Search for corrosion inhibitors of magnesium alloy in simulated biological fluids
O.A. Golovanova, D.A. Afanasiev
Omsk State University named after F.M. Dostoevsky
DOI: 10.26456/pcascnn/2026.18.832
Original article
Abstract: A study was conducted on the corrosion rate of the MA20 alloy in a simulated synovial fluid. Currently, there is an increase in the number of injuries and diseases requiring the use of surgical implants. Traditionally, titanium and other metallic structures are used for these purposes; however, after fulfilling their function, they often must be removed via a secondary surgery. Implants based on magnesium and its alloys represent a promising alternative. Magnesium is a biodegradable material that gradually degrades in the body, thereby eliminating the need for a follow-up surgical intervention. Furthermore, the mechanical properties of magnesium alloys are close to those of human bone tissue. However, the widespread application of magnesium alloys is limited by their high corrosion rate in physiological environments. If an implant degrades too rapidly, it loses its mechanical strength before the bone tissue healing is complete. This can lead to the necessity of an emergency implant replacement, additional financial costs, and prolonged patient treatment time. In this work, a series of protective coatings of various types was obtained, and their effect on the corrosion rate was evaluated. Analysis of our experimental results demonstrated that the most effective coating among those obtained was the one formed from hydroxyapatite. Apatite forms a dense insulating layer and protects the surface from the corrosive environment, which contributes to a significant reduction in corrosion, achieving a protection efficiency of 70,4%. The results of this study open new horizons for further research of the synthesis of new nanobiocomposites on the surface of magnesium alloys widely used in the development of new implants.
Keywords: magnesium, corrosion, synovial fluid, corrosion depth indicator, protective coating
- Olga A. Golovanova – Dr. Sc., Professor, Head of the Department of Inorganic Chemistry, Omsk State University named after F.M. Dostoevsky, ORCID: 0000-0001-9995-5672
- Daniil A. Afanasiev – Researcher, Department of Inorganic Chemistry, Omsk State University named after F.M. Dostoevsky
For citation:
Golovanova O.A., Afanasiev D.A. Poisk ingibitorov korrozii magnievogo splava v modelnykh biologicheskikh zhidkostyakh [Search for corrosion inhibitors of magnesium alloy in simulated biological fluids], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 832-841. DOI: 10.26456/pcascnn/2026.18.832. ⎘
Full article (in Russian): download PDF file
References:
1. James S.L., Abate D., Abate K.H. et al. Global, regional, and national incidence, prevalence, and years lived with disability for 354 diseases and injuries for 195 countries and territories, 1990-2017: a systematic analysis for the global burden of disease study, The Lancet, 2018, vol. 392, issue 10159, pp. 1789-1858. DOI: 10.1016/s0140-6736(18)32279-7.
2. Lesnyak O.M., Baranova I.A., Belova K.Yu. et al. Osteoporoz v Rossijskoj Federatsii: epidemiologiya, mediko-sotsial'nye i ekonomicheskie aspekty problemy (obzor literatury) [Osteoporosis in Russian Federation: epidemiology, socio-medical and economical aspects (review)], Travmatologiya i ortopediya Rossii [Traumatology and Orthopedics of Russia], 2018, vol. 24, no. 1, pp. 155-168. DOI: 10.21823/2311-2905-2018-24-1-155-168. (In Russian).
3. Chekisheva T.N. Nanomaterialy i ikh rol' v regeneratsii kostnoj tkani [Nanomaterials and their role in bone tissue regeneration], Klinicheskaya i eksperimental'naya morfologiya [Clinical and Experimental Morphology], 2019, vol. 8, no. 4, pp. 19-24. DOI: 10.31088/CEM2019.8.4.19-24. (In Russian).
4. Bogdanova E.A., Skachkov V.M. Izuchenie vozmozhnosti polucheniya biokomozitov na osnove nanorazmernogo gidroksiapatita s metallami i biogennymi elementami [Study of the possibility of obtaining biocomosites based on nanoscale hydroxyapatite with metals and biogenic elements], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 649-658. DOI: 10.26456/pcascnn/2023.15.649. (In Russian).
5. Liu L., Luo P., Wen P., Xu P. The role of magnesium in the pathogenesis of osteoporosis, Frontiers in Endocrinology, 2024, vol. 15, art. no. 1406248, 11 p. DOI: 10.3389/fendo.2024.1406248.
6. Banerjee P.C., Al-Saadi S., Choudhary L., Harandi S.E., Singh R. Magnesium implants: prospects and challenges. Materials, 2019, vol.12, issue 1, art. no. 136, 21 p. DOI: 10.3390/ma12010136.
7. Chen Y., Xu Z., Smith C., Sankar J. Recent advances on the development of magnesium alloys for biodegradable implants. Acta Biomaterialia, 2014, vol. 10, issue 11, pp. 4561-4573. DOI: 10.1016/j.actbio.2014.07.005.
8. Xu R.Z., Shen Y., Zheng J. et al. Effects of one-step hydrothermal treatment on the surface morphology and corrosion resistance of ZK60 magnesium alloy. Surface and Coatings Technology, 2017, vol. 309, pp. 490-496. DOI: 10.1016/j.surfcoat.2016.11.111.
9. Sedelnikova M.B., Kashin A.D., Uvarkin P.V. et al. Low-energy high-current electron beam treatment of composite coatings based on diatomite and ZrO2 particles. Letters on Materials, 2024, vol. 14, issue 3, pp. 216-222. DOI: 10.48612/letters/2024-3-216-222.
10. Gerk S.A., Golovanova O.A. Vliyanie gialuronovoy kisloty na strukturu nanogidroksiapatita i morfologicheskie kharakteristiki ikh kompozitsiy [Influence of hyaluronic acid on the structure of nanohydroxyapatite and morphological characteristics of their compositions], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and Chemical Aspects of the Study of Clusters, Nanostructures and Nanomaterials], 2024, issue 16, pp. 805-814. DOI: 10.26456/pcascnn/2024.16.805. (In Russian).
11. Kudryakova Н.О., Grishina E.P., Ramenskaya L.M. The effect of the sol-gel pH on the properties of Al2O3- and SiO2-coatings on low-alloyed 08kp steel, From Chemistry to Technology: Step by Step, 2021, vol. 2, no. 4, pp. 100-109. DOI: 10.52957/27821900_2021_04_100.
12. Bochulya R.S., Golovanova O.A. Opredelenie usloviy korrozii stali St-3 v vodnoy srede v prisutstvii oleata natriya [Determination of corrosion conditions of St-3 steel in aqueous medium in the presence of sodium oleate]. Butlerovskie soobshcheniya [Butlerov Communications], 2024, vol. 79, no. 8, pp. 73-78. DOI: 10.37952/ROI-jbc-01/24-79-8-73. (In Russian).
13. Kiselev V.M., Golovanova O.A., Fedoseev V.B. The study of modified hydroxylapatite samples using the fractal theory, Crystallography Reports, 2021, vol. 66, issue 3, pp.479-485. DOI: 10.1134/S1063774521030093.
14. Golovanova O.A., Bezzubov A.N. Sposob ingibirovaniya korrozii stali v vode [Method for inhibiting steel corrosion in water]. Patent RF, no. 2772783 C1, 2021 (In Russian).
15.GOST 9.908-85. Edinaya sistema zashchity ot korrozii i stareniya. Metally i splavy. Metody opredeleniya pokazatelej korrozii i korrozionnoj stojkosti [Unified system of corrosion and ageing protection. Metals and alloys. Methods for determination of corrosion and corrosion resistance indices]. Moscow, Izd-vo standartov Publ., 1985. 17 p. (In Russian).
16. Golovanova O.A., Zaits A.V. Biomimetic coating of a titanium substrate with silicon-substituted hydroxyapatite. Inorganic Materials, 2018, vol.54, issue 11, pp. 1124-1130. DOI: 10.1134/S0020168518110067.