Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Simulating the evaporation process of magnetic nanofluid to estimate the service life of magnetic fluid devices

A.N. Bolotov, O.O. Novikova

Tver State Technical University

DOI: 10.26456/pcascnn/2026.18.340

Original article

Abstract: A generalized approach to calculating the service life of magnetic fluid tribological units operating in vacuum and gas environments is presented. The physical mechanisms of magnetic nanofluid degradation during dispersion medium evaporation and increasing solid phase concentration are examined. A statistical approach developed by Ya. I. Frenkel is used to estimate the rate of nanofluid liquid phase evaporation into a vacuum. An equation for the time dependence of the dispersed phase concentration in a magnetic fluid was obtained for calculating the durability of magnetic fluid devices in a vacuum. The dynamics of magnetic nanofluid mass loss upon contact with a gaseous medium was described using a diffusion mass transfer equation. An electrostatic analogy method was used to solve this equation. The time during which the volume content of the dispersed phase of the magnetic nanofluid increases to a limiting value was determined for magnetic fluid tribounits with an open fluid surface and those enclosed in a chamber with a small opening. Based on the obtained calculation relationships linking evaporation parameters with changes in the volume fraction of the dispersed phase and the criterion of the maximum permissible viscosity, an engineering methodology for assessing the durability of magnetic fluid bearings and seals has been developed. Recommendations are given for the selection of magnetic fluid and operating modes that ensure an increase in its service life.

Keywords: magnetic fluid, evaporation, dispersion medium, friction unit life, viscosity, plain bearing

  • Alexander N. Bolotov – Dr. Sc., Professor, Head of the Applied Physics Department, Tver State Technical University, ORCID: 0000-0003-4054-5550
  • Olga O. Novikova – Ph. D., Full Docent, Applied Physics Department, Tver State Technical University, ORCID: 0000-0003-4133-3541

For citation:

Bolotov A.N., Novikova O.O. Modelirovanie protsessa ispareniya magnitnoj nanozhidkosti dlya otsenki prodolzhitelnosti funktsionirovaniya magnitozhidkostnykh uzlov [Simulating the evaporation process of magnetic nanofluid to estimate the service life of magnetic fluid devices], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 340-353. DOI: 10.26456/pcascnn/2026.18.340. ⎘

Full article (in Russian): download PDF file

References:

1. Orlov D.V., Mikhalev Yu.O., Myshkin N.K., Podgorkov V.V., Sizov A.P. Magnitnyye zhidkosti v mashinostroyenii [Magnetic fluids in mechanical engineering]. Moscow, Mashinostroyeniye Publ., 1993, 272 p. (In Russian).
2. Bolotov A.N., Khrenov V.L. Tribotekhnika magnitopassivnykh opor skol'zheniya [Tribotechnics of magnetopassive sliding bearings]. Tver, TGTU Publ., 2008, 124 p. (In Russian).
3. Huang W., Wang X. Ferrofluids lubrication: a status report, Lubrication Science, 2016, vol. 28, issue 1, pp. 3-26. DOI: 10.1002/ls.1291.
4. Xu M., Jin G., Dai Q., Huang W., Wang X. Ferrofluid lubrication for ball bearings to avoid starvation, Industrial Lubrication and Tribology, 2020, vol. 72, issue 10, pp. 1227-1231. DOI:10.1108/ILT-04-2020-0132.
5. Bolotov A.N., Novikov V.V., Pavlov V.G. Magnitozhidkostnyye podshipniki skol'zheniya [Magnetic fluid plain bearings], Treniye i iznos [Friction and wear], 2004, vol. 26, issue 3, pp. 286-289. (In Russian).
6. Bolotov A.N., Novikov V.V., Novikova O.O., Gorlov D.I Issledovaniye strukturnoy stabil'nosti magnitnykh masel dlya uzlov treniya [Study of structural stability of magnetic oils for friction units], Izvestiya Moskovskogo gosudarstvennogo tekhnicheskogo universiteta, MAMI [Bulletin of the Moscow State Technical University, MAMI], 2014, vol. 4, issue 2, pp. 15-17. (In Russian).
7. Ur'yev N.B. Makroskopicheskiye razryvy sploshnosti i sloistyy kharakter techeniya strukturirovannykh dispersiy v sdvigovom potoke [Macroscopic discontinuities in continuity and the layered nature of the flow of structured dispersions in a shear flow], Fizikokhimiya poverkhnosti i zashchita materialov [Physical chemistry of surfaces and protection of materials], 2012, vol. 48, issue 6, pp. 503-513. (In Russian).
8. Bolotov A.N., Novikov V.V., Novikova O.O. Dispersionnyye sredy dlya perspektivnykh smazochnykh magnitnykh zhidkostey [Dispersion media for promising lubricating magnetic fluids], 19-ya mezhdunarodnaya Plesskaya nauchnaya konferentsiya po nanodispersnym magnitnym zhidkostyam: Sbornik nauchnykh trudov, Ivanovo, 08–11 sentyabrya 2020 [19-th International Ples Scientific Conference on Nanodispersed Magnetic Fluids: Collection of Scientific Papers, Ivanovo, September 8–11, 2020]. Ivanovo, Ivanovo State Power Engineering University named after V.I. Lenin, 2020, pp. 287-294. (In Russian).
9. Iossel Yu.Ya., Kochanov E.S., Strunsky M.G. Raschet elektricheskoy yemkosti [Calculation of electrical capacitance]. Moscow, Energoizdat Publ., 1981, 288 p. (In Russian).
10. Saltykov S.A. Stereometricheskaya metallografiya [Stereometric metallography]. Moscow, Metallurgiya Publ., 1976, 270 p. (In Russian).
11. Zamkov Ye.T., Paliy A.V., Serba P.V. Opredeleniye tolshchiny pogranichnogo sloya pri obtekanii tela aerodinamicheskim potokom metodom elektrostaticheskoy analogii [Determination of the boundary layer thickness in an aerodynamic flow around a body using the electrostatic analogy method], Izvestiya YUFU. Tekhnicheskiye nauki [Bulletin of SFedU. Technical sciences], 2012, no. 1(126), pp. 191-196. (In Russian).
12. Frenkel' YA.I. Kineticheskaya teoriya zhidkostey [Kinetic theory of liquids]. Moscow, Publishing House of the USSR Academy of Sciences, 1945, 424 p. (In Russian).
13. Bolotov A.N., Novikova O.O. Vliyaniye nanodispersnoy fazy magnitnykh masel na ikh smazochnyye svoystva [Influence of the nanodispersed phase of magnetic oils on their lubricating properties], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 545-560. DOI 10.26456/pcascnn/2022.14.545.
14. Bolotov A.N., Novikova O.O. Eksperimental'noye issledovaniye tekuchesti nanostrukturirovannoy magnitnoy zhidkosti v sil'nom magnitnom pole [Experimental study of the fluidity of nanostructured magnetic fluid in a strong magnetic field], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 692-700. DOI: 10.26456/pcascnn/2023.15.692. (In Russian).
15. Sobolevskiy M.V., Skorokhodov I.I., Grinevich K.P. et al. Oligoorganosiloksany. Svoystva, polucheniye, primeneniye [Oligoorganosiloxanes. Properties, production, application], ed. by M.V. Sobolevskiy. Moscow, Khimiya Publ., 1985, 264 p. (In Russian).

Content |