Sorption analysis and photocatalytic activity of graphitic carbon nitride powder
C.D. Bui1, Z.V. Shomakhov2, S.S. Nalimova1, E.V. Maraeva1, A.A. Naimark1, E.S. Popov1, A.I. Maximov1, V.A. Moshnikov1
1 Saint Petersburg Electrotechnical University «LETI»
2 Kabardino-Balkarian State University named after H.M. Berbekov
DOI: 10.26456/pcascnn/2026.18.604
Original article
Abstract: Graphitic carbon nitride (g‒C3N4) is considered a promising metal-free photocatalyst for the efficient degradation of stable organic dyes in wastewater, however, the relationship between its structural-dispersive characteristics and photocatalytic activity remains insufficiently studied. In this work, a comprehensive characterization was performed on g‒C3N4 powder synthesized via thermal polycondensation of urea at 550°C, followed by treatment with hydrochloric acid and ultrasonic exfoliation. The specific surface area, determined by the Brunauer-Emmett-Teller method, was 52 m2/g. Based on experimental sorption data, geometric parameters of the particles were evaluated within the framework of the nanosheet model. It is shown that the nanosheet thickness depends only weakly on the aspect ratio and is 17 nm, which corresponds to approximately 50 atomic layers under partial exfoliation of blocks. The photocatalytic activity of the material was investigated during the degradation of Rhodamine 6G dye under ultraviolet irradiation (395 nm). The degradation process obeys pseudo-first-order kinetics. As the catalyst loading is increased from 12 to 26 mg, the degradation degree of the dye over 120 minutes rises from 23,2% to 67,9%, and the rate constant increases from 2,1·10-3 to 9,3·10-3 min-1 due to the growth in the number of available active sites.
Keywords: graphitic carbon nitride, Brunauer-Emmett-Teller method, specific surface area, nanosheets, photocatalytic degradation of rhodamine 6G
- Cong D. Bui – 4th year postgraduate student, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI», ORCID: 0000-0002-9937-9078
- Zamir V. Shomakhov – Ph. D., Director of the Institute of Electronics, Robotics and Artificial Intelligence, Kabardino-Balkarian State University named after H.M. Berbekov, ORCID: 0000-0001-5738-2626
- Svetlana S. Nalimova – Ph. D., Associate Professor, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI», ORCID: 0000-0003-3065-3961
- Evgeniya V. Maraeva – Ph. D., Associate Professor, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI», ORCID: 0000-0002-0000-7953
- Aleksei A. Naimark – 4th year student, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI»
- Eremei S. Popov – 4th year student, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI»
- Alexander I. Maximov – Ph. D., Associate Professor, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI», ORCID: 0000-0003-0195-8870
- Vyacheslav A. Moshnikov – Dr. Sc., Professor, Department of Micro- and Nanoelectronics, Saint Petersburg Electrotechnical University «LETI», ORCID: 0000-0001-6500-5492
For citation:
Bui C.D., Shomakhov Z.V., Nalimova S.S., Maraeva E.V., Naimark A.A., Popov E.S., Maximov A.I., Moshnikov V.A. Sorbtsionnyj analiz i fotokataliticheskaya aktivnost poroshka grafitopodobnogo nitrida ugleroda [Sorption analysis and photocatalytic activity of graphitic carbon nitride powder], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 604-611. DOI: 10.26456/pcascnn/2026.18.604. ⎘
Full article (in Russian): download PDF file
References:
1. Bui C.D., Nalimova S.S., Nguyen V.T.A. Grafitopodobnyi nitrid ugleroda: svoistva i primenenie v gazovoi sensorike. Obzor [Graphite-like carbon nitride: properties and application in gas sensorics. Review], Kondensirovannye sredy i mezhfaznye granitsy [Condensed Matter and Interphases], 2025, vol. 27, no. 2, pp. 177-189. DOI: 10.17308/kcmf.2025.27/12763. (In Russian).
2. Bui C.D., Nalimova S., Kondratev V. et al. Alcohol sensing behavior and impedance spectroscopy characterization of g–C3N4 nanosheets, Nanomaterials, 2026, vol. 16, issue 3, art. no. 213, 16 p. DOI: 10.3390/nano16030213.
3. Wu M.-R., Gao M.-Y., Zhang S.-Y. et al. High-performance lithium-sulfur battery based on porous N-rich g–C3N4 nanotubes via a self-template method, International Journal of Minerals, Metallurgy and Materials, 2021, vol. 28, issue 10, pp. 1656-1665. DOI: 10.1007/s12613-021-2319-x.
4. Cao S., Yu J. g–C3N4-based photocatalysts for hydrogen generation, The Journal of Physical Chemistry Letters, 2014, vol. 5, issue 12, pp. 2101-2107. DOI: 10.1021/jz500546b.
5. Beyhaqi A., Azimi S.M.T., Chen Z. et al. Exfoliated and plicated g–C3N4 nanosheets for efficient photocatalytic organic degradation and hydrogen evolution, International Journal of Hydrogen Energy, 2021, vol. 46, issue 39, pp. 20547-20559. DOI: 10.1016/j.ijhydene.2021.03.174.
6. Stefa S., Griniezaki M., Dimitropoulos M. et al. Highly porous thin-layer g–C3N4 nanosheets with enhanced adsorption capacity, ACS Applied Nano Materials, 2023, vol. 6, issue 3, pp. 1732-1743. DOI: 10.1021/acsanm.2c04632.
7. Das S., Pramanik S., Nair R.G. et al. Unlocking the potential of thermally exfoliated ultrathin g–C3N4 nanosheets: abundant active sites for enhanced solar photocatalysis, New Journal of Chemistry, 2023, vol. 47, issue 26, pp. 12418-12430. DOI: 10.1039/D3NJ01946B.
8. Kong L., Wang J., Mu X. et al. Porous size dependent g–C3N4 for efficient photocatalysts: regulation syntheses and physical mechanism, Materials Today Energy, 2019, vol. 13, pp. 11-21. DOI: 10.1016/j.mtener.2019.04.011.
9. Zhang M., Xing M., Dong B. et al. Thermal polymerisation synthesis of g–C3N4 for photocatalytic degradation of Rhodamine B dye under natural sunlight, Water, 2023, vol. 15, issue 16, art. no. 2903, 15 p. DOI: 10.3390/w15162903.
10. Salve V., Agale P., Balgude S. et al. Enhanced photocatalytic activity of SnO2@g–C3N4 heterojunctions for methylene blue and bisphenol-A degradation: effect of interface structure and porous nature, RSC Advances, 2025, vol. 15, issue 20, pp. 15651-15669. DOI: 10.1039/D5RA01762A.
11. Chandio A.G., Memon A.W., Nahyoon N.A. et al. Synthesis of visible-light-driven heterojunction graphitic carbon nitride (g–C3N4/FeO/TiP) material: an efficient photocatalytic agent for degradation of Rhodamine 6G from wastewater, Diamond and Related Materials, 2024, vol. 148, art. no. 111398, 11 p. DOI: 10.1016/j.diamond.2024.111398.
12. Chubenko E., Maximov S., Bui C.D. et al. Optical properties of carbon nitride thin films fabricated by rapid chemical vapor deposition, Materials Science in Semiconductor Processing, 2025, vol. 195, art. no. 109617, 9 p. DOI: 10.1016/j.mssp.2025.109617.
13. Banu A., Sinha B., Sikdar S. Synthesis of polymeric 2D-graphitic carbon nitride (g–C3N4) nanosheets for sustainable photodegradation of organic pollutants, Heliyon, 2024, vol. 10, issue 13, art. no. e33354, 15 p. DOI: 10.1016/j.heliyon.2024.e33354.
14. Maraeva E.V., Moshnikov V.A. Teplovaya desorbtsiya azota kak sposob kontrolya razmerov nanochastits v kompozitsiyakh na osnove oksida tsinka i gidroksiapatita [Nitrogen thermal desorption of as a control method for determination of the nanoparticle size in compositions based on zinc oxide and hydroxyapatite], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2021, issue 13, pp. 294-299. DOI: 10.26456/pcascnn/2021.13.294.
15. Maraeva E., Radaykin D., Bobkov A. et al. Sorption analysis of composites based on zinc oxide for catalysis and medical materials science, Chimica Techno Acta, 2022, vol. 9, issue 4, art. no. 20229422, 6 p. DOI: 10.15826/chimtech.2022.9.4.22.
16. Abrashova E.V., Anikina M.A., Bobkov A.A. et al. Nanochastitsy, nanosistemy i ikh primenenie. Kataliticheskie nanosistemy [Nanoparticles, nanosystems and their application. Catalytic nanosystems], ed. by V.A. Moshnikov, A.I. Maksimov. St. Petersburg, SPbETU «LETI» Publ., 2022, 220 p. (In Russian).