Processes of structural disordering in the solid solution Li0,015Na0,985Ta0,1Nb0,9O3

N.A. Teplyakova

Tananaev Institute of Chemistry – Subdivision of the Federal Research Centre «Kola Science Centre of the RAS»

DOI: 10.26456/pcascnn/2026.18.164

Original article

Abstract: Temperature-induced changes in the Raman spectra of the Li0,015Na0,985Ta0,1Nb0,9O3 solid solution have been studied in the low-frequency region. This region encompasses the fully symmetric librations of the oxygen octahedra as a whole, vibrations of the Li and Na cations in the cuboctahedral voids, and vibrations of the Nb and Ta cations in the octahedral voids in the temperature range of 22-400°C. As the temperature increases, a significant broadening of the Raman spectrum bands appears. This indicates disordering of the solid solution structure. However, a “softening” (decrease in frequency) of the band in the 50-80 cm-1 region corresponding to the totally symmetric librations of the oxygen octahedra as a whole is also observed. This fact indicates a misorientation in the structure of the Li0,015Na0,985Ta0,1Nb0,9O3 solid solution of oxygen octahedra, while the possibilities for transport of Li ions at high temperatures increase. A predominant broadening (compared to other spectral bands) and a decrease in band intensity have been detected In the 110-160 cm-1 range. These bands correspond to vibrations of Na+ and Li+ cations in Li/NaO12 polyhedra. This indicates “melting” of the alkali metal sublattice. Such behavior of the Raman spectrum bands indicates the existence of a phase transition to a state with superionic conductivity in the studied Li0,015Na0,985Ta0,1Nb0,9O3 solid solutions.

Keywords: ceramic solid solutions; phase transition; superionic conductivity; Raman scattering

  • Natalya A. Teplyakova – Ph. D., Leading Researcher, Vibrational Spectroscopy Sector of the Electronic Engineering Materials Laboratory, Tananaev Institute of Chemistry – Subdivision of the Federal Research Centre «Kola Science Centre of the RAS»

For citation:

Teplyakova N.A. Protsessy strukturnogo razuporyadocheniya v tverdom rastvore Li0,015Na0,985Ta0,1Nb0,9O3 [Processes of structural disordering in the solid solution Li0,015Na0,985Ta0,1Nb0,9O3], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 164-170. DOI: 10.26456/pcascnn/2026.18.164. ⎘

Full article (in Russian): download PDF file

References:

1. Palatnikov M.N., Sidorov N.V., Kalinnikov V.Т. Segnetoelektricheskie tverdye rastvory na osnove oksidnykh soedinenij niobiya i tantala: sintez, issledovanie strukturnogo uporyadocheniya i fizicheskikh kharakteristik [Ferroelectric solid solutions on the basis of niobium and tantalum oxyde compounds: synthesis, investigation of structural ordering and physical characteristics]. Saint Petersburg, Nauka Publ., 2002, 304 p. (In Russian).
2. Sidorov N.V., Palatnikov M.N., Teplyakova N.A., Kalinnikov V.Т. Segnetoelektricheskie tverdye rastvory LixNa1-xTayNb1-yO3. Sintez, struktura, svojstva [Ferroelectric solid solutions LixNa1-xTayNb1-yO3. Synthesis, structure, properties]. Moscow, Nauka Publ., 2015. – 231 р. (In Russian).
3. Zhang G., Jin L., Zhang R. et al. Recent advances in the development of electronically and ionically conductive metal-organic frameworks, Coordination Chemistry Reviews, 2021, vol. 439, art. no 213915, 30 p. DOI: 10.1016/j. ccr.2021.213915.
4. Papac M., Stevanovi´c V., Zakutayev A. et al. Triple ionic–electronic conducting oxides for next-generation electrochemical devices, Nature Materials, 2021, vol. 20, pp. 301-313, DOI: 10.1038/s41563-020-00854-8.
5. Zvonareva I., Fu X.-Z., Medvedev D. et al. Electrochemistry and energy conversion features of protonic ceramic cells with mixed ionic-electronic electrolytes, Energy and Environmental Science, 2022, vol. 15, issue 2, pp. 439-465. DOI: 10.1039/D1EE03109K.
6. Hboub H., Zelmati O., Masaif N. Theoretical approach to study Li self-diffusivities dependence on composition in lithium niobate single crystals, Physica Scripta, 2025, vol. 100, no. 4, art. no. 045916, 23 p. DOI: 10.1088/1402-4896/adbb2c
7. Deng W., Li X., Shi W. et al. Enhancing ionic conductivity of glass-type electrolyte by strategically increasing the concentration of charge carrier, Journal of Alloys and Compounds, 2020, vol. 843, art. no. 155942, 17 p. DOI: 10.1016/j. jallcom.2020.155942.
8. Fop S., McCombie K.S., Wildman E.J. et al. High oxide ion and proton conductivity in a disordered hexagonal perovskite, Nature Materials, 2020, vol. 19, pp. 752-757. DOI: 10.1038/s41563-020-0629-4.
9. Blázquez-Castro A., García-Cabañes A., Carrascosa M. Biological applications of ferroelectric materials, Applied Physics Reviews, 2018, vol. 5, no. 4, pp. 041101-1-041101-19. DOI: 10.1063/1.5044472.
10. Teplyakova N.A., Sidorov N.V., Palatnikov M.N. Investigating ionic mobility in solid solutions of LiхNa1-хTaуNb1-уO3 Raman spectroscopy, Bulletin of the Russian Academy of Sciences: Physics, 2014, vol. 78, issue 8, pp. 796-798.
11. Palatnikov M.N., Sandler Yu.A., Serebryakov Yu.A., et al., Litievye superionnye provodniki na osnove segnetoelektricheskikh tverdykh rastvorov LiхNa1-хTaуNb1-уO3 [Lithium superionic conductors based on ferroelectric solid solutions LiхNa1-хTaуNb1-уO3], Neorganicheskie Materialy [Inorganic Materials], 1992, vol. 28, no. 9, pp. 1995-1998. (In Russian).
12. Efremov V.V., Shcherbina O.B., Radyush Yu.V. et al. Mikrostruktura, fazovye sostoyaniya, dielektricheskie i uprugie svojstva keramicheskikh tverdykh rastvorov Li0,17Na0,83TaуNb1-уO3, poluchennykh pri vysokom davlenii [Microstructure, phase states, dielectric and elastic properties of ceramic solid solutions Li0,17Na0,83TaуNb1-уO3 obtained at higt pressure], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2018, no. 10, pp. 252-261. DOI: 10.26456/pcascnn/2018.10.252 (In Russian).
13. Palatnikov M.N., Sidorov N.V., Kalinnikov V.Т. Tehnologiya upravlyaemogo sinteza monokristallicheskikh i keramicheskikh materialov na osnove niobatov-tantalatov shchelochnykh metallov [The technology of controlled synthesis of single crystal and ceramic materials on the basis of alkali metal niobates-tantalates], Czvetnye metally [Non-ferrous metals], 2000, no. 10, pp. 54-59. (In Russian).

Content |