Determination of the surface energy of the phase components of structural steel by the fatigue crack growth kinetics
L.P. Aref'eva, V.V. Kovaleva
Don State Technical University
DOI: 10.26456/pcascnn/2026.18.522
Original article
Abstract: The work is devoted to the determination of the surface energy of steel from experimental data on the crack growth and comparison with results of numerical modeling. The kinetics of fatigue fracture of a steel 1.0481 sample with a line ferrite-martensite structure obtained as a result of incomplete hardening and subsequent low-temperature tempering is investigated. Numerical modeling of the values of the surface energy of the ferrite and martensite crystallite faces is carried out by the electron-statistical method. As a result of a graphical differentiation of the dependence of the crack length on the number of loading cycles, the values of the crack propagation rate were obtained, the crack lengths were also estimated, and the surface energies of each phase were calculated in the Griffiths model. The error in determining the indirect values, obtained as a result of statistical data processing, is approximately 1%. The analysis conducted shows that the values of the crack growth rate are in good agreement with the results of studies on the rate of crack formation in normalized structural steels. The numerical simulation data are in agreement with experimental data within 16% and with reference data within 18%.
Keywords: surface energy, tensile strength, crack, structural steel, ferrite, martensite, two-phase structure
- Ludmila P. Aref'eva – Dr. Sc., Associate Professor, Professor, Department of Materials Science and Technology of Metals, Faculty of Mechanical Engineering Technology, Don State Technical University, ORCID: 0000-0003-2431-6897
- Valentina V. Kovaleva – Senior Lecturer, Department of Materials Science and Technology of Metals, Faculty of Mechanical Engineering Technology, Don State Technical University, ORCID: 0000-0001-7266-7224
For citation:
Aref'eva L.P., Kovaleva V.V. Opredelenie poverkhnostnoj energii fazovykh sostavlyayushchikh konstruktsionnoj stali po kinetike rosta ustalostnoj treshchiny [Determination of the surface energy of the phase components of structural steel by the fatigue crack growth kinetics], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 522-529. DOI: 10.26456/pcascnn/2026.18.522. ⎘
Full article (in Russian): download PDF file
References:
1. Gorbovets M.A., Khodinev I.A., Monin S.A. Ispytaniya konstruktsionnykh metallicheskikh materialov na skorost' rosta treshchiny ustalosti v korrozionno-aktivnoy srede (obzor) [Tests of structural metallic materials for the fatigue crack growth rate in a corrosive environment (review)], Trudy VIAM [Proceedings of VIAM], 2022, no. 12 (118), pp. 135-144. DOI: 10.18577/2307-6046-2022-0-12-135-144. (In Russian).
2. Pustovoit V.N., Dolgachev Yu.V., Dombrovskii Yu.M. Ballisticheskaya stoykost' stali so strukturoy yestestvennogo ferrito-martensitnogo kompozita [Ballistic resistance of steel with the structure of a natural ferrite-martensitic composite], Bezopasnost' tekhnogennykh i prirodnykh system [Safety of Technogenic and Natural Systems], 2022, no. 3, pp. 54-59. DOI: 10.23947/2541-9129-2022-3-54-59. (In Russian).
3. Atroshenko S.A., Maier S.S., Smirnov V.I. Structural phase state of the metal of a rail with an internal crack after long-term operation, Technical Physics, 2021, vol. 66, issue 11, pp 1171-1176. DOI: 10.1134/S1063784221090024.
4. Islamova A.G., Feoktistov D.V., Orlova E.G. Vliyanie sherokhovatosti na poverkhnostnuyu energiyu i smachivaemost' poverkhnostey medi i stali [Influence of the copper and steel surfaces’ roughness on surface energy and wettability], Vestnik Tyumenskogo gosudarstvennogo universiteta. Fiziko-matematicheskoe modelirovanie. Neft', gaz, energetika [Tyumen State University Herald. Physical and Mathematical Modeling. Oil, Gas, Energy], 2021, vol. 7, no. 1 (25), pp. 60-78. DOI: 10.21684/2411-7978-2021-7-1-60-78. (In Russian).
5. Musokhranov M.V., Kalmykov V.V., Malyshev E.N. Experimental research of variability of surface energy value of Fe37-3FN, C45 and 41Cr4 steels, International Journal of Applied Engineering Research, 2017, vol. 12, no. 17, pp. 6428-6433.
6. Pustovoit V.N., Dolgachev YU.V., Dombrovskii YU.M., Duka V.V. Strukturnaya organizatsiya i svoystva yestestvennogo stal'nogo ferritno-martensitnogo kompozita [The structure and properties of a natural steel ferritic-martensitic composite], Metallovedeniye i termicheskaya obrabotka metallov [Metal Science and Heat Treatment], 2020, no. 6(780), pp.15-21. DOI: 10.30906/mitom.2020.6.15-21. (In Russian).
7. Pustovoit V.N., Dolgachev Yu.V., Ivankov I.V. Structural organization of steel to ensure special equipment safety, Safety of Technogenic and Natural Systems, 2023, no. 1, pp. 70-75. DOI: 10.23947/2541-9129-2023-1-70-75
8. Duka V.V., Aref’eva L.P. Surface morphology identification of steel natural ferrite-martensitic composite using imagej software, Safety of Technogenic and Natural Systems, 2025, vol. 9, no. 3, pp. 221-229. DOI: 10.23947/2541-9129-2025-9-3-221-229. (In Russian).
9. Pustovoit V.N., Grishin S.A., Dolgachev YU.V., Duka V.V. Ustalostnoye razrusheniye stali so strukturoy ferrito-martensitnogo kompozita [Fatigue fracture of steel with ferrite-martensite composite structure], Izvestiya vuzov. Chernaya metallurgiya [Izvestiya. Ferrous metallurgy], 2022, vol. 65, no. 2, pp. 92-97. DOI: 10.17073/0368-0797-2022-2-92-97. (In Russian).
10. Shebzukhova I.G., Aref'eva L.P. Anisotropy of the surface energy and work function of IIB metals, Technical Physics, 2019, vol. 64, issue 2, pp. 274-277. DOI: 10.1134/S1063784219020208.
11. Aref’eva L.P., Duka V.V., Zabiyaka I.Y. Relationship between the structural-phase composition and the fracture mechanism of high-strength contraction steel, Technical Physics Letters, 2022, vol. 48, no. 4, pp. 72-74. DOI: 10.21883/TPL.2022.04.53490.19093.
12. Golubovskiy E.R., Volkov M.E., Emmausskiy N.M. Metod opredeleniya granits stadii ustoychivogo rosta treshchiny ustalosti i parametrov uravneniya Perisa [A method for determination of the boundaries of the stage of steady fatigue crack growth and parameters of Paris equation], Zavodskaya laboratoriya. Diagnostika materialov [Industrial laboratopy. Diagnostics of materials], 2019, vol. 85, no. 9, pp. 66-74. DOI: 10.26896/1028-6861-2019-85-9-66-74. (In Russian).
13. Pustovoit V.N., Dolgachev YU.V., Dombrovskii YU.M., Duka V.V. Structural organization and properties of a natural ferrite-martensite steel composite, Metal Science and Heat Treatment, 2020, vol. 62, issue 5-6, pp. 369-375. DOI: 10.1007/s11041-020-00570-9.
14. Klevtsov G.V., Merson D.L., Klevtsova N.A. et al Kinetika i mekhanizm ustalostnogo razrusheniya obraztsov iz staley 40KH i 38KH2N2MA [The kinetics and mechanism of the fatigue fracture of samples of 40H and 38H2N2MA steels], Vektor nauki tol'yattinskogo gosudarstvennogo universiteta [Science Vector of Togliatti State University], 2019, no. 1(47), pp. 30-36. DOI: 10.18323/2073-5073-2019-1-30-36. (In Russian).
15. Savkin A.N., Sunder R., Badikov K.A., Sedov A.A. Kinetika i prodolzhitel'nost' rosta ustalostnykh treshchin v stalyakh pri peremennom nagruzhenii [Fatigue crack growth kinetic on steels under variable amplitude loading], Vestnik Permskogo natsional'nogo issledovatel'skogo politekhnicheskogo universiteta. Mekhanika [PNRPU Mechanics Bulletin], 2018, no. 3, pp. 61-70. DOI: 10.15593/perm.mech/2018.3.07. (In Russian).
16. Svoystva elementov. Spravochnik [Properties of elements. Handbook], ed. M.E. Drits, Moscow, Metallurgiya Publ., 1985, 672 p. (In Russian).