Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Patterns of calcium phosphate degradation in lactic acid

A.A. Provorkina, O.A. Golovanova

Omsk State University named after F.M. Dostoevsky

DOI: 10.26456/pcascnn/2026.18.908

Original article

Abstract: Modern regenerative medicine and dentistry are in urgent need of mild methods for the degradation of calcium phosphate deposits, as well as the development of biodegradable composite materials based on polylactic acid and apatites. In this context, fundamental studies on the degradation of apatites in lactic acid are of paramount importance for optimizing the synthesis of biodegradable implants and developing caries prevention strategies. The aim of this study was to determine the thermodynamic and kinetic parameters of the interaction between hydroxyapatite (fluorapatite) and lactic acid, as well as to elucidate the underlying reaction mechanism. The degradation processes were investigated using thermodynamic modeling, direct potentiometry, and X-ray diffraction analysis. Based on the performed calculations, thermodynamic surfaces were constructed, and the critical acidity thresholds at which apatite dissolution becomes thermodynamically unfavorable were established: the maximum pH values were found to be 5,2 for hydroxyapatite and 4,5 for fluorapatite. Experimental results demonstrate that the maximum degradation rate is achieved in a strongly acidic medium, where the active protonated form of lactic acid predominates in the solution. It was revealed that the system reaches equilibrium rapidly due to a self-inhibition effect, which corresponds to crystals reaching a critical nanoscale size limit by the crystals. A reaction mechanism is proposed, involving the protonation of the phosphate groups within the crystal lattice followed by the chelation of the released Ca2+-ions by lactate anions, which effectively prevents kinetic inhibition of the process. The obtained data provide a solid foundation for developing methods for the controlled resorption of biodegradable implants and dental materials.

Keywords: hydroxyapatite, fluorapatite, lactic acid, resorption, thermodynamic modeling

  • Anastasiya A. Provorkina – Lecturer, Department of Inorganic Chemistry, Omsk State University named after F.M. Dostoevsky, ORCID: 0009-0005-7951-5924
  • Olga A. Golovanova – Dr. Sc., Professor, Head of the Department of Inorganic Chemistry, Omsk State University named after F.M. Dostoevsky, ORCID: 0000-0001-9995-5672

For citation:

Provorkina A.A., Golovanova O.A. Zakonomernosti degradatsii fosfatov kaltsiya v molochnoj kislote [Patterns of calcium phosphate degradation in lactic acid], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 908-916. DOI: 10.26456/pcascnn/2026.18.908. ⎘

Full article (in Russian): download PDF file

References:

1. da Silva D., Kaduri M., Poley M. et al. Biocompatibility, biodegradation and excretion of polylactic acid (PLA) in medical implants and theranostic systems, Chemical Engineering Journal, 2018, vol. 340, pp. 9-14. DOI: 10.1016/j.cej.2018.01.010.
2. Borkowski L., Przekora A., Belcarz A. et al. Fluorapatite ceramics for bone tissue regeneration: Synthesis, characterization and assessment of biomedical potential, Materials Science and Engineering, 2020, vol. 116, art. no. 111211, 10 p. DOI: 10.1016/j.msec.2020.111211.
3. Dorozhkin S.V. Dissolution mechanism of calcium apatites in acids: a review of literature, World Journal of Methodology, 2015, vol. 2, issue 1, pp. 1-17. DOI: 10.5662/wjm.v2.i1.1.
4. Avnimelech Y., Moreno E.C., Brown W.E. Solubility and surface properties of finely divided hydroxyapatite, Journal of Research of the National Bureau of Standards Section A: Physics and Chemistry, 1973, vol. 77A, issue 1, pp. 149-155. DOI: 10.6028/jres.077A.008.
5. McCann H.G. The solubility of fluorapatite and its relationship to that of fluorite, Archives of Oral Biology, 1968, vol. 13, issue 8, pp. 987-1001. DOI: 10.1016/0003-9969(68)90014-9.
6. Christoffersen J., Christoffersen M.R., Johansen T. Kinetics of growth and dissolution of fluorapatite, Journal of Crystal Growth, 1996, vol. 163, issue 3, pp. 295-303. DOI: 10.1016/0022-0248(95)00962-0. DOI: 10.1016/0022-0248(95)00962-0.
7. Chaïrat C., Oelkers E.H., Schott J., Lartigue J.E. Fluorapatite surface composition in aqueous solution deduced from potentiometric, electrokinetic, and solubility measurements, and spectroscopic observations, Geochimica et Cosmochimica Acta, 2017, vol. 71, issue 24, pp. 5888-5900. DOI: 10.1016/j.gca.2007.09.026.
8. Margolis H.C., Moreno E.C. Kinetics of hydroxyapatite dissolution in acetic, lactic, and phosphoric acid solutions, Calcified Tissue International, 1992, vol. 50, issue 2, pp. 137-143. DOI: 10.1007/BF00298791.
9. Tõnsuaadu K., Kallas J., Kuusik R. et al. A new perspective on fluorapatite dissolution in hydrochloric acid: thermodynamic calculations and experimental study, Inorganics, 2021, vol. 9, issue 8, art. no. 65, 11 p. DOI: 10.3390/inorganics9080065.
10. Sabirzyanov N.A., Bogdanova E.A., Khonina T.G. Sposob polucheniya suspenzii gidroksiapatita [A method of obtaining a suspension of hydroxyapatite]. Patent RF, no. 2406693, 2010. (In Russian).
11. Hochrein O., Zahn D. On the molecular mechanisms of the acid-induced dissociation of hydroxyapatite in water, Journal of Molecular Modeling, 2011, vol. 17, issue 6, pp. 1525-1528. DOI: 10.1007/s00894-010-0855-9.
12. Xie J., Zhang Q., Mao S. et al. Anisotropic crystal plane nature and wettability of fluorapatite, Applied Surface Science, 2019, vol. 493, pp. 294-307. DOI: 10.1016/j.apsusc.2019.06.195.
13. Zakharov N.A., Aliev A.D., Matveev V.V. et al. Synthesis and properties of hydroxyapatite – fluorapatite solid solutions, Journal of Advanced Materials and Technologies, 2023, vol. 8, issue 2, pp. 120-129. DOI: 10.17277/jamt.2023.02.pp.120-129.
14. Termicheskie konstanty veshchestv [Thermal constants of substances]. Available at: https://www.chem.msu.ru/cgi-bin/tkv.pl?show=welcome.html (accessed 07.06.2026). (In Russian).
15. Tang R., Wang L., Nancollas G.H. Size-effects in the dissolution of hydroxyapatite: an understanding of biological demineralization, Journal of Materials Chemistry, 2004, vol. 14, issue 14, pp. 2341-2346. DOI: 10.1039/b401097c.
16. Tavoni M., Dapporto M., Tampieri A., Sprio S. Bioactive calcium phosphate-based composites for bone regeneration, Journal of Composites Science, 2021, vol. 5, issue 9, art. no. 227, 27 p. DOI: 10.3390/jcs5090227.

Content |