Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Coalescence and sintering in a ternary nanosystem Pt+Cu+Pd: molecular dynamics simulation

V.V. Puytov, V.M. Samsonov, S.A. Vasilyev

Tver State University

DOI: 10.26456/pcascnn/2026.18.455

Original article

Abstract: Using the LAMMPS soft-ware and the embedded atom method, molecular dynamics simulation has been performed of sintering and coalescence in a system of three monometallic nanoparticles (Pd1700 + Cu5100 + Pt1700), whose centers of mass were located on the same straight line. The process was carried out during uniform heating of the system up to a temperature of 2300 K, corresponding to the daughter nanodroplet, and subsequent cooling (quenching) it to the initial temperature of 300 K. We found that as a result of low-temperature sintering (heating to 500-900 K), a ternary analogue of the Janus structure was formed. Solidification of the nanodroplet resulted in the ternary nanocrystal formation. Temperature dependences of radial distributions of atomic fractions of the components were found and analyzed. It was established that during both sintering solid nanoparticles and cooling (quenching) nanodroplets, Pd atoms migrate to the outer atomic monolayer, whereas in solidified nanodroplets, Pt atoms have segregated toward the second monolayer and the center of the nanoparticle. In addition to chemical segregation, i.e., the spatial separation of components, structural segregation was observed in the solidified nanodroplets. This segregation yields grains in the form of bands with a defective fcc structure, separated from each other by boundaries represented by atoms identified by the Ovito program as a local hcp structure.

Keywords: LAMMPS, molecular dynamics, embedded atom potential, sintering, coalescence, surface segregation

  • Vladimir V. Puytov – Laboratory Assistant, Management of Scientific Research, Tver State University, ORCID: 0009-0008-6947-6847
  • Vladimir M. Samsonov – Dr. Sc., Full Professor, General Physics Department, Tver State University, ORCID: 0000-0003-2929-8069
  • Sergey A. Vasilyev – Ph. D., Docent, Department of Applied Physics, Tver State University, ORCID: 0000-0002-4918-8855

For citation:

Puytov V.V., Samsonov V.M., Vasilyev S.A. Koalestsentsiya i spekanie v ternarnoj nanosisteme Pt+Cu+Pd: molekulyarno-dinamicheskoe modelirovanie [Coalescence and sintering in a ternary nanosystem Pt+Cu+Pd: molecular dynamics simulation], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 455-465. DOI: 10.26456/pcascnn/2026.18.455. ⎘

Full article (in Russian): download PDF file

References:

1. Samsonov V.M., Talyzin I.V., Vasilyev S.A., Alymov M.I. Mechanisms of coalescence of metallic nanodroplets and sintering of metallic nanoparticles, Doklady Physics, 2019, vol. 64, issue 12, pp. 453-455. DOI: 10.1134/S1028335819120061.
2. Samsonov V.M., Talyzin I.V., Vasilyev S.A., Alymov M.I. On the mechanisms of coalescence of nanodroplets and sintering of solid particles, Colloid Journal, 2020, vol. 82, issue 5, pp. 573-583. DOI: 10.1134/S1061933X20050154.
3. Samsonov V.M., Talyzin I.V., Puytov V.V., Vasilyev S.A., Romanov A.A., Alymov M.I. When mechanisms of coalescence and sintering at the nanoscale fundamentally differ: Molecular dynamics study, The Journal of Chemical Physics, 2022, vol. 156, issue 21, art.no. 214302, 15 p. DOI: 10.1063/5.0075748.
4. Samsonov V.M., Alymov M.I., Talyzin I.V., Vasilyev S.A. Size dependence of the melting temperature and mechanisms of the coalescence/sintering on the nanoscale, Journal of Physics: Conference Series, 2019, vol. 1352, issue 1, art.no. 012044, 7 p. DOI: 10.1088/1742-6596/1352/1/012044.
5. Sdobnyakov N.Yu., Kolosov A.Yu., Bogdanov S.S. Modelirovanie protsessov koalestsentsii i spekaniya v mono- i bimetallicheskikh nanosistemakh: monografiya [Simulation of the processes of coalescence and sintering in mono- and bimetallic nanosystems: monograph]. Tver, Tver State University Publ., 2021, 168 p. DOI: 10.26456/skb.2021.168. (In Russian).
6. Kolosov A.Yu., Sdobnyakov N.Yu., Komarov P.V. et al. Modelirovanie protsessa koalestsentsii nanochastits zolota metodom Monte-Karlo [Simulation of the coalescence process of gold nanoparticles by Monte-Carlo method], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2012, issue 4, pp. 129-142. (In Russian).
7. Surrey A., Pohl D., Schultz L., Rellinghaus B. Quantitative measurement of the surface self-diffusion on Au nanoparticles by aberration-corrected transmission electron microscopy, Nano Letters, 2012, vol. 12, issue 12, pp. 6071-6077. DOI: 10.1021/nl302280x.
8. Yuk J.M., Jeong M., Kim S.Y. et al., In situ atomic imaging of coalescence of Au nanoparticles on graphene: rotation and grain boundary migration, Chemical Communications, 2013, vol. 49, issue 98, pp. 11479-11481. DOI: 10.1039/C3CC46545D.
9. Alymov M.I., Timofeev A.A., Gnedovets A.G. Coagulation of gold nanoparticles in thin amorphous films under irradiation with a fast electron beam, Nanotechnologies in Russia, 2013, vol. 8, issue 11-12, pp. 727-736. DOI: 10.1134/S1995078013060037.
10. Suliz K.V., Kolosov A.Yu., Myasnichenko V.S. et al. Control of cluster coalescence during formation of bimetallic nanoparticles and nanoalloys obtained via electric explosion of two wires, Advanced Powder Technology, 2022, vol. 33, issue 3, art. no. 103518, 15 p. DOI: 10.1016/j.apt.2022.103518.
11. Puytov V.V., Romanov A.A., Talyzin I.V., Samsonov V.M., Features and mechanisms of coalescence of nanodroplets and sintering of metal nanoparticles: molecular dynamics simulation, Russian Chemical Bulletin, 2022, vol. 71, issue 4, pp. 686-693. DOI: 10.1007/s11172-022-3466-6.
12. Nelli D., Cerbeland M., Ferrando R., Minnai Ch., Tuning the coalescence degree in the growth of Pt–Pd nanoalloys, Nanoscale advances, 2021, vol. 3, issue. 3, pp. 836-846. DOI: 10.1039/d0na00891e.
13. Grammatikopoulos P., Sowwan M., Kioseoglou J., Computational modeling of nanoparticle coalescence, Advanced Theory and Simulations, 2019, vol. 2, issue 6, art.no. 1900013, 26 p. DOI: 10.1002/adts.201900013.
14. Toulkeridou E., Kioseoglou J., Grammatikopoulos P., On the melting point depression, coalescence, and chemical ordering of bimetallic nanoparticles: the miscible Ni–Pt system, Nanoscale advances, 2022, vol. 4, issue 22, pp. 4819-4828. DOI: 10.1039/d2na00418f.
15. Jamshideasli D., Shamsaei N., Mahjouri-Samani M., Shao S., Molecular dynamics simulations of nanoparticle sintering in additive nanomanufacturing: insights from sintering mechanisms, Green Manufacturing Open, 2024, vol. 2, issue 4, art.no. 16, 20 p. DOI: 10.20517/gmo.2024.062001.
16. Sdobnyakov N., Khort A., Myasnichenko V., et al. Solution combustion synthesis and Monte Carlo simulation of the formation of CuNi integrated nanoparticles, Computational Materials Science, 2020, vol. 184, art. no 109936, 12 p. DOI: 10.1016/j.commatsci.2020.109936.
17. Romanovski V., Sdobnyakov N., Roslyakov S. et al. Bimetallic CuNi nanoparticle formation: solution combustion synthesis and molecular dynamic approaches, Inorganic Chemistry, 2024, vol. 63, issue 52, pp. 24844-24854. DOI: 10.1021/acs.inorgchem.4c04260.
18. Naunheim Y., Schuh C.A., Multicomponent alloys designed to sinter, Nature Communications, 2024, vol. 15, art. № 8028, 9 p. DOI: 10.1038/s41467-024-52261-1.
19. Sdobnyakov N., Kolosov A., Savina K. et al. Coalescence behavior of Al-Li-Cu-Zr and Cu nanoparticles: structure formation under molecular dynamics simulation, Materials Letters, 2026, vol. 409, art.no. 140181, 3 p. DOI: 10.1016/j.matlet.2026.140181.
20. Samsonov V.M., Zhigunov D.V., Sinitsa I.P. et al., Chemical and structural segregation in ternary Pt-Pd-Cu nanoparticles: molecular dynamics simulation, Colloid Journal, 2026, vol. 88, issue 4, pp. 605-618. DOI: 10.1134/S1061933X26600296
21. Chertkov D.V., Pujtov V.V., Talyzin I.V., Samsonov V.M. Sravnitelnoe molekulyarno-dinamicheskoe modelirovanie koalestsentsii i spekaniya v sistemakh Au-Au i Si-Si [Comparative molecular dynamics simulation of coalescence and sintering in Au-Au and Si-Si systems], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 522-536. DOI: 10.26456/pcascnn/2025.17.522.
22. Thompson A.P., Aktulga H.M., Berger R. et al. LAMMPS - a flexible simulation tool for particle-based materials modeling at the atomic, meso, and continuum scales, Computer Physics Communications, 2022, vol. 271, art. no. 108171, 34 p. DOI: 10.1016/j.cpc.2021.108171.
23. Zhou X.W., Johnson R.A., Wadley H.N.G. Misfit-energy-increasing dislocations in vapor-deposited CoFe/NiFe multilayers, Physical Review B, 2004, vol. 69, issue 14, pp. 113-114. DOI: 10.1103/PhysRevB.69.144113.
24. Missaen J.M., Voytovych R., Gilles B., Eustathopoulos N., Solid state spreading in the Cu/Cu system, Journal of Materials Science, 2005, vol. 40, issue 9-10, pp. 2377-2381. DOI: 10.1007/s10853-005-1962-3.
25. Samsonov V.M., Bembel A.G., Popov I.V. et al. Solid-state wetting at the nanoscale: molecular dynamics and surface diffusion approach, Surface Innovations, 2017, vol. 5, issue 3, pp. 161-169. DOI: 10.1680/jsuin.17.00015.
26. Fizicheskie velichiny: Spravochnik [Physical Quantities: Handbook], ed. by I.S. Grigoriev, E.Z. Meilikhov. Moscow: Energoatomizdat Publ., 1991, 1232 p. (In Russian).
27. Stukowski A. Visualization and analysis of atomistic simulation data with OVITO – the open visualization tool, Modelling and Simulation in Materials Science and Engineering, 2010, vol. 18, issue 1, pp. 015012-1-015012-7. DOI: 10.1088/0965-0393/18/1/015012.
28. Samsonov V.M., Talyzin I.V., Romanov A.A. et al. On the relation between spontaneous segregation of components in ternary Pt–Pd–Ni nanoparticles and stability of core–shell nanostructures: molecular dynamics study, Colloid Journal, 2025, vol. 87, issue 4, pp. 547-559. DOI: 10.1134/S1061933X25600605.
29. Wu Z.-P, Caracciolo D.T., Maswadeh Y. et al., Alloying-realloying enabled high durability for Pt-Pd-3d-transition metal nanoparticle fuel cell catalysts, Nature Communications, 2021, vol. 12, art. no. 859, 12 p. DOI: 10.1038/s41467-021-21017-6.
30. Zhang Y., Li H., Yan X. et al., Composition-controlled synthesis of Pt–Pd–Cu ternary metal nanoparticles for an enhanced electrocatalytic hydrogen evolution reaction, Nanoscale, 2025, vol. 17, issue 23, pp. 14415-14423. DOI: 10.1039/D5NR01065A.
31. Akbarzadeh H., Mehrjouci E., Abbaspour M., Shamkhali A.N. Melting behavior of bimetallic and trimetallic nanoparticles: a review of MD simulation studies, Topics in Current Chemistry, 2021, vol. 379, issue 3, art. no. 22, 40 p. DOI: 10.1007/s41061-021-00332-y.
32. Gilroy K.D., Ruditskiy A., Peng H.-C. et al., Bimetallic nanocrystals: Syntheses, properties, and applications, Chemical Reviews, 2016, vol. 116, issue 18, pp. 10414-10472. DOI: 10.1021/acs.chemrev.6b00211.