Influence of electrophysical and thermodynamic parameters of electroexplosive synthesis on the crystal structure and dispersed composition of multicomponent NiFeCoCrCuAlMoW nanoparticles
K.V. Suliz, A.V. Pustovalov, M.I. Lerner, A.V. Pervikov
Panin Institute of Strength Physics and Materials Science of Siberian Branch of RAS
DOI: 10.26456/pcascnn/2026.18.966
Original article
Abstract: Using NiFeCoCrCuAlMoW alloy as example, the effects of the energy input into the wires and the thermal conductivity of the buffer gas on the average size and phase composition of particles forming in He, N2 and Ar were studied for the first time. The average size of nanoparticles increases in the series He < N2 < Ar, which is due to a decrease in the thermal conductivity of the gas and an increase in the residence time of the metal vapor in a state favorable for coalescence. The particles obtained in He at lower values of Eint/Esub have a smaller size compared to the particles obtained in N2 at higher values of Eint/Esub. The obtained samples are characterized by the presence of FCC and BCC phases corresponding to substitutional solid solutions, as well as a BCC phase of a refractory metal-based substitutional solid solution and intermetallic with a µ-phase structure. The relationship between the phase composition of the samples, and the synthesis parameters revealed an ambiguous dependence. The obtained results did not confirm a direct dependence between the energy input into the wires and the content of the refractory metal-based bcc substitutional solid solution phase in the samples. On the basis of the findings, we have concluded that several independent processes occur during the formation of the phase composition of multicomponent nanoparticles obtained by the electrical explosion of wires.
Keywords: Nanoparticles, high-entropy alloy, electrical explosion of wires, current, segregation, intermetallic compound, solid solution, shunting discharge
- Konstantin V. Suliz – Junior Researcher, Laboratory of Nanobioengineering, Panin Institute of Strength Physics and Materials Science of Siberian Branch of RAS, ORCID: 0000-0001-5556-2113
- Alexey V. Pustovalov – Researcher, Laboratory of Physical Chemistry of Ultrafine Materials, Panin Institute of Strength Physics and Materials Science of Siberian Branch of RAS, ORCID: 0000-0002-5183-2603
- Marat I. Lerner – Dr. Sc., Principal Researcher, Laboratory of Physical Chemistry of Ultrafine Materials, Panin Institute of Strength Physics and Materials Science of Siberian Branch of RAS, ORCID: 0000-0001-8565-1344
- Alexander V. Pervikov – Ph. D., Senior Researcher, Laboratory of Physical Chemistry of Ultrafine Materials, Panin Institute of Strength Physics and Materials Science of Siberian Branch of RAS, ORCID: 0000-0001-7593-0710
For citation:
Suliz K.V., Pustovalov A.V., Lerner M.I., Pervikov A.V. Vliyanie elektrofizicheskikh i termodinamicheskikh parametrov elektrovzryvnogo sinteza na kristallicheskuyu strukturu i dispersnyj sostav mnogokomponentnykh nanochastits NiFeCoCrCuAlMoW [Influence of electrophysical and thermodynamic parameters of electroexplosive synthesis on the crystal structure and dispersed composition of multicomponent NiFeCoCrCuAlMoW nanoparticles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 966-975. DOI: 10.26456/pcascnn/2026.18.966. ⎘
Full article (in Russian): download PDF file
References:
1. Liu S., Dun C., Urban J.J., Swihart M.T. Non-equilibrium synthesis methods to create metastable and high-entropy nanomaterials, Advanced Science, 2026, vol. 13, issue 11, art. no e21953, 37 p. DOI: 10.1002/advs.202521953.
2. Suliz K.V., Sdobnyakov N.Yu., Pervikov A.V. Strukturno-fazovye sostoyaniya nanochastits CoMoFeNiCu, poluchennykh sovmestnym elektricheskim vzryvom provolochek [Structural-phase states of the multicomponent alloy nanoparticles CoMoFeNiCu produce by of joint exploding wires], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 861-868. DOI: 10.26456/pcascnn/2023.15.861.
3. Suliz K.V., Pervikov A.V. Kristallicheskaya struktura i dispersnyj sostav nanochastits mnogokomponentnykh NiFeCoCrCuAlMo, NiFeCoCrCuAlMoW splavov, poluchennykh sovmestnym elektricheskim vzryvom provolok [Crystal structure and dispersed composition of multicomponent NiFeCoCrCuAlMo and NiFeCoCrCuAlMoW alloy nanoparticles obtained by joint exploding wires], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 211-220. DOI: 10.26456/pcascnn/2025.17.211.
4. Liang L., Wu J., Yin Z. et al. Synthesis of fcc structure Fe10Co25Ni34Cu23Al8 high-entropy-alloy nanoparticles by electrical wire explosion: for electromagnetic wave absorption, Applied Physics Letters, 2024, vol. 124, issue 5, art. no. 053502, 5 р. DOI: 10.1063/5.0187760.
5. Liang L., Wu J., Li X., et al. Synergistic dynamic phase transformation during wire electro-explosion enables high-entropy alloys nanoparticles with efficient electromagnetic absorption, ACS Applied Materials & Interfaces, 2026, vol. 18, issue 36, pp. 49624-49639. DOI: 10.1021/acsami.6c08448.
6. Suliz K.V., Shmakov V.V., Pervikov A.V., Sdobnyakov N.Yu. Kristallicheskaya struktura i dispersnyy sostav nanochastits mnogokomponentnogo (NiFeCoCuZn)xOy oksida, poluchennykh sovmestnym elektricheskim vzryvom provolok[Crystal structure and dispersed composition of multicomponent (NiFeCoCuZn)XOY oxide nanoparticles obtained by joint exploding wires], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 203-210. DOI: 10.26456/pcascnn/2025.17.203. (In Russian).
7. Suliz K.V., Pustovalov A.V., Pervikov A.V. Kristallicheskaya struktura i dispersnyy sostav nanochastits mnogokomponentnogo (NiCoCrFeAl)xOy oksida, poluchennykh sovmestnym elektricheskim vzryvom provolochek [Crystal structure and dispersed composition of multicomponent oxide (NiCoCrFeAl)xOy nanoparticles obtained via joint exploding wires], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 916-927. DOI: 10.26456/pcascnn/2025.17.916. (In Russian).
8. Liu S., Liu K., Qi L. et al. Synthesis of high-entropy oxide nanopowders with different crystal structures by electrical explosion of wires, Nanomaterials, 2025, vol. 15, issue 8, art. no. 571, 17 p. DOI: 10.3390/nano15080571.
9. Romanova V.M., Ivanenkov G.V., Mingaleev A.R. et al. Electric explosion of fine wires: three groups of materials, Plasma Physics Reports, 2015, vol. 41, issue 8, pp. 617-636. DOI: 10.1134/S1063780X15080085.
10. Kotov, Yu. A. The electrical explosion of wire: A method for the synthesis of weakly aggregated nanopowders, Nanotechnologies in Russia, 2009, vol. 4, issue 7-8, pp. 415-424. DOI: 10.1134/S1995078009070039.
11. Haynes W.M. CRC handbook of chemistry and physics, 95th ed. Boca Raton, CRC Press, 2014, 2704 p. DOI: 10.1201/b17118.
12. Kvartskhava I.F., Bondarenko V.V., Pliutto A.A., Chernov A.A. Oscillographic determination of energy of electric explosion of wires, Journal of Experimental and Theoretical Physics, 1957, vol. 4, issue 5, pp. 623-629.
13. Kraus W., Nolze G. POWDER CELL–a program for the representation and manipulation of crystal structures and calculation of the resulting X-ray powder patterns, Journal of Applied Crystallography, 1996, vol. 29, issue 3, pp. 301-303. DOI: 10.1107/S0021889895014920.
14. Bai J., Shi Z., Huang C., et al. Electrical explosion of aluminum wire for preparation of nanoparticles: an experimental study, Journal of Physics D: Applied Physics, 2019, vol. 52, issue 42, art. no. 425201, 10 p. DOI: DOI: 10.1088/1361-6463/ab3362.
15. Guillermet, A.F. The Fe−Mo (iron−molybdenum) system, Bulletin of Alloy Phase Diagrams, 1982, vol. 3, issue 3, pp. 359-367. DOI: 10.1007/BF02869315.