Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Development of a computational model for stability assessment of N-vinylcaprolactam – N-vinylimidazole copolymers in a selective solvent

M.K. Glagolev1, A.V. Vorozheykina1, I.K. Patrenkov2, P.V. Komarov1

1 A.N. Nesmeyanov Institute of Organoelement Compounds of RAS
2 Tver State University

DOI: 10.26456/pcascnn/2026.18.391

Original article

Abstract: Computer simulation of the behavior of thermosensitive copolymers of N-vinylcaprolactam and N-vinylimidazole in a water environment was performed using a pipeline of unidirectionally coupled simulation models, namely Dissipative Particle Dynamics, Langevin Dynamics, and All-atom Molecular Dynamics. The pipeline allows first to determine a possible sequence of monomer units in a model copolymer, then to determine the morphology of the globules formed in a selective solvent, and finally to assess the aggregation stability of the globules. It utilizes the fast relaxation dynamics in Dissipative Particle Dynamics Simulations, efficiency of implicit solvent consideration in Langevin dynamics, and experimentally verified atom interaction force-field in All-atom Molecular dynamics simulations. The approach exploits the strengths of each of the simulation methods, and the relevance of the simulation results is ensured by the ultimate transition to the all-atom detailed representation. Here we describe the models and the algorithms of transformation between the models, and present the data for their initial validation. The behavior of the studied models in an aqueous environment allows us to conclude that the constructed systems are structurally stable. The globules have a distinct core-shell structure, with N-vinylcaprolactam monomer units forming the core and N-vinylimidazole monomer units forming the outer shell. Water molecules penetrate the globule primarily through the shell, which is rich in N-vinylimidazole units.

Keywords: poly(N-vinylcaprolactam), poly(N-vinylimidazole), thermosensitive copolymers, computer simulation, thermally-switched catalysts

  • Mikhail K. Glagolev – Ph. D., Researcher, Laboratory of Physical Chemistry of Polymers, A.N. Nesmeyanov Institute of Organoelement Compounds of RAS, ORCID: 0000-0003-1128-649X
  • Alesya V. Vorozheykina – Ph. D., Laboratory of Physical Chemistry of Polymers, A.N. Nesmeyanov Institute of Organoelement Compounds of RAS, ORCID: 0000-0002-0919-7458
  • Ivan K. Patrenkov – graduate student, Department of General Physics, Tver State University
  • Pavel V. Komarov – Dr. Sc., Docent, Leading Researcher, Laboratory of Physical Chemistry of Polymers, A.N. Nesmeyanov Institute of Organoelement Compounds of RAS, ORCID: 0000-0003-2138-5088

For citation:

Glagolev M.K., Vorozheykina A.V., Patrenkov I.K., Komarov P.V. Razrabotka kompyuternoj modeli dlya otsenki stabilnosti sopolimerov N-vinilkaprolaktama – N-vinilimidazola v selektivnom rastvoritele [Development of a computational model for stability assessment of N-vinylcaprolactam – N-vinylimidazole copolymers in a selective solvent], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 391-400. DOI: 10.26456/pcascnn/2026.18.391. ⎘

Full article (in Russian): download PDF file

References:

1. Zhang Y., Lei F., Qian W. et al. Designing intelligent bioorthogonal nanozymes: recent advances of stimuli-responsive catalytic systems for biomedical applications, Journal of Controlled Release, 2024, vol. 373, pp. 929-951. DOI: 10.1016/j.jconrel.2024.07.073.
2. Ge Z., Xie D., Chen D. et al. Stimuli-responsive double hydrophilic block copolymer micelles with switchable catalytic activity, Macromolecules, 2007, vol. 40, issue 10, pp. 3538-3546. DOI: 10.1021/ma070550i.
3. Wang B., Liu H.J., Jiang T.T. et al. Thermo-, and pH dual-responsive poly(N-vinylimidazole): preparation, characterization and its switchable catalytic activity, Polymer, 2014, vol. 55, issue 23, pp. 6036-6043. DOI: 10.1016/j.polymer.2014.09.051.
4. Musarurwa H., Tavengwa N. T. Thermo-responsive polymers and advances in their applications in separation science, Microchemical Journal, 2022, vol. 179, art. no. 107554, 14 p. DOI: 10.1016/j.microc.2022.107554.
5. Xiao Q., Cui Y., Meng Y. et al. PNIPAm hydrogel composite membrane for high-throughput adsorption of biological macromolecules, Separation and Purification Technology, 2022, vol. 294, art. no. 121224, 11 p. DOI: 10.1016/j.seppur.2022.121224.
6. Yao T., Feng C., Yan H. Current developments and applications of smart polymers based aqueous two-phase systems, Microchemical Journal, 2024, vol. 204, art. no. 111170, 15 p. DOI: 10.1016/j.microc.2024.111170.
7. Lozinsky V. I., Simenel I. A., Kulakova V. K. et al. Synthesis and studies of N-vinylcaprolactam/N-vinylimidazole copolymers that exhibit the «proteinlike» behavior in aqueous media, Macromolecules, 2003, vol. 36, issue 19, pp. 7308-7323. DOI: 10.1021/ma034456n.
8. Lozinskii V.I., Simenel I.A., Khokhlov A.R. Catalytic properties of the protein-like copolymer of N-vinylcaprolactam and N-vinylimidazole in the hydrolysis of an ester substrate, Doklady Chemistry, 2006, vol. 410, issue 2, pp. 170-173. DOI: 10.1134/S0012500806100028.
9. Lozinsky V.I., Zaborina O.E., Klimova T.P. et al. Copolymers containing functional groups intrinsic to the active centers of serine hydrolases: synthesis and evaluation of catalytic capability, Polymer Science, Series B, 2016, vol. 58, issue 1, pp. 27-37. DOI: 10.1134/S156009041601005X.
10. Barabanova A.I., Vorozheykina A.V., Glagolev M.K. et. al. Synthesis and theoretical studies of the conformational behaviour of N-vinylcaprolactam/N-vinylimidazole copolymers in selective solvent, Molecular Systems Design & Engineering, 2024, vol. 9, issue 10, pp. 1017-1022. DOI: 10.1039/D4ME00085D.
11. Vyshivannaya O.V., Parkhomenko E.R., Barabanova A.I. et al. Thermo- and pH-sensitive behavior of copolymers of N-vinylcaprolactam with N-vinylimidazole, Polymer Science, Series A, 2023, vol. 65, issue 3, pp. 235-245. DOI: 10.1134/S0965545X2370092X.
12. Dubovik A.S., Burova T.V., Grinberg N.V. et al. Solvent-free copolymerization of N-vinylcaprolactam with N-vinylimidazole. energetics of cooperative transitions of copolymers in aqueous solutions by high-sensitivity differential scanning calorimetry, Macro Chemistry & Physics, 2026, vol. 227, issue 2, p. e00399, 7 p. DOI: 10.1002/macp.202500399.
13. Hoogerbrugge P.J., Koelman J.M.V.A. Simulating microscopic hydrodynamic phenomena with dissipative particle dynamics, Europhysics Letters, 1992, vol. 19, no. 3, pp. 155-160. DOI: 10.1209/0295-5075/19/3/001.
14. Groot R.D., Warren P.B. Dissipative particle dynamics: Bridging the gap between atomistic and mesoscopic simulation, The Journal of Chemical Physics, 1997, vol. 107, issue 11, pp. 4423-4435. DOI: 10.1063/1.474784.
15. Van Gunsteren W.F., Berendsen H. . C. Algorithms for brownian dynamics, Molecular Physics, 1982, vol. 45, issue 3, pp. 637-647. DOI: 10.1080/00268978200100491.
16. Paquet E., Viktor H.L. Molecular dynamics, Monte Carlo simulations, and Langevin dynamics: a computational review, BioMed Research International, 2015, vol. 2015, art. id. 183918, 18 p. DOI: 10.1155/2015/183918.
17. Gartner T.E., Jayaraman A. Modeling and simulations of polymers: a roadmap, Macromolecules, 2019, vol. 52, issue 3, pp. 755-786. DOI: 10.1021/acs.macromol.8b01836.
18. Hollingsworth S.A., Dror R.O. Molecular dynamics simulation for all, Neuron, 2018, vol. 99, issue 6, pp. 1129-1143. DOI: 10.1016/j.neuron.2018.08.011.
19. Sun H. Ab initio calculations and force field development for computer simulation of polysilanes, Macromolecules, 1995, vol. 28, issue 3, pp. 701-712. DOI: 10.1021/ma00107a006.
20. Thompson A. P., Aktulga H. M., Berger R. et al. LAMMPS - a flexible simulation tool for particle-based materials modeling at the atomic, meso, and continuum scales, Computer Physics Communications, 2022, vol. 271, art. no. 108171, 34 p. DOI: 10.1016/j.cpc.2021.108171.
21. Gissinger J.R., Jensen B.D., Wise K.E. Modeling chemical reactions in classical molecular dynamics simulations, Polymer, 2017, vol. 128, pp. 211-217. DOI: 10.1016/j.polymer.2017.09.038.
22. Baburkin P.O., Komarov P.V., Barabanova A.I. et. al. Mesoscopic simulation of the synthesis of enzyme-like catalysts, Doklady Physical Chemistry, 2016, vol. 470, issue 1, pp. 129-132. DOI: 10.1134/S0012501616090025.
23. Gissinger J.R., Jensen B.D., Wise K.E. REACTER: a heuristic method for reactive molecular dynamics, Macromolecules, 2020, vol. 53, issue 22, pp. 9953-9961. DOI: 10.1021/acs.macromol.0c02012.
24.Gissinger J.R., Jensen B.D., Wise K.E. Molecular modeling of reactive systems with REACTER, Computer Physics Communications, 2024, vol. 304, art. no. 109287, 16 p. DOI: 10.1016/j.cpc.2024.109287.
25. Glagolev M., Glagoleva A., Vasilevskaya V. MOUSE2: molecular ordering utilities for simulations, edition 2, Supercomputing Frontiers and Innovations, 2023, vol. 10, issue 3, pp. 73-87. DOI: 10.14529/jsfi230307.
26. Humphrey W., Dalke A., Schulten K. VMD: visual molecular dynamics, Journal of Molecular Graphics, 1996, vol. 14, issue 1, pp. 33-38. DOI: 10.1016/0263-7855(96)00018-5.
27. Voevodin Vl., Antonov A., Nikitenko D. et. al. Supercomputer Lomonosov-2: large scale, deep monitoring and fine analytics for the user community, Supercomputing Frontiers and Innovations, 2019, vol. 6, issue 2, pp. 4-11. DOI: 10.14529/jsfi190201.

Content |