Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Dependence of sintering parameters for nanosized complex oxide powders on intensity of charge generation during synthesis from nitrate-organic precursors

A.A. Ostroushko, A.E. Permyakova, T.Yu. Zhulanova

Ural Federal University named after the first President of Russia B.N. Yeltsin

DOI: 10.26456/pcascnn/2026.18.102

Original article

Abstract: Parameters of the sintering process for compacted complex oxide powders based on lanthanum strontium manganite with a perovskite-type structure were studied: the temperature of intensive sintering and the achieved shrinkage of the workpiece. The studied complex oxide samples were obtained in the combustion reactions of nitrate-organic precursors (the so-called solution combustion method). During the synthesis, the composition of the precursors was varied: the nature of the organic component (polyvinyl alcohol, polyvinylpyrrolidone, glycine) and its relative content in relation to the stoichiometry of the combustion reaction with the formation of water vapor, molecular nitrogen and carbon dioxide as gaseous products. At the same time, positive or negative electric charges were generated in the precursors due to the formation and carry-over with the released gases of ionized molecular groups. The intensity of this process was monitored using an electrostatic field meter. The ground-precursor potential difference, depending on the composition of the initial composition, ranged from values close to zero to several tens of volts. With intensive generation due to the accumulation of the excess surface energy of mutually repulsive nanoparticles of the complex oxide, the temperature of intensive sintering decreased by 350 degrees compared to that (1050°C) for materials obtained from precursors with a low intensity of charge formation. The relative shrinkage of samples of the first type increased from 3 to 23%. The established correlation was universal and practically independent of the sign of the generated charge.

Keywords: nanosized powders, synthesis of nitrate-organic precursors in combustion reactions, charge generation, sintering, complex oxides, lanthanum-strontium manganite

  • Alexander A. Ostroushko – Dr. Sc., Professor, Head of Department of Chemical Materials Science, Chief Researcher, Institute of Natural Sciences and Mathematics, Ural Federal University named after the first President of Russia B.N. Yeltsin, ORCID: 0000-0003-0206-5513
  • Anastasiya E. Permyakova – 3rd year postgraduate student, Department of Physical and Inorganic Chemistry, Ural Federal University named after the first President of Russia B.N. Yeltsin, ORCID: 0009-0004-3194-4626
  • Tatiana Yu. Zhulanova – Laboratory Research Assistant, Department of Chemical Materials Science, Institute of Natural Sciences and Mathematics, Ural Federal University named after the first President of Russia B.N. Yeltsin, ORCID: 0000-0002-8009-4398

For citation:

Ostroushko A.A., Permyakova A.E., Zhulanova T.Yu. Zavisimost parametrov spekaniya nanorazmernykh slozhnooksidnykh poroshkov ot intensivnosti generirovaniya zaryadov pri sinteze iz nitrat-organicheskikh prekursorov [Dependence of sintering parameters for nanosized complex oxide powders on intensity of charge generation during synthesis from nitrate-organic precursors], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 102-111. DOI: 10.26456/pcascnn/2026.18.102. ⎘

Full article (in Russian): download PDF file

References:

1. Aruna S.T., Mukasyan A.S. Combustion synthesis and nanomaterials, Current Opinion in Solid State and Materials Science, 2008, vol. 12, issue 3-4, pp. 44-50. DOI: 10.1016/j.cossms.2008.12.002.
2. Manukyan K.V., Cross A., Roslyakov S. et al. Solution combustion synthesis of nano-crystalline metallic materials: mechanistic studies, Journal of Physical Chemistry C, 2013, vol. 117, issue 46, pp. 24417-24427. DOI: 10.1021/jp408260m.
3. Wen W., Wu J-M. Nanomaterials via solution combustion synthesis: a step nearer to controllability, RSC Advances, 2014, vol. 4, issue 101, pp. 58090-58100. DOI: 10.1039/C4RA10145F.
4. Varma A., Mukasyan A.S., Rogachev A.S., Manukyan K.V. Solution combustion synthesis of nanoscale materials, Chemical Reviews, 2016, vol. 11, issue 23, pp. 14493-14586. DOI: 10.1021/acs.chemrev.6b00279.
5. Thoda O., Xanthopoulou G., Vekinis G., Chroneos A. Review of Recent Studies on Solution Combustion Synthesis of Nanostructured Catalysts, Advanced Engineering Materials, 2018, vol. 20, issue 8, art. no. 1800047, 30 p. DOI: 10.1002/adem.201800047.
6. Deganello F., Tyagi A.K. Solution combustion synthesis, energy and environment: Best parameters for better materials, Progress in Crystal Growth and Characterization of Materials, 2018, vol. 64, issue 2, pp. 23-61. DOI: 10.1016/j.pcrysgrow.2018.03.001.
7. Novitskaya E., Kelly J.P., Bhaduri S., Graeve O.A. A review of solution combustion synthesis: an analysis of parameters controlling powder characteristics, International Materials Reviews, 2021, vol. 66, issue 3, pp. 188-214. DOI: 10.1080/09506608.2020.1765603.
8. Parauha Y.R., Sahu V., Dhoble S.J. Prospective of combustion method for preparation of nanomaterials: a challenge, Materials Science and Engineering B, 2021, vol. 267, art. no. 115054, 29 p. DOI: 10.1016/j.mseb.2021.115054.
9. Padayatchee S., Ibrahim H., Friedrich H.B. et al. Solution combustion synthesis for various applications: a review of the mixed-fuel approach, Fluids, 2025, vol. 10, issue 4, art. no. 82, 24 p. DOI: 10.3390/fluids10040082.
10. Tomina E.V., Kurkin N.A., Doroshenko A.V. Synthesis of nanoparticulate cobalt ferrite and its catalytic properties for fenton-like processes, Inorganic Materials, 2022, vol. 58, issue 7, pp. 701-705. DOI: 10.1134/S0020168522070135.
11. Tomina E.V., Kurkin N.A., Cherednichenko I.S., Lukin A.N. The effect of the synthesis method on the composition, morphology, and catalytic properties of nanosized bismuth ferrite, Russian Journal of Inorganic Chemistry, 2024, vol. 69, issue 11, pp. 1626-1636. .
12. Ostroushko A.A., Sennikov, M.Yu. Thermochemical charge generation in polymer-salt films, Russian Journal of Inorganic Chemistry, 2005, vol. 50, issue 6, pp. 933-936.
13. Ostroushko A.A., Russkikh O.V., Maksimchuk T.Yu. Charge generation during the synthesis of doped lanthanum manganites via combustion of organo-inorganic precursors, Ceramic International, 2021, vol. 47, issue 15, pp. 21905-21914. DOI: 10.1016/j.ceramint.2021.04.208.
14. Ostroushko A.A., Russkikh O.V., Gagarin I.D., Filonova E.A. Izuchenie generirovaniya zaryadov pri sinteze nanorazmernykh slozhnykh oksidov v reaktsiyakh organo-neorganicheskikh prekursorov [Study of the charge generation in the synthesis of nanosized complex oxides in the combustion reactions of organo-inorganic precursors], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2019, issue 11, pp. 215-222. DOI: 10.26456/pcascnn/2019.11.215.
15. Ostroushko A.A., Zhulanova T.Y., Permyakova A.E., Russkikh O.V. Determinative factors for the thermochemical generation of electric charges upon combustion of nitrate–organic precursors for materials based on lanthanum manganite and cerium dioxide, Russian Journal of Inorganic Chemistry, 2022, vol. 67, issue 6, pp. 799-809. DOI: 10.1134/S0036023622060171.
16. Russkikh O., Permyakova A., Filonova E. et al. Synthesis, structure and catalytic activity features of alkali-substituted nanostructured lanthanum manganites, Materialia, 2026, vol. 45, art. no. 102665, 28 p. DOI: 10.1016/j.mtla.2026.102665.
17. Ostroushko A.A., Vylkov A.I., Zhulanova T.Yu. et al. Vliyanie nanorazmernykh dobavok na temperaturu spekaniya oksida alyuminiya [Influece of nanoscale additives on the sintering temperature of aluminium oxide], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue. 15, pp. 799-806. DOI: 10.26456/pcascnn/2023.15.799. (In Russian).
18. Ivanov V.V., Kotov Yu.A., Lipilin A.S. et al. Elektroliticheskoe formirovanie tonkoplionochnogo electrolyta na nesushchem katode TOTE [Electrophoretic formation of electrolyte layer on cathode surface of cathode supported SOFC], Mezhdunarodnyj nauchnyj zhurnal «Al'ternativnaya energetika i ekologiya» [International scientific journal «Alternative Energy and Ecology»], 2008, no. 10 (66), pp. 36-50. (In Russian).
19. Ostroushko A.A., Gagarin I.D., Kudyukov E.V. et al. Synthesis of lanthanum manganite powders via combustion reactions: some aspects of the influence of magnetic field and charge generation in precursors on the formation of properties, Nanosistemy: fizika, khimiya, matematika [Nanosystems: Physics, Chemistry, Mathematics], 2023, vol. 14, issue 5, pp. 571-583. DOI: 10.17586/2220-8054-2023-14-5-571-583.

Content |