Dependence of the interfacial energy of molybdenum faces at the boundary with organic liquids on the dielectric constant
A.M. Apekov1, I.G. Shebzukhova2, L.A. Khamukova1
1 North-Caucasus Center for Mathematical Research, North-Caucasus Federal University
2 Kabardino-Balkarian State University named after H.M. Berbekov
DOI: 10.26456/pcascnn/2026.18.332
Short communication
Abstract: The study of the interfacial energy of molybdenum at the interface with organic liquids is of considerable interest for the development of modern technologies in energy, catalysis, materials science, and biomedicine. Molybdenum, having high refractoriness, mechanical strength, and pronounced catalytic activity, is widely used in functional materials, including metal-organic skeleton structures, composites, and heterogeneous catalysts. Understanding energy characteristics at the metal-organic interface is critically important for optimizing the processes of adsorption, wetting, formation of strong interfacial contacts and control of the reactivity of active centers. In this work, calculations of the interfacial energy of molybdenum at the boundary of crystallographic faces with nonpolar organic liquids are performed using the electron statistical method. The dispersion interaction of Wigner–Seitz cells, the oscillation of the electron density in the transition layer, and the polarization of surface metal ions and organic liquid molecules in the field of a semi-infinite metal are taken into account. The dependences of the interfacial energy and corrections on the orientation of the molybdenum crystal lattice and the dielectric constant of an organic liquid are established. It is shown that the dispersion and oscillation corrections increase the interphase energy, while the polarization correction reduces it. The face (110) has the highest value of the interphase energy, and the face (111) has the lowest value of it.
Keywords: molybdenum, interfacial energy, polarization correction, dispersion correction, electron statistical method, nonpolar organic liquid
- Aslan M. Apekov – Ph. D., Deputy Director, North-Caucasus Center for Mathematical Research, North-Caucasus Center for Mathematical Research, North-Caucasus Federal University, ORCID: 0000-0002-6269-3717
- Irina G. Shebzukhova – Dr. Sc., Professor, Professor of the Department of Theoretical and Experimental Physics, Institute of Mathematics and Natural Sciences, Kabardino-Balkarian State University named after H.M. Berbekov, ORCID: 0000-0002-1532-1873
- Liana A. Khamukova – Ph. D., Senior Researcher, North-Caucasus Center for Mathematical Research, North-Caucasus Center for Mathematical Research, North-Caucasus Federal University, ORCID: 0000-0002-7830-7614
For citation:
Apekov A.M., Shebzukhova I.G., Khamukova L.A. Zavisimost mezhfaznoj energii granej molibdena na granitse s organicheskimi zhidkostyami ot dielektricheskoj pronitsaemosti [Dependence of the interfacial energy of molybdenum faces at the boundary with organic liquids on the dielectric constant], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 332-339. DOI: 10.26456/pcascnn/2026.18.332. ⎘
Full article (in Russian): download PDF file
References:
1. Gupta S. Advances in molybdenum enriched MOF derived nano-composites for applications outside energy research, Discover Materials, 2025, vol. 5, issue 1, art. № 262, p. 12 DOI: 10.1007/s43939-025-00447-9.
2. Fan Q., Song H., Gao B. et al. Recent progress of molybdenum-based nitrides/carbides catalysts for lithium-sulfur batteries, Energy Materials, 2025, vol. 5, issue 9, art. no. 500105, 25 p. DOI: 10.20517/energymater.2025.33.
3. Chen Y.H., Shen C.H., Chang T.E. et al. Molybdenum-functionalized metal–organic framework crystals interconnected by carbon nanotubes as negative electrodes for supercapacitors, MRS Energy and Sustainability, 2022, vol. 9, issue 2, pp. 332-341. DOI: 10.1557/s43581-022-00034-y.
4. Li Z., Sami, I., Yang, J. et al. Lithiated metallic molybdenum disulfide nanosheets for high-performance lithium–sulfur batteries, Nature Energy, 2023, vol. 8, pp. 84–93. DOI: 10.1038/s41560-022-01175-7.
5. Ryder M.R., Tan J.-C. Nanoporous metal organic framework materials for smart applications, Materials Science and Technology, 2014, vol. 30, issue 13, pp. 1598-1612. DOI: 10.1179/1743284714y.0000000550.
6. Butova V.V., Soldatov M.A., Guda A.A. et al. Metal-organic frameworks: structure, properties, methods of synthesis and characterization, Russian Chemical Reviews, 2014, vol. 85, issue 3, pp. 280-307. DOI: 10.1070/RCR4554.
7. Zhang W., Xiong R.-G. Ferroelectric metal–organic frameworks, Chemical Reviews, 2012, vol. 112, issue 2, pp. 1163-1195. DOI: 10.1021/cr200174w.
8. Barea E., Montoro C., Navarro J. Toxic gas removal – metal–organic frameworks for the capture and degradation of toxic gases and vapours, Chemical Society Reviews, 2014, vol. 43, issue 16, pp. 5419-5430. DOI: 10.1039/c3cs60475f.
9. Qiu S., Xue M., Zhu G. Metal–organic framework membranes: from synthesis to separation application, Chemical Society Reviews, 2014, vol. 43, issue 16, pp. 6116-6140. DOI: 10.1039/C4CS00159A.
10. Rodenas T., Luz I., Prieto G. et al. Metal–organic framework nanosheets in polymer composite materials for gas separation, Nature Materials, 2015, vol. 14, pp. 48-55. DOI: 10.1038/nmat4113.
11. Li J.-R., Kuppler R.J., Zhou H.-C. Selective gas adsorption and separation in metal–organic frameworks, Chemical Society Reviews, 2009, vol. 38, issue 5, pp. 1477-1504. DOI: 10.1039/B802426J.
12. Xiao B., Wheatley P.S., Zhao X. et al. High-capacity hydrogen and nitric oxide adsorption and storage in a metal-organic framework, Journal of the American Chemical Society, 2007, vol. 129, issue 5, pp. 1203-1209. DOI: 10.1021/ja066098k.
13. Horcajada P., Chalati T., Serre C. et al. Porous metal-organic-framework nanoscale carriers as a potential platform for drug delivery and imaging, Nature Materials, 2010, vol. 9, pp. 172-178. DOI: 10.1038/nmat2608.
14. Horcajada P., Gref R., Baati T. et al. Metal–organic frameworks in biomedicine, Chemical Reviews, 2012, vol. 112, issue 2, pp. 1232-1268. DOI: 10.1021/cr200256v.
15. Yang S., Li D., Chen L. et al. Coupling metal organic frameworks with molybdenum disulfide nanoflakes for targeted cancer theranostics, Biomaterials Science, 2021, vol. 9, issue9, pp. 3306-3318. DOI: 10.1039/d0bm02012e.
16. Karami M., Jazani O.M. The progress of molybdenum disulfide 2D nanosheets as bionanocarriers for drug delivery systems: a groundbreaking approach with multiple therapeutic applications, Journal of Inorganic and Organometallic Polymers and Materials, 2025, vol. 35, issue 9, pp. 7129-7158. DOI: 10.1007/s10904-025-03735-2.
17. Jin H.S., Ri K.S., Choe Y.M., Yang H. Evaluation of surface energy and its anisotropy for bcc transition metals by modified embedded atom method, Indian Journal of Physics, 2022, vol. 96, issue 11, pp. 3099-3104. DOI: 10.1007/s12648-021-02237-4.
18. Li C., Lu S., Divinski S., Vitos L. Theoretical and experimental grain boundary energies in body-centered cubic metals, Acta Materialia, 2023, vol. 255, art. № 119074, p. 15. DOI: 10.1016/j.actamat.2023.119074.
19. Apekov А.М., Shebzukhova I.G. Orientatsionnaya zavisimost' mezhfaznoj energii nizkotemperaturnoj modifikatsii titana na granitse s organicheskoj zhidkost' [Orientational dependence of the interphase energy of low-temperature modification of titanium at the boundary with an organic liquid], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 17-23. DOI: 10.26456/pcascnn/2022.14.017. (In Russian).
20. Apekov A.M., Shebzukhova I.G. Interface energy of crystal faces of IIА-type metals at boundaries with nonpolar organic liquids, allowing for dispersion and polarization corrections, Bulletin of Russian Academy of Science. Physics, 2019, vol. 83, issue 6, pp. 760-763. DOI: 10.3103/S1062873819060078.
21. Apekov A.M., Shebzukhova I.G., Khamukova L.A. Mezhfaznaya energiya kristallov alyuminiya na granitsy s nepolyarnymi organicheskimi zhidkostyami. [Interphase energy of aluminum crystals at the boundary with nonpolar organic liquids], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 318-326. DOI: 10.26456/pcascnn/2024.16.318. (In Russian).
22. Apekov A.M., Shebzukhova I.G., Khamukova L.A. Mezhfaznaya energiya kristallov palladiya na granitse s nepolyarnymi organicheskimi zhidkostyami. [Interfacial energy of palladium crystals at the boundary with nonpolar organic liquids], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 250-258. DOI: 10.26456/pcascnn/2025.17.250. (In Russian).
23. Apekov A.M., Shebzukhova I.G. Polarization correction to the interfacial energy of faces of alkali metal crystals at the borders with a nonpolar organic liquid, Bulletin of Russian Academy of Science. Physics, 2018, vol. 82, issue 7, pp. 789-792. DOI: 10.3103/S1062873818070067.
24. Apekov A.M., Shebzukhova I.G. Vklad dispersionnogo vzaimodejstviya v mezhfaznuyu energiyu kristallov kobal'ta na granitse s nepolyarnymi organicheskimi zhidkostyami [Contribution of the dispersion interaction to the interface energy of cobalt crystals at the boundary with nonpolar organic liquids], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 231-238. DOI: 10.26456/pcascnn/2023.15.231. (In Russian).
25. Apekov A.M., Shebzukhova I.G. Temperaturnyy vklad v mezhfaznuyu energiyu graney kristallov Sc, α-Ti I αCo na granitse s organicheskimi zhidkostyami [Temperature contribution to the interfacial energy of the crystals faces of Sc, α-Ti and α-Co at the boundary with the organic liquids], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 19-25. DOI: 10.26456/pcascnn/2016.8.019. (In Russian).