Temperature-catalytic control over the formation of a layered sp/sp2-carbon nanomaterial under palladium-free Sonogashira cross-coupling conditions
D.S. Ryashentsev, D.S. Polyakov, N.V. Chernikov
Chelyabinsk State University
DOI: 10.26456/pcascnn/2026.18.943
Original article
Abstract: The possibility of replacing the palladium catalyst with 3d metals (iron, cobalt, nickel, and copper) in the synthesis of a layered sp/sp2-carbon nanomaterial via the Sonogashira cross-coupling reaction has been investigated. Acetates of the corresponding metals were used as precatalysts, o-phenanthroline served as the ligand, and copper iodide as the cocatalyst. The synthesis was carried out in dimethyl sulfoxide at 100℃ and 140℃ for 24 hours under an argon atmosphere using hexaiodobenzene and calcium carbide as sources of aromatic and acetylenic fragments. The products were subjected to multi-stage purification, including sequential washing with solutions of ammonium chloride, nitric acid, and sodium thiosulfate, followed by thermal treatment at 200℃. Using X-ray diffraction, infrared and Raman spectroscopy, it was established that the synthesis temperature and the nature of the transition metal jointly determine the structural characteristics and the degree of defectiveness of the final material. Raman spectroscopy confirmed the presence of acetylenic bridges between benzene rings. The ratio of the D– and G–band intensities varies from 0,17 to 0,31, indicating a tunable defectiveness of the sp2 matrix, while the IY/IG intensity ratios vary from 0,06 to 0,13. The obtained results demonstrate the fundamental possibility of temperature-catalytic control over the structure of graphyne-like materials without the use of a palladium catalyst.
Keywords: γ-graphyne, Sonogashira reaction, palladium-free catalysis, transition metals, layered nanostructures
- Dmitry S. Ryashentsev – Ph. D., Associate Professor, Solid State Chemistry and Nanoprocesses Department, Chelyabinsk State University, ORCID: 0009-0000-0346-2380
- Dmitry S. Polyakov – 4th year student, Solid State Chemistry and Nanoprocesses Department, Chelyabinsk State University
- Nikolai V. Chernikov – 4th year student, Solid State Chemistry and Nanoprocesses Department, Chelyabinsk State University
For citation:
Ryashentsev D.S., Polyakov D.S., Chernikov N.V. Temperaturno-kataliticheskij kontrol formirovaniya sloistogo sp/sp2-uglerodnogo nanomateriala v usloviyakh bespalladievogo kross-sochetaniya Sonogashiry [Temperature-catalytic control over the formation of a layered sp/sp2-carbon nanomaterial under palladium-free Sonogashira cross-coupling conditions], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 943-953. DOI: 10.26456/pcascnn/2026.18.943. ⎘
Full article (in Russian): download PDF file
References:
1. Belenkov E.A., Mavrinskii V.V., Belenkova T.E. et al. Structural modifications of graphyne layers consisting of carbon atoms in the sp- and sp2-hybridized states, Journal of Experimental and Theoretical Physics, 2015, vol. 120, issue 5, pp. 820-830. DOI: 10.1134/S1063776115040214.
2. Hiu X., Xie Z., Li C. Study of electronic structure, thermal conductivity, elastic and optical properties of α, β, γ-graphyne, Materials, 2018, vol. 11, issue 2, art. no 188, 14 p. DOI: 10.3390/ma11020188.
3. Jiang P.H., Liu H.J., Cheng L. et al. Thermoelectric properties of γ-graphyne from first-principles calculations, Carbon, 2017, vol. 113, pp. 108-113. DOI: 10.1016/j.carbon.2016.11.038.
4. Chandran D.G., Ramkumar N., Biswas R. A review on the recent advances in graphyne-based materials and their applications, Journal of Materials Chemistry A, 2026, vol. 14, issue 14, pp. 7909-7953. DOI: 10.1039/d5ta08904b.
5. Peng Q., Dearden A.K., Crean J. et al. New materials graphyne, graphdiyne, graphone, and graphane: review of properties, synthesis, and application in nanotechnology, Nanotechnology, Science and Applications, 2014, vol. 7, pp. 1-29. DOI: 10.2147/NSA.S40324.
6. Li J., Han Y. Artificial carbon allotrope γ-graphyne: synthesis, properties, and applications, Giant, 2023, vol. 13, art. no 100140, 15 p. DOI: 10.1016/j.giant.2023.100140.
7. Barua M., Saraswat A., Rao C.N.R. A novel method for synthesis of γ-graphyne and their charge transfer properties, Carbon, 2022, vol. 200, pp. 247-252. DOI: 10.1016/j.carbon.2022.08.061.
8. Mohjer F., Mofatehnia P., Rangraz Y. et al. Pd-free, Sonogashira cross-coupling reaction. An update, Journal of Organometallic Chemistry, 2021, vol. 936, art. no 121712, 25 p. DOI: 10.1016/j.jorganchem.2021.121712.
9. Liori A.A., Stamatopoulos I.K., Papastavrou A.T. et al. A Novel, sustainable, user-friendly protocol for the Pd-free Sonogashira coupling reaction, European Journal of Organic Chemistry, 2018, vol. 2018, issue 44, pp. 6134-6139. DOI: 10.1002/ejoc.201800827.
10. Tran N.T., Cho C.S., Sohn H.-S. et al. Iron powder-CuI cooperative catalytic system in Sonogashira cross-coupling reaction, Bulletin of the Korean Chemical Society, 2011, vol. 32, issue 3, pp. 1080-1082. DOI: 10.5012/bkcs.2011.32.3.1080.
11. Nair P.P., Philip R.M., Anilkumar G. Nickel catalysts in Sonogashira coupling reactions, Organic & Biomolecular Chemistry, 2021, vol. 19, issue 19, pp. 3950-3966. DOI: 10.1039/d1ob00280e.
12. Feng L., Liu F., Sun P. et al. Sonogashira reaction of aryl halides with terminal alkynes catalyzed by cobalt hollow nanospheres, Synlett, 2008, vol. 2008, issue 9, pp. 1415-1417. DOI: 10.1055/s-2008-1072615.
13. Arundhathi K.V., Vaishnavi P., Aneeja T. et al. Copper-catalyzed Sonogashira reactions: advances and perspectives since 2014, RSC Advances, 2023, vol. 13, issue 7, pp. 4823-4835. DOI: 10.1039/d2ra07685c.