Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Bessel pulses in an inhomogeneous array of carbon nanotubes under mechanical action

N.N. Yanyushkina

Volgograd State University

DOI: 10.26456/pcascnn/2026.18.322

Original article

Abstract: In this work, the propagation of non-diffracting Bessel pulses in an inhomogeneous array of carbon nanotubes containing both metallic (armchair) and semiconducting (zigzag) tubes is numerically investigated. The relevance arises from the fact that real synthesized samples always represent a mixture of tubes of different chiralities, which significantly affects the dynamics of electromagnetic fields. Based on a model that accounts for the nonlinear response of the medium and the spatial modulation of the tube density, an evolution equation for the vector potential is solved. It is shown that Bessel pulses retain their localization over significant distances even in an inhomogeneous nanotube array and in the presence of mechanical deformations. Special attention is paid to the effect of mechanical loading (external compression or tension), which is modeled via an external stress field. It is found that varying the concentration of metallic tubes along with deformation enables effective control of the pulse shape and suppression of their spreading. The obtained results open up prospects for the development of optomechanical devices, in which mechanical loading serves as an efficient tool for controlling the parameters of the Bessel pulses.

Keywords: zigzag and armchair carbon nanotubes, Bessel pulses, mechanical deformation

  • Natalia N. Yanyushkina – Dr. Sc., Professor, Department of information systems and computer simulation, Volgograd State University

For citation:

Yanyushkina N.N. Impulsy Besselya v neodnorodnom massive uglerodnykh nanotrubok pri mekhanicheskom vozdejstvii [Bessel pulses in an inhomogeneous array of carbon nanotubes under mechanical action], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 322-331. DOI: 10.26456/pcascnn/2026.18.322. ⎘

Full article (in Russian): download PDF file

References:

1. Durnin J., Miceli J.J., Eberly J.H. Diffraction-free beams, Physical Review Letters, 1987, vol. 58, issue 15, pp. 1499-1501. DOI: 10.1103/PhysRevLett.58.1499.
2. Berry M.V., Balazs, N.L. Nonspreading wave pockets, American Journal of Physics, 1979, vol. 47, issue 3, pp. 264-267. DOI: 10.1119/1.11855.
3. Khonina S.N., Kazanskiy N.L., Karpeev S.V. et al. Bessel beam: significance and applications – a progressive review, Micromachines, 2020, vol. 11, issue 11, art. no. 997, 27 p. DOI: 10.3390/mi11110997.
4. Moreno I., Davis J.A., Sánchez-López M.M. et al. Nondiffracting Bessel beams with polarization state that varies with propagation distance, Optics Letters, 2015, vol. 40, issue 23, pp. 5451-5454. DOI: 10.1364/OL.40.005451.
5. Moura T.A., Andrade U.M.S., Mendes J.B.S. et al. Modulating the trapping and manipulation of semiconductor particles using Bessel beam optical tweezers, Optics and Lasers in Engineering, 2023, vol. 170, art. no. 107778, 9 p. DOI: 10.1016/j.optlaseng.2023.107778.
6. Belonenko M.B., Lebedev N.G., Popov A.S. Two-dimensional light bullets in an array of carbon nanotubes, JETP Letters, 2010, vol. 91, issue 9, pp. 461-465. DOI: 10.1134/S0021364010090067.
7. Konobeeva N.N., Fedorov E.G., Rosanov N.N. et al. Stabilization of ultrashort pulses by external pumping in an array of carbon nanotubes subject to piezoelectric effects, Journal of Applied Physics, 2019, vol. 126, issue 20, art. no. 203103, 8 p. DOI: 10.1063/1.5128365.
8. Belonenko M.B., Konobeeva N.N. Two-dimensional non-topological solutions of Maxwell’s equations in a medium of strained carbon nanotubes with impurities, Nanosystems: Physics, Chemistry, Mathematics, 2022, vol.13, issue 1, pp. 45-49. DOI: 10.17586/2220-8054-2022-13-1-45-49.
9. Belonenko A.M., Dvuzhilov I.S., Dvuzhilova Yu.V. et al. Light bullets with Bessel cross section in the environment carbon nanotubes, Optics and Spectroscopy, 2022, vol. 130, issue 3, pp. 407-413. DOI: 10.21883/OS.2022.03.52170.2642-21.
10. Artyukhov V.I., Penev E.S., Yakobson B.Y. Why nanotubes grow chiral, Nature Communications, 2014, vol. 5. art. no. 4892, 6 p. DOI: 10.1038/ncomms5892.
11. Zhang S., Lin D., Liu W. et al. Growth of single‐walled carbon nanotubes with different chirality on same solid cobalt catalysts at low temperature, Small, 2019, vol. 15, issue. 46, art. no. 1903896, 6 p. DOI: 10.1002/smll.201903896.
12. Li Y., Li L., Jiang H. et al. An efficient approach toward production of near-zigzag single-chirality carbon nanotubes, Science Advances, 2024, vol. 10, issue 14, art. no. eadn6519, 8 p. DOI: 10.1126/sciadv.adn651.
13. Hu L., Hecht D.S., Gruner G. Percolation in transparent and conducting carbon nanotube networks, Nano Letters, 2004, vol. 4, issue 12, pp. 2513-2517. DOI: 10.1021/nl048435y.
14. Wang X., Jin C., Bai Z. Review of carbon nanotube-based flexible wearable strain sensors: from materials to applications for human body, Sensors and Actuators A: Physical, 2025, vol. 395, art. no. 117071, 22 p. DOI: 10.1016/j.sna.2025.117071.
15. Kozlov S.A., Sazonov S.V. Nonlinear propagation of optical pulses of a few oscillations duration in dielectric media, Journal of Experimental and Theoretical Physics, 1997, vol. 84, issue 2, pp. 221-228. DOI: 10.1134/1.558109.
16. Kohls A., Ditty M.M., Dehghandehnavi F. et al. Vertically aligned carbon nanotubes as a unique material for biomedical applications, ACS Applied Materials and Interfaces, 2022, vol. 14, issue 5, pp. 6287-6306. DOI: 10.1021/acsami.1c20423.
17. Belonenko M.B., Demushkina E.V., Lebedev N.G. Electromagnetic solitons in a system of carbon nanotubes, Journal of Russian Laser Research, 2006, vol. 27, issue 5, pp. 457-465. DOI: 10.1007/s10946-006-0027-7.
18. Lyapkosova O.S., Lebedev N.G., Belonenko M.B. Extremely short optical pulses in strained graphene in terms of the gauge theory, Physics of the Solid State, 2013, vol. 55, issue 12, pp. 2602-2607. DOI: 10.1134/S1063783413120226.
19. Bass F.G., Bulgakov A.A., Tetrvov A.P. Vysokochastotnye svoystva poluprovodnikov so sverkheshetkami [High-frequency properties of semiconductors with superlattices]. Moscow, Nauka, 1989, 286 p. (In Russian).
20. Saito R., Dresselhaus G., Dresselhaus M.S. Physical properties of carbon nanotubes. London: Imperial College Press, 1998, XII+259 p.
21. Chiu C.W., Shyu F.L., Chang C.P. et al. Electron lifetime in armchair carbon nanotubes, Journal of the Physical Society of Japan, 2004, vol. 73, no. 11, pp. 2936-2939. DOI: 10.1143/jpsj.73.2936.
22. Cristoloveanu S., Lee K.H., Park H. et al. The concept of electrostatic doping and related devices, Solid State Electronics, 2019, vol. 155, pp. 32-43. DOI: 10.1016/j.sse.2019.03.017.
23. Chong A., Renninger W.H., Christodoulides D.N. et al. Airy–Bessel wave packets as versatile linear light bullets, Nature Photonics, 2010, vol. 4, pp. 103-106. DOI: 10.1038/nphoton.2009.264.

Content |