Spectral-luminescent properties of Nd-containing perovskite quantum dots in a pseudocumene matrix and the effect of 2,5-diphenyloxazole
A.M. Pshukov, A.A. Kokoeva, D.N. Ermolenko, Kh.R. Akhmedova, M.U. Shokumova, M.M. Shogenova
Kabardino-Balkarian State University named after H.M. Berbekov
DOI: 10.26456/pcascnn/2026.18.926
Short communication
Abstract: It has been experimentally demonstrated that Nd-containing mixed-halide perovskite quantum dots retain an optically active luminescent state after incorporation into a pseudocumene matrix. Dilutions of the dispersion at 1:10, 1:20, and 1:30 were compared without 2,5-diphenyloxazole and with 2,5-diphenyloxazole at a concentration of 2 g/L. Emission spectra and excitation-emission matrices were recorded under identical settings. In all compositions, a dominant band at 501,5-505,5 nm was observed and 2,5-diphenyloxazole changed the peak position by no more than 1,0 nm. Upon addition of PPO, the maximum intensity and the band area decreased by 2,2 and 2,3% for 1:10, by 20,3 and 15,9% for 1:20, and by 48,8 and 35,3% for 1:30, respectively. Consequently, pseudocumene is a viable organic matrix for the quantum dots under study during photoluminescence diagnostics, whereas 2,5-diphenyloxazole at a concentration of 2 g/L does not sensitize their photoluminescence. This result establishes the conditions for further optimization but does not replace measurements of radioluminescence and γ-excited light yield.
Keywords: perovskite quantum dots, neodymium, pseudocumene matrix, 2,5-diphenyloxazole, photoluminescence, energy transfer, self-absorption, liquid organic scintillator
- Adam M. Pshukov – Ph. D., Leading Researcher, Director of the International Center for Detector Technologies and Functional Nanomaterials, Kabardino-Balkarian State University named after H.M. Berbekov, ORCID: 0000-0003-2849-1238
- Aneta A. Kokoeva – Ph. D., Senior Researcher, International Center for Detector Technologies and Functional Nanomaterials, Kabardino-Balkarian State University named after H.M. Berbekov, ORCID: 0000-0002-6583-8555
- Danil N. Ermolenko – Research Intern, International Center for Detector Technologies and Functional Nanomaterials, Kabardino-Balkarian State University named after H.M. Berbekov
- Khadizha R. Akhmedova – Research Intern, International Center for Detector Technologies and Functional Nanomaterials, Kabardino-Balkarian State University named after H.M. Berbekov
- Mariya U. Shokumova – Research Intern, International Center for Detector Technologies and Functional Nanomaterials, Kabardino-Balkarian State University named after H.M. Berbekov
- Mariya M. Shogenova – Research Intern, International Center for Detector Technologies and Functional Nanomaterials, Kabardino-Balkarian State University named after H.M. Berbekov
For citation:
Pshukov A.M., Kokoeva A.A., Ermolenko D.N., Akhmedova Kh.R., Shokumova M.U., Shogenova M.M. Spektralno-lyuminestsentnye svojstva Nd-soderzhashchikh perovskitnykh kvantovykh tochek v matritse psevdokumola i vliyanie 2,5-difeniloksazola [Spectral-luminescent properties of Nd-containing perovskite quantum dots in a pseudocumene matrix and the effect of 2,5-diphenyloxazole], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 926-933. DOI: 10.26456/pcascnn/2026.18.926. ⎘
Full article (in Russian): download PDF file
References:
1. Winslow L., Simpson R. Characterizing quantum-dot-doped liquid scintillator for applications to neutrino detectors, Journal of Instrumentation, 2012, vol. 7, issue 7, art. no. P07010, 12 р. DOI: 10.1088/1748-0221/7/07/P07010.
2. Aberle C., Li J.J., Weiss S., Winslow L. Optical properties of quantum-dot-doped liquid scintillators, Journal of Instrumentation, 2013, vol. 8, issue 10, art. no. P10015, 22 p. DOI: 10.1088/1748-0221/8/10/P10015.
3. Cho S., Kim S., Kim J. et al. Hybridisation of perovskite nanocrystals with organic molecules for highly efficient liquid scintillators, Light: Science & Applications, 2020, vol. 9, art. no. 156, 9 p. DOI: 10.1038/s41377-020-00391-8.
4. Yu H., Chen T., Han Z., Fan J., Pei Q. Liquid scintillators loaded with up to 40 weight percent cesium lead bromide quantum dots for gamma scintillation, ACS Applied Nano Materials, 2022, vol. 5, issue 10, pp. 14572-14581. DOI: 10.1021/acsanm.2c02930.
5. Kim N.-R., Joo K.-K., Lee H.-G. Investigating the potential of perovskite nanocrystal-doped liquid scintillator: a feasibility study, Sensors, 2023 vol. 23, issue 23, art. no. Р9490, 14 p. DOI: 10.3390/s23239490.
6. Baravaglio M., Sabot B., Maddalena F. et al. Energy deposition in liquid scintillators composed of CsPbBr3 colloidal nanocrystal dispersions, Nanoscale, 2024, vol. 16, issue 36, pp. 17176-17186. DOI: 10.1039/D4NR02401J.
7. Pshukov A.M., Kokoeva A.A., Ermolenko D.N., Kashezhev A.Z. O vozmozhnosti ispol'zovaniya naftalinovykh kristallov pri poluchenii zhidkikh organicheskikh stsintillyatorov dlya ispol'zovaniya v nejtrinnoj fizike [On the possibility of using naphthalene crystals in liquid organic scintillators for neutrino physics]. Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 148-160. DOI: 10.26456/pcascnn/2025.17.148. (In Russian).
8. Pshukov A.M., Kokoeva A.A., Yakuba Yu.F., Kashezhev A.Z. Kvantovye tochki perovskita, legirovannye ionom neodima: sintez, opticheskie svojstva [Neodymium-doped perovskite quantum dots: synthesis and optical properties]. Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 742-751. DOI: 10.26456/pcascnn/2025.17.742. (In Russian).
9. Altudov Yu.K., Pshukov A.M., Kokoeva A.A. et al. Colloidal synthesis and optical properties of Nd-containing mixed-halide CsPbBr3−γClγ quantum dots with λem≈458 nm and PLQY≈56%, Physchem, 2026, vol. 6, issue 2, art. no. 37, 13 p. DOI: 10.3390/physchem6020037.
10. Shamsi J., Urban A.S., Imran M., De Trizio L., Manna L. Metal halide perovskite nanocrystals: synthesis, post-synthesis modifications, and their optical properties, Chemical Reviews, 2019, vol. 119, issue 5, pp. 3296-3348. DOI: 10.1021/acs.chemrev.8b00644.