Effects of calcium ions on the relaxation processes in ceramics based on barium titanate
O.V. Malyshkina1, R.A. Petrov1, N.E. Malysheva2
1 Tver State University
2 The Zhukov Air and Space Defense Academy
DOI: 10.26456/pcascnn/2026.18.062
Original article
Abstract: Comparative studies of experimental and calculated dielectric responses of barium-calcium titanate ceramic samples with different Ba/Ca. ratios based on a mathematical model were conducted. Based on mathematical modeling, it has been shown that for Ba1-xCaxTiO3 samples with a calcium concentration of x < 0,25, there are only two relaxation processes: high-frequency (with the most probable relaxation time of ~ 10-8s), corresponding to the thermal ionic polarization, and low-frequency (with the most probable relaxation time of ~ 1 s), corresponding to the migration polarization. The presence of individual grains of calcium titanate in the sample, which occurs at x > 0,25, leads to an increase in the number of low-frequency relaxation processes, as evidenced by the presence of not one, but several most probable relaxation times (with values from 10–2 to 1 s). Analysis using mathematical modeling revealed the absence of a contribution to the dielectric response of barium titanate-based ceramics from the low-frequency conductivity, which is present in sodium niobate-based ceramics, despite the fact that both materials have a perovskite-type structure.
Keywords: piezoelectric ceramics, lead-free materials, barium titanate ceramics, calcium titanate, dispersion of complex permittivity, relaxation processes, resonant polarization
- Olga V. Malyshkina – Dr. Sc., Professor, Head of the Department of Computer Security and Mathematical Control Methods, Tver State University, ORCID: 0000-0001-5885-2511
- Roman A. Petrov – 4th year postgraduate student, Tver State University
- Nataliya E. Malysheva – Senior Lecture, Department no. 13, The Zhukov Air and Space Defense Academy, ORCID: 0009-0006-8937-5715
For citation:
Malyshkina O.V., Petrov R.A., Malysheva N.E. Vliyanie ionov kaltsiya na protekanie relaksatsionnykh protsessov v keramike na osnove titanata bariya [Effects of calcium ions on the relaxation processes in ceramics based on barium titanate], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 62-71. DOI: 10.26456/pcascnn/2026.18.062. ⎘
Full article (in Russian): download PDF file
References:
1. Saito Y., Takao H., Tani T. et al. Lead-free piezoceramics, Nature, 2004, vol. 432, issue 7013, pp. 84-87. 10.1038/nature03028.
2. Rödel J., Webber K.G., Dittmer R. et al. Transferring lead-free piezoelectric ceramics into application, Journal of the European Ceramic Society, 2015, vol. 35, issue 6, pp. 1659-1681. DOI:10.1016/j.jeurceramsoc.2014.12.013.
3. Advanced piezoelectric materials. Science and technology, ed. by K. Uchino. Oxford, Cambridge, Philadelphia, New Delhi, Woodhead Publishing Limited, 2010, 696 p.
4. Golovnin V.А., Kaplunov I.А., Malyshkina O.V., Ped'ko B.B., Movchikova А.А. Fizicheskie osnovy, metody issledovaniya i prakticheskoe primenenie p'ezomaterialov [Physical foundations, research methods and practical application of piezomaterials]. Moscow, TEKHNOSFERА Publ., 2013, 272 p. (In Russian).
5. Polar oxides: properties, characterization, and imaging, ed. by R. Waser, U. Böttger, S. Tiedke. Weinheim, John Wiley & Sons, 2006, 391 p.
6. Smolensky G.A., Isupov V.A. Segnetoelektricheskie svojstva tverdykh rastvorov stanata bariya v titanate bariya [Ferroelectric properties of solid solutions of barium stanate in barium titanate], Zhurnal tekhnicheskoj fiziki [Journal of Technical Physics], 1954, vol. 24, issue 8, pp. 1375-1386. (In Russian).
7. Buscaglia M.T., Buscaglia V., Viviani M. et al. Influence of foreign ions on the crystal structure of BaTiO3 Journal of the European Ceramic Society, 2000, vol. 20, issue 12, pp. 1997-2007. DOI: 10.1016/S0955-2219(00)00076-5.
8. Eklund C.J., Fennie C.J., Rabe K.M. Strain-induced ferroelectricity in orthorhombic CaTiO3 from first principles. Physical Review B. Condensed Matter and Materials Physics, 2009, vol. 79, issue 22, pp. 220101-1-2220101-4. DOI: 10.1103/PhysRevB.79.220101.
9. Železný V., Cockayne Eric, Petzelt J. et al. Temperature dependence of infrared-active phonons in CaTiO3: a combined spectroscopic and first-principles study, Physical Review B, 2002, vol. 66, issue 22, pp. 224303-1224303-12. DOI: 10.1103/PhysRevB.66.224303.
10. Moriwake H., Kuwabara A., Fisher C.A.J. et al. First-principles calculations of lattice dynamics in CdTiO3 and CaTiO3: Phase stability and ferroelectricity. Physical Review B, 2011, vol. 84, issue10, pp. 104114-1-104114-8. DOI: https://doi.org/10.1103/PhysRevB.84.104114.
11. Petrov R.A., Malyshkina O.V., Ivanova A.I. Ustanovleniye oblasti nesmeshivayemosti titanata bariya i titanata kal'tsiya pri obrazovanii keramiki [Determination of the miscibility gap of barium titanate and calcium titanate during the formation of ceramics], Fizika tverdogo tela [Physics of the Solid State], 2026, vol. 68, issue 4, pp. 591-596. DOI: 10.61011/FTT.2026.04.63321.8998.
12. Poplavko Yu.M. Fizika dielektrikov [Physics of dielectrics]. Kiev, Vishcha shkola, Golovnoe izd-vo, 1980, 400 p. (In Russian).
13. Jonscher A.K. Universal relaxation law: a sequel to dielectric relaxation in solids. London, Chelsea Dielectrics Press Limited, 1996, 415 p.
14. Malysheva N.E., Dyakova E.V., Malyshkina O.V. Modelirovaniye dielektricheskogo otklika p'yezoelektricheskoy keramiki [Simulation of the dielectric response of piezoelectric ceramics], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 481-494. DOI: 10.26456/pcascnn/2023.15.481. (In Russian).
15. Malyshkina O.V., Malysheva N.E., Dyakova E.V., Ali M. Reasons for the negative dielectric response in the frequency range 0.5–20 MHz: modeling and experiment (using the example of sodium niobate ceramics), Physics of the Solid State, 2024, vol. 66, issue 8, pp. 1329-1335. DOI: DOI: 10.61011/PSS.2024.08.59056.100.
16. Malyshkina O.V., Malysheva N.E., Mamaev D.V. Relaksatsionnyye protsessy v poristoy keramiki niobata kaliya-natriya, Physics of the Solid State, 2025, vol. 67, issue 5, pp. 816-823. DOI: 10.61011/PSS.2025.05.61495.87-25.