Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Temperature dependence of the ellipsometric parameters of thin films of the AIST phase-change chalcogenide

A.A. Nevzorov1,2, V.A. Mikhalevsky1, A.A. Burtsev1, V.V. Ionin1, A.V. Kiselev1, N.N. Eliseev1, A.A. Lotin1,3

1 National Research Centre «Kurchatov Institute»
2 University of Science and Technology MISIS
3 Mendeleev University of Chemical Technology

DOI: 10.26456/pcascnn/2026.18.094

Short communication

Abstract: This work is devoted to the study of the temperature dependences of the refractive index (n) and extinction coefficient (k) of thin films of the phase-change chalcogenide AIST (Ag5In5Sb60Te30) in the spectral range of 380-1000 nm. Using spectroscopic ellipsometry, a direct comparison of optical properties of the amorphous and crystalline phases was performed during heating from room temperature to 170°C. It was found that heating the amorphous film to 100°C leads to a decrease in n by 3,2% and an increase in k by 2,55% at a wavelength of 780 nm, as well as a decrease in n by 5,0% and a decrease in k by 4,2% at a wavelength of 910 nm. The observed behavior indicates a notable instability of both the amorphous and crystalline phases of the investigated AIST material. The quantitative data obtained provide a necessary experimental basis for accurate thermal and optical modeling of phase-change memory devices operating in the near-infrared range. The effective application of this material requires optimization and control of synthesis methods, thin-film properties, and the precise kinetics of phase transformations. Nevertheless, AIST can be recommended for applications where high switching speed is a priority, rather than requirements for stability and multilevel state storage.

Keywords: chalcogenides, phase change materials, thin films, crystallization, optical properties

  • Alexey A. Nevzorov – Ph. D., Researcher, National Research Centre «Kurchatov Institute», Researcher at Laboratory of Photonic Gas Sensors University of Science and Technology MISIS, ORCID: 0000-0001-5602-6355
  • Vladimir A. Mikhalevsky – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-6234-1084
  • Anton A. Burtsev – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0003-0280-7943
  • Vitaly V. Ionin – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-1253-2261
  • Alexey V. Kiselev – Ph. D., Senior Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0003-0292-9553
  • Nikolay N. Eliseev – Junior Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-8864-3961
  • Andrey A. Lotin – Dr. Sc, Deputy Head of the branch, National Research Centre «Kurchatov Institute», Deputy Director of the Department of Scientific and Technical Policy Mendeleev University of Chemical Technology, ORCID: 0000-0001-9051-7158

For citation:

Nevzorov A.A., Mikhalevsky V.A., Burtsev A.A., Ionin V.V., Kiselev A.V., Eliseev N.N., Lotin A.A. Temperaturnaya zavisimost ellipsometricheskikh parametrov tonkikh plyonok fazoizmenyaemogo khalkogenida AIST [Temperature dependence of the ellipsometric parameters of thin films of the AIST phase-change chalcogenide], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 94-101. DOI: 10.26456/pcascnn/2026.18.094. ⎘

Full article (in Russian): download PDF file

References:

1. Kolobov A.V., Tominaga J. Chalcogenides: Metastability and Phase Change Phenomena. Berlin, Heidelberg, Springer-Verlag, 2012, XVI+284 p. DOI: 10.1007/978-3-642-28705-3.
2. Phase change materials. science and applications, ed. by S. Raoux and M. Wutting. New York, Springer Science+Business Media, LLC, 2009, 450 p. DOI: 10.1007/978-0-387-84874-7.
3. Sarwat S.G. Materials science and engineering of phase change random access memory, Materials Science and Technology, 2017, vol. 33, issue 16, pp. 1890-1906. DOI: 10.1080/02670836.2017.1341723.
4. Zhou G.F. Materials aspects in phase change optical recording, Materials Science and Engineering: A, 2001, vol. 304-306, pp. 73-80. DOI: 10.1016/S0921-5093(00)01448-9.
5. Kalb J.A., Spaepen F., Wuttig M. Kinetics of crystal nucleation in undercooled droplets of Sb- and Te-based alloys used for phase change recording, Journal of Applied Physics, 2005, vol. 98, issue 5, pp. 054910-1-054910-70. DOI: 10.1063/1.2037870.
6. Papandreou N., Pantazi A., Sebastian A. et al. Multilevel phase-change memory, 17th IEEE International Conference on Electronics, Circuits and Systems, 2010, pp. 1017-1020. DOI: 10.1109/ICECS.2010.5724687.
7. Christian J.W. The theory of transformations in metals and alloys, 3rd ed. Oxford, Pergamon, 2002, vol. 1-2, 1200 p. DOI: 10.1016/B978-0-08-044019-4.X5000-4.
8. Wuttig M., Yamada N. Phase-change materials for rewriteable data storage, Nature materials, 2007, vol. 6, issue 11, pp. 824-832. DOI: 10.1038/nmat2009.
9. McGieson I., Bird V. L., Barr C. M. et. al. Crystallization kinetics and thermodynamics of an Ag–In–Sb–Te phase change material using complementary in situ microscopic techniques, Journal of Materials Research, 2022, vol. 37, issue 7, pp. 1281-1295. DOI: 10.1557/s43578-022-00486-5.
10. Zhang W., Mazzarello R., Wuttig M., Ma E. Designing crystallization in phase-change materials for universal memory and neuro-inspired computing, Nature Reviews Materials, 2019, vol. 4, issue 3, pp. 150-168. DOI: 10.1038/s41578-018-0076-x.
11. Wuttig M., Raoux S. The science and technology of phase change materials, Zeitschrift für anorganische und allgemeine Chemie, 2012, vol. 638, issue 15, pp. 2455-2465. DOI: 10.1002/zaac.201200448.
12. Kozyukhin S.A., Lazarenko P.I., Popov A.I., Eremenko I.L. Phase change memory materials and their applications, Russian Chemical Reviews, 2022, vol. 91, issue 9, art. no. RCR5033, 37 p. DOI: 10.1070/RCR5033.
13. Lee S., Shelby R.M., Raoux S. et al. Nanoscale nuclei in phase change materials: Origin of different crystallization mechanisms of Ge2Sb2Te5 and AgInSbTe, Journal of Applied Physics, 2014, vol. 115, issue 6, art. no. 063506, 10 p. DOI: 10.1063/1.4865295.
14. Ziegler S.; Wuttig M. Nucleation of AgInSbTe films employed in phase-change media, Journal of Applied Physics, 2006, vol. 99, issue 6, art. no. 064907. – 8 p. DOI: 10.1063/1.2184428.
15. Matsunaga T., Akola J., Kohara S. et al. From local structure to nanosecond recrystallization dynamics in AgInSbTe phase-change materials, Nature Materials, 2011, vol. 10, pp. 129-134. DOI: 10.1038/nmat2931.

Content |