Electroexplosive synthesis of micro- and nanoparticles of high-entropy alloys NiFeCoCrCuAl and NiFeCoCrCuMo for extrusion 3D printing with granules
A.V. Pervikov1, N.V. Svarovskaya1, E.A. Glazkova2, E.E. Ryumin1, K.V. Suliz1, S.O. Kazantsev1, M.I. Lerner1
1 National Research Tomsk State University
2 Panin Institute of Strength Physics and Materials Science of Siberian Branch of RAS
DOI: 10.26456/pcascnn/2026.18.740
Original article
Abstract: High-entropy alloy powders were synthesized for the first time as a homogeneous micro/nanoparticle mixture via the co-electrical wire explosion of various metals and alloys. Scanning electron microscopy and X-ray diffraction determined the particle size distribution and crystal structure, revealing the critical effect of wire explosion energy parameters on the particle phase formation. The particle size distribution was found to be bimodal, with particle sizes varying from 30 nm to 15 µm. The crystal structure of the particles corresponds to substitutional solid solutions with fcc and bcc lattices. The powders were compounded into oxidized polyethylene wax and polymethyl methacrylate granules. Granules containing 50 vol.% alloy particles were extrusion-printed into block structures with straight and gyroidal channels. Structural characterization of the sintered components showed that the crystal structure consists of substitutional solid solutions with fcc and bcc lattices. Compression tests indicated that the ultimate strength is comparable to the characteristic values of the austenitic Cantor alloy family.
Keywords: nanoparticles, high entropy alloy, exploding wires, fused granular fabrication, shunting discharge, current, voltage
- Alexander V. Pervikov – Ph. D., Senior Researcher, Laboratory of metallurgy nanotechnology, Faculty of physics and technology, National Research Tomsk State University, ORCID: 0000-0001-7593-0710
- Natalia V. Svarovskaya – Ph. D., Senior Researcher, Laboratory of metallurgy nanotechnology, Faculty of physics and technology, National Research Tomsk State University, ORCID: 0000-0002-1190-8909
- Elena A. Glazkova – Ph. D., Senior Researcher, Laboratory of physical chemistry of highly dispersed materials, Panin Institute of Strength Physics and Materials Science of Siberian Branch of RAS, ORCID: 0000-0002-5311-52
- Egor E. Ryumin – Engineer, Laboratory of metallurgy nanotechnology, Faculty of physics and technology, National Research Tomsk State University, ORCID: 0009-0005-2303-9519
- Konstantin V. Suliz – Research Engineer, Laboratory of metallurgy nanotechnology, Faculty of physics and technology, National Research Tomsk State University, ORCID: 0000-0001-5556-2113
- Sergey O. Kazantsev – Ph.D., Senior Researcher, Laboratory of metallurgy nanotechnology, Faculty of physics and technology, National Research Tomsk State University, ORCID: 0000-0002-1728-7947
- Marat I. Lerner – Dr. Sc., Principal Researcher, Laboratory of metallurgy nanotechnology, Faculty of physics and technology, National Research Tomsk State University, ORCID: 0000-0001-8565-1344
For citation:
Pervikov A.V., Svarovskaya N.V., Glazkova E.A., Ryumin E.E., Suliz K.V., Kazantsev S.O., Lerner M.I. Elektrovzryvnoj sintez mikro- i nanochastits vysokoentropijnykh splavov NiFeCoCrCuAl i NiFeCoCrCuMo dlya ekstruzionnoj 3D-pechati granulami [Electroexplosive synthesis of micro- and nanoparticles of high-entropy alloys NiFeCoCrCuAl and NiFeCoCrCuMo for extrusion 3D printing with granules], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 740-750. DOI: 10.26456/pcascnn/2026.18.740. ⎘
Full article (in Russian): download PDF file
References:
1. Curmi A., Rochman A. Screw extrusion fused granulate fabrication: trends, materials, extruder classification and future development, Polymer, 2025, vol. 130, art. no. 128459, 19 р. DOI: 10.1016/j.polymer.2025.128459.
2. Heuer С., Bock-Seefeld B., Kaiser P. et al. 3D printing of alumina components via Fused Granulate Fabrication technology and solvent-free debinding of highly filled feedstocks comprising (LD)-polyethylene and cellulose, Ceramics International, 2025, vol. 51, issue 28, pp. 58287-58296. DOI: 10.1016/j.ceramint.2025.10.048.
3. Kerber F., Malczyk P., Hubálková J. et al. Effect of heating rate on powder-bed pre-debinding of thermal-shock-resistant 3D-printed alumina for hydrogen-combustion applications, Ceramics International, 2026, vol. 52, issue 20, pp. 36093-36103. DOI: 10.1016/j.ceramint.2026.06.117.
4. Martínez-Fuentes J.C., Chirita D.A., Martínez-Lopez I. et al. 3D-printed high-reliability alloy-based monoliths as structured supports for CO2 methanation catalysts, Chemical Engineering Journal, 2026, vol.547, art. no. 181376, 15 p. DOI: 10.1016/j.cej.2026.181376.
5. Mazeeva A., Masaylo D., Konov G., Popovich A. Multi-Metal additive manufacturing by extrusion-based 3D printing for structural applications: A Review, Metals, 2024, vol. 14, issue 11, art. no 1296, 53 р. DOI: 10.3390/polym13183160.
6. Pervikov A., Glazkova E., Lerner M. Energy characteristics of the electrical explosion of two intertwined wires made of dissimilar metals, Physics of Plasmas, 2018, vol. 25, issue 7, art. no. 070701, 7 р. DOI: 10.1063/1.5034184.
7. Kotov Yu.A. The electrical explosion of wire: a method for the synthesis of weakly aggregated nanopowders, Nanotechnologies in Russia, 2009, vol. 4, issue 7-8, pp. 415-424. DOI: 10.1134/S1995078009070039.
8. Zhang B., Mu Q., Pei Y. et al. Synthesis strategies and multi-field applications of nanoscale high-entropy alloys, Nano-Micro Letters, 2025, vol. 17, issue 1, art. no. 283, 38 p. DOI: 10.1007/s40820-025-01779-0.
9. Yang Y.-F., Hu F., Xia T. et al. High entropy alloys: A review of preparation techniques, properties and industry applications, Journal of Alloys and Compounds, 2025, vol. 1010, art. no. 177691, 24 p. DOI: 10.1016/j.jallcom.2024.177691.
10. Yeh J.-W., Chen S.-K., Lin S.-J. et al. Nanostructured high-entropy alloys with multiple principal elements: novel alloy design concepts and outcomes, Advanced Engineering Materials, 2004, vol. 6, issue 5, pp. 299-303. DOI: 10.1002/adem.200300567.
11. Haynes W.M. CRC handbook of chemistry and physics, 95th ed. Boca Raton, CRC Press, 2014, 2704 p. DOI: 10.1201/b17118
12. Kvartskhava I.F., Bondarenko V.V., Pliutto A.A., Chernov A.A. Oscillographic determination of energy of electric explosion of wires, Journal of Experimental and Theoretical Physics, 1957, vol. 4, issue 5, pp. 623-629.
13. Zeng Z., Xiang M., Zhang D. et al. Mechanical properties of Cantor alloys driven by additional elements: a review, Journal of Materials Research and Technology, 2021, vol. 15, pp. 1920-1934. DOI: 10.1016/j.jmrt.2021.09.019.