Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Charge transfer effects in Me-Al2O3-SiO2-Si structures

G.A. Mustafayev1, N.V. Cherkesova1, A.G. Mustafayev2

1 Kabardino-Balkarian State University
2 Dagestan State University of National Economy

DOI: 10.26456/pcascnn/2026.18.082

Original article

Abstract: The aim of the work is to experimentally study the effects of charge transfer and flat-band voltage shift in metal-Al2O3-SiO2-Si structures under high-temperature treatment and applied bias. It was found that a negative bias resulted in the formation of an «instantaneous» polarization component of the shift, while a positive bias additionally produced a thermally activated «slow» component with a delay time of ~10 min at 125°C. The dependence of the shift on applied voltage at 190°C is linear. It was determined that charge transfer from the metal-Al2O3 interface to the Si-SiO2 interface was caused by the thermal release of carriers from bulk traps with an activation energy of 1,2 eV. A correlation was found between aluminum oxide thickness and the stability of the structure’s parameters, with the minimum mobile charge density observed at a layer thickness of 70 nm. Practical significance is as follows: optimizing the Al2O3 layer thickness to 70 nm ensures maximum stability of the electrical characteristics of metal-insulator-semiconductor structures under combined thermal and electrical loads. The obtained patterns and physical model of charge transport can be used in the technological design of reliable microelectronic devices.

Keywords: metal-insulator-semiconductor-structures, flat-band voltage, capacitance-voltage characteristics, high-temperature processing, multilayer dielectric, charge traps, stability of parameters

  • Gasan A. Mustafayev – Dr. Sc., Professor, Department of Electronics and Digital Information Technologies, Kabardino-Balkarian State University
  • Natalya V. Cherkesova – Ph. D., Associate Professor, Department of Electronics and Digital Information Technologies, Kabardino-Balkarian State University
  • Arslan G. Mustafayev – Dr. Sc., Professor, Department of Information Technologies and Information Security, Dagestan State University of National Economy, ORCID: 0000-0003-3463-4303

For citation:

Mustafayev G.A., Cherkesova N.V., Mustafayev A.G. Effekty perenosa zaryada v strukturakh Me-Al2O3-SiO2-Si [Charge transfer effects in Me-Al2O3-SiO2-Si structures], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 82-93. DOI: 10.26456/pcascnn/2026.18.082. ⎘

Full article (in Russian): download PDF file

References:

1. Khosla R., Rolseth E.G., Kumar P. et al. Charge trapping analysis of metal/Al2O3/SiO2/Si gate stack for emerging embedded memories, IEEE Transactions on Device and Materials Reliability, 2017, vol. 17, issue 1, pp. 80-89. DOI: 10.1109/TDMR.2017.2659760.
2. Gritsenko V.A., Islamov D.R. Fizika dielectricheskikh plenok. Mekhanizmy transporta zaryada i fizicheskie osnovy priborov pamyati [Physics of dielectric films. Charge transport mechanisms and physical basis of memory devices]. Novosibirsk, IPF SB RAS Publ., 2017, 351 p. (In Russian).
3. Fitting H.-J., Meyza X., Guerret-Piécourt C. et al. Selfconsistent electrical charging in insulators, Journal of the European Ceramic Society, 2005, vol. 25, issue 12, pp. 2799-2803. DOI: 10.1016/j.jeurceramsoc.2005.03.143.
4. Kim A.S., Serko N.A., Khakuashev P.E., et al. Application of Al2O3 film for stabilization of the charge properties of the SiO2/p–Si interface, Russian Microelectronics, 2023, vol. 52, issue 8, pp. 835-841. DOI: 10.1134/S1063739723080012.
5. Glavatskikh A., Kortov V.S., Fitting H.–J. Self-consistent electrical charging of insulating layers and metal-insulator-semiconductor structures, Journal of Applied Physics, 2001, vol. 89, issue 1, pp. 440-448. DOI: 10.1063/1.1330242.
6. Novikov Y.N., Gritsenko V.A., Nasyrov K.A. Multiphonon mechanism of the ionization of traps in Al2O3: experiment and numerical simulation, JETP Letters, 2009, vol. 89, issue 10, pp. 506-509. DOI: 10.1134/S0021364009100075.
7. Novikov Y.N., Gismatulin A.A., Hallac B., et al. Bipolar charge transport and contact phenomena in Al2O3, Thin Solid Films, 2023, vol. 781, art. no. 140004, 7 p. DOI: 10.1016/j.tsf.2023.140004.
8. Patel H., Reichel C., Richter A. et al. Effective charge dynamics in Al2O3/SiO2 multilayer stacks and their influence on silicon surface passivation, Applied Surface Science, 2022, vol. 579, art. no. 152175, 8 p. DOI: 10.1016/j.apsusc.2021.152175.
9. Pantisano L., Lucci L., Cartier E. et al. Impact of band structure on charge trapping in thin SiO2/Al2O3/poly–Si gate stacks, IEEE Electron Device Letters, 2004, vol. 25, issue 5, pp. 320-322. DOI: 10.1109/LED.2004.826534.
10. Tsepulin V.G., Tolstoguzov V.L., Karasik V.E. et al. Izmerenie raspredeleniya tolshchin mnogoslojnykh plenochnykh struktur metodami spektral'noj reflektometrii [Thickness distribution measurement of multilayer film structures by spectral reflectometry methods], Vestnik Moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana. Seriya Priborostroenie [Herald of the Bauman Moscow State Technical University. Series Instrument Engineering], 2016, no. 3 (108), pp. 3-12. (In Russian).
11. Goldman E.I., Kuharskaya N.F., Levashov S.A. et al. Determination of the parameters of metal–insulator–semiconductor structures with ultrathin insulating layer from high-frequency capacitance–voltage measurements, Semiconductors, 2019б vol. 53, issue 1, pp. 42-45. DOI: 10.1134/S1063782619010081.
12. Andreev V.V., Stolyarov A.A., Vasyutin D.S., Mikhal'kov A.M. Kontrol' kachestva dielektricheskikh sloyov integral'nykh mikroskhem i izdelij mikrosistemnoj tekhniki [Quality control of dielectric layers of integrated circuits and microsystem technology products], Naukoemkie tekhnologii [Science-intensive Technologies], 2010, no. 7, pp. 44-52. (In Russian).
13. Tsujide T. C‑V shift characteristics of metal‑Al2O3‑Si and metal‑Al2O3‑SiO2‑Si structures, Japanese Journal of Applied Physics, 1972, vol. 11, issue 1, pp. 62-69. DOI: 10.1143/JJAP.11.62.
14. Liu Y., Chen T.P., Ding L., et al. Temperature dependence of current transport in Al/Al2O3 nanocomposite thin films, Journal of Applied Physics, 2011, vol. 110, issue 9, pp. 096108-1-096108-3. DOI: 10.1063/1.3663313.

Content |