Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Study of the parameters of carbon nanostructures synthesis in microwave co-pyrolysis of polystyrene and microcrystalline cellulose

A.N. Zaritovskii1, E.N. Kotenko1, S.V. Grishchuk1, V.A. Glazunova2,1, G.K. Volkova2,1

1 L.M. Litvinenko Institute of Physical Organic and Coal Chemistry
2 Galkin Donetsk Institute for Physics and Engineering

DOI: 10.26456/pcascnn/2026.18.624

Original article

Abstract: The parameters of the synthesis of carbon nanostructures during microwave catalytic co-pyrolysis of polymer materials were studied. Polystyrene, which is a typical high-carbon synthetic polymer, and microcrystalline cellulose, a renewable environmentally friendly source of carbon of plant origin, were selected as carbon donors. The processes were carried out in the presence of a mixture of nickel and iron oxalates, which serve as metal catalysts precursors, using granulated activated carbon of AG-3 grade as a microwave absorber to convert electromagnetic energy into thermal energy. The effect of microwave acceptor concentration, treatment time and method of preparing the reaction mixture on the formation of multi-walled carbon nanotubes was investigated. It has been established that the optimal conditions for the synthesis process of the target product are achieved at a microwave acceptor concentration of 40% (wt.) and a cyclic exposure to microwave radiation with a power of 1000 W for 5-12 minutes. The results of studies were confirmed by the data of transmission electron microscopy and X-ray phase analysis.

Keywords: microwave pyrolysis, carbon nanostructures, polystyrene, microcrystalline cellulose, nickel and iron oxalates, activated carbon

  • Aleksandr N. Zaritovskii – Ph. D., Senior Researcher, Department of Supramolecular Chemistry, L.M. Litvinenko Institute of Physical Organic and Coal Chemistry, ORCID: 0009-0001-1614-3087
  • Elena N. Kotenko – Researcher, Department of Supramolecular Chemistry, L.M. Litvinenko Institute of Physical Organic and Coal Chemistry, ORCID: 0009-0001-2026-7322
  • Svetlana V. Grishchuk – Junior Researcher, Department of Supramolecular Chemistry, L.M. Litvinenko Institute of Physical Organic and Coal Chemistry, ORCID: 0009-0006-0103-1898
  • Valentina A. Glazunova – Researcher, Department of Physics and Engineering of High Pressure and Advanced Technologies, Galkin Donetsk Institute for Physics and Engineering, Engineer, Department of Supramolecular Chemistry L.M. Litvinenko Institute of Physical Organic and Coal Chemistry
  • Galina K. Volkova – Researcher, Department of Physics and Engineering of High Pressure and Advanced Technologies, Galkin Donetsk Institute for Physics and Engineering, Engineer, Department of Supramolecular Chemistry L.M. Litvinenko Institute of Physical Organic and Coal Chemistry

For citation:

Zaritovskii A.N., Kotenko E.N., Grishchuk S.V., Glazunova V.A., Volkova G.K. Izuchenie parametrov sinteza uglerodnykh nanostruktur v mikrovolnovom sovmestnom pirolize polistirola i mikrokristallicheskoj tsellyulozy [Study of the parameters of carbon nanostructures synthesis in microwave co-pyrolysis of polystyrene and microcrystalline cellulose], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 624-633. DOI: 10.26456/pcascnn/2026.18.624. ⎘

Full article (in Russian): download PDF file

References:

1. Waluyo J., Purba I.T., Linanggeng Z.A. et al. Biomass pyrolysis: a comprehensive review of production methods, derived products, and sustainable applications in advanced materials, Applied Science and Engineering Progress, 2025, vol. 18, no. 2, art. no. 7645, 49 p. DOI: 10.14416/j.asep.2024.11.009.
2. Osman A.I., Nasr M., Aniagor C.O. et al. Synergistic technologies for a circular economy: upcycling waste plastics and biomass, Frontiers of Chemical Science and Engineering, 2025, vol. 19, issue 1, art. no. 2, 35 p. DOI: 10.1007/s11705-024-2507-0.
3. Cukierman A.L., Bonelli P.B. Strategies for sustainable synthesis processes of nanocarbons from biomass, Bio-Based Nanomaterials: Synthesis Protocols, Mechanisms and Applications, ed. by A.K. Mishra, C.N. Hussain. Amsterdam: Elsevier, 2022, chapter 2, pp. 21-51. DOI: 10.1016/B978-0-323-85148-0.00011-7.
4. Bazargan A., McKay G. A review – synthesis of carbon nanotubes from plastic wastes, Chemical Engineering Journal, 2012, vol. 195-196, pp. 377-391. DOI: 10.1016/j.cej.2012.03.077.
5. Williams P.T. Hydrogen and carbon nanotubes from pyrolysis-catalysis of waste plastics: a review, Waste and Biomass Valorization, 2021, vol. 12, issue 1, pp. 1-28. DOI: 10.1007/s12649-020-01054-w.
6. Zaritovskii A.N., Kotenko E.N., Grishchuk S.V. Vliyanie parametrov protsessa mikrovolnovogo kataliticheskogo piroliza tsellyulozy na sintez uglerodnykh nanostruktur [Influence of the parameters of microwave catalytic pyrolysis of cellulose on the carbon nanostructures synthesis], Fiziko-himičeskie aspekty izučeniâ klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 841-850. DOI: 10.26456/pcascnn/2025.17.841. (In Russian).
7. Weldekidan H., Mohanty A.K., Misra M. Upcycling of plastic wastes and biomass for sustainable graphitic carbon production: a critical review, ACS Environmental Au, 2022, vol. 2, issue 6, pp. 510-522. DOI: 10.1021/acsenvironau.2c00029.
8. Kovaleva N.Yu. Pererabotka otkhodov biomassy i plastikov metodom ikh sovmestnogo piroliza. Obzor [Processing of biomass and plastics waste by their copyrolysis – a review], Khimiczeskaya bezopasnost [Chemical Safety Science], 2023, vol. 7, no. 2, pp. 95-133. DOI: 10.25514/CHS.2023.2.25007. (In Russian).
9. Deng J., Yi B., Mašek O. et al. Co-pyrolysis of biomass and plastic waste into carbon materials with environmental applications: a critical review, Green Chemistry, 2025, vol. 27, issue 22, pp. 6320-6341. DOI: 10.1039/D4GC04842C.
10. Li Z., Peng K., Ji N. et al. Advanced mechanisms and applications of microwave-assisted synthesis of carbon-based materials: a brief review, Nanoscale Advances, 2025, vol. 7, issue 2, pp. 419-432. DOI: 10.1039/d4na00701h.
11. Kovaleva N.Yu. Perspektivy primeneniya mikrovolnovogo izlucheniya dlya piroliza razlichnykh vidov plastikovykh otkhodov [Prospects for the application of microwave radiation for the pyrolysis of various plastic waste types], Khimiczeskaya bezopasnost [Chemical Safety Science], 2025, vol. 9, no. 1, pp. 105-137. DOI: 10.25514/CHS.2025.1.28006. (In Russian).
12. Suriapparao D.V., Vinu R. Resource recovery from synthetic polymers via microwave pyrolysis using different susceptors, Journal of Analytical and Applied Pyrolysis, 2015, vol. 113, pp. 701-712. DOI: 10.1016/j.jaap.2015.04.21.
13. Yang C., Shang H., Li J. et al. Review on the microwave-assisted pyrolysis of waste plastics, Processes, 2023, vol. 11, art. no. 1487, 22 p. DOI: 10.3390/pr11051487.
14. Caroko N., Saptoadi H., Rohmat T.A. A review on microwave-assisted co-pyrolysis of biomass-polymer, International Review of Mechanical Engineering (IREME), 2020, vol. 14, no. 5, pp. 339-350. DOI: 10.15866/ireme.v14i5.19002.
15. Suriapparao D.V., Vinu R., Shukla A., Haldar S. Effective deoxygenation for the production of liquid biofuels via microwave assisted co-pyrolysis of agro residues and waste plastics combined with catalytic upgradation, Bioresource Technology, 2020, vol. 302, art. no. 122775, 10 p. DOI: 10.1016/j.biortech.2020.12277.
16. Suriapparao D.V., Tejasvi R. A review on role of process parameters on pyrolysis of biomass and plastics: present scope and future opportunities in conventional and microwave-assisted pyrolysis technologies, Process Safety and Environmental Protection, 2022, vol. 162, pp. 435-462. DOI: 10.1016/j.psep.2022.04.024.

Content |