Can the presence of a cavity alter the nature of structural transformations during a cycle of thermally induced treatment, taking Ag-Ni-Pd ternary nanoparticles as an example?

E.S. Mitinev, K.G. Savina, O.V. Polev, M.G. Gostintsev, A.Yu. Kolosov, D.N. Sokolov, I.A. Vzglyadov, I.S. Dmitriev, P.M. Ershov, N.Yu. Sdobnyakov

Tver State University

DOI: 10.26456/pcascnn/2026.18.271

Original article

Abstract: A comparative molecular dynamics study was conducted on equiatomic Ag-Ni-Pd ternary nanoparticles with two types of initial configurations: a nanoparticle containing a central cavity and a nanoparticle without a hollow core. A cycle of thermally induced treatment (heating and cooling) was performed at a rate of 0,3 K/ps. Specific features of the structural behavior of these objects during heating and subsequent melting were identified. In particular, the fraction of atoms forming a local hcp structure is significantly higher for the nanoparticle with a hollow core in the temperature range from 660 K up to the melting point. The temperature dependencies of specific internal energy during cooling are virtually identical for the two initial configurations; however, the process of nickel core formation exhibits distinct characteristics regarding the number of nucleated clusters and their subsequent internal coalescence. Furthermore, polyhedral template matching analysis reveals differences between the two initial configurations regarding the formation of local fcc and hcp environments by the constituent elements (Ag, Ni, Pd) of the ternary alloy at the end of the thermal cycle (at 300 K). Thus, the presence of an artificially created cavity or bulk defect in equiatomic Ag-Ni-Pd ternary nanoparticles influences not only the parameters of phase transitions associated with melting and crystallization but, to a greater extent, the patterns of chemical and structural segregation.

Keywords: molecular dynamics method, MDSym, tight-binding potential, ternary nanoparticles, cavity, phase transition, segregation, local structure

  • Egor S. Mitinev – 2nd year postgraduate student, General Physics Department, Tver State University
  • Kseniya G. Savina – 4th year postgraduate student, General Physics Department, Tver State University, ORCID: 0000-0002-4916-4968
  • Oleg V. Polev – 1st year postgraduate student, General Physics Department, Tver State University
  • Michael G. Gostintsev – 1st year graduate student, General Physics Department, Tver State University
  • Andrei Yu. Kolosov – Ph. D., Researcher, General Physics Department, Tver State University, ORCID: 0000-0003-3805-0567
  • Denis N. Sokolov – Ph. D., Researcher, General Physics Department, Tver State University, ORCID: 0000-0003-2411-0143
  • Ivan A. Vzglyadov – 4th year student, General Physics Department, Tver State University
  • Ivan S. Dmitriev – 4th year student, General Physics Department, Tver State University
  • Pavel M. Ershov – Junior Researcher, General Physics Department, Tver State University, ORCID: 0000-0002-7083-214X
  • Nickolay Yu. Sdobnyakov – Dr. Sc., Docent, Professor, General Physics Department, Tver State University, ORCID: 0000-0003-1749-0336

For citation:

Mitinev E.S., Savina K.G., Polev O.V., Gostintsev M.G., Kolosov A.Yu., Sokolov D.N., Vzglyadov I.A., Dmitriev I.S., Ershov P.M., Sdobnyakov N.Yu. Mozhet li nalichie polosti izmenit kharakter strukturnykh prevrashchenij v tsikle termoindutsirovannogo vozdejstviya na primere ternarnykh nanochastits Ag-Ni-Pd? [Can the presence of a cavity alter the nature of structural transformations during a cycle of thermally induced treatment, taking Ag-Ni-Pd ternary nanoparticles as an example?], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 271-281. DOI: 10.26456/pcascnn/2026.18.271. ⎘

Full article (in Russian): download PDF file

References:

1. Kim Y., Lee Y.W., Lee S. et al. One-pot synthesis of ternary alloy hollow nanostructures with controlled morphologies for electrocatalysis, ACS Applied Materials & Interfaces, 2021, vol. 13, issue 38, pp. 45538-45545. DOI: 10.1021/acsami.1c13171.
2. Li Z., Yu C., Kang Y. et al. Ultra-small hollow ternary alloy nanoparticles for efficient hydrogen evolution reaction, National Science Review, 2021, vol. 8, issue 7, art. no. nwaa204, 13 p. DOI: 10.1093/nsr/nwaa204.
3. Wang J., Chen F., Tang Q. et al. Transition from core-shell to janus segregation pattern in AgPd nanoalloy by Ni doping for the formate oxidation, Applied Catalysis B: Environmental, 2020, vol. 270, art. no. 118861, 13 p. DOI: 10.1016/j.apcatb.2020.118861.
4. El Mel A.-A., Nakamura R., Bittencourt C. The Kirkendall effect and nanoscience: hollow nanospheres and nanotubes, Beilstein Journal of Nanotechnology, 2015, vol. 6, pp. 1348-1361. DOI: 10.3762/bjnano.6.139.
5. Sdobnyakov N.Yu. [Modelirovanie strukturnykh prevrashchenij v odnokomponentnykh i mnogokomponentnykh metallicheskikh nanosistemakh: uchebnik] Simulation of structural transformations in single-component and multi-component metallic nanosystems: a textbook. Tver, Tver State University Publ., 2025, 408 p. DOI: 10.26456/sny.2025.408. (In Russian).
6. Samsonov V., Nepsha N., Sdobnyakov N. et al. Chemical and structural segregation in Pt-Pd-Ni ternary nanosystems: molecular dynamics simulation, Materials Chemistry and Physics, 2025, vol. 340, art. no. 130827, 11 p. DOI: 10.1016/j.matchemphys.2025.130827.
7. Nepsha N.I., Sdobnyakov N.Yu., Samsonov V.M. et al. Atomistic simulation of segregation in ternary Pt–Pd–Ni nanoalloy, Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques, 2024, vol. 18, issue 6, pp. 1388-1394. DOI: 10.1134/S1027451024701295.
8. Samsonov V.M., Talyzin I.V., Romanov A.A. et al. On the relation between spontaneous segregation of components in ternary Pt–Pd–Ni nanoparticles and stability of core–shell nanostructures: molecular dynamics study, Colloid Journal, 2025, vol. 87, issue 4, pp. 547-559. DOI: 10.1134/S1061933X25600605.
9. Akin M., Bekmezci M., Catal C. et al. GCE surface coating with PdNiAg nanocatalysts to ensure high performance and stability in alcohol oxidation, RSC Advances, 2025, vol. 15, issue 35, pp. 28555-28564. DOI: 10.1039/d5ra02762d.
10. Sdobnyakov N.Yu., Kolosov A.Yu., Sokolov D.N., Savina K.G. MDSym. Certificate RF, no. 2025683621, 2025. (In Russian).
11. Cleri F., Rosato V. Tight-binding potentials for transition metals and alloys, Physical Review B, 1993, vol. 48, issue 1, pp. 22-33. DOI: 10.1103/PhysRevB.48.22.
12. Nosé S. A unified formulation of the constant temperature molecular dynamics methods, The Journal of Chemical Physics, 1984, vol. 81, issue 1, pp. 511-519. DOI: 10.1063/1.447334.
13. Leimkuhler B., Noorizadeh E., Theil F. A gentle stochastic thermostat for molecular dynamics, Journal of Statistical Physics, 2009, vol. 135, issue 2, pp. 261-277. DOI: 10.1007/s10955-009-9734-0.
14. Stukowski A. Visualization and analysis of atomistic simulation data with OVITO – the open visualization tool, Modelling and Simulation in Materials Science and Engineering, 2010, vol. 18, issue 1, pp. 015012-1-015012-7. DOI: 10.1088/0965-0393/18/1/015012.
15. Sun L., Lv H., Feng J. et al. Noble-metal-based hollow mesoporous nanoparticles: synthesis strategies and applications, Advanced Materials, 2022, vol. 34, art. no. 2201954, 16 p. DOI: 10.1002/adma.202201954.
16. Akbarzadeh H., Mehrjouei E., Shamkhali A.N. et al. Stability of Pd@void@M (M=Ni, Ag, and Pt) yolk shell nanoparticles controlled by structural factors: a molecular dynamics perspective, Colloids and Surfaces A: Physicochemical and Engineering Aspects, 2021, vol. 610, art. no. 125920, 12 p. DOI: 10.1016/j.colsurfa.2020.125920.

Content |