Hydrothermal and solvothermal syntheses of calcium phosphates in the form of cotton wool
V.K. Krut'ko1, L.Yu. Maslova1, O.N. Musskaya1, E.N. Krutsko1, I.E. Glazov1, T.V. Safronova2, A.I. Kulak1
1 Institute of General and Inorganic Chemistry of the NAS of Belarus
2 Lomonosov Moscow State University
DOI: 10.26456/pcascnn/2026.18.868
Original article
Abstract: The physicochemical properties and microstructure of fibrous calcium phosphates in the form of cotton-wool-like nanofibers were studied. The phosphates were obtained by: 1) hydrothermal synthesis in the presence of a 1 M urea solution during 18-52 hours of boiling at 90°C, 2) solvothermal synthesis in the presence of calcium oleate at 180°C during 5 hours of autoclaving. Under hydrothermal conditions, a single-phase octacalcium phosphate with a fibrous microstructure was synthesized, which dries at 37°C in a cotton-wool-like form, and after annealing at 800°C, it crystallizes predominantly into β-tricalcium phosphate with 20% β-calcium pyrophosphate. Amorphized hydroxyapatite was obtained by solvothermal synthesis. At 60°C, it dries to soft conglomerates and, after annealing at 800°C, crystallizes into hydroxyapatite with 20% β-tricalcium phosphate. The formed loose calcium phosphate precipitates must be repeatedly washed to remove urea or oleate. Calcium phosphate wool obtained by various methods is represented by long, thin, randomly oriented nanofibers up to 1 nm wide and 4-6 nm in diameter. In samples with a short boiling time of up to 18 hours, near-spherical nuclei up to 10 nm in diameter were visualized, from which nanofibers form and grow. Increasing the boiling time to 52 hours, the synthesis temperature to 180°C, and annealing at 800°C lead to shortening and thickening of the nanofibers to 10-40 nm and an increase in the nucleus size to 18 nm. This synthesis method allows for the control of the phase composition and the required degree of bioresorbability of calcium phosphate wool. Synthetic calcium phosphate wool with a voluminous fibrous microstructure and the ability to be absorbed due to soluble forms of calcium phosphates can be used in bone tissue engineering with drug delivery or as temporary absorbable barriers.
Keywords: fibrous calcium phosphates, hydrothermal synthesis, octacalcium phosphate, solvothermal synthesis, hydroxyapatite, calcium phosphate wool
- Valentina K. Krut'ko – Ph. D., Assistant Professor, Head of the Laboratory of Photochemistry and Electrochemistry, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0000-0002-1670-207X
- Lyubov Yu. Maslova – Researcher, Photochemistry and Electrochemistry Laboratory, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0009-0002-8533-743X
- Olga N. Musskaya – Ph. D., Assistant Professor, Leading Researcher, Photochemistry and Electrochemistry Laboratory, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0000-0002-9821-8969
- Evgeny N. Krutsko – Senior Researcher, Photochemistry and Electrochemistry Laboratory, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0009-0005-7441-6986
- Ilya E. Glazov – Ph. D., Senior Researcher, Laboratory of Photochemistry and Electrochemistry, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0000-0003-2183-6715
- Tatyana V. Safronova – Ph. D., Assistant Professor, Senior Researcher, Faculty of Chemistry, Lomonosov Moscow State University, ORCID: 0000-0002-9799-5029
- Anatoly I. Kulak – Academician, Dr. Sc., Professor, Director, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0000-0002-1398-3806
For citation:
Krut'ko V.K., Maslova L.Yu., Musskaya O.N., Krutsko E.N., Glazov I.E., Safronova T.V., Kulak A.I. Gidrotermalnyj i solvotermalnyj sintezy kaltsijfosfatov v forme vaty [Hydrothermal and solvothermal syntheses of calcium phosphates in the form of cotton wool], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 868-876. DOI: 10.26456/pcascnn/2026.18.868. ⎘
Full article (in Russian): download PDF file
References:
1. Jeong J., Kim J.H., Shim J.H. et al. Bioactive calcium phosphate materials and applications in bone regeneration, Biomaterials Research, 2019, vol. 23, issue 1, art. id s40824-018-0149-3, 11 p. DOI: 10.1186/s40824-018-0149-3.
2. Tavoni M., Dapporto M., Tampieri A., Sprio S. Bioactive calcium phosphate-based composites for bone regeneration, Journal of Composites Science, 2021, vol. 5, issue 9, art. no. 227, 27 p. DOI: 10.3390/jcs5090227.
3. Montesissa M., Tommasini V., Rubini K. et al. State of art and perspective of calcium phosphate-based coatings coupled with bioactive compounds for orthopedic applications, Nanomaterials, 2025, vol. 15, issue 15, art. no. 1199, 38 p. DOI: 10.3390/nano15151199.
4. Schneider O.D., Weber F., Brunner T.J. et al. In vivo and in vitro evaluation of flexible, cottonwool-like nanocomposites as bone substitute material for complex defects, Acta Biomaterialia, 2009, vol. 5, issue 5, pp. 1775-1784. DOI: 10.1016/j.actbio.2008.11.030.
5. Silva V.C., Farias R.M.C., Bonan R.F. et al. Novel synthesis of BCP cotton-wool-like nanofibrous scaffolds by air-heated solution blow spinning (A-HSBS) technique, Ceramics International, 2023, vol. 49, issue 14, part A, pp. 24084-24092. DOI: 10.1016/j.ceramint.2023.04.241.
6. Furko M., Balázsi K., Balázsi C. Calcium phosphate loaded biopolymer composites – a comprehensive review on the most recent progress and promising trends, Coatings, 2023, vol. 13, issue 2, art. no. 360, 30 p. DOI: 10.3390/coatings13020360.
7. Trifan A., Popescu-Pelin G., Popescu R.-C. et al. MAPLE deposition of resorbable calcium phosphates on electrospun nylon nanofibres for bone tissue engineering, Materials, 2026, vol. 19, issue 11, art. no.2375, 21 p. DOI: 10.3390/ma19112375.
8. Farjam P., Luckabauer M., de Vries E.G. et al. Bioactive calcium phosphate coatings applied to flexible poly(carbonateurethane) foils, Surface and Coatings Technology, 2023, vol. 470, art. no. 129838, 9 p. DOI: 10.1016/j.surfcoat.2023.129838.
9. Zhu Y.-J., Lu B.-Q. Deformable biomaterials based on ultralong hydroxyapatite nanowires, ACS Biomaterials Science and Engineering, 2019, vol. 5, issue 10, pp. 4951-4961. DOI: 10.1021/acsbiomaterials.9b01183.
10. Yu H.-P., Zhu Y.-J., Xiong Z.-C., Lu B.-Q. Bioinspired fiberboard-and-mortar structural nanocomposite based on ultralong hydroxyapatite nanowires with high mechanical performance, Chemical Engineering Journal, 2020, vol. 399, art. no. 125666, 10 p. DOI: 10.1016/j.cej.2020.125666.
11. Goto T., Yin S., Asakura Y. et al. Simultaneous synthesis of hydroxyapatite fibres and β-tricalcium phosphate particles via a water controlled-release solvothermal process, CrystEngComm, 2023, vol. 25, issue 14, pp. 2021-2026. DOI: 10.1039/d2ce01703b.
12. Li Ch., Ge X., Li G. et al. A facile hydrothermal method for synthesis of submillimeter-long octacalcium phosphate and hydroxyapatite as drug carriers with sustained release behaviors, Advanced Powder Technology, 2014, vol. 25, issue 6, pp. 1661-1666. DOI: 10.1016/j.apt.2014.06.001.
13. Lu B.-Q., Zhu Y.-J., Chen F. et al. Solvothermal transformation of a calcium oleate precursor into large-sized highly ordered arrays of ultralong hydroxyapatite microtubes, Chemistry – A European Journal, 2014, vol. 20, issue 25, pp. 7116-7121. DOI: 10.1002/chem.201400252.
14. Lu B.-Q., Zhu Y.-J., Chen F. Highly flexible and nonflammable inorganic hydroxyapatite paper, Chemistry – A European Journal, 2014, vol. 20, issue 5, pp. 1242-1246. DOI: 10.1002/chem.201304439.
15. Crystallography Open Database. Available at: www.url: https://www.crystallography.net/cod/ (accessed 15.06.2026).
16. Krut'ko V.K., Doroshenko A.E., Musskaya O.N., Kulak A.I. Poluchenie oktakal'cijfosfata v vodnoj srede pri vzaimodejstvii kal'cita s monokal'cijfosfatom monogidratom [Obtaining octacalcium phosphate in an aqueous medium by the interaction of calcite with monocalcium phosphate monohydrate], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 782-790. DOI: 10.26456/pcascnn/2022.14.782. (In Russian).
17. Krut'ko V.K., Doroshenko A.E., Musskaya O.N. i dr. Formirovanie oktakal'cijfosfata pri vzaimodejstvii karbonata kal'ciya i monokal'cijfosfata monogidrata v gal'vanostaticheskih usloviyah [Formation of octacalcium phosphate in the interaction of calcium carbonate and monocalcium phosphate monohydrate under galvanostatic conditions], Izvestiya Natsional'noj akademii nauk Belarusi. Seriya khimicheskikh nauk [News of the National Academy of Sciences of Belarus. Series of Chemical Sciences], 2022, vol. 58, issue 3, pp. 263-272. DOI: 10.29235/1561-8331-2022-58-3-263-272. (In Russian).
18. Glazov I.E., Krut'ko V.K., Musskaya O.N., Kulak A.I. Stabilization of amorphous calcium phosphate within the structure of hydroxyapatite by blood-derived biopolymers and subsequent crystallization into α-tricalcium phosphate, Materials Today Chemistry, 2026, vol. 56, art. no. 103865, 10 p. DOI: 10.1016/j.mtchem.2026.103865.
19. Gurin A.N., Komlev V.S., Fadeeva I.V., Barinov S.M. Oktakal'cij fosfat – prekursor biologicheskoj mineralizacii, perspektivnyj osteoplasticheskij material [Octacalcium phosphate is a precursor of biological mineralization and a promising osteoplastic material], Stomatologiya [Dentistry], 2010, issue 4, pp. 65-72. (In Russian).