Effect of active environment on the orientational organization of rod-like nanoparticle: mesoscale simulations
A.E. Virskiy1, M.D. Malyshev1, P.V. Komarov2
1 Tver State University
2 A.N. Nesmeyanov Institute of Organoelement Compounds of RAS
DOI: 10.26456/pcascnn/2026.18.380
Original article
Abstract: This work examines the possibility of controlling the spatial orientation of rod-like nanoparticle through the influence of molecules of active environment. We consider ordered layers formed by smectic molecules as an active environment. To model the supramolecular organization in such conditions, we employed the dissipative particle dynamics method. Our result shows that when the nanoparticle length is twice the length of a molecule of the active environment, three types of orientational ordering are possible: localization inside a domain formed by the head groups of molecules of active environment (type I), inside a domain formed by the tail groups of molecules of the active environment (type II), and perpendicular to the domains of active environment (type III). The first two orientations are stable, while the orientation perpendicular domains is unstable for long simulation times. This may indicate the potential instability of such states. We also studied the influence of the nanoparticle length and the presence of residual solvent on the stability of the identified orientational orderings of the considered nanosystems. These results could be useful for developing liquid crystal materials reinforced with rod-like nanoparticles or a switchable nanoparticles orientation.
Keywords: self-assembly, dissipative particle dynamics, nanoparticles, active environment
- Alexander E. Virskiy – 2nd year student, Tver State University, ORCID: 0009-0007-3139-8241
- Maxim D. Malyshev – Ph. D., Associate Professor of Physical Chemistry Department, Tver State University, ORCID: 0000-0002-2799-7512
- Pavel V. Komarov – Dr. Sc., Docent, Leading Researcher, Laboratory of Physical Chemistry of Polymers, A.N. Nesmeyanov Institute of Organoelement Compounds of RAS, ORCID: 0000-0003-2138-5088
For citation:
Virskiy A.E., Malyshev M.D., Komarov P.V. Vliyanie aktivnoj sredy na prostranstvennuyu organizatsiyu sterzhneobraznoj nanochastitsy: mezomasshtabnoe modelirovanie [Effect of active environment on the orientational organization of rod-like nanoparticle: mesoscale simulations], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 380-390. DOI: 10.26456/pcascnn/2026.18.380. ⎘
Full article (in Russian): download PDF file
References:
1. Singh M., Kaur N., Comini E. The role of self assembled monolayers in electronic devices, Journal of Materials Chemistry C, 2020, vol. 8, issue 12, pp. 3938-3955, DOI: 10.1039/D0TC00388C.
2. Weiden J., Bastings M.M.C. DNA origami nanostructures for controlled therapeutic drug delivery, Current Opinion in Colloid & Interface Science, 2021, vol. 52, art. no. 101411, 14 p. DOI: 10.1016/j.cocis.2020.101411.
3. Mizeikis V., Juodkazis S., Marcinkevicius A. et al. Tailoring and characterization of photonic crystals, Journal of Photochemistry and Photobiology C: Photochemistry Reviews, 2001, vol. 2, issue 1, pp. 35-69, DOI: 10.1016/S1389-5567(01)00009-0.
4. Burnett B.J., Choe W. Sequential self assembly in metal–organic frameworks, Dalton Transactions, 2012, vol. 41, issue 13, pp. 3889-3894, DOI: 10.1039/C2DT12103D.
5. Khalatur P.G., Khokhlov A.R. Nonconventional scenarios of polymer self assembly, Soft Matter, 2013, vol. 9, issue 45, art. no. 10943, 12 p. DOI: 10.1039/c3sm52181h.
6. Kato T. Self assembly of phase segregated liquid crystal structures, Science, 2002, vol. 295, issue 5564, pp. 2414-2418, DOI: 10.1126/science.1070967 a.
7. Ondreas F., Lepcio P., Zboncak M. et al. Effect of nanoparticle organization on molecular mobility and mechanical properties of polymer nanocomposites, Macromolecules, 2019, vol. 52, issue 16, pp. 6250-6259, DOI: 10.1021/acs.macromol.9b01197.
8. Coetzee D., Venkataraman M., Militky J., Petru M. Influence of nanoparticles on thermal and electrical conductivity of composites, Polymers, 2020, vol. 12, issue 4, art. no. 742, 25 p. DOI: 10.3390/polym12040742.
9. Chen J., Yan L. Effect of carbon nanotube aspect ratio on the thermal and electrical properties of epoxy nanocomposites, Fullerenes, Nanotubes and Carbon Nanostructures, 2018, vol. 26, issue 11, pp. 793-800. DOI: 10.1080/1536383X.2018.1476345.
10. Wu Q., Miao W.S., Zhang Y.D. et al. Mechanical properties of nanomaterials: a review, Nanotechnology Reviews, 2020, vol. 9, issue 1, pp. 259-273, DOI: 10.1515/ntrev 2020 0021.
11. Sides S.W., Kim B.J., Kramer E.J., Fredrickson G.H. Hybrid particle field simulations of polymer nanocomposites, Physical Review Letters, 2006, vol. 96, issue 25, pp. 250601-1-250601-4. DOI: 10.1103/PhysRevLett.96.250601.
12. Bukowczan A., Hebda E., Pielichowski K. The influence of nanoparticles on phase formation and stability of liquid crystals and liquid crystalline polymers, Journal of Molecular Liquids, 2020, vol. 322, art. no. 114849, 31 p. DOI: 10.1016/j.molliq.2020.114849.
13. Malyshev M., Guseva D., Komarov P. Two state nanocomposite based on symmetric diblock copolymer and planar nanoparticles: Mesoscopic simulation, Molecular Systems Design & Engineering, 2024, vol. 9, issue 5, pp. 409-422, DOI: 10.1039/D3ME00176H.
14. Cheng C.C., Liu M.H., Mou C.Y., Chen Y.F. Controllable orientation of assembled gold nanorods on unstructured substrates, RSC Advances, 2013, vol. 3, issue 40, pp. 17696-17699, DOI: 10.1039/c3ra41357h.
15. Smith P.A., Nordquist C.D., Jackson et al. Electric field assisted assembly and alignment of metallic nanowires, Applied Physics Letters, 2000, vol. 77, issue 9, pp. 1399-1401. DOI: 10.1063/1.1290272.
16. Español P., Warren P.B. Perspective: dissipative particle dynamics, Journal of Chemical Physics, 2017, vol. 146, issue 15, pp. 150901-1-150901-16, DOI: 10.1063/1.4979514.
17. Komarov, P.V., Malyshev, M.D., Baburkin, P.O. Mesoscale modeling of solvent evaporation from the surface of a jet of spinning solution of polyacrylonitrile in dimethyl sulfoxide, Journal of Structural Chemistry, 2025, vol. 66, issue 12, pp. 2674-2683, DOI: 10.1134/s0022476625120194.
18. Hildebrand, J.H., Scott, R.L. The solubility of nonelectrolytes. New York: Reinhold Publishing, 1950, 488 p.
19. Thompson A.P., Aktulga H.M., Berger R. et al. LAMMPS – a flexible simulation tool for particle based materials modeling at the atomic, meso, and continuum scales, Computer Physics Communications, 2022, vol. 271, art. no. 108171, 34 p. DOI: 10.1016/j.cpc.2021.108171.
20. Rudzinski J.F. Recent progress towards chemically specific coarse grained simulation models with consistent dynamical properties, Computation, 2019, vol. 7, issue 3, art. no. 42, 28 p. DOI: 10.3390/computation7030042.
21. Voevodin Vl., Antonov A., Nikitenko D. et. al. Supercomputer Lomonosov-2: large scale, deep monitoring and fine analytics for the user community, Supercomputing Frontiers and Innovations, 2019, vol. 6, issue 2, pp. 4-11. DOI: 10.14529/jsfi190201.