Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Surface modification of TiNi-based alloys by high-current low-energy electron beams

A.A. Klopotov1, Y.A. Abzaev1, Y.F. Ivanov2, G.G. Volokitin1, O.M. Loskutov1

1 Tomsk State University of Architecture and Building
2 Institute of High Current Electronics of the Siberian Branch of RAS

DOI: 10.26456/pcascnn/2026.18.657

Original article

Abstract: Titanium nickelide alloys TiNi exhibit a high sensitivity of their fine crystalline structure to external energy inputs, which governs their functional properties (the shape-memory effect and superelasticity). Exposure to high-current low-energy electron beams produces metastable nanocrystalline states in the near-surface layers; however, the quantitative analytical relationship between the integral irradiation energy and the evolution of structural parameters remains insufficiently developed. Based on X-ray diffraction data and computer simulation of heat transfer, a physical and mathematical model has been developed that describes the kinetics of changes in the unit-cell parameter a, second-kind microstrains ε = <Δd/d>, and coherent scattering region sizes DCSR as functions of the integral energy W = N ∙ ES. Exponential saturation of the decrease in the lattice parameter a(W), with a limiting contraction Δa/a0 ≈ 0,69% caused by selective titanium evaporation, has been established. The dependences ε(W) and DCSR(W) were obtained and approximated by threshold functions reflecting the competition between the defect generation and annealing over different activation-energy spectra. The dislocation density ρ = (1,5-16,7)∙1014 m-2 and elastic energy of the defect subsystem Udisl ≈ 4,0 ∙ 107 J/m3 were calculated. The proposed model predicts the structural state of the modified layer with an accuracy of R2 > 0,96 and elucidates the physical mechanisms governing threshold changes in the fine crystalline structure, thereby providing a basis for targeted control of the functional responses of shape-memory alloys.

Keywords: titanium nickelide, high-current electron beams, X-ray diffraction analysis, lattice parameter, thermodynamic modeling

  • Anatoly A. Klopotov – Dr. Sc., Professor, Department of Applied Mechanics and Materials Science, Tomsk State University of Architecture and Building, ORCID: 0000-0002-3690-0436
  • Yuri A. Abzaev – Dr. Sc., Professor, Department of Higher Mathematics, Tomsk State University of Architecture and Building, ORCID: 0000-0002-6939-1658
  • Yuri F. Ivanov – Dr. Sc., Chief Researcher, Laboratory of Plasma Emission Electronics, Institute of High Current Electronics of the Siberian Branch of RAS, ORCID: 0000-0001-8022-7958
  • Gennadii G. Volokitin – Dr. Sc., Professor, Head of Department of Applied Mechanics and Materials Science, Tomsk State University of Architecture and Building, ORCID: 0009-0004-3884-3481
  • Oleg M. Loskutov – Ph. D., Associate Professor, Department of Applied Mechanics and Materials Science, Tomsk State University of Architecture and Building, ORCID: 0000-0002-8509-4899

For citation:

Klopotov A.A., Abzaev Y.A., Ivanov Y.F., Volokitin G.G., Loskutov O.M. Modifikatsiya poverkhnosti splavov na osnove TiNi vysokotochnym nizkoenergeticheskim elektronnym puchkom [Surface modification of TiNi-based alloys by high-current low-energy electron beams], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 657-667. DOI: 10.26456/pcascnn/2026.18.657. ⎘

Full article (in Russian): download PDF file

References:

1. Rotshtein V.P., Proskurovsky D.I., Ozur G.E., Ivanov Yu.F. Modifikatsiya poverkhnostnykh sloyev metallicheskikh materialov nizkoenergeticheskimi sil'notochnymi elektronnymi puchkami [Modification of Surface Layers of Metallic Materials by Low-Energy High-Current Electron Beams]. Nauka Publ., Novosibirsk, 2019, 346 p. DOI: 10.7868/978-5-02-038809-3. (In Russian).
2. Devyatkov V.N., Koval N.N., Schanin P.M. et. al. Generation and propagation of high-current low-energy electron beams, Laser and Particle Beams, 2003, vol. 21, issue 2, pp. 243-248. DOI: 10.1017/S026303460321212X.
3. Yakovlev E.V., Solovyev A.V., Markov A.B. at al. Cracking during the formation of chromium-based surface alloys by a low-energy high-current electron beam, Russian Physics Journal, 2022, vol. 64, issue 12, pp. 2214-2218. DOI: 10.1007/s11182-022-02579-4.
4. Nagase T., Umakoshi Y. Temperature dependence in density-fluctuation-induced crystallization in metallic glass by MeV electron irradiation, Intermetallics, 2010, vol. 18, issue 10, pp. 1803-1808. DOI: 10.1016/j.intermet.2010.02.044.
5. Meisner L.L., Ostapenko M.G., Lotkov A.I., Neyman А.А. The special features of the phase formation and distribution in the titanium nickelide surface layers treated by electron beams, Russian Physics Journal, 2015, vol. 58, issue 5, pp. 670-677. DOI: 10.1007/s11182-015-0549-y.
6. Klopotov A.A., Ivanov Yu.F., Vlasov V.A., Potekaev A.I. Termodinamicheskij analiz fazoobrazovaniya v nerzhaveyushchej stali, obrabotannoj vysokointensivnym impulsnym elektronnym puchkom [Thermodynamic analysis of phase formation in stainless steel treated with a high-intensity pulsed electron beam], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 155-163. DOI: 10.26456/pcascnn/2016.8.155. (In Russian).
7. Ivanov Yu.F., Klopotov A.A., Petrikova E.A., Regina M.E., Tolkachev O.S., Klopotov V.D. Strukturno-fazovoe sostoyanie silumina zaevtekticheskogo sostava, obluchennogo impulsnym elektronnym puchkom [Structural-phase state of silumin of hypereutectic composition irradiated by a pulsed electron beam], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 89-102. DOI: 10.26456/pcascnn/2020.12.089. (In Russian).
8. Klopotov A.A., Ivanov Yu.F., Ustinov A.M. et al. Influence of modification of the surface of a metal matrix on the mechanical properties of silumin/CFRP layered composites, Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques, 2023, vol. 17, issue 3, pp. 548-555. DOI: 10.1134/S1027451023030072.
9. Potekaev A.I., Klopotov A.A., Kulagina V.V. et al. Alloys based on TiNi in pretransition low-stability states. structure and properties, Advanced Structured Materials. Singapore, Springer, 2024, vol. 216, VII+284 p. DOI: 10.1007/978-981-97-5149-5.
10. Meisner L.L., Markov A.B., Proskurovsky D.I. et al. Effect of inclusions on cratering behavior in TiNi shape memory alloys irradiated with a low-energy, high-current electron beam, Surface and Coatings Technology, 2016, vol. 302, pp. 495-506. DOI: 10.1016/j.surfcoat.2016.06.036.
11. Neiman A.A., Meisner L.L., Lotkov A.I. et al. Cross-sectional TEM analysis of structural phase states in TiNi alloy treated by a low-energy high-current pulsed electron beam, Applied Surface Science, 2015, vol. 327, pp. 321-326. DOI: 10.1016/j.apsusc.2014.11.173.
12. Gudimova E., Semin V., Meisner L. et al. Influence of pulsed electron-beam alloying with tantalum on structural phase states in TiNi alloy, Materials Today: Proceedings, 2017, vol. 4, issue 3, part B, pp. 4670-4674. DOI: 10.1016/J.MATPR.2017.04.049.
13. Neiman A.A., Meisner L.L., Lotkov A.I. et al. Chemical composition and structure of the TiNi alloy surface layer formed after electron beam melting and crystallization, AIP Conference Proceedings, 2016, vol. 1783, issue 1, pp. 020163-1–020163-5. DOI: 10.1063/1.4966456.
14. Williamson G.K., Hall W.H. X-ray line broadening from filed aluminium and wolfram, Acta Metallurgica, 1953, vol. 1, issue 1, pp. 22-30. DOI: 10.1016/0001-6160(53)90006-6.
15. Landa A., Klepeis J.E., Rudd R.E. et al. Analytic binary alloy volume–concentration relations and the deviation from Zen’s law, Applied Sciences, 2021, vol. 11, issue 13, art. no. 6231, 25 p. DOI: 10.3390/app11136231.
16. Smithells metals reference book, 8th ed., ed. By W.F. Gale, T.C. Totemeier. Oxford, Butterworth-Heinemann, 2004, 2080 p.
17. Valiev R.Z., Islamgaliev R.K., Alexandrov I.V. Bulk nanostructured materials from severe plastic deformation, Progress in Materials Science, 2000, vol. 45, issue 2, pp. 103-189. DOI: 10.1016/S0079-6425(99)00007-9.
18. Gleiter H. Nanostructured materials: basic concepts and microstructure, Acta Materialia, 2000, vol. 48, issue 1, pp.1-29. DOI: 10.1016/S1359-6454(99)00285-2.