QTAIM analysis of tetracene, pentacene, and their monochloro-substituted derivatives: the effect of positional isomerism on the topology of electron density and semiconductor parameters
A.M. Rikhmaier, E.M. Chernova, Yu.D. Orlov, M.A. Rikhmaier
Tver State University
DOI: 10.26456/pcascnn/2026.18.493
Original article
Abstract: Using the B3LYP density functional theory method with a 6-311G basis set and subsequent topological analysis of the electron density within the framework of the quantum theory of atoms in a molecule, a systematic study of tetracene, pentacene, and their monochloro-substituted positional isomers was conducted. For each of the considered compounds, the ionization energies and electron affinities were calculated, as well as the band gap width. By means of topological analysis of the electron density, changes in the charges and volumes of atomic fragments caused by the substitution of one of the hydrogen atoms by chlorine are quantitatively characterized. It is revealed that monochloro substitution leads to a local redistribution of the electron density. The maximum changes in integral parameters are observed in the immediate vicinity of the substitution site. It is shown that the perturbation decays at a distance of 3 or more bonds, and the connecting carbon atoms remain practically inert to the substitution. The results of this study can serve as a basis for developing a method for predicting the semiconductor properties of monochlorinated polyaromatic hydrocarbons by varying the position of the chlorine atom in the compound structure, which opens up opportunities for molecular design of organic semiconductors with predefined parameters.
Keywords: positional isomerism, tetracene, pentacene, DFT, QTAIM, ionization energy, electron affinity energy, band gap, atomic charge, atomic volume
- Artem M. Rikhmaier – 3rd year postgraduate student, General Physics Department, Tver State University, ORCID: 0009-0000-0993-5118
- Elena M. Chernova – Ph. D., Associate Professor, General Physics Department, Tver State University, ORCID: 0000-0001-8734-2350
- Yuri D. Orlov – Dr. Sc., Professor, Head of the General Physics Department, Tver State University, ORCID: 0000-0003-1291-6019
- Maria A. Rikhmaier – 1st year postgraduate student, General Physics Department, Tver State University, ORCID: 0009-0002-3978-9304
For citation:
Rikhmaier A.M., Chernova E.M., Orlov Yu.D., Rikhmaier M.A. QTAIM-analiz tetratsena, pentatsena i ikh monokhlorzameshchennykh proizvodnykh: vliyanie pozitsionnoj izomerii na topologiyu elektronnoj plotnosti i poluprovodnikovye parametry [QTAIM analysis of tetracene, pentacene, and their monochloro-substituted derivatives: the effect of positional isomerism on the topology of electron density and semiconductor parameters], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 493-503. DOI: 10.26456/pcascnn/2026.18.493. ⎘
Full article (in Russian): download PDF file
References:
1. Zade S.S., Bendikov M. Reactivity of acenes: mechanisms and dependence on acene length, Journal of Physical Organic Chemistry, 2012, vol. 25, issue 6, pp. 452-461. DOI: 10.1002/poc.1941.
2. Musa A., Saeed M.A., Shaari A. et al. Linear acenes linked thiophene, electronic and chemical properties: prospects for molecular organic electronic material, Jurnal Teknologi, 2016, vol. 78, no. 6-11, pp. 67-72. DOI: 10.11113/jt.v78.9199.
3. Chow T.J. Hexacene: synthesis, properties and future perspectives, The Chemical Record, 2015, vol. 15, issue 6, pp. 1137-1139. DOI: 10.1002/tcr.201510003.
4. Stuart A.N., Kee T.W., Huang D.M. Role of singlet and triplet excited states in the oxygen-mediated photophysics and photodegradation of polyacenes, Journal of the American Chemical Society, 2024, vol. 146, issue 3, pp. 2174-2186. DOI: 10.1021/jacs.3c12245.
5. Tang M.L., Oh J.H., Reichardt A.D., Bao Z. Chlorination: a general route toward electron transport in organic semiconductors, Journal of the American Chemical Society, 2009, vol. 131, issue 10, pp. 3733-3740. DOI: 10.1021/ja809045s.
6. Bader R.F.W. Atoms in molecules: a quantum theory, International series of monographs on chemistry, Oxford, Clarendon Press, 1990, vol. 22, 438 p.
7. Popelier P.L.A. Atoms in molecules: an introduction. Essex, Pearson Education, 2000, 164 p.
8. Chernova E.M., Miroshnichenko E.A., Rihmaier M.A., Orlov M.Yu., Orlov Yu.D. Issledovanie e`lektronnogo stroeniya molekuly` naftalina i ego radikalov [Investigation of the electronic structure of the naphthalene molecule and its radicals]. Vestnik Tverskogo gosudarstvennogo universiteta. Seriya «Khimiya» [Bulletin of Tver State University. Chemistry Series], 2022, no. 3 (49), pp. 125-129. DOI: 10.26456/vtchem2022.3.15. (In Russian).
9. Сhernova E.M., Rusakova N.P., Miroshnichenko E.A., Orlov Yu.D. Vliyanie svobodnoj valentnosti na raspredelenie elektronnoj plotnosti v benzol'nom kol'tse [Effect of free valence on the electron density distribution in a benzene ring], Vestnik Tverskogo gosudarstvennogo universiteta. Seriya «Khimiya» [Bulletin of Tver State University. Chemistry Series], 2021, no. 4 (46), pp. 85-89. DOI: 10.26456/vtchem2021.4.10. (In Russian).
10. Frisch M.J., Trucks G.W., Schlegel H.B. et al. Gaussian 16 (Revision B. 0.1), Wallingford CT, Gaussian Inc., 2016.
11. Lu L., Hu H., Hou H., Wang B. An improved B3LYP method in the calculation of organic thermochemistry and reactivity, Computational and Theoretical Chemistry, 2013, vol. 1015, pp. 64-71. DOI: 10.1016/j.comptc.2013.04.009.
12. Keith T.A. AIMAll (Version 11.09.18, Professional). Available at: www.url: http://aim.tkgristmill.com. (accessed 1.06.2025).
13. Rodrigues J.A., Cortez-Guzman F., Anderson J.S.M. Advanced in quantum chemical topology beyond QTAIM. Amsterdam, Elsevier, 2022, 568 p. DOI: 10.1016/C2020-0-03379-7.
14. Mamand D. M., Rasul H.H., Omer P.K., Qadr H.M. Theoretical and experimental investigation on ADT organic semiconductor in different solvents, Kondensirovannye sredy i mezhfaznye granitsy [Condensed Matter and Interphases], 2022, vol. 24, no.2, pp. 227-242. DOI: 10.17308/kcmf.2022.24/9263.
15. Kronik L., Kümmel S. Piecewise linearity, freedom from self-interaction, and a Coulomb asymptotic potential: Three related yet inequivalent properties of the exact density functional, Physical Chemistry Chemical Physics, 2020, vol. 22, issue 29, pp. 16467-16481. DOI: 10.1039/D0CP02564J.
16. Zhan C.-G., Nichols J.A., Dixon D.A. Ionization potential, electron affinity, electronegativity, hardness, and electron excitation energy: molecular properties from density functional theory orbital energies, Journal of Physical Chemistry A, 2003, vol. 107, issue 20, pp. 4184-4195. DOI: 10.1021/jp0225774.
17. Zhang G., Musgrave C. Comparison of DFT methods for molecular orbital eigenvalue calculations, Journal of Physical Chemistry A, 2007, vol. 111, issue 8, pp. 1554-1561. DOI: 10.1021/jp061633o.
18. Orlov Yu.D., Lavrov V.O., Lebedev Yu.A. Determination of enthalpies of formation of organic free radicals based on bond dissociation energies. 4. Alkyl-substituted derivatives of phenyl and benzyl, Russian Chemical Bulletin, 2001. vol. 50, issue 6, pp. 963-969. DOI: 10.1023/A:1011392513152.