Study of the possibility of obtaining porous bioceramics based on calcium phosphates by the method of burnout additives
S.A. Bibanaeva1, V.M. Skachkov1, E.A. Bogdanova2
1 Institute of Solid State Chemistry of the Ural Branch of RAS
2 JSC «Giredmet»
DOI: 10.26456/pcascnn/2026.18.550
Original article
Abstract: The article discusses possibility of producing porous calcium phosphate-based bioceramics using a burnout additive method. Nanostructured precipitated hydroxyapatite (mechanically activated hydroxyapatite, titanium dioxide-reinforced hydroxyapatite, and fluorinated hydroxyapatite) and tricalcium phosphate were used as a bioactive matrix for producing porous ceramics. Natural and commercially available starch and gelatin were used as some pore-forming agents. Materials with a three-dimensional porous structure were obtained by mechanochemical synthesis of the bioactive matrix with a calculated amount of a pore-forming agent, followed by high-temperature processing. The synthesized samples were certified using modern physicochemical analytical methods. The influence of the qualitative and quantitative composition of the material on the sintering processes, structure, and strength characteristics of the studied samples is demonstrated. Experiments have shown that gelatin is the most promising pore-forming agent for the studied systems. It has been shown that to achieve a balance between porosity and strength, the hydroxyapatite content in the sample should not exceed 10% by weight. Despite differences in microhardness, the tensile strength of porous ceramics based on hydroxyapatite obtained using the burnout method meets the strength requirements for implant materials, opening up opportunities for further research aimed at implementing them in medical practice.
Keywords: calcium phosphates, hydroxyapatite, biomaterials, porous ceramics, synthesis, pore-forming agents, starch, gelatin, burnout method
- Svetlana A. Bibanaeva – Researcher, Laboratory of heterogeneous processes chemistry, Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0002-1181-8735
- Vladimir M. Skachkov – Ph. D., Senior Researcher, Laboratory of heterogeneous processes chemistry, Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0003-2551-3235
- Ekaterina A. Bogdanova – Ph. D., Leading Researcher, Laboratory of materials and technologies of the fourth energy transition, JSC «Giredmet», ORCID: 0000-0002-6947-5368
For citation:
Bibanaeva S.A., Skachkov V.M., Bogdanova E.A. Issledovanie vozmozhnosti polucheniya poristoj biokeramiki na osnove fosfatov kaltsiya metodom vygorayushchikh dobavok [Study of the possibility of obtaining porous bioceramics based on calcium phosphates by the method of burnout additives], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 550-566. DOI: 10.26456/pcascnn/2026.18.550. ⎘
Full article (in Russian): download PDF file
References:
1. Mondal S., Park S., Choi J., et al. Hydroxyapatite: a journey from biomaterials to advanced functional materials, Advances in Colloid and Interface Science, 2023, vol. 321, art. no. 103013, 27 p. DOI: 10.1016/j.cis.2023.103013.
2. Barinov S.M., Komlev V.S. Biokeramika na osnove fosfatov kal'tsiya [Calcium phosphate bioceramics]. Moscow, Nauka Publ., 2006, 204 p. (In Russian).
3. Iwamoto T., Hieda Y., Kogai Y. Physicochemical characterization and cell behavior of porous hydroxyapatite ceramics doped with Ag ions: Fluorescence quenching in fluorescence-labeled cells, Applied Materials Today, 2024. – vol. 36, art. no. 102029, 6 p. DOI: 10.1016/j.apmt.2023.102029.
4 Hashimoto K., Ohtsuki N., Tsuchiya K., et al. Fabricating ordered porous β-tricalcium phosphate ceramics having specific structure via the replica method using 3D-CAD-designed polymeric templates, Open Ceramics, 2026, vol. 25, art. no. 100928, 11 p. DOI: 10.1016/j.oceram.2026.100928.
5. Hutmacher D.W. Scaffolds in tissue engineering bone and cartilage, Biomaterials, 2000, vol. 21, issue 24, pp. 2529-2543. DOI: 10.1016/S0142-9612(00)00121-6.
6. Karageorgiou V., Kaplan D. Porosity of 3D biomaterial scaffolds and osteogenesis, Biomaterials, 2005, vol. 26, issue 27, pp. 5474-5491. DOI: 10.1016/j.biomaterials.2005.02.002.
7. O’Brien F.J. Biomaterials & scaffolds for tissue engineering, Materials Today, 2011, vol. 14, issue 3, pp. 85-95. DOI: 10.1016/S1369-7021(11)70058-X.
8. Hollister S.J. Porous scaffold design for tissue engineering, Nature Materials, 2005, vol. 4, issue 7, pp. 518-524. DOI: 10.1038/nmat1421.
9. Kasten P., Beyen I., Niemeyer P., et al. Porosity and pore size of β-tricalcium phosphate scaffold can influence protein production and osteogenic differentiation of human mesenchymal stem cells: An in vitro and in vivo study, Acta Biomaterials, 2008, vol. 4, issue 6, pp. 1904-1915. DOI: 10.1016/j.actbio.2008.05.017.
10. Tripathi G., Basu B. A porous hydroxyapatite scaffold for bone tissue engineering: physico-mechanical and biological evaluations, Ceramics International, 2012, vol. 38, issue 1, pp. 341-349. DOI: 10.1016/j.ceramint.2011.07.012.
11. Nandi S.K., Kundu B., Mukherjee J., et al. Converted marine coral hydroxyapatite implants with growth factors: In vivo bone regeneration, Materials Science and Engineering: C, 2015, vol. 49, pp. 816-823. DOI: 10.1016/j.msec.2015.01.078.
12. de Oliveira P.T., Nanci A. Nanotexturing of titanium-based surfaces upregulates expression of bone sialoprotein and osteopontin by cultured osteogenic cells, Biomaterials, 2004, vol. 25, issue 3, pp. 403-413. DOI: 10.1016/S0142-9612(03)00539-8.
13. Bogdanova E.A., Skachkov V.М., Medyankina I.S. et al. Formation of nanodimensional structures in precipitated hydroxyapatite by fluorine substitution, SN Applied Sciences, 2020, vol. 2, issue 9, art. no. 1565, 7 p. DOI: 10.1007/s42452-020-03388-5.
14. Bogdanova E.A., Skachkov V.M. Biomeditsinskiy material na osnove gidroksiapatita i sposob yego polucheniya [Biomedical material based on hydroxyapatite and method for its production]. Patent RF, no. 2782925, 2022. (In Russian).
15. Iwamoto T., Kogai Y. Influence of titanium ion doping on structural changes in porous hydroxyapatite ceramics, Solid State Sciences, 2023, vol. 142, art. no. 107222, 7 p. DOI: 10.1016/j.solidstatesciences.2023.107222.
16. Fedotov A.S., D.YU. Grachev, Kapustin R.D. Osnovnye svojstva, sposoby polucheniya i napravleniya primeneniya poristykh keramicheskikh materialov [Basic properties, methods of production and areas of application of porous ceramic materials], Neftekhimiya [Petroleum Chemistry], 2024, vol. 64, no. 4, pp. 317-360. DOI: 10.31857/S0028242124040031. (In Russian).
17. Albano М.Р., Genova L.A., Garrido L.В. et al. Processing of porous yttria-stabilized zirconia by tape-casting, Ceramics International, 2008, vol. 34, issue 8, pp. 1983-1988. DOI: 10.1016/j.ceramint.2007.07.028.
18. Chen Q., Zou B., Wang X. et al. SLA-3d printed building and characteristics of GelMA/HAP biomaterials with gradient porous structure, Journal of the Mechanical Behavior of Biomedical Materials, 2024, vol. 155, art. no. 106553, 12 p. DOI: 10.1016/j.jmbbm.2024.106553.
19. GOST R 23999‑80. Kal'tsiya fosfat kormovoj. Tekhnicheskie usloviya [Fodder calcium phosphate. Specifications]. Moscow, Standartov Publ., 1980, 24 p. (In Russian).
20. Sabirzyanov N.A., Bogdanova E.A., Khonina T.G. Sposob polucheniya suspenzii gidroksiapatita [A method of obtaining a suspension of hydroxyapatite]. Patent RF, no. 2406693, 2010. (In Russian).
21. Sabirzyanov N.A., Bogdanova E.A., Skachkov V.M. Sposob polucheniya suspenzii apatita [Method of preparing apatite suspension]. Patent RF, no. 2652193, 2018. (In Russian).
22. Bogdanova E.A., Nefedova K.V., Skachkov V.M. Sposob izgotovleniya granul iz bioaktivnogo materiala na osnove ftoapatita i gidroksiapatita [Method for manufacturing granules from bioactive material based on hydroxyapatite or fluorapatite]. Patent RF, no. 2753529, 2021. (In Russian).
23. GOST R 53876-2010. Krakhmal kartofel'nyj. Tekhnicheskie usloviya [Potato starch. General specifications]. Moscow, Standartinform Publ., 2019, 11 p. (In Russian).
24. GOST 11293-89. Zhelatin. Tekhnicheskie usloviya [Gelatin. Specifications: State Standard 11293-89]. Moscow, IPK Standartov Publ., 1989, 24 p. (in Russian).
25. Powder Diffraction File JCPDS-ICDD PDF-2 (Set 1-47). (Release, 2016). – Режим доступа: www.url: https://www.icdd.com/pdf-2/. – 15.05.2026.
26. Schmidt-Nielsen K. Scaling: why is animal size so important?. Cambridge, Cambridge University Press, 1984, 241 p.
27. Currey J.D. Mechanical properties of vertebrate hard tissues, Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine, 1998, vol. 212, issue 6, pp. 399-411. DOI: 10.1243/0954411981534178.
28. Avrunin A.S., Melnikov B.E., Л.К. Parshin L.K. et al. O fizicheskoj prirode zhestkosti i prochnosti kostnoj tkani [On the physical nature of bone tissue rigidity and strength], Nauchno-tekhnicheskie vedomosti SPbGPU. Nauka i obrazovanie [Scientific and Technical Bulletin of SPbSPU. Science and Education], 2010, no. 31 (106), pp. 205-210. (In Russian). 27. Zaytsev D.V, Grigoryev S.S., Antonova O.V. et al. Deformatsiya i razrushenie chelovecheskogo dentina [Deformation and destruction of human dentin], Deformatsiya i razrushenie materialov [Deformation and destruction of materials], 2011, no. 6, pp. 37-44. (In Russian). 28. Zaytsev D.V., Panfilov P.Е. Prochnostnye svojstva dentina i emali zubov cheloveka pri odnoosnom szhatii [Strength properties of human dentin and enamel under uniaxial compression], Vestnik Tambovskogo universiteta. Seriya Estestvennye nauki [Tambov University Bulletin. Natural Sciences Series], 2016, vol. 21, issue 3, pp. 802-804. DOI:10.20310/1810-0198-2016-21-3-802-804. (In Russian).
29 Petrakova N.V., Barinov S.M., Evstratov E.V. et al. Uplotnenie nanoporoshkov gidroksiapatita s primeneniem gidrostaticheskogo pressovaniya [Compaction of hydroxyapatite nanopowders using hydrostatic pressing], Materialovedenie [Materials Science], 2016, no. 11, pp. 35-41. (In Russian).
30. Bakunova N.V., Barinov S.M., Ievlev V.M. et al. Vliyanie termoobrabotki na spekanie i prochnost' keramiki iz nanoporoshkov gidroksiapatita [Effect of heat treatment on sintering and strength of ceramics made of hydroxyapatite nanopowders], Materialovedenie [Materials Science], 2010, no. 12, pp. 11-15. (In Russian).
31. Safronova T.V., Shekhirev M.A., Putlyaev V.I., Tret'yakov Yu.D. Hydroxyapatite-based ceramic materials prepared using solutions of different concentrations, Inorganic Materials, 2007, vol. 43, issue 8, pp. 901-909. DOI: 10.1134/S0020168507080158.