Magnetic nanofluids in tribology: achievements, challenges, and future research directions
A.N. Bolotov, O.O. Novikova
Tver State Technical University
DOI: 10.26456/pcascnn/2026.18.575
Review
Abstract: This article presents a systematic review of current research on magnetic lubricating nanofluids (ferrofluids) as a class of intelligent tribological media whose properties are controlled by an external magnetic field. The aim of the work is to summarize and critically analyze scientific concepts regarding the colloidal structure, synthesis methods, tribological characteristics, and engineering applications of such fluids. The classification of magnetic lubricants, the historical evolution of approaches (including studies from 1988–1991 that established the magnetotribological effect and the role of structural components), and current trends are discussed. The mechanisms of colloidal stabilization, the influence of Fe3O4 nanoparticle size and concentration, the magnetoviscous effect, and field-induced structure formation are analyzed in detail. It is shown that an optimal particle concentration (approximately 5 wt.%) reduces wear by up to 90%, while exceeding this concentration leads to abrasive wear. Four main mechanisms for reducing friction and wear are identified: rolling bearing, tribochemical film formation, self-healing of microcracks, and magnetic removal of wear debris. It was established that the effectiveness of a magnetic field depends significantly on its orientation and gradient, as well as the material of the friction pair. The main areas of application (magnetic seals, bearings, controlled tribosystems, heat transfer), limitations (aggregate instability, particle abrasion, scaling), and development prospects, including active feedback systems and hybrid compositions, are discussed. It is concluded that the main value of magnetic lubricating nanofluids lies in their ability not only to simply lubricate but also to control lubrication, opening up new operating principles for friction units in precision, vacuum, and microengineering.
Keywords: magnetic lubricating nanofluids, ferrofluids, tribology, Fe3O4 nanoparticles, magnetically viscous effect, boundary lubrication, wear, magnetic field, smart lubricants
- Alexander N. Bolotov – Dr. Sc., Professor, Head of the Applied Physics Department, Tver State Technical University, ORCID: 0000-0003-4054-5550
- Olga O. Novikova – Ph. D., Full Docent, Applied Physics Department, Tver State Technical University, ORCID: 0000-0003-4133-3541
For citation:
Bolotov A.N., Novikova O.O. Magnitnye nanozhidkosti v tribologii: dostizheniya, problemy i napravleniya dalnejshikh issledovanij [Magnetic nanofluids in tribology: achievements, challenges, and future research directions], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 575-593. DOI: 10.26456/pcascnn/2026.18.575. ⎘
Full article (in Russian): download PDF file
References:
1. Säynätjoki M., Holmberg K. Magnetic fluids in sealing and lubrication: a state of the art review, Lubrication Science, 1993, vol. 10, issue 2, pp. 119-132. DOI: 10.1002/jsl.3000100203.
2. Li D., Li Y., Li Z., Wang Y. Theory analyses and applications of magnetic fluids in sealing, Friction, 2023, vol. 11, issue 10, pp. 1771-1793. DOI: 10.1007/s40544-022-0676-8.
3. Sun L., Zhang Y., Cui X. et al. Magnetic lubricants: preparation, physical mechanism, and application, Friction, 2025, vol. 13, issue 7, art. no. 9441010, 29 p. DOI: 10.26599/FRICT.2025.9441010.
4. Orlov D.V., Mikhalev Yu.O., Myshkin N.K., Podgorkov V.V., Sizov A.P. Magnitnyye zhidkosti v mashinostroyenii [Magnetic fluids in mechanical engineering]. Moscow, Mashinostroyeniye Publ., 1993, 272 p. (In Russian).
5. Bolotov A.N., Burdo G.B. Germetizatsiya s pomoshch'yu magnitnykh zhidkostey [Sealing with magnetic fluids], Vestnik Tverskogo gosudarstvennogo tekhnicheskogo universiteta. Seriya: Tekhnicheskie nauki [Bulletin of the Tver State Technical University. Series: Engineering sciences], 2023, vol. 3, issue 19, pp. 25-32. DOI: 10.46573/2658-5030-2023-3-25-32. (In Russian).
6. Bolotov A.N., Novikova O.O., Ratkevich Ye.A. Sovremennyye issledovaniya magnitnykh smazochnykh materialov [Modern research on magnetic lubricants], Vestnik Tverskogo gosudarstvennogo tekhnicheskogo universiteta. Seriya: Tekhnicheskie nauki [Bulletin of the Tver State Technical University. Series: Engineering sciences], 2026, vol. 1, issue 29, pp. 5-14. DOI: 10.46573/2658-5030-2026-1-5-14. (In Russian).
7. Bolotov A.N., Lochagin N.V., Mikhalev Yu.O. Rol' magnitnogo polya pri trenii poverkhnostey, smazyvayemykh magnitnym maslom [Role of magnetic field in friction of surfaces lubricated by magnetic oil], Treniye i iznos [Friction and wear], 1988, vol. 9, issue 5, pp. 870-878. (In Russian).
8. Wang X., Liu H., Zhao Q., Wang X., Lou W. Viscosity variations and tribological performances of oleylamine-modified Fe₃O₄ nanoparticles as mineral oil additives, Lubricants, 2023, vol. 11, issue 3, art. № 149? 13 p. DOI: 10.3390/lubricants11030149.
9. Zhang Q., Yu X., Xu X. et al. A review of research on the effect of electromagnetic field on friction and wear, Lubricants, 2025, vol. 13, issue 10, art. no. 454, 18 p. DOI: 10.3390/lubricants13100454.
10. Odenbach S. Magnetic hybrid-materials: multi-scale modelling, synthesis, and applications. Berlin, Boston, De Gruyter, 2021, XXX+781 p. DOI: 10.1515/9783110569636.
11. Bolotov A.N. Tribotekhnika magnitopassivnykh i magnitozhidkostnykh podshipnikovykh opor skol'zheniya: [Tribotechnics of magneto-passive and magnetic-fluid sliding bearing assemblies]. Dr. eng. sci: 05.02.04. Moscow: IMASH RAN Publ., 1993, 555 p. (In Russian).
12. Bolotov A.N., Sozonov K.K., Orlov D.V. On the role of structural components of magnetic oil in the boundary lubrication conditions, Journal of Friction and Wear, 1991, vol. 12, issue 5, pp. 824-831.
13. Bolotov A.N., Novikov V.V., Novikova O.O. Studying tribotechnical properties of nanostructured lubricating oils with various dispersive media, Journal of Friction and Wear, 2017, vol. 38, issue 2, pp. 121-125.
14. Berkovsky B.M., Medvedev V.F., Krakov M.S. Magnetic Fluids: Engineering Applications. Oxford, Oxford University Press, 1993, 243 p.
15. Rosensweig R.E. Ferrohydrodynamics. Cambridge, Cambridge University Press, 1985, 344 p.
16. Bolotov A.N., Novikova O.O. Magnitnye svojstva magnitnykh nanodispersnykh smazochnykh masel [Magnetic properties of the magnetic nanodispersed lubricant oils], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2019, issue 11, pp. 564-573. DOI: 10.26456/pcascnn/2019.11.564. (In Russian).
17. Bolotov A.N., Novikova O.O. Smazochnye svojstva magnitnykh nanozhidkostej na osnove efirov karbonovykh kislot [Lubrication properties of magnetic nanoliquids based on carboxylic acids], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2019, issue 11, pp. 555-563. DOI: 10.26456/pcascnn/2019.11.555. (In Russian).
18. Bolotov A.N., Novikov V.V., Novikova O.O. Lubricating oils obtained via modifying magnetic nanofluids, Inorganic Materials: Applied Research, 2020, vol. 11, issue 4, pp. 865-871. DOI: 10.1134/S2075113320040073.
19 Bolotov A.N., Afanasiyeva L.Ye., Meshkov V.V. Smazochnyye svoystva nanodispersnykh magnitnykh masel na osnove netraditsionnykh tekhnicheskikh zhidkostey [Lubricant properties of nanodisperse magnetic oils based on novel technical liquids], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 679-691. DOI: 10.26456/pcascnn/2023.15.679. (In Russian).
20. Bolotov A.N., Novikova O.O. Eksperimental'noye issledovaniye tekuchesti nanostrukturirovannoy magnitnoy zhidkosti v sil'nom magnitnom pole [Experimental study of the fluidity of nanostructured magnetic fluid in a strong magnetic field], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 692-700. DOI: 10.26456/pcascnn/2023.15.692. (In Russian).
21. Sahoo R., Ussa-Aldana P., Lancon D., Rondelez F., Morillas J.R., Hidalgo-Alvarez R., de Vicente J. Design of smart lubricants using the inverse ferrofluid approach, Tribology International, 2022, vol. 166, art. no. 107346, 12 p. DOI: 10.1016/j.triboint.2021.107346.
22. Li D., Li R., Lee C. Effect of ferromagnetic metal base on friction and wear of 3D-printed aluminum alloy surface under magnetorheological fluid action, Lubricants, 2023, vol. 11, issue 7, art. no. 273, 20 p. DOI: 10.3390/lubricants11070273.