Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Thermal desorption kinetics of titanium and titanium-vanadium gas absorbers

A.V. Parashchuk, E.P. Sheshin

Moscow Institute of Physics and Technology (National Research University)

DOI: 10.26456/pcascnn/2026.18.730

Original article

Abstract: The processes of gas release from titanium and titanium-vanadium getter materials used in electrovacuum devices were studied using thermodesorption spectroscopy. Two consecutive heating cycles were performed at a rate of 5°C/min, followed by an isothermal annealing at the end of the heating process. The activation energies of desorption for H2, H2O, CO2 and CH4 were calculated using the Redhead method. It has been shown that during secondary heating after 5 days of keeping in a vacuum, the hydrogen peaks are restored, some new high-temperature water peaks appear, and methane is formed, which was not present during the primary heating. For the Ti-V alloy, all desorption processes are shifted to lower temperatures (maximum of 550°C) with an activation energy of 2,52 eV compared to 3,62 eV for pure titanium. It has been established that during exposure at room temperature, getters sorb hydrogen, oxygen, and carbon-containing gases from the residual atmosphere, and the sorbated components enter into chemical interaction.

Keywords: thermodesorption spectroscopy, getter, titanium, titanium-vanadium alloy, activation energy, desorption, sorption, electrovacuum devices, Redhead method

  • Anastasia V. Parashchuk – Postgraduate, Moscow Institute of Physics and Technology (National Research University), ORCID: 0009-0009-4173-9227
  • Evgeniy P. Sheshin – Dr. Sc., Professor, Deputy Head of Department of Electronics, Head of Laboratory of Vacuum and Microwave Electronics, Moscow Institute of Physics and Technology (National Research University), ORCID: 0000-0003-2750-4797

For citation:

Parashchuk A.V., Sheshin E.P. Kinetika termodesorbtsii titanovykh i titan-vanadievykh gazopoglotitelej [Thermal desorption kinetics of titanium and titanium-vanadium gas absorbers], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 730-739. DOI: 10.26456/pcascnn/2026.18.730. ⎘

Full article (in Russian): download PDF file

References:

1. Paraschuk A.V., Sheshin E.P., Khanbekov I.F. [Development of an experimental setup for studying surface phenomena in electronic devices of the magnetron type], Proceedings of the 67th All-Russian Scientific Conference of MIPT. Electronics, Photonics, and Molecular Physics [Trudy 67-j Vserossijskoj nauchnoj konferentsii MFTI. Elektronika, fotonika i molekulyarnaya fizika], March 31 - April 5, 2025, Moscow. Moscow, Fizmatlit Publ., 2025, pp. 230-231. (In Russian).
2. Ma M., Liang L., Wang L. et al. Phase transformations of titanium hydride in thermal desorption process with different heating rates, International Journal of Hydrogen Energy, 2015, vol. 40, issue 29, pp. 8926-8934. DOI: 10.1016/j.ijhydene.2015.05.083.
3. Tyurin Y.I., Chernov I.P., Silkin V.M. et al. Electron-stimulated hydrogen desorption from nickel and palladium, Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques, 2018, vol. 12, issue 1, pp. 21-26. DOI: 10.1134/S1027451018010184.
4. Sobyanin V.A., Bulgakov N.N., Gorodetskii V.V. Dissociative adsorption of oxygen and hydrogen, and the formation of hydroxyl groups on the surface of Cu, Ag, Ni, Pd and Pt, Reaction Kinetics and Catalysis Letters, 1977, vol. 6, issue 2, pp. 125-132. DOI: 10.1007/BF02084187.
5. Ben David R., Finkelstein Y., Nativ-Roth E., Danon A., Cohen D., Rabkin E. The role of surface coarsening and sintering during thermal decomposition of titanium hydride, International Journal of Hydrogen Energy, 2019, vol. 44, issue 12, pp. 6045-6054. DOI: 10.1016/j.ijhydene.2019.01.070.
6. Yang H., Whitten J.L. Energetics of hydroxyl and influence of coadsorbed oxygen on metal surfaces, The Journal of Physical Chemistry B, 1997, vol. 101, issue 20, pp. 4090-4096. DOI: 10.1021/jp9702311.
7. Galimov R.M., Kudiyarov V.N., Lider A.M. et al. Kinetika raspada gidridnykh faz v titanovom splave VT1-0 pri termicheskom vozdejstvii i obluchenii rentgenovskim puchkom sinkhrotronnogo izlucheniya [Kinetics of decomposition of hydride phases in titanium alloy VT1-0 under thermal exposure and irradiation with an X-ray beam of synchrotron radiation], Izvestiya vysshikh uchebnykh zavedenij. Fizika [Russian Physics Journal], 2013, vol. 56, no. 11-3, pp 43-47. (In Russian).
8. Yan H., Kim J., Tasan C.C. In-situ scanning electron microscope thermal desorption spectroscopy (SEM-TDS) analysis of thermally-induced titanium hydride decomposition and reformation, Acta Materialia, 2022, vol. 226, art. no. 117562, 28 p. DOI: 10.1016/j.actamat.2021.117562.
9. Sandim H.R.Z., Morante B.V., Suzuki P.A. Kinetics of thermal decomposition of titanium hydride powder using in situ high-temperature X-ray diffraction (HTXRD), Materials Research, 2005, vol. 8, issue 3, pp. 293-297. DOI: 10.1590/S1516-14392005000300012.
10. Suwarno S., Yartys V.A. Kinetics of hydrogen absorption and desorption in titanium, Bulletin of Chemical Reaction Engineering & Catalysis, 2017, vol. 12, issue 3, pp. 312-317. DOI: 10.9767/bcrec.12.3.810.312-317.
11. Qiu J., Yang Y., Wan H. et al. Interface-engineered TiV bimetal catalysts with synergistic effects for enhancing hydrogen storage performance in Mg–Ni-based material, The Journal of Physical Chemistry Letters, 2025, vol. 16, issue 32, pp. 8084-8091. DOI: 10.1021/acs.jpclett.5c01248.
12. Aleksanyan A., Sisakyan N., Mayilyan N. Hydride cycle synthesis of Ti0.5V2Cr0.5 alloy and its composites with ZrNi/Zr7Ni10 additives by a novel technological approach, International Journal of Self-Propagating High-Temperature Synthesis, 2025, vol. 34, issue 3, pp. 192-208. DOI: 10.3103/S1061386225700177.
13. Kumar A., Banerjee S., Pillai C.G.S., Bharadwaj S.R. Hydrogen storage properties of Ti₂₋ₓCrVMₓ (M = Fe, Co, Ni) alloys, International Journal of Hydrogen Energy, 2013, vol. 38, issue 30, pp. 13335-13342. DOI: 10.1016/j.ijhydene.2013.07.096.

Content |