Phase and structural evolution of red muds during chemical looping reforming of methane
I.V. Shamsutov, L.A. Pasechnik, O.V. Merkulov
Institute of Solid State Chemistry of the Ural Branch of RAS
DOI: 10.26456/pcascnn/2026.18.976
Original article
Abstract: The accumulation of red mud – a large‑tonnage waste from alumina production – poses a serious environmental challenge: with an annual waste output exceeding 150 million tons, the global utilisation rate remains below 5%. At the same time, the polymetallic oxide composition of red muds (Fe2O3 up to 45–49 %, Al2O3, SiO2, CaO, TiO2, Na2O) provides opportunities for their use as oxygen carriers in chemical reforming of methane, thereby combining waste utilization with syngas production. Two types of materials were investigated: the original red mud from the Bogoslovsk Aluminum Smelter and a magnetite‑enriched mud with reduced aluminum content, obtained by hydrothermal leaching of the original red mud. Granules (3-5 mm) prepared by sintering at 1050°C were tested in cyclic «methane reduction – air oxidation» runs at 900°C in a fixed‑bed reactor; the evolution of phase composition and microstructure was monitored. It is established that, during cycling, iron oxides are reduced to metallic Fe, while aluminosilicate phases (gehlenite Ca2Al2SiO7, CaFeAlSiO6) acted as structural stabilisers, preventing particle sintering. For red mud, a steady‑state regime with CH4 conversion of ~75% and CO selectivity of ~85-90% is reached after 6-7 cycles; for magnetite‑enriched mud this occurs after 10 cycles, which is attributed to larger aggregates of iron oxides and their sintering, as well as to the formation of a layered porous structure. At the same time, magnetite‑enriched mud exhibits a slightly higher overall oxygen capacity. In both cases, the H2/CO ratio in the products remains at 1,75-1,80. It is shown that the key factor for long‑term stability is the balance between the content of the active component (iron oxides) and the amount of aluminosilicate stabilizers. The obtained results open up prospects for the targeted modification of red mud composition to create efficient and durable oxygen carriers for cyclic hydrocarbon processing.
Keywords: bauxite residue of red mud, oxygen carriers, methane reforming, chemical looping, synthesis gas, magnetite, hematite, cyclic stability, structural evolution
- Ivan V. Shamsutov – 3rd year postgraduate student, Junior Researcher, Laboratory of Selectively Permeable Ceramics and Engineering, Institute of Solid State Chemistry of the Ural Branch of RAS
- Liliya A. Pasechnik – Ph. D., Leading Researcher, Laboratory of Heterogeneous Processes, Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0002-0631-5287
- Oleg V. Merkulov – Ph. D., Head of the Laboratory of Selectively Permeable Ceramics and Engineering, Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0002-8275-4126
For citation:
Shamsutov I.V., Pasechnik L.A., Merkulov O.V. Fazovaya i strukturnaya evolyutsiya krasnykh shlamov pri khimicheskom tsiklicheskom riforminge metana [Phase and structural evolution of red muds during chemical looping reforming of methane], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 976-984. DOI: 10.26456/pcascnn/2026.18.976. ⎘
Full article (in Russian): download PDF file
References:
1. Xu H., Li D., Qian A. et al. Red mud as the catalyst for energy and environmental catalysis: a review, Energy & Fuels, 2024, vol. 38, issue 15, pp. 13737-13759. DOI: 10.1021/acs.energyfuels.4c02269.
2. Zinoveev D., Pasechnik L., Fedotov M. et al. Extraction of valuable elements from red mud with a focus on using liquid media—a review, Recycling, 2021, vol. 6, issue 2, art. no. 38, 32 p. DOI: 10.3390/recycling6020038.
3. Agrawal S., Dhawan N. Evaluation of red mud as a polymetallic source – a review, Minerals Engineering, 2021, vol. 171, art. no. 107084, 32 p. DOI: 10.1016/j.mineng.2021.107084.
4. Mukiza E., Zhang L., Liu X., Zhang N. Utilization of red mud in road base and subgrade materials: a review, Resources, Conservation and Recycling, 2019, vol. 141, pp. 187-199. DOI: 10.1016/j.resconrec.2018.10.031.
5. Li G., Liu J., Yi L.et al. Bauxite residue (red mud) treatment: current situation and promising solution, Science of the Total Environment, 2024, vol. 948, art. no. 174757, 24 p. DOI: 10.1016/j.scitotenv.2024.174757.
6. Jahromi H., Agblevor F.A. Hydrodeoxygenation of pinyon juniper catalytic pyrolysis oil using red mud supported nickel catalysts, Applied Catalysis B: Environmental, 2018, vol. 236, pp. 1-12. DOI: 10.1016/j.apcatb.2018.05.008.
7. Ramdhani E.P., Santoso E., Jovita S. et al. The Si/Al ratios effect on Fe aluminosilicate from red mud for sustainable green diesel production, Molecular Catalysis, 2025, vol. 584, art. no. 115295, 13 p. DOI: 10.1016/j.mcat.2025.115295.
8. Mei D., Abad A., Zhao H. et al. On a highly reactive Fe₂O₃/Al₂O₃ oxygen carrier for in situ gasification chemical looping combustion, Energy & Fuels, 2014, vol. 28, issue 11, pp. 7043-7052. DOI: 10.1021/ef501981g.
9. Shamsutov I.V., Ryzhov D.A., Zavyalov M.A. et al. Performance evaluation of SrFe12O19 and Fe2O3/Al2O3 oxygen carriers in chemical looping reforming with water splitting, Energy & Fuels, 2024, vol. 38, issue 15, pp. 14534-14547. DOI: 10.1021/acs.energyfuels.4c02073.
10. Shamsutov I.V., Markov A.A., Merkulov O.V. Thermodynamic screening of SrFe12O19 vs supported Fe2O3 oxygen carriers for chemical looping reforming with water splitting, Industrial & Engineering Chemistry Research, 2026, vol. 65, issue 13, pp. 6833-6847. DOI: 10.1021/acs.iecr.5c04964.
11. Li C., Su X., Chen J. et al. Evaluation of different red muds as oxygen carriers in a fluidized bed thermogravimetric analyzer, Energy & Fuels, 2021, vol. 35, issue 18, pp. 14805-14815. DOI: 10.1021/acs.energyfuels.1c02456.
12. Lu C., Xu R., Muhammad I. et al. Thermodynamic evolution of magnetite oxygen carrier via chemical looping reforming of methane, Journal of Natural Gas Science and Engineering, 2021, vol. 85, art. no. 103704. 13 p. DOI: 10.1016/j.jngse.2020.103704.
13. Pasechnik L.A., Skachkov V.M., Bibanaeva S.A. et al. Composition and properties of iron oxides in the products of hydrothermal treatment of red mud and bauxites, Russian Journal of Inorganic Chemistry, 2022, vol. 67, issue 7, pp. 1101-1107. DOI: 10.1134/S0036023622060183.