Features of the defect structure of LiNbO3:Tb single-crystal plates with a post-threshold concentration of terbium ions
L.A. Bobreva1,2, N.V. Sidorov1, A.Yu. Pyatyshev3, M.N. Palatnikov1
1 Tananaev Institute of Chemistry – Subdivision of the Federal Research Centre «Kola Science Centre of the Russian Academy of Sciences»
2 Murmansk Arctic University
3 P.N. Lebedev Physical Institute of the RAS
DOI: 10.26456/pcascnn/2026.18.567
Original article
Abstract: A comparative analysis of the defect structure of Z-oriented LiNbO3:Tb (2,25 wt.%) and LiNbO3:Tb (2,9 wt.%) single-crystal plates was performed using infrared absorption spectroscopy in the region of OH⁻-group stretching vibrations. It was found that the complex multicomponent profile of the spectral structure in the 3000-4000 cm-1 range is formed not only by local vibrations of hydroxyl groups near various lattice defects, but also due to the superposition of weak electronic f-f transitions of Tb3+ ions, which become allowed under the action of the crystal field. By decomposing the spectra, absorption bands corresponding to various defects were identified: absorption bands near 3466 cm-1 are associated with a violation of stoichiometry, and absorption bands in the 3490-3600 cm-1 range with the mechanism of dopant incorporation. It was shown that the sample with a lower terbium content (2,25 wt.%) is characterized by a higher volume concentration of OH⁻ groups, compared to the sample with a terbium content of 2,9 wt.%. This effect is associated with a change in stoichiometry and the formation of two types of complex defects: (VLi–)-OH and 5(TbLi2+)-2(VNb5-)-OH. The obtained results allow us to clarify the mechanisms of defect formation and can serve as a basis for optimizing the technological modes for producing crystals intended for the creation of nonlinear optical elements with controlled domain structures.
Keywords: lithium niobate, terbium, infrared absorption spectrum, electronic transitions, OH⁻ groups, complex defects
- Lyubov A. Bobreva – Ph. D., Researcher, Vibrational Spectroscopy Sector of the Electronic Engineering Materials Laboratory, Tananaev Institute of Chemistry – Subdivision of the Federal Research Centre «Kola Science Centre of the Russian Academy of Sciences», Assistant Professor, Department of Physics, Biology and Engineering Technologies Murmansk Arctic University, ORCID: 0000-0001-5367-295X
- Nikolay V. Sidorov – Dr. Sc., Professor, Chief Researcher and Head of Vibrational Spectroscopy Sector of the Electronic Engineering Materials Laboratory, Tananaev Institute of Chemistry – Subdivision of the Federal Research Centre «Kola Science Centre of the Russian Academy of Sciences», ORCID: 0000-0003-1075-7421
- Alexander Yu. Pyatyshev – Ph. D., Senior Researcher, Raman laboratories, P.N. Lebedev Physical Institute of the RAS, ORCID: 0000-0001-6663-9737
- Mikhail N. Palatnikov – Dr. Sc., Chief Researcher and Head of the Electronic Engineering Materials Laboratory, Tananaev Institute of Chemistry – Subdivision of the Federal Research Centre «Kola Science Centre of the Russian Academy of Sciences», ORCID: 0000-0001-9686-0563
For citation:
Bobreva L.A., Sidorov N.V., Pyatyshev A.Yu., Palatnikov M.N. Osobennosti defektnoj struktury monokristallicheskikh plastin LiNbO3:Tb s posleporogovoj kontsentratsiej ionov terbiya [Features of the defect structure of LiNbO3:Tb single-crystal plates with a post-threshold concentration of terbium ions], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 567-574. DOI: 10.26456/pcascnn/2026.18.567. ⎘
Full article (in Russian): download PDF file
References:
1. Jüstel T., Nikol H., Ronda C. New developments in the field of luminescent materials for lighting and displays, Angewandte Chemie International Edition, 1998, vol. 37, issue 22, pp. 3084-3103. DOI: 10.1002/(SICI)1521-3773(19981204)37:22<3084::AID-ANIE3084>3.0.CO;2-W.
2. Lyu T., Dorenbos P., Wei Z. Designing LiTaO3:Ln3+, Eu3+ (Ln = Tb or Pr) perovskite dosimeter with excellent charge carrier storage capacity and stability for anti-counterfeiting and flexible X-ray imaging, Chemical Engineering Journal, 2023, vol. 461, art. no. 141685, 15 p. DOI: 10.1016/j.cej.2023.141685.
3. Lisiecki R., Macalik B., Kowalski R. et al. Effect of temperature on luminescence of LiNbO3 crystals single-doped with Sm3+, Tb3+, or Dy3+ ions, Crystals, 2020, vol. 10, issue. 11, art. no. 1034, 15 p. DOI: 10.3390/cryst10111034.
4. Long S., Liu Z., Wang B. Manometry strategy based on excitation spectral shift induced by pressure-controlled intervalence charge transfer in Tb3+:LiTaO3, Ceramics International, 2025, vol. 51, issue 13, pp. 17912-17918. DOI: 10.1016/j.ceramint.2025.01.563.
5. Palatnikov M., Sidorov N., Kadetova A. et al. Growth and concentration dependences of properties of LiNbO3:Tb crystals grown in a single technological cycle, Optical Materials, 2021, vol. 122, part A, art. no. 111755, 9 p. DOI: 10.1016/j.optmat.2021.111755.
6. Palatnikov M.N., Sidorov N.V., Palatnikova O.V., Biryukova I.V. Defektnaja struktura kristallov niobata litija odinarnogo i dvojnogo legirovanija [Defect structure of single and double doped lithium niobate crystals]. Moscow, RAS, Publ., 2024, 332 p. (In Russian).
7. Slautin B. N., Zhu H., Shur V.Ya. Submicron periodical poling in Z-cut lithium niobate thin films, Ferroelectrics, 2021, vol. 576, issue 1, pp. 119-128. DOI: 10.1080/00150193.2021.1888270.
8. Savelyev E., Akhmatkhanov A., Tronche H. et al. Kinetics of the domain structure in uniform electric field in LiNbO3 with surface layer modified by soft proton exchange, Physica status solidi (RRL)–Rapid Research Letters, 2024, vol. 18, issue 4, art. no. 2300420, 6 p. DOI: 10.1002/pssr.202300420.
9. Klauer S., Wöhlecke M., Kapphan S. Influence of the H-D isotopic substitution on the protonic conductivity in LiNbO3 crystal, Physical Review B, 1992, vol. 45, issue 6, pp. 2786-2799. DOI: 10.1103/physrevb.45.2786.
10. Lengyel K., Péter Á., Kovács L. et al. Growth, defect structure, and THz application of stoichiometric lithium niobate, Applied Physics Reviews, 2015, vol. 2, issue 4, pp. 040601-1-040601-28. DOI: 10.1063/1.4929917.
11. Cabrera J.M., Olivares J., Carrascosa M. et al. Hydrogen in lithium niobate, Advances in Physics, 1996, vol. 45, issue 5, pp. 349-392. DOI: 10.1080/00018739600101517.
12. Lee S.M., Shur J.W., Shin T I. et al. Characteristic investigations of stoichiometric LiNbO3 single crystal fiber co-doped with Tb and Mn, Materials Science Forum, 2004, vol. 449-452, pp. 985-988. DOI: 10.4028/www.scientific.net/MSF.449-452.985.
13. Garcı́a Solé J., Bausá L. E., Jaque D. et al. Rare earth and transition metal ion centers in LiNbO3, Spectrochimica Acta Part A: Molecular and Biomolecular Spectroscopy, 1998, vol. 54, issue 11, pp. 1571-1581. DOI: 10.1016/s1386-1425(98)00084.