Thermal phenomena induced by pulsed current in titanium during tensile deformation
A.A. Misochenko, O.E. Korolkov
Mechanical Engineering Research Institute of RAS
DOI: 10.26456/pcascnn/2026.18.072
Original article
Abstract: The study analyzes the thermal effect of pulsed current during tensile testing in Grade 2 and Grade 4 titanium in coarse‑grained and ultrafine‑grained states. The work demonstrates the determining role of the current duty cycle in the manifestation of electroplastic and thermal effects. It is shown that in the single‑pulse mode (duty cycle 5000-10000), there is a correspondence between the onset of the temperature peak and the yield stress jump. In the multi‑pulse current mode (duty cycle 10), the maximum temperatures increase linearly with increasing current density above 40 A/mm2 and can reach approximately 170°C at a current density of 100 A/mm2. When the duty cycle is below 5000, thermal effects become the dominant mechanisms. The results of comparing the electroplastic effect manifestation in coarse‑grained and ultrafine‑grained Grade 4 titanium are presented, demonstrating the structural sensitivity of the effect to grain size. A comparison was made of the reduction in the flow stress under the influence of current versus heating by an external source, demonstrating the presence of other contributions to the electroplastic effect besides the thermal one. At the same time, the thermal contribution of the current to the reduction of the flow stress in ultrafine‑grained titanium is smaller than in coarse‑grained titanium.
Keywords: electroplastic effect, tension, pulsed current, titanium, thermal effect of pulsed current
- Anna A. Misochenko – Ph. D., Senior Researcher, Mechanical Engineering Research Institute of RAS, ORCID: 0000-0002-2885-1996
- Oleg E. Korolkov – Researcher, Mechanical Engineering Research Institute of RAS, ORCID: 0000-0001-7433-479X
For citation:
Misochenko A.A., Korolkov O.E. Teplovye effekty impulsnogo toka v titane pri rastyazhenii [Thermal phenomena induced by pulsed current in titanium during tensile deformation], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 72-81. DOI: 10.26456/pcascnn/2026.18.072. ⎘
Full article (in Russian): download PDF file
References:
1. Sheng Y., Hua Y., Wang X. et al. Application of high-density electropulsing to improve the performance of metallic materials: mechanisms, microstructure and properties, Materials, 2018, vol. 11, issue 2, art. no. 185, 25 p. DOI: 10.3390/ma11020185.
2. Lee C.H., Choi S.-W., Narayana P.L. et al. Effect of electric current heat treatment on commercially pure titanium sheets, Metals, 2021, vol. 11, issue 5, art. no. 783, 12 p. DOI: 10.3390/met11050783.
3. Pan D., Wang Y., Guo Q. et al. Grain refinement of Al–Mg–Si alloy without any mechanical deformation and matrix phase transformation via cyclic electro-pulsing treatment, Materials Science and Engineering: A, 2021, vol. 807, art. no. 144510, 14 p. DOI: 10.1016/j.msea.2021.140916.
4. Troitskii O.A. Electromechanical effect in metals, Journal of Experimental and Theoretical Physics Letters, 1969, vol. 1, no. 1, pp. 18-22.
5. Stolyarov V.V. Erratum to: Role of the Pulse Current Duty Cycle during Titanium Tension, Journal of Machinery Manufacture and Reliability, 2024, vol. 53, issue 3, p. 300. DOI: 10.1134/S1052618824700146.
6. Dimitrov N.K., Liu Y., Horstemeyer M.F. Electroplasticity: A review of mechanisms in electro-mechanical coupling of ductile metals, Mechanics of advanced materials and structures, 2020, vol. 29, issue 5, pp. 705-716. DOI: 10.1080/15376494.2020.1789925.
7. Ruszkiewicz B. J., Grimm T., Ragai I., Mears L., Roth J. T. A review of electrically assisted manufacturing with emphasis on modeling and understanding of the electroplastic effect, Journal of Manufacturing Science and Engineering, 2017, vol. 139, issue 11, art. no. 110801, 15 p. DOI: 10.1115/1.4036716.
8. Hariharan K., Lee M.-G., Kim M.-J. et al. Decoupling thermal and electrical effect in an electrically assisted uniaxial tensile test using finite element analysis, Metallurgical and Materials Transactions, 2015, vol. 46, issue 7, pp. 3043-3051. DOI: 10.1007/s11661-015-2879-3.
9. Ruszkiewicz B. J., Mears L., Roth J. T. Investigation of heterogeneous joule heating as the explanation for the transient electroplastic stress drop in pulsed tension of 7075-T6 aluminum, Journal of Manufacturing Science and Engineering, 2018, vol. 140, issue 9, art. no. 091014, 11 p. DOI: 10.1115/1.4040349.
10. Wang X., Xu J., Shan D., Guo B., Cao J. Modeling of thermal and mechanical behavior of a magnesium alloy AZ31 during electrically-assisted micro-tension, International Journal of Plasticity, 2016, vol. 85, pp. 230-257. DOI: .
11. Ugurchiev U. Kh., Novikova N. N. Comparative analysis of measuring the thermal effect during extension without a current and with a current, Journal of Machinery Manufacture and Reliability, 2021, vol. 50, issue 5, pp. 469-473. DOI: 10.3103/S1052618821050138.
12. Misochenko A.A., Stolyarov V.V. Teplovoe dejstvie impul'snogo toka v splavakh s razlichnymi teplofizicheskimi svojstvami [Thermal effect of pulsed current in alloys with different thermophysical properties], Stankoinstrument, 2023, issue 4, pp. 34-41. DOI: 10.22184/2499-9407.2023.33.4.34.41. (In Russian).