Effect of ultraviolet radiation on the selectivity of zinc oxide gas sensors

N.A. Klychkov, V.V. Simakov, I.V. Sinev, A.D. Chirkova

Saratov State University

DOI: 10.26456/pcascnn/2026.18.668

Original article

Abstract: This work investigates the effect of ultraviolet irradiation intensity on the response and selectivity of gas sensors based on zinc oxide ZnO layers. The ZnO layers were synthesized by chemical deposition followed by thermal annealing at 400°C in an oxygen-containing atmosphere. It is shown that UV irradiation at 365 nm with intensities from 5 mW/cm² to 20 mW/cm² enhances the sensor response to ethanol, isopropanol, and acetone vapors by up to 10 times. The dependence of the photo-response magnitude on the gas environment observed upon irradiation at 400 nm and 525 nm indicates ionization of deep impurity centers induced by adsorbed gas molecules. From the concentration dependences of the sensor response, the selectivity and specificity coefficients are calculated, demonstrating a 2‑fold increase in selectivity to ethanol with increasing illumination intensity. The obtained results reveal that varying the illumination intensity enables control over the sensor selectivity through the selective ionization of surface states associated with different adsorbed gases.

Keywords: zinc oxide, photoactivation, gas sensor response, selectivity, specificity, impurity centers

  • Nikita A. Klychkov – 4th year postgraduate student, Assistant at the Department of Materials Science, Technology and Quality Management, Saratov State University, ORCID: 0009-0003-7969-3291
  • Viacheslav V. Simakov – Dr. Sc., Professor, Material Sciences, Technologies and Quality Management Department, Saratov State University, ORCID: 0000-0001-9665-5930
  • Ilya V. Sinev – Ph. D., Docent, Material Sciences, Technologies and Quality Management Department, Saratov State University, ORCID: 0000-0002-1005-1616
  • Anastasiya D. Chirkova – Senior Laboratory Specialist, Saratov State University

For citation:

Klychkov N.A., Simakov V.V., Sinev I.V., Chirkova A.D. Vliyanie ultrafioletovogo izlucheniya na selektivnost gazovykh sensorov na osnove oksida tsinka [Effect of ultraviolet radiation on the selectivity of zinc oxide gas sensors], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 668-678. DOI: 10.26456/pcascnn/2026.18.668. ⎘

Full article (in Russian): download PDF file

References:

1. Espid E., Taghipour F. UV-LED photo-activated chemical gas sensors: a review, Critical Reviews in Solid State and Materials Sciences, 2017, vol. 42, issue 5, pp. 416-432. DOI: 10.1080/10408436.2016.1226161.
2. de Lacy Costello B.P.J., Ewen R.J., Ratcliffe N.M., Richards M. Highly sensitive room temperature sensors based on the UV-LED activation of zinc oxide nanoparticles, Sensors and Actuators B: Chemical, 2008, vol. 134, issue 2, pp. 945-952. DOI: 10.1016/j.snb.2008.06.055.
3. Korotcenkov G. Metal oxides for solid-state gas sensors: What determines our choice?, Materials Science and Engineering B, 2007, vol. 139, issue 1, pp. 1-23. DOI: 10.1016/j.mseb.2007.01.044.
4. Klychkov N.A., Simakov V.V., Sinev I.V. et al. Upravlenie morfologiej i provodimostyu geksagonalnykh nanosterzhnej ZnO s pomoshchyu termoobrabotki dlya prilozhenij gazovoj sensoriki [Morphology and conductivity control in hexagonal ZnO nanorods through annealing for gas sensor applications], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 649-657. DOI: 10.26456/pcascnn/2025.17.649. (In Russian).
5. Wang C., Yin L., Zhang L., Xiang D., Gao R. Metal oxide gas sensors: sensitivity and influencing factors, Sensors, 2010, vol. 10, issue 3, pp. 2088-2106. DOI: 10.3390/s100302088.
6. Yoshikawa H., Adachi S. Optical constants of ZnO, Japanese Journal of Applied Physics, 1997, vol. 36, no. 10R, pp. 6237-6243. DOI: 10.1143/JJAP.36.6237.
7. Geng Q., He Z., Chen X. et al. Gas sensing property of ZnO under visible light irradiation at room temperature, Sensors and Actuators B: Chemical, 2013, vol. 188, pp. 293-297. DOI: 10.1016/j.snb.2013.07.001.
8. Wang Y., Li X., Wang N. et al. Controllable synthesis of ZnO nanoflowers and their morphology-dependent photocatalytic activities, Separation and Purification Technology, 2008, vol. 62, issue 3, pp. 727-732. DOI: 10.1016/j.seppur.2008.03.035.
9. Ryabko A.A., Nalimova S.S., Mazing D.S. et al. Sensitization of ZnO nanorods by AgInS2 colloidal quantum dots for adsorption gas sensors with light activation, Technical Physics, 2022, vol. 67, no. 6, pp. 717-722. DOI: 10.21883/TP.2022.06.54418.15-22.
10. Klychkov N.A., Simakov V.V., Sinev I.V. Light-assisted gas identification using ZnO semiconductor sensors, Semiconductors, 2025, vol. 59, issue 5, pp. 241-245. DOI: 10.61011/SC.2025.05.61987.7910.
11. Vorobyeva N., Rumyantseva M., Konstantinova E. et al. Inversion of NH₃ sensor signal and paramagnetic centers of nanocrystalline ZnO(Ga), Procedia Engineering, 2011, vol. 25, pp. 296-299. DOI: 10.1016/j.proeng.2011.12.073.
12. Fan S.W., Srivastava A.K., Dravid V.P. UV-activated room-temperature gas sensing mechanism of polycrystalline ZnO, Applied Physics Letters, 2009, vol. 95, issue 14, art. no. 142106, 3 p. DOI: 10.1063/1.3243458.
13. Gulyaeva I.A., Ivanisheva A.P., Volkova M.G. et al. Investigation of electrophysical, photo- and gas-sensitive properties of ZnO–SnO₂ sol-gel films, Journal of Advanced Dielectrics, 2024, vol. 14, no. 1, art. no. 2245002, 9 p. DOI: 10.1142/S2010135X22450023.
14. Deng Q., Gao S., Lei T. et al. Temperature and light modulation to enhance the selectivity of Pt-modified zinc oxide gas sensor, Sensors and Actuators B: Chemical, 2017, vol. 247, pp. 903-915. DOI: 10.1016/j.snb.2017.03.107.
15. Simakov V.V., Yakusheva O.V., Grebennikov A.I., Kisin V.V. Current-voltage characteristics of thin-film gas sensor structures based on tin dioxide, Technical Physics Letters, 2005, vol. 31, issue 4, pp. 339-340.
16. Smirnov A.V., Grebennikov A.I., Gribov A.N. et al. Otklik gazochuvstvitel`noj mikrosistemy` na zapax peregretoj izolyacii e`lektricheskogo kabelya [Response of a gas-sensitive microsystem to the smell of overheated electrical cable insulation], Nano-i mikrosistemnaya tekhnika [Nano- and Microsystems Technology], 2014, no. 2, pp. 53-56. (In Russian).
17. Sinev I.V., Klychkov N.A., Timoshenko D.A., Simakov V.V. Vliyanie osveshcheniya na raspoznavatelnuyu sposobnost multisensornikh mikrosistem na osnove nitevidnikh nanokristallov dioksida olova [Illumination effect on recognition ability of multisensor microsystems based on tin oxide nanowhiskers], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 713-721. DOI: 10.26456/pcascnn/2020.12.713.
18. Danzer K. Selectivity and specificity in analytical chemistry. General considerations and attempt of a definition and quantification, Fresenius' Journal of Analytical Chemistry, 2001, vol. 369, issue 5, pp. 397-402. DOI: 10.1007/s002160000684.

Content |