Modeling the thermal effect on the surface energy and electron work function of a monocrystal thallium
I.G. Shebzukhova1, L.P. Aref`eva2
1 Kabardino-Balkarian State University named after H.M. Berbekov
2 Don State Technical University
DOI: 10.26456/pcascnn/2026.18.289
Original article
Abstract: The aim of this work was to carry out numerical modeling of thermal influence on energy and force characteristics of monocrystal thallium. The surface energies and work function of faces of thallium crystals are calculated using the electron-statistical method taking into account quantum corrections. The influence of polymorphic transformations and temperature on anisotropy of these properties is analyzed. The cohesive energy of α- and β- thallium has also been estimated based on the values of surface and interfacial energies, which include the average configuration energy and the energy of chemical interaction between two parts of the metal, and the temperature dependence of the chemical interaction energy has been investigated. The contact potential difference for pairs of close-packed faces has been calculated. Computer simulations of the mechanical properties have been performed using the Griffiths model, and the tensile strength of thallium has been obtained, which allows for the prediction of the material’s service life.
Keywords: surface energy, electron work function, anisotropy, polymorphic modifications of thallium, cohesive energy, crack resistance
- Irina G. Shebzukhova – Dr. Sc., Professor, Professor, Department of Theoretical and Experimental Physics, Institute of Mathematics and Natural Sciences, Kabardino-Balkarian State University named after H.M. Berbekov
- Ludmila P. Aref`eva – Dr. Sc., Associate Professor, Professor, Department of Materials Science and Technology of Metals, Faculty of Mechanical Engineering Technology, Don State Technical University, ORCID: 0000-0003-2431-6897
For citation:
Shebzukhova I.G., Aref`eva L.P. Modelirovanie termicheskogo vliyaniya na poverkhnostnuyu energiyu i rabotu vykhoda elektrona monokristallicheskogo talliya [Modeling the thermal effect on the surface energy and electron work function of a monocrystal thallium], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 289-295. DOI: 10.26456/pcascnn/2026.18.289. ⎘
Full article (in Russian): download PDF file
References:
1. GOST 18337-95. Interstate Standard. Tallij. Tekhnicheskie usloviya [Thallium. Specifications]. Minsk, Publishing standards, 1999, 11 p. (In Russian).
2. Alexeev P.N., Kotov IA.L., Shimkevich A.L. Ispol'zovanie eutekticheskogo Na-Tl-teplonositelya v modul'nom bystro'm reaktore [The use of eutectic Na-Tl coolant in small fast reactor], Voprosy atomnoj nauki i tekhniki. Seriya: fizika yadernykh reaktorov [Problems of Atomic Science and Engineering. Series: Physics of Nuclear Reactors] 2022, vol. 2, pp. 83-89. (In Russian).
3. Kutuev R.A. Zavisimost poverkhnostnogo natyazheniya i plotnosti rasplavov indiy-talliy i olovo-talliy ot sostava i temperatury [Dependence of surface tension and density of indium-thallium and tin-thallium melts on composition and temperature], Inzhenernaya fizika [Engineering Physics], 2023, 3, pp. 57-62. DOI: 10.25791/infizik.3.2023.1319. (In Russian).
4. Savvin V.S., Anokhina N.N., Povzner A.A. Processes at the liquid/crystal boundary upon contact melting in the system with intermediate solid phases, Physics of metals and metallography, 2012, vol. 113, issue 4, pp. 406-410. DOI: 10.1134/S0031918X12040138.
5. Savvin V.S., Density and molar volume of liquid amalgams of thallium, lead, and bismuth, High Temperature, 2023, vol. 61, issue 3, pp. 339-343. DOI: 10.1134/s0018151x23030161.
6. Chernyshikin S.V., Zhevnenko S.N., Zakirov A.V. et al. Surface tension measurements of NiTi alloy for the melt pool simulation during laser powder bed fusion, Materials letters, 2026, vol. 405, art. no. 139696, 4 p. DOI: 10.1016/j.matlet.2025.139696.
7. Gershman E.I., Zhevnenko S.N. Method of in situ measuring surface tension of a solid-gas interface, Physics of metals and metallography, 2010, vol. 110, issue 1, pp. 102-107. DOI: 10.1134/S0031918X10070124.
8. Shebzukhova I.G., Aref'eva L.P. Anisotropy of the surface energy and work function of IIB metals, Technical Physics, 2019, vol. 64, issue 2, pp. 274-277. DOI: 10.1134/S1063784119020208.
9. Shebzukhova I.G., Aref’eva L.P. Poverkhnostnaya energiya i rabota vykhoda elektrona polimorfnykh modifikatsij titana [Surface energy and electron work function for polimorphyc modifications of titanium], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 288-298. DOI: 10.26456/pcascnn/2023.15.288 (In Russian).
10. Manohin S.S., Betekhtin V.I., Kadomtsev A.G. et al. Study of the structural features of microcrystalline aluminum after tests for long-term strength, Physics of the solid state, 2023, vol. 65, issue 1, pp. 126-132. DOI: 10.21883/pss.2023.01.54986.492.
11. Yurov V.M., Guchenko S.A., and K.M. Makhanov Poverkhnostnaya energija i iznosostojkost' vysokojentropijnykh pokrytij [Surface energy and wear resistance of high-entropy coatings], Tendentsiya i razvitiya nauki i obrazovaniya [Trends and Development of Science and Education], 2020, vol. 64, no. 1, pp. 72-77. DOI: 10.18411/lj-08-2020-13. (In Russian).
12. Rusanov A.I. Thermodynamic aspects of materials science, Russian Chemical Rewiews, 2016, vol. 85, issue 1, pp. 1-13. DOI: 10.1070/RCR4568.
13. Shebzukhova I.G., Aref`eva L.P. Otsenka polyarizatsionnoj i dispersionnoj popravok k poverkhnostnoj energii granej metallicheskikh kristallov [Estimation of the polarization and dispersion corrections to the surface energy of the faces of metal crystals], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 319-325. DOI: 10.26456/pcascnn/2020.12.319. (In Russian).
14. Li Y., Li D.Y. Electron work function, adhesion, and friction between 3d transition metals under light loads Wear, 2005, vol. 259, issue 7-12, pp. 1432-1436. DOI: 10.1016/j.wear.2005.01.027.
15. Shebzukhova I.G., Khokonov Kh. B. Poverkhnostnoe natyazhenie tverdykh metallov v gazovykh sredakh [Surface tension of solid metals in gas media], Izvestiya Rossijskoj akademii nauk. Seriya fizicheskaya [Bulletin of Russian Academy of Sciences: Physics], 2012, vol. 76, issue 13, pp. 86-88. (In Russian).
16. Svoystva elementov. Spravochnik [Properties of elements. Handbook], ed. M.E. Drits, Moscow, Metallurgiya Publ., 1985, 672 p. (In Russian).