Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Structure and properties of a novel hexagonal C108 clathrate

V.A. Greshnyakov1,2

1 Chelyabinsk State University
2 Immanuel Kant Baltic Federal University

DOI: 10.26456/pcascnn/2026.18.223

Original article

Abstract: The structure and properties of a new clathrate variety of carbon (C108) have been studied for the first time using density functional theory with a generalized gradient approximation. The new nanostructured phase has a hexagonal crystal lattice belonging to the P6m2 space group, with parameters a = 6,813 Å and c = 18,07 Å, which can be considered intermediate between the lattices of type II carbon clathrate and the hexagonal C40 clathrate. The structure of the C108 clathrate consists of fullerene-like blocks C20, C24, C26, and C28, due to which its density is 13,8% lower than that of diamond. Since the total energy of the new clathrate is only 0,10 eV/atom higher than that of diamond, the proposed phase should stably exist under normal conditions. The hexagonal C108 clathrate is expected to be a wide-bandgap semiconductor with high mechanical properties: a bulk modulus of 384 GPa, the Young’s modulus of ~880-890 GPa, and a Vickers hardness of 81 GPa. It has also been established that the structure of the C108 clathrate should be stable under strong hydrostatic compression at least up to 70 GPa. Identification of the new phase is possible using X-ray diffraction methods.

Keywords: nanostructured compounds, carbon clathrate, mechanical properties, stability, first-principles calculations

  • Vladimir A. Greshnyakov – Dr. Sc., Assistant Professor, Condensed Matter Physics Department, Chelyabinsk State University, Leading Researcher Immanuel Kant Baltic Federal University, ORCID: 0000-0002-2686-374X

For citation:

Greshnyakov V.A. Struktura i svojstva novogo geksagonalnogo klatrata C108 [Structure and properties of a novel hexagonal C108 clathrate], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 223-232. DOI: 10.26456/pcascnn/2026.18.223. ⎘

Full article (in Russian): download PDF file

References:

1. Belenkov E.A., Greshnyakov V.A. Classification schemes of carbon phases and nanostructures, New Carbon Materials, 2013, vol. 28, issue 4, pp. 273-283. DOI: 10.1016/S1872-5805(13)60081-5.
2. Bean J.J., Katiyar N.K., Forrest R.M. et al. Resolving Lonsdaleite's decade-long controversy: Atomistic insights into a metastable diamond polymorph, Diamond and Related Materials, 2025, vol. 157, art. no. 112405, 9 p. DOI: 10.1016/j.diamond.2025.112405.
3. Yu T., Zhu S. Hexagonal diamond formation mechanism: a review, Matter and Radiation at Extremes, 2026, vol. 11, issue 3, art. no. 033801, 12 p. DOI: 10.1063/5.0310909.
4. Belenkov E.A., Greshnyakov V.A. Structure, properties, and possible mechanisms of formation of diamond-like phases, Physics of the Solid State, 2016, vol. 58, issue 10, pp. 2145-2154. DOI: 10.1134/S1063783416100073.
5. Kou J., Zhou Y., Luo P., Gan L.-H. sp3-Hybridized superhard trigonal carbon allotropes: A first principle study, Computational Materials Science, 2021, vol. 190, art. no. 110269, 8 p. DOI: 10.1016/j.commatsci.2020.110269.
6. Gao Q., Ou L., Hu Z. Architecture design of novel carbon family: Polyhedra as building blocks, Carbon Trends, 2023, vol. 11, art. no. 100256, 8 p. DOI: 10.1016/j.cartre.2023.100256.
7. Wan T., Fan Q., Wei M. et al. Design and physical property study of seven novel carbon allotropes by random methods combined group and graph theories, Computational Materials Science, 2024, vol. 244, art. no. 113179, 14 p. DOI: 10.1016/j.commatsci.2024.113179.
8. Belenkov E.A., Greshnyakov V.A. Structural varieties of polytypes, Physics of the Solid State, 2017, vol. 59, issue 10, pp. 1926-1933. DOI: 10.1134/S1063783417100055.
9. Zhu J., Xu Ke, Zhang Z. et al. Carbon clathrates as strong lightweight structures, International Journal of Mechanical Sciences, 2021, vol. 202-203, art. no. 106509, 9 p. DOI: 10.1016/j.ijmecsci.2021.106509.
10. Greshnyakov V.A., Pavlik V.V., Belenkov M.E. et al. Carbon clathrates C24, C28 and CA6: Structure formation and properties, Letters on Materials, 2026, vol. 16, issue 1, pp. 23-29. DOI: 10.48612/letters/2026-1-23-29.
11. Li S., Zhang J., Wang J. et al. Dense as diamond: Pn-C10, a superhard sp3 carbon allotrope, Applied Physics Letters, 2021, vol. 118, issue 1, art. no. 012107, 6 p. DOI: 10.1063/5.0032528.
12. Li Z., Hu M., Ma M. et al. Superhard superstrong carbon clathrate, Carbon, 2016, vol. 105, pp. 151-155. DOI: 10.1016/j.carbon.2016.04.038.
13. Liu H., Xing M., Fan Q. Four superhard tetragonal carbon allotropes: First-principles calculations, Diamond and Related Materials, 2023, vol. 135, art. no. 109854, 9 p. DOI: 10.1016/j.diamond.2023.109854.
14. Baimova J.A. An overview of mechanical properties of diamond-like phases under tension, Nanomaterials, 2024, vol. 14, issue 2, art. no. 129, 16 p. DOI: 10.3390/nano14020129.
15. Giannozzi P., Andreussi O., Brumme T. et al. Advanced capabilities for materials modelling with Quantum ESPRESSO, Journal of Physics: Condensed Matter, 2017, vol. 29, no. 46, art. no. 465901, 31 p. DOI: 10.1088/1361-648X/aa8f79.
16. Perdew J.P., Burke K., Ernzerhof M. Generalized gradient approximation made simple, Physical Review Letters, 1996, vol. 77, issue 18, pp. 3865-3868. DOI: 10.1103/physrevlett.77.3865.
17. Belenkov E.A., Greshnyakov V.A. Modeling of phase transitions of graphites to diamond-like phases, Physics of the Solid State, 2018, vol. 60, issue 7, pp. 1294-1302. DOI: 10.1134/S1063783418070065.
18. Greshnyakov V.A., Belenkov E.A. Formirovanie novogo almazopodobnogo bisloya na osnove grafena 5-7 [Formation of a novel diamond-like bilayer based on 5-7 graphene], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2021, issue 13, pp. 76-84. DOI: 10.26456/pcascnn/2021.13.076. (In Russian).
19. Umanskii Ya.S., Skakov Yu.A., Ivanov A.N., Rastorguev L.N. Kristallografiya, rentgenografiya i elektronnaya mikroskopiya. Moscow, Metallurgiya Publ., 1982, 632 p. (In Russian).
20. Greshnyakov V.A., Belenkov E.A. Technique for calculating the bulk modulus, Russian Physics Journal, 2014, vol. 57, issue 6, pp. 731-737. DOI: 10.1007/s11182-014-0297-4.
21. Gao F., He J., Wu E. et al. Hardness of covalent crystals, Phys. Rev. Lett., 2003, vol. 91, issue 1, art. no. 015502, 4 p. DOI: 10.1103/PhysRevLett.91.015502.
22. Stokes H.T., Hatch D.M. Program for identifying the space group symmetry of a crystal, Journal of Applied Crystallography, 2005, vol. 38, issue 1, pp. 237-238. DOI: 10.1107/s0021889804031528.
23. Greshnyakov V.A., Belenkov E.A. Calculation of the physicochemical characteristics of a new orthorhombic form of diamond, Inorganic Materials, 2018, vol. 54, issue 2, pp. 111-116. DOI: 10.1134/S0020168518020061.
24. Wang J.-T., Chen C., Wang D.-S. et al. Phase stability of carbon clathrates at high pressure, Journal of Applied Physics, 2010, vol. 107, issue 6, art. no. 063507, 4 p. DOI: 10.1063/1.3359682.
25. Vollondat R., Roques S., Chevalier C. et al. Synthesis and characterization of silicon clathrates of type I Na8Si46 and type II NaxSi136 by thermal decomposition, Journal of Alloys and Compounds, 2022, vol. 903, art. no. 163967, 7 p. DOI: 10.1016/j.jallcom.2022.163967.