Preparation and study of properties of structured hexacyanoferrates of d‑elements doped with platinum nanoparticles
M.A. Yasnaya1, A.A. Blinova2, I.M. Shevchenko2, A.V. Prasolova2, V.I. Shipulin2, V.P. Torgunov2
1 Branch of JSC NPO «Mikrogen» in Stavropol «Allergen»
2 North Caucasus Federal University
DOI: 10.26456/pcascnn/2026.18.996
Original article
Abstract: In this work, samples of hexacyanoferrates of d-elements (Co, Ni, Fe) containing from 0,1 to 5 wt.% platinum were obtained. Scanning electron microscopy revealed that samples of hexacyanoferrates of d-elements (Co, Ni, Fe) doped with platinum were aggregates of various shapes with sizes from 1 to 70 microns, with clearly defined boundaries and a layered structure. The aggregates are formed by spherical nanoparticles with a size ranging from 10 to 70 nm. Analysis of the energy-dispersive X-ray spectroscopy spectra of samples of hexacyanoferrates of d-elements (Co, Ni, Fe) doped with platinum showed that platinum was identified in samples containing 1 to 5 wt.% Pt. At the same time, the actual platinum content in the materials differs from the theoretically calculated amount, which is due, firstly, to the reduction of some platinum ions in the solution volume and their removal during the sample washing process, and secondly, to the adsorption of platinum ions in the structure (channels) of hexacyanoferrates of d-elements. Analysis of the phase composition of samples of hexacyanoferrates of d-elements (Co, Ni, Fe) doped with platinum showed that the main crystalline phases were the corresponding hexacyanoferrates of d-elements with a face-centered cubic crystal lattice (Fm3m); impurity phases of mixed hexacyanoferrates were also present. Phases of metallic platinum are not identified on the diffraction patterns regardless of the concentration of the noble metal.
Keywords: structured hexacyanoferrates of d-elements, noble metal nanoparticles, doping with platinum nanoparticles, surface microstructure, elemental composition, phase composition
- Maria A. Yasnaya – Ph. D., Associate Professor, Head of the Department of Registration of Medicines, Branch of JSC NPO «Mikrogen» in Stavropol «Allergen», ORCID: 0000-0002-4486-4834
- Anastasia A. Blinova – Ph. D., Associate Professor, Department of Pharmacy and Pharmacognosy, Faculty of Medicine and Biology, North Caucasus Federal University, ORCID: 0000-0001-9321-550X
- Irina M. Shevchenko – Ph. D., Associate Professor, Head of the Department of Standardization, Metrology and Quality Management, Faculty of Food Engineering and Biotechnology named after academician A.G. Khramtsov, North Caucasus Federal University, ORCID: 0009-0005-9113-9335
- Alina V. Prasolova – Lecturer, Department of Pharmacy and Pharmacognosy, Faculty of Medicine and Biology, North Caucasus Federal University, ORCID: 0009-0003-7629-4391
- Valentin I. Shipulin – Dr. Sc., Professor, Professor at the Department of Standardization, Metrology and Quality Management, Faculty of Food Engineering and Biotechnology named after academician A.G. Khramtsov, North Caucasus Federal University, ORCID: 0000-0002-7046-2601
- Vyacheslav P. Torgunov – 4th year student, Department of Standardization, Metrology and Quality Management, Faculty of Food Engineering and Biotechnology named after academician A.G. Khramtsov, North Caucasus Federal University
For citation:
Yasnaya M.A., Blinova A.A., Shevchenko I.M., Prasolova A.V., Shipulin V.I., Torgunov V.P. Poluchenie i issledovanie svojstv strukturirovannykh geksatsianoferratov d-elementov, dopirovannykh nanochastitsami platiny [Preparation and study of properties of structured hexacyanoferrates of d‑elements doped with platinum nanoparticles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 996-1006. DOI: 10.26456/pcascnn/2026.18.996. ⎘
Full article (in Russian): download PDF file
References:
1. Wang W., Liu C., Lin P. et al. Toward continuous and non-invasive monitoring: a scoping review of in vitro blood glucose devices from electrochemistry to optics and micro-system integration, Journal of Materials Chemistry B, 2026, vol. 14, issue 11, pp. 3383-3402. DOI: 10.1039/d5tb02338f.
2. Dedov I.I., Shestakova M.V., Mokrysheva N.G. et al. Kliniko-epidemiologicheskij analiz pokazatelej sakharnogo diabeta v Rossijskoj Federatsii, status 01.01.2026 g. [Clinical and Epidemiological Analysis of Diabetes Mellitus Indicators in the Russian Federation, updated January 1, 2026], Sakharnyi diabet [Diabetes mellitus], 2026, vol. 29, no. 2, pp. 104-136. DOI: 10.14341/DM13485. (In Russian).
3. Alsunaidi B., Althobaiti M., Tamal M., Albaker W., Al-Naib I. A Review of Non-Invasive Optical Systems for Continuous Blood Glucose Monitoring, Sensors (Basel), 2021, vol. 21, issue 20, art. no. 6820, 19 p. DOI: 10.3390/s21206820.
4. Moses J.C., Adibi S., Wickramasinghe N. et al. Non-invasive blood glucose monitoring technology in diabetes management: review, Mhealth, 2023, vol. 10, issue 9, 16 p. DOI: 10.21037/mhealth-23-9.
5. Pullano S.A., Greco M., Bianco M.G. et al. Glucose biosensors in clinical practice: principles, limits and perspectives of currently used devices, Theranostics, 2022, vol. 12, issue 2, pp. 493-511. DOI: 10.7150/thno.64035.
6. Uluç N., Glasl S., Gasparin F. et al. Non-invasive measurements of blood glucose levels by time-gating mid-infrared optoacoustic signals, Nature Metabolism, 2024, vol. 6, issue 4, pp. 678-686. DOI: 10.1038/s42255-024-01016-9.
7. Zhang Y., Sun J., Liu L., Qiao H. A review of biosensor technology and algorithms for glucose monitoring, Journal of Diabetes and its Complications, 2021, vol. 35, issue 8, pp. 107-929. DOI: 10.1016/j.jdiacomp.2021.107929.
8. Johnston L., Wang G., Hu K. et al. Advances in biosensors for continuous glucose monitoring towards wearables, Frontiers in Bioengineering and Biotechnology, 2021, vol. 19, issue 9, pp. 733-810. DOI: 10.3389/fbioe.2021.733810.
9. Parrilla M., Detamornrat U., Domínguez-Robles J. et al. Wearable hollow microneedle sensing patches for the transdermal electrochemical monitoring of glucose, Talanta, 2022, vol. 1, issue 249, art. no 123695, 9 p. DOI: 10.1016/j.talanta.2022.123695.
10. Oglou R.C., Ghobadi T.G.U., Ozbay E., Karadas F. Electrodeposited cobalt hexacyanoferrate electrode as a non-enzymatic glucose sensor under neutral conditions, Analytica Chimica Acta, 2021, vol. 1188, art. no 339188, 7 p. DOI: 10.1016/j.aca.2021.339188.
11. Yu H., Yu J., Li L. et al. Recent progress of the practical applications of the platinum nanoparticle-based electrochemistry biosensors, Frontiers in Chemistry, 2021, vol. 3, issue 9, pp. 677-876. DOI: 10.3389/fchem.2021.677876.
12. Shevchenko I.M., Gvozdenko A.A., Yasnaya M.A. et al. Perspektivnye sensornye materialy na osnove geksatsianoferrata (III) zheleza, modifitsirovannogo nanorazmernym serebrom [Promising sensor materials based on iron(III) hexacyanoferrate modified with nanoscale silver], Nanoindustriya [Nanoindustry], 2025, vol. 18, no. 7-8, pp. 458-465. DOI: 10.22184/1993-8578.2025.18.7-8.458.465. (In Russian).
13. Shevchenko I.M., Gvozdenko A.A., Yasnaya M.A. et al. Geksatsianoferrat (III) nikelya, dopirovannyj serebrom, kak material dlya sozdaniya sensorov na glyukozu [Silver-doped nickel hexacyanoferrate (iii) as a material for creating glucose sensors], Nanoindustriya [Nanoindustry], 2025, vol. 18, no. 7-8, pp. 440-448. DOI: 10.22184/1993-8578.2025.18.7-8.440.448. (In Russian).
14. Shevchenko I.M., Gvozdenko A.A., Yasnaya M.A. et al. Modifikatsiya matritsy geksatsianoferrata kobal'ta nanorazmernym serebrom [Modification of a cobalt hexacyanoferrate matrix with nanosized silver], Nanotekhnologii: razrabotka, primenenie – ХХI vek [Nanotechnology: development and applications – XXI century], 2025, vol. 17, no. 4, pp. 5-14. DOI: 10.18127/j22250980-202504-01. (In Russian).