Dielectric response in thin-film heterostructures with AlGaN nanolayers
I.T. Zezyanov1, A.V. Solnyshkin1, O.N. Sergeeva1, Sh.Sh. Sharofidinov2, I.P. Pronin2, N.V. Sharenkova2, E.Yu.. Kaptelov2, M.V. Staritsyn3
1 Tver State University
2 Ioffe Institute
3 Central Research Institute of Structural Materials «Prometey» named by I.V. Gorynin of National Research Center «Kurchatov Institute»
DOI: 10.26456/pcascnn/2026.18.044
Original article
Abstract: AlGaN-based heterostructures are functional materials for various applications in microelectronics and optics, owing to the preservation of their thermal and electrical properties over a wide temperature range. In this study, AlxGa1-xN thin-film multilayer structures were grown on SiC/Si substrates using hydride vapour phase epitaxy. Their microstructural characteristics were investigated using X-ray diffraction, phase analysis, and scanning electron microscopy. Microstructural analysis reveals that the thin-film structures under investigation are complex compounds containing AlGaN nanolayers of different composition. An analysis of the formation processes of the interlayers within the periodic AlGaN structure indicates that this structure results from the compositional self-organization and formation of a complex composite material. Studies of the dielectric response of AlGaN-based films have revealed that composites incorporating a multilayer structure exhibit dielectric permittivity dispersion; the magnitude of the permittivity increases significantly – particularly in the low-frequency range – due to enhanced ohmic conductivity. The complex behaviour of the dielectric loss tangent and the capacitance-voltage characteristics corroborates the conclusion that structures containing AlGaN layers possess significant electrical conductivity. In the high-frequency range, this dielectric response can be attributed to a space-charge polarization arising at the boundaries between AlGaN layers of different compositions, as well as at the AlGaN/SiC interface.
Keywords: silicon carbide-on-silicon substrates, chloride-hydride epitaxy, epitaxial AlGaN layers, dielectric permittivity dispersion, capacitance-voltage characteristics
- Ivan T. Zezyanov – 4th year postgraduate student, Condensed Matter Department, Tver State University
- Alexander V. Solnyshkin – Dr. Sc., Professor, Condensed Matter Department, Tver State University, ORCID: 0000-0002-4044-8761
- Olga N. Sergeeva – Ph. D., Senior Engineer, Condensed Matter Department, Tver State University, ORCID: 0000-0001-9469-4063
- Shukrillo Sh. Sharofidinov – Ph. D., Senior Researcher, Ioffe Institute, ORCID: 0000-0003-0354-5981
- Igor P. Pronin – Dr. Sc., Senior Researcher, Leading Researcher, Ioffe Institute, ORCID: 0000-0003-3749-8706
- Natalya V. Sharenkova – Ph. D., Senior Researcher, Ioffe Institute, ORCID: 0000-0001-6471-6233
- Evgeny Yu.. Kaptelov – Ph. D., Senior Researcher, Ioffe Institute, ORCID: 0000-0002-7423-6943
- Mikhail V. Staritsyn – Ph. D., Senior Researcher, Central Research Institute of Structural Materials «Prometey» named by I.V. Gorynin of National Research Center «Kurchatov Institute», ORCID: 0000-0002-0088-4577
For citation:
Zezyanov I.T., Solnyshkin A.V., Sergeeva O.N., Sharofidinov Sh.Sh., Pronin I.P., Sharenkova N.V., Kaptelov E.Yu.., Staritsyn M.V. Dielektricheskij otklik v tonkoplenochnykh geterostrukturakh s nanosloyami AlGaN [Dielectric response in thin-film heterostructures with AlGaN nanolayers], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 44-53. DOI: 10.26456/pcascnn/2026.18.044. ⎘
Full article (in Russian): download PDF file
References:
1. Chen Yu., Ben J., Xu F. et al. Review on the progress of AlGaN-based ultraviolet light-emitting diodes, Fundamental Research, 2021, vol. 1, issue 6, pp.717-734. DOI: 10.1016/j.fmre.2021.11.005.
2. Baca A.G., Armstrong A.M., Klein B.A. et al Al-rich AlGaN based transistors, Journal of Vacuum Science & Technology А, 2020, vol. 38, issue 1-2, art. no. 020803, 28 p. DOI: 10.1116/1.5129803.
3. Teo K.H., Zhang Y., Chowdhury N. et al. Emerging GaN technologies for power, RF, digital, and quantum computing applications. Recent advances and prospects, Journal of Applied Physics, 2021, vol. 130, issue 16, art. no. 160902, 41 p. DOI: 10.1063/5.0061555.
4. Rabih A.A.S., Kazemi M, Ménard M. et al. Aluminum nitride out-of-plane piezoelectric MEMS actuators, Micromachines, 2023, vol. 14, issue 3, art. no. 700, 19 p. DOI: 10.3390/mi14030700.
5. Qi H., Zhang H., Gao N. et al. Simulation and preparation of FBARs based on AlN thin films, Materials Science in Semiconductor Processing, 2025, vol. 185, art. no. 108886, 25 p. DOI: 10.1016/j.mssp.2024.108886.
6. Yadav N., Dutta S., Narang K. et al. Effect of growth induced residual stress in epitaxial AlN thin film on SiC substrate for MEMS, Transactions on Electrical and Electronic Materials, 2025, vol. 26, issue 1, pp. 125-133. DOI: 10.1007/s42341-024-00580-x.
7. Cao L.C.T., Hsu S.H., Chu C.-L. Fluoride monolayer doping in GaN/AlGaN/GaN semiconductor, MRS Advances, 2023, vol. 8, issue 16, pp. 931-936. DOI: 10.1557/s43580-023-00582-6.
8. Xu X.-H., Wu H.-S., Zhang C.-J. et al. Morphological properties of AlN piezoelectric thin films deposited by DC reactive magnetron sputtering, Thin Solid Films, 2001, vol. 388, issue 1-2, pp. 62-67. DOI: 10.1016/S0040-6090(00)01914-3.
9. Barshilia H.C., Deepthi B., Rajam K.S. Growth and characterization of aluminum nitride coatings prepared by pulsed-direct current reactive unbalanced magnetron sputtering, Thin Solid Films, 2008, vol. 516, issue 12, pp. 4168-4174. DOI: 10.1016/j.tsf.2007.10.129.
10. Kukushkin S.A., Sharofidinov Sh.Sh. A new method of growing AlN, GaN, and AlGaN bulk crystals using hybrid SiC/Si substrates, Physics of the Solid State, 2019, vol. 61, issue 12, pp. 2342-2347. DOI: 10.1134/S1063783419120254.
11. Kukushkin S.A., Osipov A.V., Feoktistov N.A. Synthesis of epitaxial silicon carbide films through the substitution of atoms in the silicon crystal lattice: A review, Physics of the Solid State, 2014, vol. 56, issue 8, pp. 1507-1535. DOI: 10.1134/S1063783414080137.
12. Kukushkin S.A., Sharofidinov Sh.Sh., Osipov A.V. et al. Self-organization of the composition of AlxGa1–xN films grown on hybrid SiC/Si substrates, Physics of the Solid State, 2021, vol. 63, issue 3, pp. 442-448. DOI: 10.1134/S1063783421030100.
13. Solnyshkin A.V., Zezyanov I.T., Sergeeva O.N. et al. Vliyanie stechiometrii sostava plyonok nitrida aluminia na dielectricheskiy otklik [Influence of stoichiometry of aluminum nitride films composition on the dielectric response], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 172-181. DOI: 10.26456/pcascnn/2025.17.172. (In Russian).
14. Sharofidinov Sh.Sh., Kukushkin S.A., Staritsyn M.V. et al. Structure and properties of composites based on aluminum and gallium nitrides grown on silicon of different orientations with a buffer layer of silicon carbide, Physics of the Solid State, 2022, vol. 64, issue 5, pp. 516-521. DOI: 10.21883/PSS.2022.05.53510.250.
15. Byrum L.E., Ariyawansa G., Jayasinghe R.C. et al. Capacitance hysteresis in GaN/AlGaN heterostructures, Journal of Applied Physics, 2009, vol. 105, issue 2, art. no. 023709, 5 p. DOI: 10.1063/1.3068179.
16. Solnyshkin A.V., Sergeeva O.N., Shustova O.A. et al. Dielectric and pyroelectric properties of composites based on aluminum and gallium nitrides grown by chloride-hydride epitaxy on a silicon carbide-on-silicon substrate, Technical Physics Letters, 2021, vol.47, issue. 6, pp. 466-469. DOI: 10.1134/S1063785021050138.
17. Foutz B., Smart J., Shealy J. R. et al. Two dimensional electron gases induced by spontaneous and piezoelectric polarization in undoped and doped AlGaN/GaN heterostructures, Journal of Applied Physics, 2000, vol. 87, issue 1, pp. 334-344. DOI: 10.1063/1.371866.
18. Ambacher O., Christian B., Yassine M. et al. Polarization induced interface and electron sheet charges of pseudomorphic ScAlN/GaN, GaAlN/GaN, InAlN/GaN, and InAlN/InN heterostructures, Journal of Applied Physics, 2021, vol. 129, issue 20, art. no 204501, 15 p. DOI: 10.1063/5.0049185.
19. Sergeeva O.N., Solnyshkin A.V., Nekrasova G.M. et al. Microstructure and electrical response of thin SiC films on Si substrates of p- and n-types, Ferroelectrics, 2019, vol. 542, issue 1, pp. 52-57. DOI: 10.1080/00150193.2019.1574662.