The influence of small additives of lithium on the surface tension of alloys based on bismuth
O.Kh. Kanametova, F.F. Dyshekova
Kabardino-Balkarian State University named after Kh.M. Berbekov
DOI: 10.26456/pcascnn/2026.18.054
Short communication
Abstract: The paper presents the results of an experimental study of the temperature and concentration dependences of the surface tension of bismuth and its alloys with small additives of lithium in a composition range containing up to 0,44 at.% Li. Surface tension measurements were carried out by the large drop method using an automated experimental setup and the «SigmaDrop» hardware and software complex in the temperature range of 570-700 K; the error was of approximately 2,5%. A specially developed solid-soldered measuring cell ensured identical alloy preparation conditions and reliable thermodynamic equilibrium of the surface of each alloy with its own saturated vapor. Our study demonstrated that the temperature dependence of the surface tension of all liquid alloys is strictly linear. The concentration dependence of the surface tension at a temperature of 600 K was plotted as a monotonic curve. Based on the obtained isotherms, it was concluded that lithium is a weak surface-inactive additive in the studied composition range. The obtained results are in agreement with the criteria for the surface activity of components in binary alloys, as well as with the literature data on the activity coefficient of lithium, which maintains a constant value in the concentration range of compositions with a low lithium content in melts with bismuth.
Keywords: lithium, bismuth, alloys, surface tension, large drop method
- Oksana Kh. Kanametova – Ph. D., Senior Lecturer, Department of Theoretical and Experimental Physics, Kabardino-Balkarian State University named after Kh.M. Berbekov
- Fatima F. Dyshekova – Ph. D., Docent, Department of Theoretical and Experimental Physics, Kabardino-Balkarian State University named after Kh.M. Berbekov
For citation:
Kanametova O.Kh., Dyshekova F.F. Vliyanie malykh dobavok litiya na poverkhnostnoe natyazhenie rasplavov vismuta [The influence of small additives of lithium on the surface tension of alloys based on bismuth], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 54-61. DOI: 10.26456/pcascnn/2026.18.054. ⎘
Full article (in Russian): download PDF file
References:
1. Alchagirov B.B., Khokonov Kh.B. Shchelochnyye metally i splavy s ikh uchastiyem – perspektivnyye materialy sovremennoy tekhniki i energetiki [Alkali metals and alloys containing them – promising materials for modern engineering and energy], Fizika i khimiya perspektivnykh materialov [Physics and chemistry of advanced materials], collection of scientific papers. Nal'chik, KBSU Publ., 1998, pp. 40-44. (In Russian).
2. Subbotin V.I., Arnol'dov M.N., Kozlov F.A., Shimkevich A.L. Liquid-metal coolants for nuclear power, Atomic energy, 2002, vol. 92, no. 1, pp. 29-40. DOI: 10.1023/A:1015050512710.
3. Nizhenko V.I., Floka L.I. Poverkhnostnoye natyazheniye metallov i splavov. Spravochnik [Surface tension of metals and alloys. Handbook], Moscow, Metallurgiya Publ., 1981, 208 p. (In Russian).
4. Alchagirov B.B., Arkhestov R.Kh., Dyshekova F.F., Taova T.M. Surface tension of alloys with additives of alkali metals, High Temperature, 2013, vol. 51, issue 2, pp. 183-196. DOI: 10.1134/S0018151X13020016.
5. Sobolev V. Database of thermophysical properties of liquid metal coolants for GEN-IV: Sodium, lead, lead-bismuth eutectic (and bismuth), version v1. Mol, SCK CEN Publ., 2011, 175 p.
6. Alchagirov B.B. Poverkhnostnoye natyazheniye zhidkikh shchelochnykh metallov i splavov s ikh uchastiyem [Surface tension of liquid alkali metals and alloys containing them], Obzory po teplofizicheskim svoystvam veshchestv [Reviews on thermophysical properties of substances]. Мoscow, Institute of High Temperatures of the USSR Academy of Sciences, 1991, no. 3-4, 180 p. (In Russian).
7. Alchagirov B.B., Mozgovoi A.G., Taova T.M., Sizhazhev T.A. Termicheskiye svoystva perspektivnykh materialov i teplonositeley zhidkometallicheskogo blanketa termoyadernogo reaktora. Svinets-litiyevaya evtektika [Thermal properties of promising tritium-reproduced materials and heat-transfer agents for liquid-metal blanket of thermonuclear reactor. Pb-Li eutectic], Perspektivnye materialy, 2005, no. 6, pp. 35-42. (In Russian).
8. Alchagirov B.B., Dyshekova F.F., Arkhestov R.K. Surface tension of lead–lithium melts, Russian Journal of Physical Chemistry A, 2016, vol. 90, issue 11, pp. 2262-2269. DOI: 10.1134/S0036024416110029.
9. Alchagirov B.B., Arkhestov R.Kh., Dyshekova F.F., Kyasova O.Kh. Poverkhnostnoye natyazheniye splavov litiya na osnove vismuta [Surface tension of bismuth-based lithium alloys], Doklady Adygskoj (Cherkesskoj) mezhdunarodnoj akademii nauk [Reports of the Adyghe (Circassian) International Academy of Sciences], 2015, vol. 17, no. 3, pp. 78-85. (In Russian).
10. GOST R Р 8.585-2001. Gosudarstvennaya sistema obespecheniya edinstva izmerenij. Termopary. Nominal'nye staticheskie kharakteristiki preobrazovaniya [Russian State Standart 8.585-2001. State system for ensuring the uniformity of measurements. Thermocouples. Nominal static characteristics of conversion]. Moscow, Stadartinform Publ., 2010, 81 p. (In Russian).
11. Arnol’dov M.N., Karzhavin V.A., Trofimov A.I. Osnovy metrologicheskogo obespecheniya temperaturnogo kontrolya reaktornykh ustanovok: uchebnoye posobiye dlya vuzov [Fundamentals of metrological support for temperature monitoring of reactor facilities: a textbook for universities]. Moscow, MEI Publ., 2012, 248 p. (In Russian).
12. Alchagirov B.B., Kokov Z.A., Dyshekova F.F. et al. Programma avtomatizatsii fizicheskogo eksperimenta po izmereniyu poverhnostnogo natyazheniya zhidkostej metodom lezhashchej kapli [A program for automating a physical experiment to measure the surface tension of liquids using the sessile drop method]. Certificate RF, no. 2015614191, 2015. (In Russian).
13. Alchagirov B.B. Ustroystvo dlya opredeleniya poverkhnostnogo natyazheniya zhidkikh metallov i splavov [Device for determining the surface tension of liquid metals and alloys]. Сertificate of authorship USSR, no. 1469318, 1989. (In Russian).
14. Alchagirov B.B., Alberdieva D.Kh., Arkhestov R.Kh. et al. Pribor dlya sovmestnogo izmereniya poverkhnostnogo natyazheniya i raboty vykhoda elektrona zhidkometallicheskikh sistem s uchastiyem komponentov s vysokoy uprugost'yu nasyshchennogo para metallov i splavov [Device for joint measurement of surface tension and electron work function of liquid metal systems involving components with high saturated vapor pressure of metals and alloys], Patent RF, no. 2511277, 2014. (In Russian).
15. Maze C., Burnet G. Estimation of non-equilibrium surface tension, Surface of Science, 1971, vol. 27, issue 3, pp. 411-418. DOI: 10.1016/0039-6028(71)90178-6.
16. Fima P., Nowak R., Sobczak N. Effect of metal purity and testing procedure on surface tension measurements of liquid tin, Journal of Materials Science, 2010, vol. 45, issue 8, pp. 2009-2014. DOI: 10.1007/s10853-009-3973-y.
17. Unezhev B.Kh., Makhova M.M. K metodike izmereniya poverkhnostnogo natyazheniya zhidkikh metallov osoboy chistoty [To the method of measuring the surface tension of liquid metals of special purity], Fizika poverkhnostnykh yavleniy v rasplavakh [Physics of surface phenomena in melts]. Grozny: Chechen-Ingush State University Publ., 1977, Part 1, pp. 79-84. (In Russian).
18. GOST 10928-90. Vismut. Tekhnicheskie usloviya [Russian State Standart 10928-90. Bismuth. Specifications]. Moscow, Izdatel’stvo standartov Publ., 1990, 6 p. (In Russian).
19. GOST 8774-75. Litij. Tekhnicheskie usloviya [Russian State Standart 8774-75. Lithium. Specifications]. Moscow, IPK Standartov Publ., 2001, 5 p. (In Russian).
20. Lyakishev N.P., Bannykh O.A., Rokhlin L.L. et al. Diagrammy sostoyaniya dvoinykh metallicheskikh sistem: Spravochnik [State diagrams of binary metal systems: handbook], ed. by N.P. Lyakisheva. Moscow, Mashinostroenie Publ., 1996, vol. 1, pp. 656-658. (In Russian).
21. Sangster J., Pelton A.D. The Bi-Li (bismuth-lithium) system, Journal of Phase Equilibria, 1991, vol. 12, issue 4, p. 447-450. DOI: 10.1007/BF02645966.
22. Keene B.J. Review of data for the surface tension of pure metals, International Materials Reviews, 1993, vol. 38, issue 4, pp. 157-192. DOI: 10.1179/imr.1993.38.4.157.
23. Zadumkin S.N., Khokonov Kh.B., Karamurzov B.S. и др. Fizika mezhfaznykh yavleniy v kondensirovannykh sredakh [Physics of interfacial phenomena in condensed media], Nalchik: KBSU Publ., 2014. 247 p. (In Russian).
24. Demidov A.I., Morachevsky A.G. Termodinamicheskiye svoystva zhidkikh splavov sistemy litiy-vismut [Thermodynamic properties of liquid alloys of the lithium-bismuth system], Elektrokhimiya [Soviet Electrochemistry], 1973, vol. 9, issue 8, pp. 1393-1394. (In Russian).