Synthesis of hierarchical structures based on zinc oxide nanowires and metal-organic frameworks
S.S. Nalimova1, Z.V. Shomakhov2, V.S. Kotlyarova1, M.M. Krasnikova1, O.G. Makarova1, C.D. Bui1, A.A. Rybina1, S.S. Buzovkin1
1 Saint Petersburg Electrotechnical University «LETI»
2 Kabardino-Balkarian State University named after H.M. Berbekov
DOI: 10.26456/pcascnn/2026.18.722
Original article
Abstract: The paper discusses approaches to creating hierarchical structures based on zinc oxide nanowires modified with metal-organic framework ZIF-8. The study is relevant because it aims to improve functional properties of gas sensors and photocatalysts by increasing their specific surface area and number of active sites. Zinc oxide nanowires produced using the hydrothermal method allow for directional charge carrier transfer, while the ZIF-8 shell with its high porosity and selective adsorption capacity acts as a molecular filter. Synthesis of these composites was conducted using the solvothermal method in ethanol and dimethylformamide solvents, followed by heat treatment. The morphology, phase composition, and elemental distribution of the samples were analyzed using scanning electron microscopy, X-ray diffraction, and energy-dispersive X-ray spectroscopy. It has been found that annealing at 500°C causes the decomposition of ZIF-8 and formation of only the zinc oxide phase. The synthesis in dimethylformamide and annealing at 320°C allow us to preserve both phases and achieve a uniform coating of nanowires with a layer of the framework. However, aggregation of particles and loss of the original nanowire morphology have been observed. It has been shown that it is necessary to optimize the synthesis conditions in order to preserve the individual shape of the nanorods and ensure the availability of the active sites.
Keywords: zinc oxide, ZIF-8, hierarchical structures, solvothermal synthesis, nanocomposites
- Svetlana S. Nalimova – Ph. D., Associate Professor, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI», ORCID: 0000-0003-3065-3961
- Zamir V. Shomakhov – Ph. D., Director of the Institute of electronics, robotics and artificial intelligence, Kabardino-Balkarian State University named after H.M. Berbekov, ORCID: 0000-0001-5738-2626
- Vera S. Kotlyarova – 4th year student, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI»
- Mariya M. Krasnikova – 4th year student, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI»
- Olesya G. Makarova – 4th year student, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI»
- Cong Doan D. Bui – 4th year postgraduate student, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI», ORCID: 0000-0002-9937-9078
- Arina A. Rybina – 1st year postgraduate student, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI», ORCID: 0000-0002-9937-9078
- Sergey S. Buzovkin – 1st year postgraduate student, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI», ORCID: 0000-0002-9937-9078
For citation:
Nalimova S.S., Shomakhov Z.V., Kotlyarova V.S., Krasnikova M.M., Makarova O.G., Bui C.D., Rybina A.A., Buzovkin S.S. Sintez ierarkhicheskikh struktur na osnove nanosterzhnej oksida tsinka i metalloorganicheskikh karkasov [Synthesis of hierarchical structures based on zinc oxide nanowires and metal-organic frameworks], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 722-729. DOI: 10.26456/pcascnn/2026.18.722. ⎘
Full article (in Russian): download PDF file
References:
1. Nalimova S.S., Shomakhov Z.V., Kondratev V.M. et al. Investigation of hierarchical gas-sensing ZnFe2O4 nanostructures, Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques, 2023, vol. 17, issue S1, pp. S416-S422. DOI: 10.1134/S1027451023070376.
2. Moshnikov V.A., Gracheva I.E., Kuznezov V.V. et al. Hierarchical nanostructured semiconductor porous materials for gas sensors, Journal of Non-Crystalline Solids, 2010, vol. 356, issue 37-40, pp. 2020-2025. DOI: 10.1016/j.jnoncrysol.2010.06.030.
3. Perumal V., Sabarinathan A., Chandrasekar M. et al. Hierarchical nanorods of graphene oxide decorated SnO2 with high photocatalytic performance for energy conversion applications, Fuel, 2022, vol. 324, part B, art. no. 124599, 9 p. DOI: 10.1016/j.fuel.2022.124599.
4. Madbouly A., Elzwawy A., Morsy M. Rapid CO detection using MWCNTs/SnO2 hierarchical structure: Synthesis, characterization, and RT gas sensing features, Ceramics International, 2024, vol. 50, issue 14, pp. 25473-25483. DOI: 10.1016/j.ceramint.2024.04.280.
5. Ryabko A.A., Nalimova S.S., Permyakov N.V. et al. Architectonics of zinc oxide nanorod coatings for adsorption gas sensors, Technical Physics, 2024, vol. 69, issue 7, pp. 2103-2110. DOI: 10.1134/S1063784224070387.
6. Shomakhov Z.V., Nalimova S.S., Bobkov A.A., Moshnikov V.A. Х-ray photoelectron spectroscopy of the surface layers of faceted zinc-oxide nanorods, Semiconductors, 2022, vol. 56, issue 13, pp. 450-454. DOI: 10.1134/S1063782622130097.
7. Stock N., Biswas S. Synthesis of metal-organic frameworks (MOFs): routes to various MOF topologies, morphologies, and composites, Chemical Reviews, 2012, vol. 112, issue 2, pp. 933-969. DOI: 10.1021/cr200304e.
8. Zhang Y., Wang M., San X. et al. Highly selective gas sensors for formaldehyde detection based on ZnO@ZIF‑8 core-shell heterostructures, Sensors and Actuators B, 2024, vol. 398, art. no. 134689, 10 p. DOI: 10.1016/j.snb.2023.134689.
9. Murugesan T., Kumar R.R., Ranjan A. et al. Fabrication of large-area Au nanoparticle decorated ZnO@ZIF-8 core-shell heterostructure nanorods for ppb-level NO2 gas sensing at room temperature, Sensors and Actuators B, 2024, vol. 402, art. no. 135106, 10 p. DOI: 10.1016/j.snb.2023.135106.
10. Tran T.V., Dang H.H., Nguyen H. et al. Synthesis methods, structure, and recent trends of ZIF-8-based materials in the biomedical field, Nanoscale Advances, 2025, vol. 7, issue 13, pp. 3941-3960. DOI: 10.1039/d4na01015a.
11. Nalimova S.S., Gagarina A.Yu., Spivak Yu.M. et al. Hemorezistivnyj gazovyj sensor i sposob ego izgotovleniya [Chemoresistive gas sensor and its manufacturing method]. Patent RF, no. 2806670, 2023. (In Russian).
12. Posachayanan N., Liwetpitaya P., Thoumrungroj A. et al. Highly-efficient recovery of silver from industrial cyanide-based plating effluent on TiO2/activated carbon composites, Chemosphere, 2024, vol. 367, art. no. 143614, 10 p. DOI: 10.1016/j.chemosphere.2024.143614.
13. Yin H., Kim H., Choi J., Yip A.C.K. Thermal stability of ZIF-8 under oxidative and inert environments: A practical perspective on using ZIF-8 as a catalyst support, Chemical Engineering Journal, 2015, vol. 278, pp. 293-300. DOI: 10.1016/j.cej.2014.08.075.
14. Balderas-Xicohtencat R., Villajos J.A., Casabán J. et al. ZIF‑8 pellets as a robust material for hydrogen cryo-adsorption tanks, ACS Applied Energy Materials, 2023, vol. 6, no. 18, pp. 9145-915. DOI: 10.1021/acsaem.2c03719.