Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Investigation of magnetic properties of cobalt nanofilms and their potential for spintronic device applications

A.Yu. Fedotov, O.Yu. Severyukhina, A.Yu. Salomatina

Udmurt Federal Research Center of the Ural Branch of the RAS

DOI: 10.26456/pcascnn/2026.18.771

Original article

Abstract: In this study, performed using a hybrid method of molecular dynamics and spin modeling within the LAMMPS software package with the SPIN module, the influence of the thickness of crystalline cobalt films on their magnetic properties was investigated. The thickness varied from 1,8 to 7,1 nm. It is shown that the film thickness significantly affects its magnetic behavior due to the interplay between surface and bulk effects. In ultrathin films (less than 4,5 nm in thickness), inhomogeneity of the magnetic response is observed. This is attributed to the dominance of the surface effects and atomic-scale roughness, which creates local demagnetizing fields. As a result, domain walls behave chaotically, leading to some stepwise changes in the magnetization and inhomogeneity of its distribution. The normalized magnetic energy is the highest in such films. At thicknesses of 4,5-7,1 nm, the films exhibit the bulk magnetic behavior. Reducing the proportion of surface atoms allows the bulk properties of cobalt to dominate. The magnetization becomes more stable, and its distribution becomes uniform. The magnetic energy, normalized to the number of atoms, approaches a value characteristic of bulk cobalt. A direct proportionality was observed between this energy and the proportion of the surface atoms, clearly indicating the decisive contribution of the surface to the formation of increased energy and spatial heterogeneity of magnetic properties at the nanoscale. The obtained data can be used in the creation of spintronic elements and magnetic recording devices.

Keywords: mathematical modeling, thin films, cobalt, molecular dynamics, spin dynamics, ferromagnet, magnetic properties

  • Aleksey Yu. Fedotov – Dr. Sc., Leading Researcher, Udmurt Federal Research Center of the Ural Branch of the RAS, ORCID: 0000-0002-0463-3089
  • Olesya Yu. Severyukhina – Ph. D., Researcher, Udmurt Federal Research Center of the Ural Branch of the RAS, ORCID: 0000-0001-6014-9462
  • Anastasia Yu. Salomatina – Postgraduate student, Udmurt Federal Research Center of the Ural Branch of the RAS, ORCID: 0000-0003-4104-6454

For citation:

Fedotov A.Yu., Severyukhina O.Yu., Salomatina A.Yu. Issledovanie magnitnykh kharakteristik nanoplenok kobalta v kontekste ikh potentsiala dlya primeneniya v ustrojstvakh spintroniki [Investigation of magnetic properties of cobalt nanofilms and their potential for spintronic device applications], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 771-786. DOI: 10.26456/pcascnn/2026.18.771. ⎘

Full article (in Russian): download PDF file

References:

1. Emegha J.O., Onyenike K., Jolayemi R.O. et al. Synthesis and characterization of zinc cobalt sulphide nanofilms for optoelectronic applications, Chemistry of Inorganic Materials, 2024, vol. 4, art. no. 100068, 7 p. DOI: 10.1016/j.cinorg.2024.100068.
2. Reinhardt M., Dalgleish S., Shuku Y. et al. Molecular and thin film properties of cobalt half-sandwich compounds for optoelectronic application, Physical Chemistry Chemical Physics, 2017, vol. 19, issue 9, pp. 6768-6776. DOI: 10.1039/C6CP08685C.
3. Wöllenstein J., Burgmair M., Plescher G. et al. Cobalt oxide based gas sensors on silicon substrate for operation at low temperatures, Sensors and Actuators B: Chemical, 2003, vol. 93, issue 1-3, pp. 442-448. DOI: 10.1016/S0925-4005(03)00168-0.
4. Yadav B.C., Yadav R.C., Singh S. et al. Nanostructured cobalt oxide and cobalt titanate thin films as optical humidity sensor: a new approach, Optics & Laser Technology, 2013, vol. 49, pp. 68-74. DOI: 10.1016/j.optlastec.2012.12.011.
5. Chu Y.Q., Fu Z.W., Qin Q.Z. Cobalt ferrite thin films as anode material for lithium ion batteries, Electrochimica Acta, 2004, vol. 49, issue 27, pp. 4915-4921. DOI: 10.1016/j.electacta.2004.06.012.
6. Kang J.S., Kim J.-Y., Yoon J. et al. Room-temperature vapor deposition of cobalt nitride nanofilms for mesoscopic and perovskite solar cells, Advanced Energy Materials, 2018, vol. 8, issue 13, art. no. 1703114, 12 p. DOI: 10.1002/aenm.201703114.
7. Kaphle A., Hari P. Enhancement in power conversion efficiency of silicon solar cells with cobalt doped ZnO nanoparticle thin film layers, Thin Solid Films, 2018, vol. 657, pp. 76-87. DOI: 10.1016/j.tsf.2018.05.014.
8. Lee K.K., Chin W.S., Sow C.H. Cobalt-based compounds and composites as electrode materials for high-performance electrochemical capacitors, Journal of Materials Chemistry A, 2014, vol. 2, issue 41, pp. 17212-17248. DOI: 10.1039/C4TA02074J.
9. Zhao F., Wang Y., Xu X. et al. Cobalt hexacyanoferrate nanoparticles as a high-rate and ultra-stable supercapacitor electrode material, ACS Applied Materials & Interfaces, 2014, vol. 6, issue 14, pp. 11007-11012. DOI: 10.1021/am503375h.
10. Schmidt D., Kjerstad A.C., Hofmann T. et al. Optical, structural, and magnetic properties of cobalt nanostructure thin films, Journal of Applied Physics, 2009, vol. 105, issue 11, pp. 113508-1-113508-7. DOI: 10.1063/1.3138809.
11. Martins S., de Rojas J., Tan Z. et al. Dynamic electric-field-induced magnetic effects in cobalt oxide thin films: towards magneto-ionic synapses, Nanoscale, 2022, vol. 14, issue 3, pp. 842-852. DOI: 10.1039/D1NR06210G.
12. Hehn M., Padovani S., Ounadjela K., Bucher J.P. Nanoscale magnetic domain structures in epitaxial cobalt films, Physical Review B, 1996, vol. 54, issue 5, p. 3428-3433. DOI: 10.1103/PhysRevB.54.3428.
13. Bhatti K.P., Malik V.K., Chaudhary S. Cobalt substituted ZnO thin films: a potential candidate for spintronics, Journal of Materials Science: Materials in Electronics, 2008, vol. 19, issue 8-9, pp. 849-854. DOI: 10.1007/s10854-007-9501-4.
14. Wen T., Krishnan K.M. Cobalt-based magnetic nanocomposites: fabrication, fundamentals and applications, Journal of Physics D: Applied Physics, 2011, vol. 44, no. 39, art. no. 393001, 24 p. DOI: 10.1088/0022-3727/44/39/393001.
15. Srikala D., Singh V.N., Banerjee A., Mehta B.R., Patnaik S. Synthesis and characterization of ferromagnetic cobalt nanospheres, nanodiscs and nanocubes, Journal of Nanoscience and Nanotechnology, 2009, vol. 9, I. 9, pp. 5627-5632. DOI: 10.1166/jnn.2009.1157.
16. Londoño-Calderón C.L., Moscoso-Londoño O., Muraca D. et al. Synthesis and magnetic properties of cobalt-iron/cobalt-ferrite soft/hard magnetic core/shell nanowires, Nanotechnology, 2017, vol. 28, issue 24, art. no. 245605, 17 p. DOI: 10.1088/1361-6528/aa7010.
17. Zhao J., Spasova M., Li Z.A., Zharnikov M. Ferromagnetic cobalt nanoparticles and their immobilization on monomolecular films and chemical templates, Advanced Functional Materials, 2011, vol. 21, issue 24, pp. 4724-4735. DOI: 10.1002/adfm.201101570.
18. Senthil V.P., Gajendiran J., Raj S.G. et al. Study of structural and magnetic properties of cobalt ferrite (CoFe2O4) nanostructures, Chemical Physics Letters, 2018, vol. 695, pp. 19-23. DOI: 10.1016/j.cplett.2018.01.057.
19. Repain V., Baudot G., Ellmer H., Rousset S. Two-dimensional long-range–ordered growth of uniform cobalt nanostructures on a Au (111) vicinal template, Europhysics Letters, 2002, vol. 58, issue 5, pp. 730-736. DOI: 10.1209/epl/i2002-00410-4.
20. Kanter H., Vernon Jr. F.L. High-frequency response of josephson point contacts, Journal of Applied Physics, 1972, vol. 43, issue 7, pp. 3174-3183. DOI: 10.1063/1.1661682.
21. Khaire T.S., Khasawneh M.A., Pratt Jr. W.P., Birge N.O. Observation of spin-triplet superconductivity in Co-based Josephson junctions, Physical Review Letters, 2010, vol. 104, issue 13, pp. 137002-1-137002-4. DOI: 10.1103/PhysRevLett.104.137002.
22. Eschrig M. Spin-polarized supercurrents for spintronics, Physics Today, 2011, vol. 64, issue 1, pp. 43-49. DOI: 10.1063/1.3541944.
23. Tanaka M., Furuta M., Ichikawa T. et al. Generation of spin-polarized electronic currents using perpendicularly magnetized cobalt ferrite spin-filtering barriers grown on spinel-type-conductive layers, Applied Physics Letters, 2023, vol. 122, issue 4, art. no. 042401, 5 p. DOI: 10.1063/5.0131390.
24. Shchelkachev N.M. Critical current in superconducting quantum point contacts, Journal of Experimental and Theoretical Physics Letters, 2000, vol. 71, issue 12, pp. 504-507. DOI: 10.1134/1.1307476.
25. Vakhrushev A., Fedotov A., Sidorenko A. Simulation of multilayer nanosystems interface formation process for spintronics, Key Engineering Materials, 2021, vol. 888, pp. 57-65. DOI: 10.4028/www.scientific.net/KEM.888.57.
26. Sidorenko A.S., Morari R.A., Boian V. et al. Hybrid nanostructures superconductor-ferromagnet for superconducting spintronics, Journal of Physics: Conference Series, 2021, vol. 1758, issue 1, pp. 012037.1-5. DOI: 10.1088/1742-6596/1758/1/012037.
27. Fedotov A., Severyukhina O., Salomatina A., Sidorenko A. Modeling magnetic properties of cobalt nanofilms used as a component of spin hybrid superconductor–ferromagnetic structures, Beilstein Journal of Nanotechnology, 2025, vol. 16, pp. 1557-1566. DOI: 10.3762/bjnano.16.110.
28. Vakhrushev A.V., Fedotov A.Yu., Severyukhina O.Yu., Sidorenko A.S. The influence of structure and local structural defects on the magnetic properties of cobalt nanofilms, Beilstein Journal of Nanotechnology, 2023, vol. 14, pp. 23-33. DOI: .
29. Tranchida J., Plimpton S.J., Thibaudeau P., Thompson A.P. Massively parallel symplectic algorithm for coupled magnetic spin dynamics and molecular dynamics, Journal of Computational Physics, 2018, vol. 372, pp. 406-425. DOI: 10.1016/j.jcp.2018.06.042.
30. Ermak D.L., Buckholz H. Numerical integration of the Langevin equation: Monte Carlo simulation, Journal of Computational Physics, 1980, vol. 35, issue 2, pp. 169-182. DOI: 10.1016/0021-9991(80)90084-4.
31. Xu F., Li G., Chen J. et al. Unified framework of the microscopic Landau-Lifshitz-Gilbert equation and its application to skyrmion dynamics, Physical Review B, 2023, vol. 108, issue 14, pp. 144409-1-144409-13. DOI: 10.1103/PhysRevB.108.144409.
32. Garcia-Palacios J.L., Lazaro F.J. Langevin-dynamics study of the dynamical properties of small magnetic particles, Physical Review B, 1998, vol. 58, issue 22, pp. 14937-14958. DOI: 10.1103/PhysRevB.58.14937.
33. Baskes M.I. Modified embedded-atom potentials for cubic materials and impurities, Physical Review B, 1992, vol. 46, issue 5, pp. 2727-2742. DOI: 10.1103/PhysRevB.46.2727.
34. Plimpton S. Fast parallel algorithms for short-range molecular dynamics, Journal of Computational Physics, 1995, vol. 117, issue 1, pp. 1-19. DOI: 10.1006/jcph.1995.1039.
35. Henry Y., Ounadjela K., Piraux L. et al. Magnetic anisotropy and domain patterns in electrodeposited cobalt nanowires, The European Physical Journal B - Condensed Matter and Complex Systems, 2001, vol. 20, issue 1, pp. 35-54. DOI: 10.1007/s100510170283.
36. Guo J.G., Zhao Y.P. The size-dependent elastic properties of nanofilms with surface effects, Journal of Applied Physics, 2005, vol. 98, issue 7, pp. 074306-1-074306-11. DOI: 10.1063/1.2071453.
37. Choi D., Son B., Park T.H., Hong J. Controlled surface functionality of magnetic nanoparticles by layer-by-layer assembled nano-films, Nanoscale, 2015, vol. 7, issue 15, pp. 6703-6711. DOI: 10.1039/C4NR07373H.

Content |