modeling, machine learning, and information security. This paper presents a method for generating pseudorandom sequences based on a physical model of particle diffusion within a nanoscale periodic structure featuring a nonlinear potential and thermal noise, which serve as sources of dynamic chaos. The sequence of thermally activated transitions between potential minima exhibits irregular and chaotic behavior. The sequence generation is achieved through the digitalization of the particle’s stochastic motion along the energy landscape of the nanostructure. Particle diffusion in a nanostructured medium is described by the Langevin equation and is integrating by using the Verlet method. Additionally, a software implementation of the suggested algorithm is provided in the Ruby programming language. The obtained results demonstrate the potential for using a «pseudophysical» approach, which is based on nonlinear potentials of various physical natures, as a viable alternative to a «purely mathematical» methodology in the tasks involving the generation of random number sets.
Keywords: nanostructures, diffusion, nonlinear potential, dynamic chaos, pseudorandom numbers.

Shishulin A.V., Shishulina A.V.
On the energetics of vacancy formation and diffusion in mesoporous materials – page 304
Abstract: This paper examines the dependence of the vacancy formation energy and the activation energy of volume diffusion in the «skeleton» of a mesoporous material on the geometric characteristics (volume and shape) of the pores distributed within the material. The geometric features of the pores were defined within a fractal-geometric approach by their effective diameter and fractal dimension. The presented estimates indicate that the effect characteristic of nanoparticles, associated with the significant dependence of the vacancy formation energy and the activation energy of volume diffusion on the particle size and shape, can also occur in mesoporous materials (with a characteristic pore size from 5 to 50 nm), even though the mesoporous objects themselves can have macroscopic dimensions. Using porous gold as an example, it is shown that a decrease in the pore volume and a «complication» of their morphology lead to a noticeable reduction in the considered energy characteristics. The results were obtained within the framework of the cohesive energy-based model.
Keywords: vacancy formation energy, volume diffusion activation energy, mesoporous materials, fractal dimension, cohesion, size distribution, Hardy-Ramanujan-Rademacher formula.

Shishulin A.V., Vyalkova E.A., Shishulina A.V.
On the phase separation in nanoscale particle systems: the role of external environment (exemplified on W-Cr pseudo-alloy) – page 313
Abstract: Due to their unique combination of physicochemical properties, heavy tungsten-based pseudo-alloys with an ultrafine-grained structure produced from nanoparticles by advanced powder metallurgy techniques have become a subject of considerable research interest. In this work, within the framework of a thermodynamic approach, we simulate the features of the phase composition in core-shell nanoparticles formed from a phase-separating solid solution, using the heavy W-Cr pseudo-alloy as a model system. For a binary system with limited solid-state solubility, a specific effect is demonstrated: in contrast to macroscopic systems, the equilibrium composition and volume fraction of the coexisting nanophases vary significantly depending on the chemical nature of the external environment. The environment dictates the surface energy of the outer interface. The set of considered modellin dispersion media includes argon (a common sintering atmosphere), hydrogen (an annealing atmosphere), and several others. For two distinct heterogeneous states of the core-shell structure, temperature dependences of the equilibrium phase composition in each state were obtained. A thermodynamic interpretation of the observed regularities is provided, based on three possible mechanisms for reducing the free energy of the system.
Keywords: nanoparticles, solution decomposition, chemical thermodynamics, solubility, core-shell structure, tungsten, chromium.

Yanyushkina N.N.
Bessel pulses in an inhomogeneous array of carbon nanotubes under mechanical action – page 322
Abstract: In this work, the propagation of non-diffracting Bessel pulses in an inhomogeneous array of carbon nanotubes containing both metallic (armchair) and semiconducting (zigzag) tubes is numerically investigated. The relevance arises from the fact that real synthesized samples always represent a mixture of tubes of different chiralities, which significantly affects the dynamics of electromagnetic fields. Based on a model that accounts for the nonlinear response of the medium and the spatial modulation of the tube density, an evolution equation for the vector potential is solved. It is shown that Bessel pulses retain their localization over significant distances even in an inhomogeneous nanotube array and in the presence of mechanical deformations. Special attention is paid to the effect of mechanical loading (external compression or tension), which is modeled via an external stress field. It is found that varying the concentration of metallic tubes along with deformation enables effective control of the pulse shape and suppression of their spreading. The obtained results open up prospects for the development of optomechanical devices, in which mechanical loading serves as an efficient tool for controlling the parameters of the Bessel pulses.
Keywords: zigzag and armchair carbon nanotubes, Bessel pulses, mechanical deformation.

3. FIRST PRINCIPLES AND ATOMISTIC MODELING – page 332

Apekov A.M., Shebzukhova I.G., Khamukova L.A.
Dependence of the interfacial energy of molybdenum faces at the boundary with organic liquids on the dielectric constant – page 332
Abstract: The study of the interfacial energy of molybdenum at the interface with organic liquids is of considerable interest for the development of modern technologies in energy, catalysis, materials science, and biomedicine. Molybdenum, having high refractoriness, mechanical strength, and pronounced catalytic activity, is widely used in functional materials, including metal-organic skeleton structures, composites, and heterogeneous catalysts. Understanding energy characteristics at the metal-organic interface is critically important for optimizing the processes of adsorption, wetting, formation of strong interfacial contacts and control of the reactivity of active centers. In this work, calculations of the interfacial energy of molybdenum at the boundary of crystallographic faces with nonpolar organic liquids are performed using the electron statistical method. The dispersion interaction of Wigner–Seitz cells, the oscillation of the electron density in the transition layer, and the polarization of surface metal ions and organic liquid molecules in the field of a semi-infinite metal are taken into account. The dependences of the interfacial energy and corrections on the orientation of the molybdenum crystal lattice and the dielectric constant of an organic liquid are established. It is shown that the dispersion and oscillation corrections increase the interphase energy, while the polarization correction reduces it. The face (110) has the highest value of the interphase energy, and the face (111) has the lowest value of it.
Keywords: molybdenum, interfacial energy, polarization correction, dispersion correction, electron statistical method, nonpolar organic liquid.

Bolotov A.N., Novikova O.O.
Simulating the evaporation process of magnetic nanofluid to estimate the service life of magnetic fluid devices – page 340
Abstract: A generalized approach to calculating the service life of magnetic fluid tribological units operating in vacuum and gas environments is presented. The physical mechanisms of magnetic nanofluid degradation during dispersion medium evaporation and increasing solid phase concentration are examined. A statistical approach developed by Ya. I. Frenkel is used to estimate the rate of nanofluid liquid phase evaporation into a vacuum. An equation for the time dependence of the dispersed phase concentration in a magnetic fluid was obtained for calculating the durability of magnetic fluid devices in a vacuum. The dynamics of magnetic nanofluid mass loss upon contact with a gaseous medium was described using a diffusion mass transfer equation. An electrostatic analogy method was used to solve this equation. The time during which the volume content of the dispersed phase of the magnetic nanofluid increases to a limiting value was determined for magnetic fluid tribounits with an open fluid surface and those enclosed in a chamber with a small opening. Based on the obtained calculation relationships linking evaporation parameters with changes in the volume fraction of the dispersed phase and the criterion of the maximum permissible viscosity, an engineering methodology for assessing the durability of magnetic fluid bearings and seals has been developed. Recommendations are given for the selection of magnetic fluid and operating modes that ensure an increase in its service life.
Keywords: magnetic fluid, evaporation, dispersion medium, friction unit life, viscosity, plain bearing.

Burtsev A.A., Ionin V.V., Kiselev A.V., Nevzorov A.A., Mikhalevsky V.A., Eliseev N.N., Lotin A.A.
Modeling of light propagation in silicon nitride and zinc selenide photonic integrated circuit elements with a switchable phase-change material film – page 354
Abstract: This work presents a comparative analysis of two technological platforms for photonic integrated circuits: silicon nitride (Si₃N₄) and zinc selenide (ZnSe). Using numerical modeling, we demonstrate transmission characteristics of waveguides made of these materials upon switching of an active Ge2Sb2Te5 phase-change cell. Comparison of the two waveguide platforms with an integrated phase-change layer reveals fundamental differences in modulation physics, governed by the choice of operating wavelength. The silicon nitride waveguide (near-infrared range) exhibits strong field localization near the interface and supports several hybrid modes, some of plasmon-polariton nature. This results in a superlinear dependence of losses on the active film thickness, requiring precise optimization (20 nm) to achieve maximum contrast (246%). In contrast, the zinc selenide waveguide (mid- and far-infrared range) shows a reduced plasmonic contribution, a depleted modal composition (close to single-mode), and a quasi-linear increase in losses with film thickness. This provides a wider range of permissible active film thicknesses (20-50 nm) and stable modulation characteristics (contrast up to 112%).
Keywords: photonic integrated circuits, optical waveguides, phase-change materials, thin films.

Kolosov A.Yu., Savina K.G., Sokolov D.N., Mitinev E.S., Vzglyadov I.A., Dmitriev I.S., Sdobnyakov N.Yu.
Comparative atomistic simulation of structural stability/instability of ternary double-shell nanoparticles Pd@X@Pt, X@Pd@Pt, Pt@X@Pd and X@Pt@Pd (X – Ni, Cu) – page 363
Abstract: Ternary double-shell nanoparticles with a total number of 5100 atoms were investigated via comparative atomistic simulations using molecular dynamics and Monte Carlo methods to study their structural stability and phase transformations. Employing the many-body tight-binding potential, the caloric curves of the nanoparticles were calculated during sequential heating and cooling cycles within a temperature range of 300-1500 K. Based on the analysis of melting and crystallization intervals, it is shown that the layer ordering critically affects the thermal stability of the particles. It was established that configurations with an outer nickel layer lose their structural stability upon heating and undergo a rearrangement into asymmetric multipod structures. The Pd@Ni@Pt configuration proved to be the most stable, with its crystalline core preserving fcc symmetry at temperatures above 1500 K. The analysis of local density distributions showed that after full recrystallization of the nanoparticles, palladium atoms tend to exhibit surface segregation; furthermore, if copper was included in the composition, all three components are distributed almost uniformly throughout the volume, whereas nickel atoms occupy the central part of the nanoparticle, platinum forms the sub-surface layer, and palladium forms the outer shell.
Keywords: molecular dynamics method, Monte-Carlo method, MDSym, Metropolis, tight-binding potential, ternary double-shell nanoparticles, segregation, local structure.

Virskiy A.E., Malyshev M.D., Komarov P.V.
Effect of active environment on the orientational organization of rod-like nanoparticle: mesoscale simulations – page 380
Abstract: This work examines the possibility of controlling the spatial orientation of rod-like nanoparticle through the influence of molecules of active environment. We consider ordered layers formed by smectic molecules as an active environment. To model the supramolecular organization in such conditions, we employed the dissipative particle dynamics method. Our result shows that when the nanoparticle length is twice the length of a molecule of the active environment, three types of orientational ordering are possible: localization inside a domain formed by the head groups of molecules of active environment (type I), inside a domain formed by the tail groups of molecules of the active environment (type II), and perpendicular to the domains of active environment (type III). The first two orientations are stable, while the orientation perpendicular domains is unstable for long simulation times. This may indicate the potential instability of such states. We also studied the influence of the nanoparticle length and the presence of residual solvent on the stability of the identified orientational orderings of the considered nanosystems. These results could be useful for developing liquid crystal materials reinforced with rod-like nanoparticles or a switchable nanoparticles orientation.
Keywords: self-assembly, dissipative particle dynamics, nanoparticles, active environment.

Glagolev M.K., Vorozheykina A.V., Patrenkov I.K., Komarov P.V.
Development of a computational model for stability assessment of N-vinylcaprolactam – N-vinylimidazole copolymers in a selective solvent – page 391
Abstract: Computer simulation of the behavior of thermosensitive copolymers of N-vinylcaprolactam and N-vinylimidazole in a water environment was performed using a pipeline of unidirectionally coupled simulation models, namely Dissipative Particle Dynamics, Langevin Dynamics, and All-atom Molecular Dynamics. The pipeline allows first to determine a possible sequence of monomer units in a model copolymer, then to determine the morphology of the globules formed in a selective solvent, and finally to assess the aggregation stability of the globules. It utilizes the fast relaxation dynamics in Dissipative Particle Dynamics Simulations, efficiency of implicit solvent consideration in Langevin dynamics, and experimentally verified atom interaction force-field in All-atom Molecular dynamics simulations. The approach exploits the strengths of each of the simulation methods, and the relevance of the simulation results is ensured by the ultimate transition to the all-atom detailed representation. Here we describe the models and the algorithms of transformation between the models, and present the data for their initial validation. The behavior of the studied models in an aqueous environment allows us to conclude that the constructed systems are structurally stable. The globules have a distinct core-shell structure, with N-vinylcaprolactam monomer units forming the core and N-vinylimidazole monomer units forming the outer shell. Water molecules penetrate the globule primarily through the shell, which is rich in N-vinylimidazole units.
Keywords: poly(N-vinylcaprolactam), poly(N-vinylimidazole), thermosensitive copolymers, computer simulation, thermally-switched catalysts.

Kuz’min N.B., Komarov P.V., Samsonov V.M., Sdobnyakov N.Yu.
On the problem of observing contact melting in a molecular dynamics experiment in Ni-Al bimetallic nanolayer – page 401
Abstract: Using a bimetallic Ni-Al nanolayer as an example, molecular dynamics simulations of contact melting during annealing at 900 K were performed. The open-source LAMMPS software and the embedded-atom potential were used for this purpose. Interest in the chosen research object is due to the complexity of the phase diagram, while the temperature for the molecular dynamics experiment (900 K) was determined by considering the contact melting temperature for the macroscopic Ni-Al system and the potential size effect. Furthermore, this temperature is lower than the melting point of the lower-melting element, i.e. aluminum. During annealing for up to 100 ns, several characteristic temperatures were identified, corresponding to different stages of the diffusion process in the bimetallic Ni-Al nanolayer. The evolution of the local structure was observed using the open-source Ovito software with a modifier corresponding to the Ackland-Jones method. This approach analyzes the geometry of the angles between the bond vectors of a selected atom with its nearest neighbors. Over the selected time interval (100 ns), interface movement was identified in the Ni-Al system, but the crystalline transition layer «prevents» further «activation» of contact melting. This effect is observed for the first time for contact melting in nanoscale metallic systems.
Keywords: contact melting, bimetallic Ni-Al nanolayer, LAMMPS, molecular dynamics simulation, embedded-atom potential, local structure, Ackland-Jones method.

Lapushkin M.N.
Adsorption of a beryllium monolayer on the surface of GaN(0001) – page 409
Abstract: The density functional method was used to calculate the adsorption of a monolayer of beryllium atoms on a GaN(0001) surface. The surface was modeled within the framework of a 2×2 supercell geometry containing 10 GaN bilayers. The initial GaN(0001) surface exhibits a metallic conductivity caused by the presence of a band of surface states near the Fermi level. One beryllium monolayer corresponded to a concentration of one Be atom per one surface Ga atom. Calculations of the electron density of states and the adsorption energy were performed for a stable configuration during the adsorption of Be atoms over surface Ga atoms (on-top position) and during the formation of trimer Be clusters with a side length of 2,036 Å within the hexagonal GaN cell. It was found that adsorption is energetically most favorable in the trimer configuration. This non-standard configuration became possible due to the small size of the Be atom. The adsorption energy of Be is 2,125 eV. It was shown that the deposition of a Be monolayer causes only minor structural reconstruction of the substrate: the distance between the Ga and N layers in the surface GaN bilayer increases by 0,102 Å. The adsorption of beryllium leads to the formation of a wide band of surface states below the Fermi level, and the chemical bond with the GaN(0001) substrate is covalent in nature and is provided by the hybridization of the valence electrons of Be and the surface Ga atoms.
Keywords: density functional method, electronic structure, interface, surface, adsorption, beryllium, GaN.

Mikhailov G.P., Voronova Yu.G.
Modeling the temperature dependence of the energy gap of a subnanocluster of titanium dioxide – page 418
Abstract: Using quantum-chemical modeling methods, the temperature dependence of the energy gap of the (TiO2)15 subnanocluster was studied in the range from 10 to 900 K. Within the framework of density functional theory (M06/6-31G(d,p) approximation), it was found that the (TiO2)15 subnanocluster has a quasi-spherical shape (C2h symmetry, diameter of 0,9 nm), and its inner core exhibits the atomic order of rutile. Thermostable structures (TiO2)15 were obtained by the non-empirical molecular dynamics method using the Atom-Centered Density Matrix Propagation scheme. For each temperature, the energy gap Egap between the lowest vacant and highest occupied molecular orbitals was calculated using the M06/6-31G(d,p) approximation. The obtained data were analyzed using the Eg(T) model dependencies developed for crystalline solids. The qualitative similarity of the temperature dependencies of Eg(T) for the (TiO2)15 cluster and bulk semiconductors has been established, namely, a non-linear monotonic decrease of the Eg with increasing temperature. As the temperature increases, significant anharmonicity of the (TiO2)15 cluster vibrations is observed, and the temperature sensitivity of the O 2p (highest occupied molecular orbital) and Ti 3d (lowest unoccupied molecular orbital) molecular orbitals is different, with the titanium orbitals showing a weak dependence. The most adequate and physically interpretable results are obtained using the O’Donnell-Chen model, which takes into account the quantum nature of the subnanocluster vibrations and allows us to determine the average energy of the vibrational modes that determine the temperature dependence of the energy gap.
Keywords: nanocluster, titanium dioxide, density functional theory, energy gap.

Patrenkov I.K., Malyshev M.D., Komarov P.V.
Creation of mesoscale models of aged polymer nanoparticles using the Rosenbluth algorithm – page 428
Abstract: This paper presents a three-stage approach to constructing mesoscale models of aged polymer nanoparticles. The initial nanoparticle configuration is constructed using the lattice Rosenbluth algorithm, which has been adapted to address the current issue. This algorithm creates dense globules composed of a specified number of polymer chains, which are constructed from coarse-grained particles (beads) of a single type. Increasing the size of the nanoparticles, as determined by the number of beads they contain, results in increased polydispersivity of the polymer chains. This also results in increased shape anisotropy. For nanoparticles containing more than 100 beads, this anisotropy is preserved even after long-term relaxation, which is the second stage in the construction process. The third step involves transforming some beads into different types using a specific ratio. The type of bead, its location in the polymer chain, and its ratio are determined from literature sources. Some intra-chain bonds are broken, and new inter-chain bonds are formed. These changes form the basis of the nanoparticle aging algorithm. Applying the aging algorithm has been found to lead to the formation of large numbers of low-molecular-weight fragments inside nanoparticles. These degraded products easily desorb from nanoparticle surfaces into the surrounding environment.
Keywords: Rosenbluth algorithm, coarse-grained modeling, polymers, degradation, nanoparticles.

Serov S.V., Savina K.G., Kolosov A.Yu., Sokolov D.N., Veresov S.A., Zorin D.R., Zaytsev A.V., Simchuk N.N., Sdobnyakov N.Yu.
Features of structural transformations in four-component Cu-Au-Pt-Pd nanoalloys: multi-shell structure and alloy with uniform distribution of components – page 439
Abstract: Using two initial configurations (a multi-shell structure and an alloy with a uniform distribution of components) as an example, a molecular dynamics study was conducted to investigate the structure formation processes in quaternary Cu-Au-Pt-Pd nanoparticles (with a total of 10,000 atoms) during a sequential cycle of thermally induced exposure, including phase transitions corresponding to melting and crystallization. The thermally induced exposure was performed at three cooling/heating rates: 0,25 K/ps (typical rate), 0,5 K/ps (median rate), and 1 K/ps (high rate). For each initial configuration, the temperature dependences of the potential component of the specific internal energy were obtained during heating and cooling, and the hysteresis parameters of the melting and crystallization temperatures were determined. Additionally, the regularities of chemical and structural segregation in the configurations corresponding to the end of cooling are described. Furthermore, the component distributions in the final configurations of the Cu-Au-Pt-Pd nanoparticles were constructed and analyzed to verify the hypothesis of a specific segregation behavior of the components. It is shown that the patterns of local crystalline ordering and the width of the temperature hysteresis corresponding to melting and crystallization are determined mainly by the rate of thermally induced action, while the initial morphology has a predominant effect on the distribution of atoms between fcc and hcp local environments.
Keywords: quaternary Cu-Au-Pt-Pd nanoparticles, multi-shell structure, alloy with uniform distribution of components, molecular dynamics method, tight-binding potential, segregation.

Puytov V.V., Samsonov V.M., Vasilyev S.A.
Coalescence and sintering in a ternary nanosystem Pt+Cu+Pd: molecular dynamics simulation – page 455
Abstract: Using the LAMMPS soft-ware and the embedded atom method, molecular dynamics simulation has been performed of sintering and coalescence in a system of three monometallic nanoparticles (Pd1700 + Cu5100 + Pt1700), whose centers of mass were located on the same straight line. The process was carried out during uniform heating of the system up to a temperature of 2300 K, corresponding to the daughter nanodroplet, and subsequent cooling (quenching) it to the initial temperature of 300 K. We found that as a result of low-temperature sintering (heating to 500-900 K), a ternary analogue of the Janus structure was formed. Solidification of the nanodroplet resulted in the ternary nanocrystal formation. Temperature dependences of radial distributions of atomic fractions of the components were found and analyzed. It was established that during both sintering solid nanoparticles and cooling (quenching) nanodroplets, Pd atoms migrate to the outer atomic monolayer, whereas in solidified nanodroplets, Pt atoms have segregated toward the second monolayer and the center of the nanoparticle. In addition to chemical segregation, i.e., the spatial separation of components, structural segregation was observed in the solidified nanodroplets. This segregation yields grains in the form of bands with a defective fcc structure, separated from each other by boundaries represented by atoms identified by the Ovito program as a local hcp structure.
Keywords: LAMMPS, molecular dynamics, embedded atom potential, sintering, coalescence, surface segregation.

Savina K.G., Serov S.V., Kolosov A.Yu., Sokolov D.N., Kravchenko D.A., Grigoryev R.E., Bogdanov S.S., Arakcheev E.E., Sdobnyakov N.Yu.
Atomistic simulation of segregation in quaternary Ni-Cu-Fe-Co nanoparticles with different initial configurations – page 466
Abstract: In this work, the molecular dynamics method was used to study modeling quaternary Ni-Cu-Fe-Co nanoparticles (containing 4000 atoms) with different initial configurations: a particle with a mixed three-component core and a nickel shell, a four-shell structure with concentric shells, a nanoalloy with a uniform distribution of components, a four-layer planar structure, two symmetrical variants with seven layers of atoms. The interatomic interaction was described by the tight-binding potential. The molecular dynamics experiment was carried out according to the following scheme: 1) heating from 300 to 1800 K, and then cooling to 300 K with relaxation at each step of 10 ps, 2) relaxation for 100 ps at temperature 300 K. For the first stage, two rates of thermally induced action were selected. The temperature ranges of hysteresis of the melting and crystallization processes were determined. Segregation patterns in quaternary Ni-Cu-Fe-Co nanoparticles with different initial configurations are described using radial density distributions. The temperature parameters of the hysteresis associated with melting and crystallization processes have been evaluated. The obtained results demonstrate the variability of the properties of multicomponent nanoparticles, determined by both the initial conditions (morphology, composition, size) and the conditions of the molecular dynamics experiment (rate of thermally induced action).
Keywords: molecular dynamics, MDSym, tight-binding potential, quaternary nanoparticles, segregation, nickel, copper, cobalt, iron, local density.

Rikhmaier A.M., Chernova E.M., Orlov Yu.D., Rikhmaier M.A.
Electron density topology and molecular parameters of monochloro-substituted anthracene derivatives: QTAIM positional isomerism analysis in the context of molecular electronics – page 484
Abstract: A systematic analysis of the electron density topology in a number of positional isomers of monochloranthracene is performed. The calculations were carried out using the B3LYP electronic density functional theory with the basis 6-311G. The analysis of the obtained electronic structure was performed using the quantum theory of atoms in the molecule. It has been established that the position of the chlorine atom affects the distribution of electron density in the anthracene core, which is manifested in a change in the values of atomic charges and volumes, ionization energies, and electron affinity. It has been shown that 9-chloroanthracene is characterized by maximum delocalization of electron density, maximum electron affinity energy and minimum ionization energy, which predicts high mobility of charge carriers and the ability to form rigid crystalline packages. The findings demonstrate that descriptors of electronic topology can serve as an effective tool for predictive design of organic semiconductors at the isolated molecule level.
Keywords: anthracene, monochloranthracene, QTAIM, electron density topology, positional isomerism, molecular electronics, organic semiconductors, ionization energy, electron affinity energy, band gap.

Rikhmaier A.M., Chernova E.M., Orlov Yu.D., Rikhmaier M.A.
QTAIM analysis of tetracene, pentacene, and their monochloro-substituted derivatives: the effect of positional isomerism on the topology of electron density and semiconductor parameters – page 493
Abstract: Using the B3LYP density functional theory method with a 6-311G basis set and subsequent topological analysis of the electron density within the framework of the quantum theory of atoms in a molecule, a systematic study of tetracene, pentacene, and their monochloro-substituted positional isomers was conducted. For each of the considered compounds, the ionization energies and electron affinities were calculated, as well as the band gap width. By means of topological analysis of the electron density, changes in the charges and volumes of atomic fragments caused by the substitution of one of the hydrogen atoms by chlorine are quantitatively characterized. It is revealed that monochloro substitution leads to a local redistribution of the electron density. The maximum changes in integral parameters are observed in the immediate vicinity of the substitution site. It is shown that the perturbation decays at a distance of 3 or more bonds, and the connecting carbon atoms remain practically inert to the substitution. The results of this study can serve as a basis for developing a method for predicting the semiconductor properties of monochlorinated polyaromatic hydrocarbons by varying the position of the chlorine atom in the compound structure, which opens up opportunities for molecular design of organic semiconductors with predefined parameters.
Keywords: positional isomerism, tetracene, pentacene, DFT, QTAIM, ionization energy, electron affinity energy, band gap, atomic charge, atomic volume.

Samsonov V.M., Sdobnyakov N.Yu., Zhigunov D.V., Mitinev E.S., Sinitsa I.P., Kolosov A.Yu., Sokolov D.N.
Dynamics of thermally induced structural transformations in a ternary Pd4@Ni2@Pt2 nanocube – page 504
Abstract: Using isothermal molecular dynamics and LAMMPS software, we studied the dynamics of chemical and structural segregation upon heating Pd4@Ni2@Pt2 nanocubes from 300 to 2000 K (the subscripts indicate the number of atomic monolayers). The embedded atom method was used for simulations. The system was preliminarily subjected to relaxation for 1 ns at a temperature of 300 K. Particular attention was paid to analyzing the temperature dependence of the specific potential energy and its relationship with structural transformations at temperatures near which some jumps in this dependence occur. Several types of transitions were identified: fcc/hcp structural transitions, order/disorder transitions associated with competition between identified and unidentified crystalline phases, sphere-to-polyhedron and vice versa transitions corresponding to shape changes, and a complex melting phase transition with an atypical behavior of the temperature dependence of the specific potential energy. Two alternative approaches were used for the first time to identify the local environment: the polyhedral template method and the Ackland-Jones method. The identification results using both methods are generally in good agreement, but the Ackland-Jones method sometimes identifies as bcc instead of the hcp local environment (when the polyhedral template method was employed), and this seems apparently be due to a feature of the Ackland-Jones method based on an analysis of the distribution of bond angles between the central atom and its nearest neighbors.
Keywords: nanocube Pd4@Ni2@Pt2, Ackland-Jones method, polyhedral template matching, LAMMPS, molecular dynamics, embedded atom potential, structure transformations.

Cherepovskaya A.A., Ryzhkova D.A., Gafner Y.Ya., Starostenkov M.D.
Study of nanoparticle coalescence mechanisms using Pt and Pb as an example – page 515
Abstract: In modern materials science and nanotechnology, nanoparticle coalescence processes play a key role in determining the stability and functional properties of nanosystems. Coalescence, the fusion of two or more nanoparticles into a single structure, affects the catalytic activity, optical, and electrical characteristics of materials. In this work, mechanisms of coalescence (using the example of platinum and lead metal nanoparticles) are investigated by molecular dynamics method. The aim of the study was to determine the influence of the mutual crystallographic orientation of atoms, as well as the magnitude of the interatomic interaction on the unification process. Coalescence of Pt and Pb nanoparticles of different diameters was studied, the distance between the particles varied from 1,5 to 0,5 ns, and the simulation time corresponded to 500 ps. The actual appearance and structure of the studied nanoparticles were determined using OVITO and XMakemol visualizers. Analysis of the results shows that various coalescence mechanisms are determined by thermally activated diffusion of surface atoms.
Keywords: coalescence, platinum, lead, nanoparticles, structure, computer simulations, molecular dynamics, tight-binding.

4. PHYSICAL AND CHEMICAL BASES OF NANOTECHNOLOGIES – page 522

Aref’eva L.P., Kovaleva V.V.
Determination of the surface energy of the phase components of structural steel by the fatigue crack growth kinetics – page 522
Abstract: The work is devoted to the determination of the surface energy of steel from experimental data on the crack growth and comparison with results of numerical modeling. The kinetics of fatigue fracture of a steel 1.0481 sample with a line ferrite-martensite structure obtained as a result of incomplete hardening and subsequent low-temperature tempering is investigated. Numerical modeling of the values of the surface energy of the ferrite and martensite crystallite faces is carried out by the electron-statistical method. As a result of a graphical differentiation of the dependence of the crack length on the number of loading cycles, the values of the crack propagation rate were obtained, the crack lengths were also estimated, and the surface energies of each phase were calculated in the Griffiths model. The error in determining the indirect values, obtained as a result of statistical data processing, is approximately 1%. The analysis conducted shows that the values of the crack growth rate are in good agreement with the results of studies on the rate of crack formation in normalized structural steels. The numerical simulation data are in agreement with experimental data within 16% and with reference data within 18%.
Keywords: surface energy, tensile strength, crack, structural steel, ferrite, martensite, two-phase structure.

Afanasiev M.S., Belorusov D.A., Goldman E.I., Kiselev D.A., Sivov A.A., Chucheva G.V.
The influence of synthesis temperature on the structural and electrical properties of metal-dielectric-semiconductor structures based on hafnium oxide films – page 530
Abstract: In this work, hafnium oxide films were obtained on silicon substrates using magnetron sputtering at temperatures of 25, 300, 500, and 700°C. The results of scanning probe microscopy studies of the quality of HfO2 films and the electrophysical properties of metal-dielectric-semiconductor structures (Ni-HfO2-Si) are presented. It is shown that an increase in the synthesis temperature enlarges the crystallites (from 53 to 100 nm) and reduces the roughness. At a synthesis temperature of 500°C, an improvement in the ferroelectric parameters is observed: the built-in voltage decreases from +1,38 to +0,33 V, and the loop squareness coefficient increases from 0,34 to 0,63. The largest loop width on the capacitance-voltage characteristic (~4 V) and the best frequency stability of capacitance and dielectric losses are achieved at a synthesis temperature of 300°C. A further increase in temperature to 500-700°C increases the maximum capacitance, but narrows the hysteresis loop, reduces frequency stability, and shifts the minimum of dielectric losses to the high-frequency region. It is determined that the saturation of the field curves of high-frequency capacitances is not associated with the inversion of Si at the Si/HfO2 contact during semiconductor depletion and is not associated with deep enrichment of the silicon surface, but is due to the pinning of the Fermi level on the branches of the U-shaped density of states of electron traps in the buffer layer between the substrate and the insulating layer. It is established that the choice of the synthesis temperature allows for targeted control of the film properties: 500°C is optimal for enhancing the ferroelectric response, while 300°C is optimal for obtaining frequency-stable structures. The results are useful for the development of non-volatile memory and high-frequency devices based on HfO2.
Keywords: ferroelectric films, hafnium oxide (HfO2), structures metal-dielectric-semiconductor, electrophysical properties, polarization.

Belyavsky M.A., Kislova I.L., Karpenkov A.Yu., Ivanova A.I., Izmailov R.F., Pis’merova E.A., Solnyshkin A.V.
Microstructure and electrophysical properties of barium ferrite-based ceramics with bismuth impurity – page 541
Abstract: In this work, bismuth-doped barium ferrite ceramic BaFe12O19 samples were synthesized. Scanning electron microscopy of the samples microstructure revealed that increasing the bismuth content in the ceramics BaBixFe12-xO19 leads to a decrease in the grain size. It should be noted that this also increases the density of the synthesized ceramics. The effect of Bi doping on the electrical properties of the obtained samples was studied. Adding the bismuth oxide into the barium ferrite during solid-phase synthesis reduces the sample conductivity significantly. This effect is due to a decrease in the mobility of charge carriers because of the potential relief change. Furthermore, in the low-frequency region, the dispersion dependences of the permittivity and dielectric loss tangent change significantly with increasing frequency, further indicating increased sample conductivity. Moreover, the low-frequency dispersion significantly decreases with the addition of bismuth ions to the ceramic samples, further indicating a decrease in electrical conductivity. For all compositions BaBixFe12-xO19 at x ≥ 0,2 full magnetic hysteresis loops and partial dielectric hysteresis loops were obtained for x = 0,6 and 1. It was found that the effect of an external magnetic field reveals a clear correlation between the permittivity and the amount of introduced impurity.
Keywords: ceramics based on barium ferrite, microstructure, multiferroic, dielectric constant, magnetic hysteresis loops, dielectric hysteresis loops.

Bibanaeva S.A., Skachkov V.M., Bogdanova E.A.
Study of the possibility of obtaining porous bioceramics based on calcium phosphates by the method of burnout additives – page 550
Abstract: The article discusses possibility of producing porous calcium phosphate-based bioceramics using a burnout additive method. Nanostructured precipitated hydroxyapatite (mechanically activated hydroxyapatite, titanium dioxide-reinforced hydroxyapatite, and fluorinated hydroxyapatite) and tricalcium phosphate were used as a bioactive matrix for producing porous ceramics. Natural and commercially available starch and gelatin were used as some pore-forming agents. Materials with a three-dimensional porous structure were obtained by mechanochemical synthesis of the bioactive matrix with a calculated amount of a pore-forming agent, followed by high-temperature processing. The synthesized samples were certified using modern physicochemical analytical methods. The influence of the qualitative and quantitative composition of the material on the sintering processes, structure, and strength characteristics of the studied samples is demonstrated. Experiments have shown that gelatin is the most promising pore-forming agent for the studied systems. It has been shown that to achieve a balance between porosity and strength, the hydroxyapatite content in the sample should not exceed 10% by weight. Despite differences in microhardness, the tensile strength of porous ceramics based on hydroxyapatite obtained using the burnout method meets the strength requirements for implant materials, opening up opportunities for further research aimed at implementing them in medical practice.
Keywords: calcium phosphates, hydroxyapatite, biomaterials, porous ceramics, synthesis, pore-forming agents, starch, gelatin, burnout method.

Bobreva L.A., Sidorov N.V., Pyatyshev A.Yu., Palatnikov M.N.
Features of the defect structure of LiNbO3:Tb single-crystal plates with a post-threshold concentration of terbium ions – page 567
Abstract: A comparative analysis of the defect structure of Z-oriented LiNbO3:Tb (2,25 wt.%) and LiNbO3:Tb (2,9 wt.%) single-crystal plates was performed using infrared absorption spectroscopy in the region of OH⁻-group stretching vibrations. It was found that the complex multicomponent profile of the spectral structure in the 3000-4000 cm-1 range is formed not only by local vibrations of hydroxyl groups near various lattice defects, but also due to the superposition of weak electronic f-f transitions of Tb3+ ions, which become allowed under the action of the crystal field. By decomposing the spectra, absorption bands corresponding to various defects were identified: absorption bands near 3466 cm-1 are associated with a violation of stoichiometry, and absorption bands in the 3490-3600 cm-1 range with the mechanism of dopant incorporation. It was shown that the sample with a lower terbium content (2,25 wt.%) is characterized by a higher volume concentration of OH⁻ groups, compared to the sample with a terbium content of 2,9 wt.%. This effect is associated with a change in stoichiometry and the formation of two types of complex defects: (VLi–)-OH and 5(TbLi2+)-2(VNb5-)-OH. The obtained results allow us to clarify the mechanisms of defect formation and can serve as a basis for optimizing the technological modes for producing crystals intended for the creation of nonlinear optical elements with controlled domain structures.
Keywords: lithium niobate, terbium, infrared absorption spectrum, electronic transitions, OH⁻ groups, complex defects.

Bolotov A.N., Novikova O.O.
Magnetic nanofluids in tribology: achievements, challenges, and future research directions – page 575
Abstract: This article presents a systematic review of current research on magnetic lubricating nanofluids (ferrofluids) as a class of intelligent tribological media whose properties are controlled by an external magnetic field. The aim of the work is to summarize and critically analyze scientific concepts regarding the colloidal structure, synthesis methods, tribological characteristics, and engineering applications of such fluids. The classification of magnetic lubricants, the historical evolution of approaches (including studies from 1988–1991 that established the magnetotribological effect and the role of structural components), and current trends are discussed. The mechanisms of colloidal stabilization, the influence of Fe3O4 nanoparticle size and concentration, the magnetoviscous effect, and field-induced structure formation are analyzed in detail. It is shown that an optimal particle concentration (approximately 5 wt.%) reduces wear by up to 90%, while exceeding this concentration leads to abrasive wear. Four main mechanisms for reducing friction and wear are identified: rolling bearing, tribochemical film formation, self-healing of microcracks, and magnetic removal of wear debris. It was established that the effectiveness of a magnetic field depends significantly on its orientation and gradient, as well as the material of the friction pair. The main areas of application (magnetic seals, bearings, controlled tribosystems, heat transfer), limitations (aggregate instability, particle abrasion, scaling), and development prospects, including active feedback systems and hybrid compositions, are discussed. It is concluded that the main value of magnetic lubricating nanofluids lies in their ability not only to simply lubricate but also to control lubrication, opening up new operating principles for friction units in precision, vacuum, and microengineering.
Keywords: magnetic lubricating nanofluids, ferrofluids, tribology, Fe3O4 nanoparticles, magnetically viscous effect, boundary lubrication, wear, magnetic field, smart lubricants.

Bolshakova N.N., Galkin I.K., Ivanova A.I., Semenova E.M.
Dispersion dependences of polarization switching parameters of copper-containing triglycine sulfate crystals – page 594
Abstract: The paper presents results of an experimental study of the concentration and dispersion dependences of repolarization characteristics of copper-containing triglycine sulfate crystals. It is shown that with an increase in the impurity concentration in triglycine sulfate : Cu2+ crystals, the values of the relative and effective permittivities, switchable polarization, and unipolarity coefficient tend to increase, while the magnitudes of the coercive field, bias field, and dielectric loss tangent tend to decrease. The switching processes are significantly affected by the frequency of the alternating field, with an increase in which a transformation of the dielectric hysteresis loops is observed. As the frequency increases from 50 Hz to 2 kHz, the switchable polarization of the crystals decreases by an average of 2,5 times. At the same time, the frequency of the repolarizing field has a more significant effect on the repolarization processes of pure triglycine sulfate. A change in the repolarizing field frequency from 50 Hz to 2 kHz leads to a decrease in the dielectric viscosity coefficient of triglycine sulfate : Cu2+ crystals by an average of 3 times, which is caused by the switching off of the main switching mechanisms.
Keywords: dispersion dependences, triglycine sulfate, hysteresis properties, switchable polarization, permittivity, dielectric viscosity, domain structure.

Bui C.D., Shomakhov Z.V., Nalimova S.S., Maraeva E.V., Naimark A.A., Popov E.S., Maximov A.I., Moshnikov V.A.
Sorption analysis and photocatalytic activity of graphitic carbon nitride powder – page 604
Abstract: Graphitic carbon nitride (g‒C3N4) is considered a promising metal-free photocatalyst for the efficient degradation of stable organic dyes in wastewater, however, the relationship between its structural-dispersive characteristics and photocatalytic activity remains insufficiently studied. In this work, a comprehensive characterization was performed on g‒C3N4 powder synthesized via thermal polycondensation of urea at 550°C, followed by treatment with hydrochloric acid and ultrasonic exfoliation. The specific surface area, determined by the Brunauer-Emmett-Teller method, was 52 m2/g. Based on experimental sorption data, geometric parameters of the particles were evaluated within the framework of the nanosheet model. It is shown that the nanosheet thickness depends only weakly on the aspect ratio and is 17 nm, which corresponds to approximately 50 atomic layers under partial exfoliation of blocks. The photocatalytic activity of the material was investigated during the degradation of Rhodamine 6G dye under ultraviolet irradiation (395 nm). The degradation process obeys pseudo-first-order kinetics. As the catalyst loading is increased from 12 to 26 mg, the degradation degree of the dye over 120 minutes rises from 23,2% to 67,9%, and the rate constant increases from 2,1·10-3 to 9,3·10-3 min-1 due to the growth in the number of available active sites.
Keywords: graphitic carbon nitride, Brunauer-Emmett-Teller method, specific surface area, nanosheets, photocatalytic degradation of rhodamine 6G.

Golik A.B., Rusev N.A., Blinov A.V., Oblogin Y.A., Tatov A.V., Serov A.M., Pirogov M.A.
Synthesis and physicochemical study of pectin-stabilized selenium nanoparticles – page 612
Abstract: In this work, samples of selenium nanoparticles stabilized by citrus pectin were obtained by the method of chemical reduction of selenous acid by ascorbic acid in an aqueous medium, varying the concentrations of the precursor, stabilizer, and reducing agent according to the experimental design matrix. Computer quantum-chemical modeling of the interaction of a citrus pectin fragment consisting of three methylgalacturonic acid monomers with a selenium atom was performed using the QChem software package. It was found that the interaction is energetically favorable (the difference in total energy between citrus pectin and the molecular system of selenium with citrus pectin is ΔE > 2433 kcal/mol) and is chemically stable (chemical rigidity η ranges from 0,178 to 0,206 eV), and the most probable binding is through the hydroxyl group attached to C3 of the third A-bound methylgalacturonic acid residue (ΔE = 2433,586 kcal/mol, η = 0,206 eV). Photon correlation spectroscopy and electrophoretic light scattering methods were used to show that the average hydrodynamic diameter of the obtained particles varies from 193,70 to 1383,91 nm, and the ζ-potential ranges from -11,83 to +3,10 mV, depending on the ratio of the components; the smallest particle size and the most negative ζ-potential were achieved at the lowest concentrations of the precursor, stabilizer, and reducing agent. Using ultraviolet spectrophotometry, an absorption band with a maximum at 265 nm (the optical density is 0,8 r.u.), characteristic of nanosized selenium was detected, confirming the formation of nanoparticles. The study of the colloidal stability of the selected sample in the pH range of 1,81-11,98 showed a non-linear dependence of particle size on pH: maximum aggregation occurs in the slightly acidic region at ζ-potential values close to zero, while increasing the pH results in a more stable dispersion (ζ-potential around -20 mV) with smaller particle size.
Keywords: pectin-stabilized selenium nanoparticles, optimization of the synthesis method, stability at different pH levels, average hydrodynamic diameter, ζ potential.

Zaritovskii A.N., Kotenko E.N., Grishchuk S.V., Glazunova V.A., Volkova G.K.
Study of the parameters of carbon nanostructures synthesis in microwave co-pyrolysis of polystyrene and microcrystalline cellulose – page 624
Abstract: The parameters of the synthesis of carbon nanostructures during microwave catalytic co-pyrolysis of polymer materials were studied. Polystyrene, which is a typical high-carbon synthetic polymer, and microcrystalline cellulose, a renewable environmentally friendly source of carbon of plant origin, were selected as carbon donors. The processes were carried out in the presence of a mixture of nickel and iron oxalates, which serve as metal catalysts precursors, using granulated activated carbon of AG-3 grade as a microwave absorber to convert electromagnetic energy into thermal energy. The effect of microwave acceptor concentration, treatment time and method of preparing the reaction mixture on the formation of multi-walled carbon nanotubes was investigated. It has been established that the optimal conditions for the synthesis process of the target product are achieved at a microwave acceptor concentration of 40% (wt.) and a cyclic exposure to microwave radiation with a power of 1000 W for 5-12 minutes. The results of studies were confirmed by the data of transmission electron microscopy and X-ray phase analysis.
Keywords: microwave pyrolysis, carbon nanostructures, polystyrene, microcrystalline cellulose, nickel and iron oxalates, activated carbon.

Ivanov Y.F., Klopotov A.A., Prokopenko N.A., Petrikova E.A.
Phase-structural design of TiSiBN nanocomposite coating synthesized by vacuum-arc plasma-assisted method – page 634
Abstract: The paper considers the phase and structural conditions of the formation of a nanostructured TiSiBN coating synthesized by the vacuum-arc plasma-assisted method on a 321 steel substrate. It is shown that analysis of the ternary systems Ti-Si-N, Ti-B-N and Ti-Si-B allows one to predict in advance the limited solubility of the components and the predominant formation of some individual nitride phases. Based on the size factor, Pauling electronegativity and valence of the elements, it was established that nitrogen and boron have a significant size mismatch with titanium, which prevents the formation of extended substitutional solid solutions and enhances the tendency to form TiN- and BN-containing phases. Experimental data obtained by electron microscopy confirm the formation of a multilayer coating without a pronounced columnar structure. The main volume of the coating is represented by TiN and BN nanocrystallites 2,5-3,5 nm in size, and a transition layer up to 100 nm thick is revealed between the coating and the substrate. The average coating hardness is 32 GPa, with a range of 21-49 GPa. A physical interpretation of the hardening is proposed, based on a modified Hall-Petch dependence, suppression of dislocation nucleation in nanocrystallites, and consideration of the contribution of interphase and intraphase boundaries.
Keywords: film/substrate system, vacuum-arc plasma-assisted method, phase composition, defect substructure, phase diagram.

Kaplunov I.A., Tretiakov S.A., Ivanova A.I., Vasilyev A.D., Yushkov K.B., Rogalin V.E., Vaysburg N.Ya.
Surface modification of single-crystal germanium by femtosecond laser radiation – page 646
Abstract: This paper presents the results of a study examining the effects of femtosecond laser radiation on polished germanium single crystal surfaces with varying crystallographic orientations. In the experiments used a 1030 nm laser with an average power of 5 W and a pulse duration of 330 fs, as well as an optical setup with an automated sample position control system, enabling the radiation stability and repeatability of experimental conditions to be monitored. The resulting surface irregularities, which consisted of craters or a structure consisting of a series of peaks and valleys with the midline maintained in the plane of the original surface, were fixed using optical microscopy and subsequently examined using a profilometer and a scanning electron microscope. Morphological and 3D surface profile analysis of the obtained data at the impact points revealed features of the resulting relief depending on the crystallographic orientation of the samples and the energy characteristics of the laser radiation, where the peak pulse power, and therefore the fluence, was controlled through the average power or pulse repetition rate. Irreversible change of the surface (laser-induced damage) for single-crystal germanium is 20-30 MW in peak power per pulse with a beam diameter of 0,31 mm and an exposure duration of 20 ms, which corresponds to an fluence of 8,7-13,1 mJ/cm2.
Keywords: femtosecond laser, critical values, profilometric analysis, germanium.

Klopotov A.A., Abzaev Y.A., Ivanov Y.F., Volokitin G.G., Loskutov O.M.
Surface modification of TiNi-based alloys by high-current low-energy electron beams – page 657
Abstract: Titanium nickelide alloys TiNi exhibit a high sensitivity of their fine crystalline structure to external energy inputs, which governs their functional properties (the shape-memory effect and superelasticity). Exposure to high-current low-energy electron beams produces metastable nanocrystalline states in the near-surface layers; however, the quantitative analytical relationship between the integral irradiation energy and the evolution of structural parameters remains insufficiently developed. Based on X-ray diffraction data and computer simulation of heat transfer, a physical and mathematical model has been developed that describes the kinetics of changes in the unit-cell parameter a, second-kind microstrains ε = <Δd/d>, and coherent scattering region sizes DCSR as functions of the integral energy W = N ∙ ES. Exponential saturation of the decrease in the lattice parameter a(W), with a limiting contraction Δa/a0 ≈ 0,69% caused by selective titanium evaporation, has been established. The dependences ε(W) and DCSR(W) were obtained and approximated by threshold functions reflecting the competition between the defect generation and annealing over different activation-energy spectra. The dislocation density ρ = (1,5-16,7)∙1014 m-2 and elastic energy of the defect subsystem Udisl ≈ 4,0 ∙ 107 J/m3 were calculated. The proposed model predicts the structural state of the modified layer with an accuracy of R2 > 0,96 and elucidates the physical mechanisms governing threshold changes in the fine crystalline structure, thereby providing a basis for targeted control of the functional responses of shape-memory alloys.
Keywords: titanium nickelide, high-current electron beams, X-ray diffraction analysis, lattice parameter, thermodynamic modeling.

Klychkov N.A., Simakov V.V., Sinev I.V., Chirkova A.D.
Effect of ultraviolet radiation on the selectivity of zinc oxide gas sensors – page 668
Abstract: This work investigates the effect of ultraviolet irradiation intensity on the response and selectivity of gas sensors based on zinc oxide ZnO layers. The ZnO layers were synthesized by chemical deposition followed by thermal annealing at 400°C in an oxygen-containing atmosphere. It is shown that UV irradiation at 365 nm with intensities from 5 mW/cm² to 20 mW/cm² enhances the sensor response to ethanol, isopropanol, and acetone vapors by up to 10 times. The dependence of the photo-response magnitude on the gas environment observed upon irradiation at 400 nm and 525 nm indicates ionization of deep impurity centers induced by adsorbed gas molecules. From the concentration dependences of the sensor response, the selectivity and specificity coefficients are calculated, demonstrating a 2‑fold increase in selectivity to ethanol with increasing illumination intensity. The obtained results reveal that varying the illumination intensity enables control over the sensor selectivity through the selective ionization of surface states associated with different adsorbed gases.
Keywords: zinc oxide, photoactivation, gas sensor response, selectivity, specificity, impurity centers.

Korzh E.G., Lopatin K.M., Antipov P.E., Burlakova V.E.
The influence of conditions for obtaining shiny nickel coatings modified with nanodiamonds on their morphological features – page 679
Abstract: In this study, bright nickel coatings modified with nanodiamonds were obtained using the electrochemical method in a bright nickel plating electrolyte at cathodic current densities of 1, 3, and 5 A/dm2. The resulting bright nickel coatings with nanodiamonds were studied using atomic force microscopy. It was found that the surface topography of the bright nickel coatings with nanodiamonds varies significantly and depends on the conditions (cathode current density) of coating production. The bright nickel coatings with nanodiamonds were studied using scanning electron microscopy. It was found that the morphological features of the nickel coatings with nanodiamonds obtained at a cathodic current density of 1 A/dm2 are characterized by an increased content of pores and irregularities compared to bright nickel coatings obtained at current densities of 3 and 5 A/dm2. The presence of inclusions in the form of rounded protrusions on the surface of shiny nickel coatings obtained at current densities of 3 and 5 A/dm2 was detected. Using energy-dispersive X-ray spectra, the presence of a carbon phase in the composite shiny nickel coating was confirmed, indicating the presence of nanodiamonds in its structure. It was found that the shiny nickel coating with nanodiamonds obtained at a cathodic current density of 5 A/dm2 contains up to 10,6% of the carbon phase.
Keywords: nanodiamonds, bright nickel coating, composite coating, surface morphology.

Krot P.A., Ovchenkova Y.A., Pankratov N.Yu., Tereshina I.S., Verbetsky V.N.
Hydrogen embrittlement of high-entropy rare-earth alloys: structure and magnetic properties of the resulting trihydrides – page 687
Abstract: The synthesis and investigation of the structural and magnetic properties of the trihydrides of high entropy rare-earth alloys was carried out. It was determined that the alloys containing only heavy rare-earth elements adopted the magnesium-type structure (space group P63/mmc), while the one made of both heavy and light rare-earth elements had the rhombohedral lattice of samarium type (Rm). For all the studied trihydrides the complex hexagonal holmium trihydride-type structure (Pc1) was found. Hydrogen uptake in the alloys led to the lattice expansion, the occurrence of stress and spontaneous cracking along the grain boundaries, as a result of which the ingot crumbled into powder without mechanical grinding. Lanthanide contraction effect for both the studied alloys and their trihydrides was observed. The paramagnetic Curie temperatures, effective magnetic moments, and the prevailing type of exchange interaction were determined for each trihydride. It was found out that hydrogen uptake suppressed magnetic ordering down to 2 K.
Keywords: high-entropy alloys, rare earths, hydrides, magnetic properties, crystal structure, lanthanide contraction.

Mikhalevsky V.A., Burtsev A.A., Ionin V.V., Nevzorov A.A., Kiselev A.V., Eliseev N.N., Lotin A.A.
A planar array of GST225-based memristor elements – page 705
Abstract: This paper presents a modeling study of the electrical resistance in a memristor structure based on the phase-change Ge₂Sb₂Te₅ material. The changes in resistance are driven by some structural transformations in the active region of the memory cell under the influence of electrical control pulses. A novel planar architecture for memristor structures has been demonstrated. Using the simulation data for this architecture, temperature dynamics and phase transitions are analyzed within the framework of the classical Stefan problem. Optimal parameters for the electrical control pulses are identified. The results demonstrate that once the phase transition threshold is reached, the resistance switching time becomes essentially independent of the control parameters. The proposed memristor architecture exhibits advantages in both power efficiency and the capability for multilevel resistance states, positioning it as a key component for next-generation memristive technologies.
Keywords: memristor, chalcogenides, phase change materials, thin films, amorphization.

Mustafayev G.A., Cherkesova N.V., Mustafayev A.G.
Laser annealing of doped amorphous silicon films obtained by high frequency sputtering – page 714
Abstract: The effect of pulsed laser annealing on the structural and electrical properties of arsenic-doped amorphous silicon films (50-200 nm thick) obtained by high frequency ion sputtering is studied. It is shown that at an energy density of 1,4 J/cm2, an oxidized amorphous layer up to 75 nm thick forms on the surface, under which a crystalline layer with an As concentration exceeding the solubility limit, is detected. It is found that As diffusion into the single-crystal substrate occurs only upon melting of the latter (threshold >1,0 J/cm²) and increases with decreasing the amorphous film thickness and increasing the number of pulses. Moreover, evaporation of the material leads to a loss of up to 20% As and the formation of craters up to 100 nm deep, which is associated with the release of Ar bubbles. It was found that the minimum surface resistance (<10 Ω/□) is achieved with three pulses and a thickness of 50-100 nm, corresponding to the maximum electrical activation of the impurity. Diode structures with a saturation current density of 6,5⋅10-10 A/cm² and a leakage current density of 2,5⋅10-8 A/cm2 were formed using laser annealing, demonstrating the potential of this method for creating shallow p-n junctions.
Keywords: laser processing, amorphous films, impurity concentration, film thickness, diffusion, substrate, energy density, surface resistance, doped layer.

Nalimova S.S., Shomakhov Z.V., Kotlyarova V.S., Krasnikova M.M., Makarova O.G., Bui C.D., Rybina A.A., Buzovkin S.S.
Synthesis of hierarchical structures based on zinc oxide nanowires and metal-organic frameworks – page 722
Abstract: The paper discusses approaches to creating hierarchical structures based on zinc oxide nanowires modified with metal-organic framework ZIF-8. The study is relevant because it aims to improve functional properties of gas sensors and photocatalysts by increasing their specific surface area and number of active sites. Zinc oxide nanowires produced using the hydrothermal method allow for directional charge carrier transfer, while the ZIF-8 shell with its high porosity and selective adsorption capacity acts as a molecular filter. Synthesis of these composites was conducted using the solvothermal method in ethanol and dimethylformamide solvents, followed by heat treatment. The morphology, phase composition, and elemental distribution of the samples were analyzed using scanning electron microscopy, X-ray diffraction, and energy-dispersive X-ray spectroscopy. It has been found that annealing at 500°C causes the decomposition of ZIF-8 and formation of only the zinc oxide phase. The synthesis in dimethylformamide and annealing at 320°C allow us to preserve both phases and achieve a uniform coating of nanowires with a layer of the framework. However, aggregation of particles and loss of the original nanowire morphology have been observed. It has been shown that it is necessary to optimize the synthesis conditions in order to preserve the individual shape of the nanorods and ensure the availability of the active sites.
Keywords: zinc oxide, ZIF-8, hierarchical structures, solvothermal synthesis, nanocomposites.

Parashchuk A.V., Sheshin E.P.
Thermal desorption kinetics of titanium and titanium-vanadium gas absorbers – page 730
Abstract: The processes of gas release from titanium and titanium-vanadium getter materials used in electrovacuum devices were studied using thermodesorption spectroscopy. Two consecutive heating cycles were performed at a rate of 5°C/min, followed by an isothermal annealing at the end of the heating process. The activation energies of desorption for H2, H2O, CO2 and CH4 were calculated using the Redhead method. It has been shown that during secondary heating after 5 days of keeping in a vacuum, the hydrogen peaks are restored, some new high-temperature water peaks appear, and methane is formed, which was not present during the primary heating. For the Ti-V alloy, all desorption processes are shifted to lower temperatures (maximum of 550°C) with an activation energy of 2,52 eV compared to 3,62 eV for pure titanium. It has been established that during exposure at room temperature, getters sorb hydrogen, oxygen, and carbon-containing gases from the residual atmosphere, and the sorbated components enter into chemical interaction.
Keywords: thermodesorption spectroscopy, getter, titanium, titanium-vanadium alloy, activation energy, desorption, sorption, electrovacuum devices, Redhead method.

Pervikov A.V., Svarovskaya N.V., Glazkova E.A., Ryumin E.E., Suliz K.V., Kazantsev S.O., Lerner M.I.
Electroexplosive synthesis of micro- and nanoparticles of high-entropy alloys NiFeCoCrCuAl and NiFeCoCrCuMo for extrusion 3D printing with granules – page 740
Abstract: High-entropy alloy powders were synthesized for the first time as a homogeneous micro/nanoparticle mixture via the co-electrical wire explosion of various metals and alloys. Scanning electron microscopy and X-ray diffraction determined the particle size distribution and crystal structure, revealing the critical effect of wire explosion energy parameters on the particle phase formation. The particle size distribution was found to be bimodal, with particle sizes varying from 30 nm to 15 µm. The crystal structure of the particles corresponds to substitutional solid solutions with fcc and bcc lattices. The powders were compounded into oxidized polyethylene wax and polymethyl methacrylate granules. Granules containing 50 vol.% alloy particles were extrusion-printed into block structures with straight and gyroidal channels. Structural characterization of the sintered components showed that the crystal structure consists of substitutional solid solutions with fcc and bcc lattices. Compression tests indicated that the ultimate strength is comparable to the characteristic values of the austenitic Cantor alloy family.
Keywords: nanoparticles, high entropy alloy, exploding wires, fused granular fabrication, shunting discharge, current, voltage.

Pervikov A.V., Sagun A.I., Ryumin E.E., Suliz K.V., Lerner M.I.
Synthesis and thermal stability of high-entropy oxide (CuZnNiCoFeCrAl)xOy nanoparticles obtained by joint exploding wires – page 751
Abstract: For the first time, a high-entropy oxide nanoparticle-based powder was synthesized via a single-step method based on the co-electrical explosion of various metal/alloy wires in an oxygen-containing atmosphere. The particle size distribution and crystal structure were characterized using transmission electron microscopy and X-ray diffraction analysis. It was shown that particle sizes varied from 10 nm to 3 μm. The particles exhibited a spherical morphology with a relatively uniform distribution of metals throughout their volume. Their crystal structure was represented by spinel and rock-salt phases. Thermal stability of the powder was also investigated. Sintering at 800°C was found to lead to the emergence of weak reflections of the CuO phase. Increasing the sintering temperature to 1000°C resulted in grain growth up to 2-5 μm and the formation of distinct copper-enriched grains. The synthesized powder was used to prepare polymer pellets for the extrusion-based 3D printing of high-entropy oxide ceramic products. The obtained pellets were applied to print a block structure with gyroidal channels. The results of this study demonstrate that co-electrical explosion of wires made of different metals/alloys enables the production of particles with a controlled structure and elemental composition. Tailoring the structure, elemental composition, and metal segregation both during particle synthesis and during sintering of the extrusion-printed part opens new avenues for developing ceramic products with novel or enhanced functional properties.
Keywords: nanoparticles, high-entropy oxide, aluminum oxide, thermal stability, segregation, electrical explosion of wires, current, spinel, rock-salt, gyroid structure.

Skachkov V.M., Bibanaeva S.A., Sabirzyanov N.A.
Change in properties of diffusion-hardening composite solder when modified with stainless steel powder – page 761
Abstract: The article discusses changes in the structure and microhardness of diffusion-hardening solder based on low-melting alloy gallium (68%) -indium (23,5%) -tin (8,5%) and a solid component from copper-tin alloy powder (5%) depending on the dosage of stainless steel powder. Stainless steel powder was added in an amount of 5, 10, 15, 20% by weight, solder samples were heat treated at temperatures of 125 and 600°C, and compared with a base solder composition of 30% by weight of gallium-indium-tin alloy and 70% by weight of copper-tin alloy powder. The X-ray phase analysis method determines the phases formed as a result of the interaction of solder components under different heat treatment modes. The method of differential thermal analysis revealed thermal effects in the formation of solid solutions and intermetallic compounds of gallium with transition metals in the temperature range of 17-600°C. It has been shown that thermal treatment at temperatures above 450°C promotes the transition of the solder to an equilibrium state, which leads to an increase in hardness, in particular, due to the uniform distribution of nanoscale inclusions. Scanning electron microscopy revealed that stainless steel has limited solubility in the composition of diffusion-hardening solder, but after high-temperature treatment (600°C) reduces its hardness due to violation of the composition of the gallium-copper solid solution.
Keywords: composite diffusion-hardening solders, metal powder, properties, microhardness, differential thermal analysis.

Fedotov A.Yu., Severyukhina O.Yu., Salomatina A.Yu.
Investigation of magnetic properties of cobalt nanofilms and their potential for spintronic device applications – page 771
Abstract: In this study, performed using a hybrid method of molecular dynamics and spin modeling within the LAMMPS software package with the SPIN module, the influence of the thickness of crystalline cobalt films on their magnetic properties was investigated. The thickness varied from 1,8 to 7,1 nm. It is shown that the film thickness significantly affects its magnetic behavior due to the interplay between surface and bulk effects. In ultrathin films (less than 4,5 nm in thickness), inhomogeneity of the magnetic response is observed. This is attributed to the dominance of the surface effects and atomic-scale roughness, which creates local demagnetizing fields. As a result, domain walls behave chaotically, leading to some stepwise changes in the magnetization and inhomogeneity of its distribution. The normalized magnetic energy is the highest in such films. At thicknesses of 4,5-7,1 nm, the films exhibit the bulk magnetic behavior. Reducing the proportion of surface atoms allows the bulk properties of cobalt to dominate. The magnetization becomes more stable, and its distribution becomes uniform. The magnetic energy, normalized to the number of atoms, approaches a value characteristic of bulk cobalt. A direct proportionality was observed between this energy and the proportion of the surface atoms, clearly indicating the decisive contribution of the surface to the formation of increased energy and spatial heterogeneity of magnetic properties at the nanoscale. The obtained data can be used in the creation of spintronic elements and magnetic recording devices.
Keywords: mathematical modeling, thin films, cobalt, molecular dynamics, spin dynamics, ferromagnet, magnetic properties.

5. NANOCHEMISTRY – page 787

Bernatskii D.P., Pavlov V.G.
Changes in the mass composition of alkali metal clusters caused by the geometry of the field source surface changes – page 787
Abstract: The effect of the surface structure of a metallic crystal on the formation of clusters of alkali metal atoms adsorbed on the surface has been studied. The study was carried out using field electron microscopy, field desorption microscopy, and time-of-flight mass analysis of ions desorbed by an electric field. Crystals of tungsten and rhenium were used as substrates. The adsorbates were sodium, potassium, and cesium. Alkali metal atoms were deposited on the surface of a tungsten or rhenium field emitter from an external spray. The experiments were carried out in an ultrahigh vacuum (p < 10-9 Torr). To determine the masses, pulsed field desorption of clusters from the surface and measurement of the time of flight of ionized clusters from the sample surface to the detector were performed. As a result of the measurements, clusters containing up to seven atoms were detected. To determine the effect of the structure of metal crystals on the number of atoms in clusters, a metal crystal was heated in an electric field (thermal field treatment). As a result of this treatment, the shape of the tip and the structure of its surface changed. The number of crystal steps decreased until they completely disappeared, and the crystal shape gradually shifted from a rounded shape close to a hemisphere (annealing shape) to a polyhedron shape. The cluster composition was measured at different stages of the transition from a round crystal shape to a polyhedron, and, accordingly, with a different number of steps on the surface. As the number of steps decreased, so did the number of atoms in the cluster. Only monatomic clusters were formed on the surface of a sample completely faceted with densely packed crystal planes without steps. From the experimental results obtained, it can be concluded that the formation of clusters of alkali metal atoms on the metal surface requires the presence of crystalline steps on the surface.
Keywords: field desorption, cesium, potassium, sodium, tungsten, rhenium, electric field, ion clusters.

Bespalov D.V., Golovanova O.A.
Quantum-chemical calculation of the zinc(II) glycine complex: synthesis, structure, properties, determination of stability constants – page 800
Abstract: The combined application of quantum-chemical methods of density functional theory (DFT/B3LYP) with the 6‑31G(d,p) basis set and the semiempirical GFN2‑xTB method allowed to construct a reliable model of an isolated molecule of the zinc glycine complex. The structure was optimized, and the thermodynamic characteristics and infrared spectrum of the studied complex were calculated. Using potentiometric titration according to the Calvin-Melchior method, the stability constants of the complexes in the zinc–glycine system were determined. The ZnGly2 complex was synthesized. The 1:2 molar ratio was confirmed by complexometric and formol titration methods. The infrared spectra of the synthesized compound are presented. A comparison of the experimental and theoretical infrared spectra confirmed the reliability and consistency of the selected quantum-chemical methods. X‑ray phase analysis was used to determine the probable composition of the complex, and the unit cell parameters were calculated using the dichotomy method. The presence of a water molecule in the crystal lattice was confirmed by calculating the van der Waals volumes of atoms, and the average crystallite size was determined using the Scherrer method. The obtained data expand the understanding of the coordination chemistry of zinc and provide a basis for the rational design of bioactive compounds aimed at regulating homeostasis. These data can be used in medicine to prevent pathologies associated with impaired zinc metabolism and the formation of some nanoscale aggregates.
Keywords: synthesis, amino acids, zinc complexes, glycine, density functional method, molecular simulation.

Burlakov E.S., Vishnevetskii D.V., Polyakova E.E., Averkin D.V., Efimov A.A., Aleshina M.Yu.
The study of the interaction of L-cysteine methyl ether with silver salts – page 811
Abstract: In this work, the effect of silver salts on the self-assembly process in aqueous solutions of L-cysteine methyl ester hydrochloride was studied using UV–visible spectroscopy, dynamic light scattering, electrophoretic light scattering, pH measurements, transmission electron microscopy, and selected-area electron diffraction. The nitrate- and acetate-based systems remained visually stable after storage in the dark for 2 months, whereas the nitrite-based systems began to precipitate after several days. The UV-visible spectra showed no characteristic absorption bands and no pronounced scattering region, indicating the stability and homogeneity of the samples. According to the zeta-potential values, the solutions with L-cysteine methyl ester hydrochloride:silver salt ratios of 1:1,5 and 1:1,75 were the most stable in both systems. The dynamic light scattering results showed that only a small number of nanoparticles formed under conditions of silver ion deficiency, whereas an excess of silver ions produced sufficient scattering intensity for reliable particle-size determination. The pH measurements revealed different trends for the acetate- and nitrate-based systems. transmission electron microscopy and selected-area electron diffraction data showed that the obtained systems form predominantly amorphous, polydisperse, spherical nanoparticles ranging from 5 to 60 nm in size, with some particles reaching approximately 200 nm.
Keywords: L-cysteine methyl ester, silver nitrate, silver nitrite, silver acetate, self-assembly, nanostructured systems.

Vishnevetskii D.V., Polyakova E.E., Averkin D.V.
Cysteine-silver sol at different pH: the influence of the chemical nature of silver salts – page 823
Abstract: The effect of the chemical nature of silver salts (silver nitrate, silver nitrite, silver acetate) used as a precursor in the synthesis of cysteine-silver sols on their behavior at different medium acidities has been investigated. It has been shown that all sols, regardless of the chemical nature of the precursor, have an isoelectric point, the value of which depends on the history of sample preparation — the chemical nature of the silver salt. This behavior is associated with the presence of amino and carboxyl groups located on the surface of cysteine-silver sol nanoparticles. Based on previous results and the data obtained in this work, a structure of the nanoparticles forming the corresponding sol has been proposed.
Keywords: cysteine-silver sol, pH, isoelectric point, turbidity, zeta-potential.

Golovanova O.A., Afanasiev D.A.
Search for corrosion inhibitors of magnesium alloy in simulated biological fluids – page 832
Abstract: A study was conducted on the corrosion rate of the MA20 alloy in a simulated synovial fluid. Currently, there is an increase in the number of injuries and diseases requiring the use of surgical implants. Traditionally, titanium and other metallic structures are used for these purposes; however, after fulfilling their function, they often must be removed via a secondary surgery. Implants based on magnesium and its alloys represent a promising alternative. Magnesium is a biodegradable material that gradually degrades in the body, thereby eliminating the need for a follow-up surgical intervention. Furthermore, the mechanical properties of magnesium alloys are close to those of human bone tissue. However, the widespread application of magnesium alloys is limited by their high corrosion rate in physiological environments. If an implant degrades too rapidly, it loses its mechanical strength before the bone tissue healing is complete. This can lead to the necessity of an emergency implant replacement, additional financial costs, and prolonged patient treatment time. In this work, a series of protective coatings of various types was obtained, and their effect on the corrosion rate was evaluated. Analysis of our experimental results demonstrated that the most effective coating among those obtained was the one formed from hydroxyapatite. Apatite forms a dense insulating layer and protects the surface from the corrosive environment, which contributes to a significant reduction in corrosion, achieving a protection efficiency of 70,4%. The results of this study open new horizons for further research of the synthesis of new nanobiocomposites on the surface of magnesium alloys widely used in the development of new implants.
Keywords: magnesium, corrosion, synovial fluid, corrosion depth indicator, protective coating.

Zaporotskova I.V., Boroznin S.V., Dryuchkov E.S., El Zanin A.R., Zaporotskov P.A., Boroznina N.P.
Study of functionally modified carbon nanotubes with respect to carbon dioxide – page 842
Abstract: In this study, the sensory properties towards carbon dioxide of nanocomposites, which are carbon nanotubes with metal oxides attached to it, was studied. The study focused on the geometry and stability of adsorption complexes and the changes in the physicochemical properties (the energy gap and charge distribution) of nanostructures caused by adsorption processes. This research was conducted using computer experiments based on calculations performed with density functional theory methods and a quasi-molecular approach. The results of the computer experiment allowed us to estimate the change in the adsorption energy and the band gap. Based on this analysis, presented below, iron oxide was selected as the most effective material in terms of the adsorption energy (from 0,17 to 0,23 eV), this materials have a sufficiently strong response (in the best case the energy gap decreases from 1,644 to 1,622 eV) and, consequently, a high sensitivity to carbon dioxide. Response in the case of the carbon nanotubes (6,6)-cobalt oxide is significantly stronger (the energy gap decreases from 1,54 to 1,45 or 1,34 eV depending on the adsorption distance), but the strong interaction between composite and carbon dioxide could cause poisoning the sensor. The carbon nanotubes-copper oxide composite is characterized by weak response and, consequently, low sensitivity towards carbon dioxide. The results obtained reveal important physicochemical patterns of interaction between carbon nanotubes and metal oxides composites and carbon dioxide. These findings are significant in terms of the sensitivity and reproducibility of chemical sensors measurements, making them crucial for the development of nanoscale gas sensors.
Keywords: carbon nanotubes, metal oxides, carbon dioxide, gas sensing, density functional theory, energy gap, charge distribution.

Kozhevnikova N.S., Bogdanova E.A., Skachkov V.M., Chufarov A.Yu., Yushkov A.A., Baklanova I.V., Avdeeva Y.A.
Production of a titanium-containing composite material with a wide spectrum of action based on ultradisperse hydroxyapatite – page 857
Abstract: The aim of this work was the sol-gel synthesis of promising titanium-containing composite materials based on nanosized hydroxyapatite (the titanium content in the final product, calculated as TiO2, is 10-40 wt.%). A comprehensive study of the composition and structure of the obtained materials was carried out using modern physicochemical analytical methods: X-ray diffraction and energy-dispersive X-ray analysis, Raman spectroscopy, scanning and transmission electron microscopy. The surface characteristics of the studied samples were evaluated using the Brunauer-Emmett-Teller method. Based on the specific surface area and pycnometric density data, the average surface diameter of the particles was calculated. A correlation was revealed between the amount of introduced titanium and the crystal lattice parameters of the sample, the band gap, the surface characteristics, the density and morphology of the obtained materials, demonstrating the promise of their further research for the purpose of practical application both as ceramic materials for medical purposes and as photocatalysts.
Keywords: hydroxyapatite, titanium-containing hydroxyapatite, synthesis, precipitation from solution, sol-gel method, titanium oxide, functional materials.

Krut’ko V.K., Maslova L.Yu., Musskaya O.N., Krutsko E.N., Glazov I.E., Safronova T.V., Kulak A.I.
Hydrothermal and solvothermal syntheses of calcium phosphates in the form of cotton wool – page 868
Abstract: The physicochemical properties and microstructure of fibrous calcium phosphates in the form of cotton-wool-like nanofibers were studied. The phosphates were obtained by: 1) hydrothermal synthesis in the presence of a 1 M urea solution during 18-52 hours of boiling at 90°C, 2) solvothermal synthesis in the presence of calcium oleate at 180°C during 5 hours of autoclaving. Under hydrothermal conditions, a single-phase octacalcium phosphate with a fibrous microstructure was synthesized, which dries at 37°C in a cotton-wool-like form, and after annealing at 800°C, it crystallizes predominantly into β-tricalcium phosphate with 20% β-calcium pyrophosphate. Amorphized hydroxyapatite was obtained by solvothermal synthesis. At 60°C, it dries to soft conglomerates and, after annealing at 800°C, crystallizes into hydroxyapatite with 20% β-tricalcium phosphate. The formed loose calcium phosphate precipitates must be repeatedly washed to remove urea or oleate. Calcium phosphate wool obtained by various methods is represented by long, thin, randomly oriented nanofibers up to 1 nm wide and 4-6 nm in diameter. In samples with a short boiling time of up to 18 hours, near-spherical nuclei up to 10 nm in diameter were visualized, from which nanofibers form and grow. Increasing the boiling time to 52 hours, the synthesis temperature to 180°C, and annealing at 800°C lead to shortening and thickening of the nanofibers to 10-40 nm and an increase in the nucleus size to 18 nm. This synthesis method allows for the control of the phase composition and the required degree of bioresorbability of calcium phosphate wool. Synthetic calcium phosphate wool with a voluminous fibrous microstructure and the ability to be absorbed due to soluble forms of calcium phosphates can be used in bone tissue engineering with drug delivery or as temporary absorbable barriers.
Keywords: fibrous calcium phosphates, hydrothermal synthesis, octacalcium phosphate, solvothermal synthesis, hydroxyapatite, calcium phosphate wool.

Menshikov S.Yu., Kurmacheva V.S., Fedorov S.A., Malyshev A.N., Mikushina Yu.V., Shishmakov A.B., Tumashov A.A., Permyakova A.E., Ostroushko A.A.
Liquid-phase oxidation of ethylene glycol with hydrogen peroxide using nanostructured silver catalysts – page 877
Abstract: The catalytic activity of nanoscale silver-containing compositions in the oxidation of ethylene glycol with hydrogen peroxide, as well as the selectivity of the processes, were studied. The reactions were carried out at a temperature of 60°C using L-micro laboratory setup The degree of ethylene glycol conversion was determined by gas chromatography. The composition of the ethylene glycol oxidation products and, in addition, the oxidation products of glyoxal upon reaction with H2O2 in the presence of the same nanoscale silver-containing samples were determined by liquid chromatography and nuclear magnetic resonance spectroscopy. For comparison, colloidal silver samples and nanoscale silver samples supported on a carbon material and on a mineral support (aluminum oxide) were used as catalysts in the reactions investigated. It was established that, under the same catalyst-to-substrate mass ratio and identical conditions, the conversion of ethylene glycol was higher in the presence of the colloidal silver samples. Comparing the catalytic activity of the silver samples supported on aluminum oxide and on a carbon material, the conversion of ethylene glycol in the presence of the carbon–silver catalyst was found to be lower. Under the studied conditions of catalytic liquid-phase oxidation of ethylene glycol on silver samples of various types, the main oxidation product in the presence of an excess of the oxidant was oxalic acid.
Keywords: nanoscale silver, catalytic properties, oxidation, hydrogen peroxide, gas and liquid chromatography, nuclear magnetic resonance spectroscopy, kinetics.

Musskaya O.N., Krut’ko V.K., Aniya V., Patra Ch., Krutsko E.N., Doroshenko A.E., Glazov I.E., Pant Sh., Batsh Ch., Majeed H., Nagchowdhury P., Kulak A.I.
Film polymeric carriers of sodium carboxymethylcellulose and polyvinyl alcohol for the immobilization of nanosized calcium phosphates – page 887
Abstract: The formation features of interpolymer complexes from 0.4-7.0% aqueous solutions of sodium carboxymethyl cellulose and polyvinyl alcohol were studied. Film polymer materials were developed based on the sodium carboxymethyl cellulose / polyvinyl alcohol interpolymer complexes using the casting method. Film materials based on sodium carboxymethyl cellulose are highly soluble in aqueous media with pH of 5-7 and are more hydrophilic compared to polyvinyl alcohol and sodium carboxymethyl cellulose / polyvinyl alcohol. The possibility of increasing hydrophobic properties, as well as regulating the degree of resorption of sodium carboxymethyl cellulose / polyvinyl alcohol film composite materials, depending on their composition and heat treatment at 85ºC was demonstrated. Thermal analysis showed that the highest stability in the temperature range of 200–800ºC is characteristic of sodium carboxymethyl cellulose and sodium carboxymethyl cellulose / polyvinyl alcohol (1:1) samples. Additional treatment at 85°C for 1 hour improves the thermal stability of the materials; however, increasing the treatment time to 2 hours reduces the thermal stability of the samples. The resulting film materials are cytocompatible and hold promise as resorbable carriers for the immobilization of nanosized calcium phosphates and other bioactive components.
Keywords: film polymer materials, interpolymer complex, sodium carboxymethylcellulose, polyvinyl alcohol, calcium phosphates.

Pirogov M.A., Blinov A.V., Samovolov A.V., Tatov A.V., Rekhman Z.A., Bocharov N.M.
Investigation of the process of stabilization of nanoparticles of mixed iron oxide by beta-glucan – page 897
Abstract: In this work, samples of mixed iron oxide nanoparticles stabilized with beta-glucan were prepared by chemical precipitation in an aqueous medium from iron (III) chloride and iron (II) sulfate using ammonia as the precipitating agent. This material is of interest due to its magnetic and biocompatible properties, as well as to combination of a magnetite core and a polysaccharide shell. The Fourier transform infrared spectroscopy and diffuse reflectance spectroscopy studies were conducted, along with quantum chemical computer modeling of the elementary act of interaction of beta-glucan with iron (II) and iron (III) oxides using the QChem software. The modeling revealed that the interaction of the beta-glucan site with iron oxides is energetically favorable (the difference in the total energy of beta-glucan and the elementary act of interaction is > 1335 (for iron (II)) oxide and > 2744 kcal/mol (for iron (III) oxide)) and chemically stable (chemical hardness of 0,140-0,161 eV and 0,156-0,170 eV, respectively), with the optimal interaction being via the hydroxyl group attached to C3 of the B-linked glucopyranose residue. Infrared spectral analysis confirmed this mechanism: the intensity of the hydroxyl stretching band in the spectrum of stabilized nanoparticles is reduced compared to that of pure beta-glucan, while the appearance of a Fe–O stretching band in the 533-656 cm–¹ region confirms the formation of a magnetite crystal lattice. Analysis of the diffuse reflectance spectrum revealed that the optical properties of the sample in the visible region are determined predominantly by mixed iron oxide, with an absorption band at 450-600 nm associated with the electron transitions of Fe2+ and Fe3+ ions.
Keywords: nanoparticles, iron oxide, beta-glucan, quantum chemical modeling, diffuse reflection, Fourier transform infrared spectroscopy.

Provorkina A.A., Golovanova O.A.
Patterns of calcium phosphate degradation in lactic acid – page 908
Abstract: Modern regenerative medicine and dentistry are in urgent need of mild methods for the degradation of calcium phosphate deposits, as well as the development of biodegradable composite materials based on polylactic acid and apatites. In this context, fundamental studies on the degradation of apatites in lactic acid are of paramount importance for optimizing the synthesis of biodegradable implants and developing caries prevention strategies. The aim of this study was to determine the thermodynamic and kinetic parameters of the interaction between hydroxyapatite (fluorapatite) and lactic acid, as well as to elucidate the underlying reaction mechanism. The degradation processes were investigated using thermodynamic modeling, direct potentiometry, and X-ray diffraction analysis. Based on the performed calculations, thermodynamic surfaces were constructed, and the critical acidity thresholds at which apatite dissolution becomes thermodynamically unfavorable were established: the maximum pH values were found to be 5,2 for hydroxyapatite and 4,5 for fluorapatite. Experimental results demonstrate that the maximum degradation rate is achieved in a strongly acidic medium, where the active protonated form of lactic acid predominates in the solution. It was revealed that the system reaches equilibrium rapidly due to a self-inhibition effect, which corresponds to crystals reaching a critical nanoscale size limit by the crystals. A reaction mechanism is proposed, involving the protonation of the phosphate groups within the crystal lattice followed by the chelation of the released Ca2+-ions by lactate anions, which effectively prevents kinetic inhibition of the process. The obtained data provide a solid foundation for developing methods for the controlled resorption of biodegradable implants and dental materials.
Keywords: hydroxyapatite, fluorapatite, lactic acid, resorption, thermodynamic modeling.

Prudchenko A.P., Poliakova O.Yu., Protasevich J.S.
Influence of the nature of the organo-ligand complex of transition metals and thermochemical activation on the effectiveness of metal oxide catalysts for carbon nanotube growth in the CVD process – page 917
Abstract: This paper presents the results of a study of the effect of the nature of organic ligands, the composition of organo-ligand complexes of 3d-metals, and the conditions of their thermal degradation in the synthesis of metal oxide catalysts for the growth of carbon nanotubes on their effectiveness of the processes of catalytic chemical deposition of carbon from the gas phase. Metal oxide catalysts were synthesized using a technique combining the approaches of polymerized complex precursors, the chelation method of sol-gel technology, as well as thermal decomposition and thermochemical activation of the carrier. It has been established that the effectiveness of catalysts of the general composition Me2CO/CaCO3 (Me–Fe, Ni) in the CCVD synthesis of carbon nanotubes depends both on the nature of organic ligands of transition metal complexes and on the composition of active metals. The effect of the structure of the ligands used in the synthesis of metal oxide catalysts for both the Fe–Co and Ni–Co combinations is similar and consists in increasing the effectiveness in the following sequence: glycols < polyglycols < polyalcohols < carbohydrates (mono- and disaccharides) < branched polyalcohols (pentaerythritol). Replacing Fe with Ni in the organo-ligand complex can significantly reduce the optimal process temperature from 800°С to 500°С, as well as increase the specific yield of the carbon product. Based on the results of the analysis of temperature dependences using the example of catalysts where the ligands were sucrose, fructose, pentaerythritol and citric acid, it was assumed that the decrease in productivity observed with increasing temperature may be due to an increase in the mobility of catalytic particles, their agglomeration, sintering and, as a result, loss of activity. It has been established that, in case of significant excess, organic ligands can play the role of additional fuel in the process of thermochemical activation of the carrier, affecting its morphology, composition, surface texture, and energy efficiency.
Keywords: carbon nanotubes, metal oxide catalysts, organic ligands, chelates, CVD synthesis, carbon nanomaterials.

Pshukov A.M., Kokoeva A.A., Ermolenko D.N., Akhmedova Kh.R., Shokumova M.U., Shogenova M.M.
Spectral-luminescent properties of Nd-containing perovskite quantum dots in a pseudocumene matrix and the effect of 2,5-diphenyloxazole – page 926
Abstract: It has been experimentally demonstrated that Nd-containing mixed-halide perovskite quantum dots retain an optically active luminescent state after incorporation into a pseudocumene matrix. Dilutions of the dispersion at 1:10, 1:20, and 1:30 were compared without 2,5-diphenyloxazole and with 2,5-diphenyloxazole at a concentration of 2 g/L. Emission spectra and excitation-emission matrices were recorded under identical settings. In all compositions, a dominant band at 501,5-505,5 nm was observed and 2,5-diphenyloxazole changed the peak position by no more than 1,0 nm. Upon addition of PPO, the maximum intensity and the band area decreased by 2,2 and 2,3% for 1:10, by 20,3 and 15,9% for 1:20, and by 48,8 and 35,3% for 1:30, respectively. Consequently, pseudocumene is a viable organic matrix for the quantum dots under study during photoluminescence diagnostics, whereas 2,5-diphenyloxazole at a concentration of 2 g/L does not sensitize their photoluminescence. This result establishes the conditions for further optimization but does not replace measurements of radioluminescence and γ-excited light yield.
Keywords: perovskite quantum dots, neodymium, pseudocumene matrix, 2,5-diphenyloxazole, photoluminescence, energy transfer, self-absorption, liquid organic scintillator.

Rekhman Z.A., Pirogov M.A., Blinov A.V., Samovolov A.V., Andiralov A.Yu., Oblogin Ya.A., Tatov A.V.
Study of properties of selenium nanoparticles stabilized with K-17 polyvinyl pyrrolidone – page 934
Abstract: In this work, samples of selenium nanoparticles stabilized with polyvinylpyrrolidone K-17 were obtained by chemical reduction of selenious acid with ascorbic acid in an aqueous medium in the presence of a stabilizer. The samples were studied by Fourier transform infrared spectroscopy, dynamic and electrophoretic light scattering. Computational quantum-chemical modeling of the interaction between polyvinylpyrrolidone K-17 and a selenium atom was performed using the QChem software package. The modeling results showed that the interaction of polyvinylpyrrolidone K-17 with selenium via the ionized amino group is energetically favorable (a decrease the total energy of 2397,942 kcal/mol) and chemically stable (the chemical rigidity of the molecular system is 0,160 eV). Analysis of the infrared spectra showed a match between the main diagnostic absorption bands of polyvinylpyrrolidone (3400, 1660, and 1460 cm-1) before and after stabilization of the selenium nanoparticles, with no new absorption bands appearing, indicating that the chemical structure of the polymer is preserved during synthesis. A study of colloidal stability by dynamic and electrophoretic light scattering over a pH range of 3-11, temperatures of 25-95°C, and holding times of 5-25 min showed that the average hydrodynamic diameter of the particles ranged from 45,44 to 197,67 nm, and the ζ-potential ranged from -6,05 to -83,06 mV, with the system exhibiting the highest stability in an alkaline medium at 25°C and the lowest stability in an acidic medium and at elevated temperature (95°C).
Keywords: selenium nanoparticles, polyvinyl pyrrolidone, quantum chemical modeling, infrared spectroscopy, colloidal stability.

Ryashentsev D.S., Polyakov D.S., Chernikov N.V.
Temperature-catalytic control over the formation of a layered sp/sp2-carbon nanomaterial under palladium-free Sonogashira cross-coupling conditions – page 943
Abstract: The possibility of replacing the palladium catalyst with 3d metals (iron, cobalt, nickel, and copper) in the synthesis of a layered sp/sp2-carbon nanomaterial via the Sonogashira cross-coupling reaction has been investigated. Acetates of the corresponding metals were used as precatalysts, o-phenanthroline served as the ligand, and copper iodide as the cocatalyst. The synthesis was carried out in dimethyl sulfoxide at 100℃ and 140℃ for 24 hours under an argon atmosphere using hexaiodobenzene and calcium carbide as sources of aromatic and acetylenic fragments. The products were subjected to multi-stage purification, including sequential washing with solutions of ammonium chloride, nitric acid, and sodium thiosulfate, followed by thermal treatment at 200℃. Using X-ray diffraction, infrared and Raman spectroscopy, it was established that the synthesis temperature and the nature of the transition metal jointly determine the structural characteristics and the degree of defectiveness of the final material. Raman spectroscopy confirmed the presence of acetylenic bridges between benzene rings. The ratio of the D– and G–band intensities varies from 0,17 to 0,31, indicating a tunable defectiveness of the sp2 matrix, while the IY/IG intensity ratios vary from 0,06 to 0,13. The obtained results demonstrate the fundamental possibility of temperature-catalytic control over the structure of graphyne-like materials without the use of a palladium catalyst.
Keywords: γ-graphyne, Sonogashira reaction, palladium-free catalysis, transition metals, layered nanostructures.

Sabirzyanov N.A., Bogdanova E.A., Skachkov V.M., Bibanaeva S.A., Medyankina I.S.
Influence of synthesis method on functional characteristics of materials based on ultradispersed hydroxyapatite – page 954
Abstract: The aim of this work was the autoclave production of ultradispersed hydroxyapatite and by-products of the synthesis, in particular a calcium hydroxyapatite-pyrophosphate material, also suitable for the manufacture of pharmaceutical compositions, drugs, and preparations. In the course of the work, the obtained compounds were certified using modern physicochemical methods: X-ray phase analysis, differential thermal analysis, scanning electron microscopy, etc. The effect of the synthesis method on functional characteristics of autoclave hydroxyapatite (phase stability, thermal stability, etc.) was assessed and a comparison of the experimental data with the properties of hydroxyapatite obtained by precipitation from solution was carried out. The possibility of using the materials obtained by the autoclave method as high-temperature bioceramics was investigated. Data were obtained on the effect of firing temperature on the linear parameters, weight loss and strength characteristics of the samples. Compliance of the compressive strength limits of the studied samples with the requirements for implant materials was also assessed.
Keywords: biomaterials, hydroxyapatite, synthesis, autoclave, precipitation from solution, functional properties, strength characteristics.

Suliz K.V., Pustovalov A.V., Lerner M.I., Pervikov A.V.
Influence of electrophysical and thermodynamic parameters of electroexplosive synthesis on the crystal structure and dispersed composition of multicomponent NiFeCoCrCuAlMoW nanoparticles – page 966
Abstract: Using NiFeCoCrCuAlMoW alloy as example, the effects of the energy input into the wires and the thermal conductivity of the buffer gas on the average size and phase composition of particles forming in He, N2 and Ar were studied for the first time. The average size of nanoparticles increases in the series He < N2 < Ar, which is due to a decrease in the thermal conductivity of the gas and an increase in the residence time of the metal vapor in a state favorable for coalescence. The particles obtained in He at lower values of Eint/Esub have a smaller size compared to the particles obtained in N2 at higher values of Eint/Esub. The obtained samples are characterized by the presence of FCC and BCC phases corresponding to substitutional solid solutions, as well as a BCC phase of a refractory metal-based substitutional solid solution and intermetallic with a µ-phase structure. The relationship between the phase composition of the samples, and the synthesis parameters revealed an ambiguous dependence. The obtained results did not confirm a direct dependence between the energy input into the wires and the content of the refractory metal-based bcc substitutional solid solution phase in the samples. On the basis of the findings, we have concluded that several independent processes occur during the formation of the phase composition of multicomponent nanoparticles obtained by the electrical explosion of wires.
Keywords: Nanoparticles, high-entropy alloy, electrical explosion of wires, current, segregation, intermetallic compound, solid solution, shunting discharge.

Shamsutov I.V., Pasechnik L.A., Merkulov O.V.
Phase and structural evolution of red muds during chemical looping reforming of methane – page 976
Abstract: The accumulation of red mud – a large‑tonnage waste from alumina production – poses a serious environmental challenge: with an annual waste output exceeding 150 million tons, the global utilisation rate remains below 5%. At the same time, the polymetallic oxide composition of red muds (Fe2O3 up to 45–49 %, Al2O3, SiO2, CaO, TiO2, Na2O) provides opportunities for their use as oxygen carriers in chemical reforming of methane, thereby combining waste utilization with syngas production. Two types of materials were investigated: the original red mud from the Bogoslovsk Aluminum Smelter and a magnetite‑enriched mud with reduced aluminum content, obtained by hydrothermal leaching of the original red mud. Granules (3-5 mm) prepared by sintering at 1050°C were tested in cyclic «methane reduction – air oxidation» runs at 900°C in a fixed‑bed reactor; the evolution of phase composition and microstructure was monitored. It is established that, during cycling, iron oxides are reduced to metallic Fe, while aluminosilicate phases (gehlenite Ca2Al2SiO7, CaFeAlSiO6) acted as structural stabilisers, preventing particle sintering. For red mud, a steady‑state regime with CH4 conversion of ~75% and CO selectivity of ~85-90% is reached after 6-7 cycles; for magnetite‑enriched mud this occurs after 10 cycles, which is attributed to larger aggregates of iron oxides and their sintering, as well as to the formation of a layered porous structure. At the same time, magnetite‑enriched mud exhibits a slightly higher overall oxygen capacity. In both cases, the H2/CO ratio in the products remains at 1,75-1,80. It is shown that the key factor for long‑term stability is the balance between the content of the active component (iron oxides) and the amount of aluminosilicate stabilizers. The obtained results open up prospects for the targeted modification of red mud composition to create efficient and durable oxygen carriers for cyclic hydrocarbon processing.
Keywords: bauxite residue of red mud, oxygen carriers, methane reforming, chemical looping, synthesis gas, magnetite, hematite, cyclic stability, structural evolution.

Shevchenko I.M., Yasnaya M.A., Blinova A.A., Prasolova A.V., Goncharov A.D., Glizhova T.N.
Hybrid materials based on d-element hexacyanoferrates modified with nanosized gold – page 985
Abstract: For the first time, we present the results of a study on the influence of the composition and ratio of components in the synthesis process of hybrid materials based on hexacyanoferrates (III) of d‑elements (cobalt, nickel, iron), modified with gold nanoparticles, on the elemental and phase composition of these hybrid materials and on the microstructure of their surface. According to the results of investigations using scanning electron microscopy and energy dispersive X-ray microscopy, it was found that gold was identified in samples of hexacyanoferrates (III) of d-elements (Co, Ni, Fe) containing from 0,1 to 5,0 masses.% gold. Analysis of the phase composition of samples of hexacyanoferrates of d‑elements (Co, Ni, Fe) modified with gold showed that the main crystalline phases were the corresponding hexacyanoferrates of d‑elements with a face‑centered cubic crystal lattice (Fm3m); impurity phases of mixed hexacyanoferrates were also present. According to the results of X‑ray phase analysis, the phases of metallic gold cannot be identified. The obtained experimental data will be useful for the development and use of promising materials based on hexacyanoferrates (III) of d‑elements (cobalt, nickel, iron) as sensitive elements in glucose sensors. Additional modification of the matrix of hexacyanoferrates (III) of d‑elements (cobalt, nickel, iron), for example, with nanoparticles of noble metals, helps to increase the conductivity, selectivity, and stability of composite materials when creating sensors for assessing blood glucose levels.
Keywords: hybrid nanomaterials, hexacyanoferrates of d‑elements, gold nanoparticles, elemental composition, phase composition, surface microstructure.

Yasnaya M.A., Blinova A.A., Shevchenko I.M., Prasolova A.V., Shipulin V.I., Torgunov V.P.
Preparation and study of properties of structured hexacyanoferrates of d‑elements doped with platinum nanoparticles – page 996
Abstract: In this work, samples of hexacyanoferrates of d-elements (Co, Ni, Fe) containing from 0,1 to 5 wt.% platinum were obtained. Scanning electron microscopy revealed that samples of hexacyanoferrates of d-elements (Co, Ni, Fe) doped with platinum were aggregates of various shapes with sizes from 1 to 70 microns, with clearly defined boundaries and a layered structure. The aggregates are formed by spherical nanoparticles with a size ranging from 10 to 70 nm. Analysis of the energy-dispersive X-ray spectroscopy spectra of samples of hexacyanoferrates of d-elements (Co, Ni, Fe) doped with platinum showed that platinum was identified in samples containing 1 to 5 wt.% Pt. At the same time, the actual platinum content in the materials differs from the theoretically calculated amount, which is due, firstly, to the reduction of some platinum ions in the solution volume and their removal during the sample washing process, and secondly, to the adsorption of platinum ions in the structure (channels) of hexacyanoferrates of d-elements. Analysis of the phase composition of samples of hexacyanoferrates of d-elements (Co, Ni, Fe) doped with platinum showed that the main crystalline phases were the corresponding hexacyanoferrates of d-elements with a face-centered cubic crystal lattice (Fm3m); impurity phases of mixed hexacyanoferrates were also present. Phases of metallic platinum are not identified on the diffraction patterns regardless of the concentration of the noble metal.
Keywords: structured hexacyanoferrates of d-elements, noble metal nanoparticles, doping with platinum nanoparticles, surface microstructure, elemental composition, phase composition.