The effect of irradiation on the dynamic instability of dislocation slip in metals
V.V. Malashenko
Galkin Donetsk Institute for Physics and Engineering
DOI: 10.26456/pcascnn/2026.18.264
Original article
Abstract: Within the framework of the theory of dynamic interaction of defects, the above-barrier motion of edge dislocations in an irradiated metal containing radiation point and nanoscale defects (prismatic dislocation loops) is analyzed. Intense external loads generate high strain rate deformation of irradiated metals. During high strain rate deformation, dislocations accelerate to high velocities, and their kinetic energy exceeds the height of potential barriers generated by structural defects. During above-barrier motion of dislocations, the energy of external loads is converted into the energy of dislocation oscillations. This dissipation mechanism differs significantly from the dissipation mechanism in the low-velocity region. The presence of a gap in the dislocation oscillation spectrum significantly affects the efficiency of this mechanism. This paper considers the case where the gap is generated by the collective interaction of radiation point defects. An analytical expression defining the rate dependence of the dynamic yield strength in irradiated metal is obtained. A new region of dynamic instability of dislocation motion was predicted, caused by a high concentration of prismatic dislocation loops. This dynamic instability is the cause of plastic deformation jumps. Some analytical expressions defining the boundaries of the dynamic instability region are obtained, and numerical estimates of the boundary values are performed.
Keywords: irradiated metals, dislocations, dislocation loops, radiation defects, high-speed deformation
- Vadim V. Malashenko – Dr. Sc., Professor, Chief Researcher of the Department «Theory of kinetic and electronic properties of nonlinear systems», Galkin Donetsk Institute for Physics and Engineering, ORCID: 0000-0001-7073-8762
For citation:
Malashenko V.V. Vliyanie oblucheniya na dinamicheskuyu neustojchivost dislokatsionnogo skolzheniya v metallakh [The effect of irradiation on the dynamic instability of dislocation slip in metals], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 264-270. DOI: 10.26456/pcascnn/2026.18.264. ⎘
Full article (in Russian): download PDF file
References:
1. Verschueren J., Gurrutxaga-Lerma B., Balint D.S. et al. Instabiities of high speed dislocations, Physics Review Letters, 2018, vol. 121, issue 14, pp. 145502-1-145502-6. DOI: 10.1103/PhysRevLett.121.145502.
2. Griffiths M. Effect of neutron irradiation on the mechanical properties, swelling and creep of austenitic stainless steels, Materials, 2021, vol. 14, issue 10, art. no. 2622, 47 p. DOI: 10.3390/ma14102622.
3. Abernethy R.G., Gibson I.S.K.-L, Giannattasio A. et al. Effects of neutron irradiation on the brittle to ductile transition in single crystal tungsten, Journal of Nuclear Materials, 2019, vol. 527, art. no. 151799, 12 p. DOI: 10.1016/j.jnucmat.2019.151799.
4. Gurrutxaga-Lerma B. Quantum statistical theory of dislocation mobility in discrete lattices, Physics Review Materials, 2025, vol. 9, issue 12, pp. 123605-1-123605-40. DOI: 10.1103/zzct-418n.
5. Gurrutxaga-Lerma B, Verschueren J., Sutton A.P. et al. The mechanics and physics of high-speed dislocations: a critical review, International Materials Reviews, 2020, vol. 66, issue 4, pp. 215-255. DOI: 10.1080/09506608.2020.1749781.
6. Li P., Susmel L., Ma M. The life prediction of notched aluminum alloy specimens after laser shock peening by TCD, International Journal of Fatigue, 2023, vol. 176, art. no. 107795, 22 p. DOI: 10.1016/j.ijfatigue.2023.107795.
7. Prabhakaran S., Kulkarni A., Vasanth G. et al. Laser shock peening without coating induced residual stress distribution, wettability characteristics and enhanced pitting corrosion resistance of austenitic stainless steel, Applied Surface Science, 2017, vol. 428, pp. 17-30. DOI: 10.1016/j.apsusc.2017.09.138.
8. Walgraef D. Rate equation approach to dislocation dynamics and plastic deformation, Materials Science and Engineering: A, 2002, vol. 322, issue 1-2, pp. 167-175. DOI: 10.1016/S0921-5093(01)01676-8.
9. Tapasa K., Bacon D. J., Osetsky Yu. N. Computer simulation of dislocation–solute interaction in dilute Fe–Cu alloys, Modelling and Simulation in Materials Science and Engineering, 2006, vol. 14, no. 7, pp. 1153-1166. DOI: 10.1088/0965-0393/14/7/004.
10. Singla A., Ray A. Hugoniot elastic limit of single-crystal tantalum at normal and elevated temperatures subjected to extreme strain rates, Physical Review B, 2022, vol. 105, issue 6, pp. 064102-1-064102-19. DOI: 10.1103/PhysRevB.105.064102.
11. Malashenko V.V. Features of dry friction of dislocations in irradiated metals with giant magnetostriction, Physics of the Solid State, 2025, vol. 67, issue 10, pp. 1873-1875. DOI: 10.61011/PSS.2025.10.62640.259-25.
12. Malashenko V.V. Dynamic drag of edge dislocation by circular prismatic loops and point defects, Physica B: Condensed Matter, 2009, vol. 404, issue 21, pp. 3890-3893. DOI: 10.1016/j.physb.2009.07.122.
13. Varyukhin V.N., Malashenko V.V. Dynamic effects in a defective system of crystal, Bulletin of the Russian Academy of Sciences. Physics, 2018, vol. 82, issue 9, pp. 1101-1105. DOI: 10.3103/S1062873818090253.