Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Synthesis and physicochemical study of pectin-stabilized selenium nanoparticles

A.B. Golik, N.A. Rusev, A.V. Blinov, Y.A. Oblogin, A.V. Tatov, A.M. Serov, M.A. Pirogov

North-Caucasian Federal University

DOI: 10.26456/pcascnn/2026.18.612

Original article

Abstract: In this work, samples of selenium nanoparticles stabilized by citrus pectin were obtained by the method of chemical reduction of selenous acid by ascorbic acid in an aqueous medium, varying the concentrations of the precursor, stabilizer, and reducing agent according to the experimental design matrix. Computer quantum-chemical modeling of the interaction of a citrus pectin fragment consisting of three methylgalacturonic acid monomers with a selenium atom was performed using the QChem software package. It was found that the interaction is energetically favorable (the difference in total energy between citrus pectin and the molecular system of selenium with citrus pectin is ΔE > 2433 kcal/mol) and is chemically stable (chemical rigidity η ranges from 0,178 to 0,206 eV), and the most probable binding is through the hydroxyl group attached to C3 of the third A-bound methylgalacturonic acid residue (ΔE = 2433,586 kcal/mol, η = 0,206 eV). Photon correlation spectroscopy and electrophoretic light scattering methods were used to show that the average hydrodynamic diameter of the obtained particles varies from 193,70 to 1383,91 nm, and the ζ-potential ranges from -11,83 to +3,10 mV, depending on the ratio of the components; the smallest particle size and the most negative ζ-potential were achieved at the lowest concentrations of the precursor, stabilizer, and reducing agent. Using ultraviolet spectrophotometry, an absorption band with a maximum at 265 nm (the optical density is 0,8 r.u.), characteristic of nanosized selenium was detected, confirming the formation of nanoparticles. The study of the colloidal stability of the selected sample in the pH range of 1,81-11,98 showed a non-linear dependence of particle size on pH: maximum aggregation occurs in the slightly acidic region at ζ-potential values close to zero, while increasing the pH results in a more stable dispersion (ζ-potential around -20 mV) with smaller particle size.

Keywords: pectin-stabilized selenium nanoparticles, optimization of the synthesis method, stability at different pH levels, average hydrodynamic diameter, ζ potential

  • Alexey B. Golik – Senior Lecturer, Department of Functional Materials and Engineering Design, North-Caucasian Federal University, ORCID: 0000-0003-2580-9474
  • Nikita A. Rusev – Research Engineer, International Research Laboratory of Functional Materials and Food Systems, North-Caucasian Federal University, ORCID: 0009-0004-8503-1
  • Andrey V. Blinov – Ph. D., Associate Professor, Department of Functional Materials and Engineering Design, North-Caucasian Federal University, ORCID: 0000-0002-4701-8633
  • Yaroslav A. Oblogin – Laboratory Assistant, Department of Functional Materials and Engineering Design, North-Caucasian Federal University, ORCID: 0009-0003-5180-9045
  • Alexey V. Tatov – Laboratory Assistant, Department of Functional Materials and Engineering Design, North-Caucasian Federal University, ORCID: 0009-0003-8842-232X
  • Alexander M. Serov – Laboratory Assistant, Department of Functional Materials and Engineering Design, North-Caucasian Federal University, ORCID: 0009-0001-2929-4191
  • Maxim A. Pirogov – Assistant, Department of Functional Materials and Engineering Design, North-Caucasian Federal University, ORCID: 0000-0001-9217-6262

For citation:

Golik A.B., Rusev N.A., Blinov A.V., Oblogin Y.A., Tatov A.V., Serov A.M., Pirogov M.A. Sintez i fiziko-khimicheskoe issledovanie pektin-stabilizirovannykh nanochastits selena [Synthesis and physicochemical study of pectin-stabilized selenium nanoparticles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 612-623. DOI: 10.26456/pcascnn/2026.18.612. ⎘

Full article (in Russian): download PDF file

References:

1. Tretiyak L.N., Gerasimov E.M. Spetsifika vliyaniya selena na organizm cheloveka i zhivotnykh (primenitel'no k probleme sozdaniya selenosoderzhashchikh produktov pitaniya) [Specificity of selenium influence on human and animal's organism (with regard to the problem of creation of seleniumcontaining food stuff)], Vestnik Orenburgskogo gosudarstvennogo universiteta [Bulletin of Orenburg State University], 2007, no. 12 (79), pp. 136-145. (In Russian).
2. Spallholz J.E. On the nature of selenium toxicity and carcinostatic activity, Free Radical Biology and Medicine, 1994, vol. 17, issue 1, pp. 45-64. DOI: 10.1016/0891-5849(94)90007-8.
3. Hadrup N. Ravn-Haren G. Toxicity of repeated oral intake of organic selenium, inorganic selenium, and selenium nanoparticles: a review, Journal of Trace Elements in Medicine and Biology, 2023, vol. 79, art. no. 127235, 14 p. DOI: 10.1016/j.jtemb.2023.127235.
4. Tran P.A., Webster T.J. Selenium nanoparticles inhibit Staphylococcus aureus growth, International Journal of Nanomedicine, 2011, vol. 6, pp. 1553-1558. DOI: 10.2147/IJN.S21729.
5. Zhang J., Wang H., Yan X., Zhang L. Comparison of short-term toxicity between Nano-Se and selenite in mice, Life Sciences, 2005, vol. 76, issue 10, pp. 1099-1109. DOI: 10.1016/j.lfs.2004.08.015.
6. Wang H., Zhang J., Yu H. Elemental selenium at nano size possesses lower toxicity without compromising the fundamental effect on selenoenzymes: Comparison with selenomethionine in mice, Free Radical Biology and Medicine, 2007, vol. 42, issue 10, pp. 1524-1533. DOI: 10.1016/j.freeradbiomed.2007.02.013.
7. Wadhwani S.A., Shedbalkar U.U., Singh R., Chopade B.A. Biogenic selenium nanoparticles: current status and future prospects, Applied Microbiology and Biotechnology, 2016, vol. 100, issue 6, pp. 2555-2566. DOI: 10.1007/s00253-016-7300-7.
8.He Y., Chen S., Zhang Z. et al. Toxicity of selenium nanoparticles in male Sprague–Dawley rats at supranutritional and nonlethal levels, Life Sciences, 2014, vol. 115, issue 1-2, pp. 44-51. DOI: 10.1016/j.lfs.2014.08.023.
9. Skorinova K.D., Kuzmenko V.V., Vasilenko I.A. Perspektiva sozdaniya lekarstvennykh preparatov na osnove nanochastits selena (obzor) [The prospect of creating medicines based on selenium nanoparticles (review)], Razrabotka i registratsiya lekarstvennykh sredstv [Drug development & registration], 2020, vol. 9, no. 2, pp. 33-44. DOI: 10.33380/2305-2066-2020-9-2-33-44. (In Russian).
10. Ferro C., Florindo H.F., Santos H.A. Selenium nanoparticles for biomedical applications: from development and characterization to therapeutics, Advanced Healthcare Materials, 2021, vol. 10, issue 16, art. no. 2100598, 50 p. DOI: 10.1002/adhm.202100598.
11. Yunusov K.E., Sarymsakov A.A., Turakulov F.M. Synthesis and physicochemical properties of the nanocomposites based on sodium carboxymethyl cellulose and selenium nanoparticles, Polymer Science, Series B, 2022, vol. 64, issue 1, pp. С. 68-77. DOI: 10.31857/S2308113922010089.
12. Panov D.A., Katsev A.M., Omel'chenko A.V. Sintez i svoistva nanochastits selena v matritse prirodnykh polisakharidov [Synthesis and properties of selenium nanoparticles in natural polysaccharides matrix], Khimiya rastitel'nogo syr'ya [Chemistry of Plant Raw Materials], 2022, no. 1, pp. 81-91. DOI: 10.14258/jcprm.2022019275. (In Russian).
13. Chen Z., Shen Y., Xie A. et al. L-Cysteine-assisted controlled synthesis of selenium nanospheres and nanorods, Crystal Growth & Design, 2009, vol. 9, issue 3, pp. 1327-1333. DOI: 10.1021/cg800398b.
14. Torres S.K., Campos V.L., León C.G. et al. Biosynthesis of selenium nanoparticles by Pantoea agglomerans and their antioxidant activity, Journal of Nanoparticle Research, 2012, vol. 14, issue 11, art. no. 1236. DOI: 10.1007/s11051-012-1236-3.
15. Saifina D.F., Nikolaeva E.Yu., Tsepaeva O.V., Iskhakova G.G. Pektin: poluchenie, struktura i perspektivy primeneniya [Pectin: production, structure, and application prospects], Georesursy [Georesources], 2000, no. 2 (3), pp. 36-38. (In Russian).
16. Bisht N., Phalswal P., Khanna P.K. Selenium nanoparticles: A review on synthesis and biomedical applications, Materials Advances, 2022, vol. 3, issue 3, pp. 1415-1431. DOI: 10.1039/d1ma00639h.
17. Peng D., Zhang J., Liu Q., Taylor E.W. Size effect of elemental selenium nanoparticles (Nano-Se) at supranutritional levels on selenium accumulation and glutathione S-transferase activity, Journal of Inorganic Biochemistry, 2007, vol. 101, issue 10, pp. 1457-1463. DOI: 10.1016/j.jinorgbio.2007.06.021.
18. Blinov A., Nagdalian A., Serov A. et al. Selenium nanoparticles stabilized with Tween 80: Synthesis, characterization, and application in fortified milk and fermented dairy products, Colloids and Surfaces A: Physicochemical and Engineering Aspects, 2025, vol. 706, art. no. 1358202, 10 p. DOI: 10.1016/j.colsurfa.2024.135822.
19. Kopeikin V.V., Valueva S.V., Kipper A.I. et al. Synthesis of selenium nanoparticles in aqueous solutions of poly(vinylpyrrolidone) and morphological characteristics of the related nanocomposites, Polymer Science, Series A, 2003, vol. 45, issue 4, pp. 374-379.
20. IQmol Molecular Viewer. Available at: www.url: http://www.iqmol.org/ (accessed 12.06.2026).
21. Q-Chem 6.3 User’s Manual. Available at: https://manual.q-chem.com/6.3/ (accessed 12.06.2026).
22. Valueva S.V., Borovikova L.N. Effect of the type of biologically active stabilizers on the spectral and dimensional characteristics of selenium-containing hybrid nanosystems, Russian Journal of Physical Chemistry A, 2019, vol. 93, issue 1, pp. 129-134. DOI: 10.1134/S0036024419010308.
23. Rekhman Z.A., Pirogov M.A., Blinov A.V. et al. Issledovanie svoistv nanochastits selena, stabilizirovannykh polivinilpirrolidonom marki K-17 [Study of properties of selenium nanoparticles stabilized with K-17 polyvinyl pyrrolidone], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 934-942. DOI: 10.26456/pcascnn/2026.18.934 (In Russian).

Content |