Problems and strategies of epitaxial growth of III-V-Bi semiconductor thin films: a review
O.V. Devitsky1,2
1 Federal Research Center Southern Scientific Center of the RAS
2 North Caucasus Federal University
DOI: 10.26456/pcascnn/2026.18.244
Review
Abstract: This review article systematically summarizes fundamental and applied research concerning the epitaxy of metastable III-V–Bi solid solutions. The main challenge in obtaining thin films of III-V–Bi is their thermodynamic instability, which results from a wide miscibility gap and extremely low equilibrium solubility of bismuth in III-V compounds. It is demonstrated that overcoming these limitations is only possible through kinetic stabilization methods. Key strategies to enhance bismuth incorporation are identified, including lowering the substrate temperature to 200-350°C, manipulating surface stoichiometry by shifting to gallium-rich regimes, and employing surface reconstructions such as the 2×1 pattern. Additional approaches involve engineering tensile strain to increase bismuth solubility by up to 100 times and using high-index substrates like (115)A and (311)B, along with congruent transfer techniques. The paper also thoroughly discusses strategies for improving structural quality, such as suppressing bismuth droplet formation, implementing two-temperature growth procedures, and performing in-situ and post-growth annealing. A comparative analysis of molecular beam epitaxy, metal-organic vapor phase epitaxy, and pulsed laser deposition methods is presented within the context of producing high-quality III-V–Bi thin films. The review concludes that further progress in developing devices based on III-V–Bi requires shifting from empirical process optimization to precise control of surface kinetics and atomic-level defect management.
Keywords: GaAsBi, thin films, III-V-Bi, molecular beam epitaxy, metal-organic vapor phase epitaxy, pulsed laser deposition
- Oleg V. Devitsky – Ph. D., Leading Researcher, Laboratory of Physics and Technology of Semiconductor Nanoheterostructures for Microwave Electronics and Photonics, Federal Research Center Southern Scientific Center of the RAS, Leading Researcher at the Research and Educational Center for Photovoltaics and Nanotechnology, Associate Professor at the Department of Physical Chemistry North Caucasus Federal University, ORCID: 0000-0003-3153-696X
For citation:
Devitsky O.V. Problemy i strategii epitaksialnogo rosta poluprovodnikovykh tonkikh plenok III-V-Bi: obzor [Problems and strategies of epitaxial growth of III-V-Bi semiconductor thin films: a review], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 244-255. DOI: 10.26456/pcascnn/2026.18.244. ⎘
Full article (in Russian): download PDF file
References:
1. Francoeur S., Seong M.J., Mascarenhas A. et al. Band gap of GaAs1-xBix, 0
3. Samajdar D.P., Dhar S. Influence of Bi-related impurity states on the bandgap and spin-orbit splitting energy of dilute III-V-Bi alloys: InP1-xBix, InAs1-xBix, InSb1-xBix and GaSb1-xBix, Superlattices and Microstructures, 2016, vol. 89, pp. 112-119. DOI: 10.1016/j.spmi.2015.10.048
4. Hild K., Batool Z., Jin S.R. et al. Auger recombination suppression and band alignment in GaAsBi/GaAs heterostructures, AIP Conference Proceedings, 2013, vol. 1566, issue 1, pp. 488-489. DOI: 10.1063/1.4848498.
5. Ammar I.,Sfina N.,Fnaiech M. Optical gain and threshold current density for mid-infrared GaSbBi/GaSb quantum-well laser structure, Materials Science and Engineering: B, 2021, vol. 266, art. no. 115056, 10 p. DOI: 10.1016/j.mseb.2021.115056.
6. Stringfellow G.B. Epitaxial growth of metastable semiconductor alloys, Journal of Crystal Growth, 2021, vol. 564, art. no. 126065, 13 p. DOI: 10.1016/j.jcrysgro.2021.126065.
7. Guan Y., Luo G., Morgan D. et al. Thermodynamic stability analysis of Bi-containing III-V quaternary alloys and the effect of epitaxial strain, Journal of Physics and Chemistry of Solids, 2020, vol. 138, art. no. 109245, 12 p. DOI: 10.1016/j.jpcs.2019.109245.
8. Baladés N., Sales D.L., Herrera M. et al. Analysis of Bi distribution in epitaxial GaAsBi by aberration-corrected HAADF-STEM, Nanoscale Research Letters, 2018, vol. 13, issue 1, art. no. 125, 8 p. DOI: 10.1186/s11671-018-2530-5.
9. Yoshida J., Kita T., Wada O. et al. Temperature dependence of GaAs1-xBix band gap studied by photoreflectance spectroscopy, Japanese Journal of Applied Physics, 2003, vol. 42, no. 2R, pp. 371-374. DOI: 10.1143/JJAP.42.371.
10. Gelczuk Ł., Kopaczek J., Pucicki D. et al. Effects of rapid thermal annealing on deep-level defects and optical properties of n-type GaAsBi alloys grown by molecular beam epitaxy at low temperature, Materials Science in Semiconductor Processing, 2024, vol. 169, art. no. 107888, 10 p. DOI: 10.1016/j.mssp.2023.107888.
11 Pashchenko A.S., Devitsky O.V., Lunin L.S. et al. Growth of nanotextured thin films of GaInAsP and GaInAsSbBi solid solutions on GaP substrates by pulsed laser deposition, Nanosystems: Physics, Chemistry, Mathematics, 2023, vol. 14, issue 5, pp. 601-605. DOI: 10.17586/2220-8054-2023-14-5-601-605.
12. Devitsky O.V., Kravtsov A.A., Sysoev I.A. Issledovanie sostava plenok GaAs1-yBiy, poluchennykh metodom impul'snogo lazernogo napyleniya [Study of the composition of GaAs1-yBiy films obtained by pulsed laser deposition], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2021, issue 13, pp. 96-105. DOI: 10.26456/pcascnn/2021.13.096. (In Russian).
13. Bennarndt W., Boehm G., Amann M.C. Domains of molecular beam epitaxial growth of Ga(In)AsBi on GaAs and InP substrates, Journal of Crystal Growth, 2016, vol. 436, pp. 56-61. DOI: 10.1016/j.jcrysgro.2015.11.021.
14. Lewis R.B., Masnadi-Shirazi M., Tiedje T. Growth of high Bi concentration GaAs1-xBix by molecular beam epitaxy, Applied Physics Letters, 2012, vol. 101, issue 8, art. no. 82112, 5 p. DOI: 10.1063/1.4748172.
15. Jacobsen H., Puchala B., Kuech T.F. et al. Ab initio study of the strain dependent thermodynamics of Bi doping in GaAs, Physical Review B - Condensed Matter and Materials Physics, 2012, vol. 86, issue 8, art. no. 085207, 10 p. DOI: 10.1103/PhysRevB.86.085207.
16. Luo G., Yang S., Li J. et al. First-principles studies on molecular beam epitaxy growth of GaAs1-xBix, Physical Review B - Condensed Matter and Materials Physics, 2015, vol. 92, issue 3, art. no. 035415, 10 p. DOI: 10.1103/PhysRevB.92.035415.
17. Himwas C., Yordsri V., Thanachayanont C. et al. High verticality vapor-liquid-solid growth of GaAs0.99Bi0.01 nanowires using Ga-Bi assisted catalytic droplets, Nanoscale Advances, 2024, vol. 6, issue 3, pp. 846-854. DOI: 10.1039/d3na00428g.
18. Forghani K., Anand A., Mawst L.J. et al. Low temperature growth of GaAs1-yBiy epitaxial layers, Journal of Crystal Growth, 2013, vol. 380, pp. 23-27. DOI: 10.1016/j.jcrysgro.2013.05.033.
19. Puustinen J., Hilska J., Guina M. Analysis of GaAsBi growth regimes in high resolution with respect to As/Ga ratio using stationary MBE growth, Journal of Crystal Growth, 2019, vol. 511, pp. 33-41. DOI: 10.1016/j.jcrysgro.2019.01.010.
20. Knaub N., Beyer A., Wegele T. et al. Quantification of Bi distribution in MOVPE-grown Ga(AsBi) via HAADF STEM, Journal of Crystal Growth, 2016, vol. 433, pp. 89-96. DOI: 10.1016/j.jcrysgro.2015.10.007.
21. Stevens M.A., Grossklaus K.A., Vandervelde T.E. Strain stabilization of far from equilibrium GaAsBi films, Journal of Crystal Growth, 2019, vol. 527, art. no. 125216, 5 p. DOI: 10.1016/j.jcrysgro.2019.125216.
22. Chomdech S., Sigmarsson V., Pumee W. et al. Impact of growth temperature and Bi flux on InPBi layers grown on GaSb (001), Materials Science in Semiconductor Processing, 2026, vol. 205, art. no. 110382, 7 p. DOI: 10.1016/j.mssp.2025.110382.
23. Sweeney S.J., Hild K., Jin S. The potential of GaAsBiN for multi-junction solar cells, IEEE 39th Photovoltaic Specialists Conference (PVSC), 16-21 June 2013. Tampa, IEEE Publ., 2013, pp. 2474-2478. DOI: 10.1109/PVSC.2013.6744977.
24. Ludewig P., Bushell Z.L., Nattermann L. et al. Growth of Ga(AsBi) on GaAs by continuous flow MOVPE, Journal of Crystal Growth, 2014, vol. 396. pp. 95-99. DOI: 10.1016/j.jcrysgro.2014.03.041
25. Zaied I., Alghurabi A.M., Fitouri H. et al. Structural and optical properties of diluted GaAsBi alloys grown on GaAs(115) substrate by MOVPE, Materials Science in Semiconductor Processing, 2025, vol. 195, art. no. 109649, 7 p. DOI: 10.1016/j.mssp.2025.109649.
26. Steele J.A., Lewis R.A., Horvat J. et al. Surface effects of vapour-liquid-solid driven Bi surface droplets formed during molecular-beam-epitaxy of GaAsBi, Scientific Reports, 2016, vol. 6, art. no. 28860, 17 p. DOI: 10.1038/srep28860.
27. Patil P.K., Ishikawa F., Shimomura S. Bismuth flux dependence of GaAsBi/GaAs MQWs grown by molecular beam epitaxy using two-substrate-temperature technique, Superlattices and Microstructures, 2017. vol. 106. pp. 50-57. DOI: 10.1016/j.spmi.2017.03.021.
28. Štaupienė A., Jokubauskaitė M., Zelioli A. et al. Improving optical properties through growth temperatures and post-growth annealing in parabolic GaAsBi/AlGaAs quantum wells, Journal of Alloys and Compounds, 2026, vol. 1060, art. no. 187230, 6 p. DOI: 10.1016/j.jallcom.2026.187230.
29. Luna E., Puustinen J., Hilska J., Guina M. et al. Detection of BiGa hetero-antisites at Ga(As,Bi)/(Al,Ga)As interfaces, Journal of Applied Physics, 2024, vol. 135, issue 12, art. no. 125303, 10 p. DOI: 10.1063/5.0195965.
30. Alhassni A.A., Felix J.F., Marroquin J.F.R. et al. Dilute GaAs1−xBix epilayers with different bismuth concentrations grown by Molecular Beam Epitaxy: A promising candidate for gamma radiation sensor applications, Applied Surface Science, 2023, vol. 636, art. no. 157787, 10 p. DOI: 10.1016/j.apsusc.2023.157787.
31. Devitsky O.V. Struktura i sostav tonkikh plenok GaAs1-x-yNxBiy, poluchennykh metodom impul'snogo lazernogo napyleniya [Structure and composition of thin GaAs1-x-yNxBiy films produced by pulsed laser deposition], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 593-601. DOI: 10.26456/pcascnn/2022.14.593. (In Russian).
32. Devitsky O.V. Impul'snoe lazernoe napylenie poluprovodnikovykh tonkikh plenok III-V: obzor [Pulsed laser deposition of III-V semiconductor thin films: review], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 621-630. DOI: 10.26456/pcascnn/2024.16.621. (In Russian).
33. Pashchenko A.S., Devitsky O. V., Lunina M.L. et al. Epitaxial growth of GaInAsBi thin films on Si (001) substrate using pulsed laser deposition, Vacuum, 2024, vol. 227, art. no. 113372, 9 p. DOI: 10.1016/j.vacuum.2024.113372.
34. Abdelwahed A.Ben, Zouaghi S., Fitouri H. et al. MOVPE growth and characterization of GaAs/GaAsBi/GaAs p-i-n structure, Optical Materials, 2024, vol. 155, art. no. 115822, 7 p. DOI: 10.1016/j.optmat.2024.115822.
35. Maßmeyer O., Hepp T., Günkel R. et al. In situ analysis of Bi terminated GaAs (001) and Ga(As,Bi) surfaces during growth by MOVPE, Applied Surface Science, 2020, vol. 533, art. no. 147401, 12 p. DOI: 10.1016/j.apsusc.2020.147401.