Study of nanoparticle coalescence mechanisms using Pt and Pb as an example

A.A. Cherepovskaya1,2, D.A. Ryzhkova1, Y.Ya. Gafner1, M.D. Starostenkov2

1 Katanov Khakass State University
2 Polzunov Altai State Technical University

DOI: 10.26456/pcascnn/2026.18.515

Short communication

Abstract: In modern materials science and nanotechnology, nanoparticle coalescence processes play a key role in determining the stability and functional properties of nanosystems. Coalescence, the fusion of two or more nanoparticles into a single structure, affects the catalytic activity, optical, and electrical characteristics of materials. In this work, mechanisms of coalescence (using the example of platinum and lead metal nanoparticles) are investigated by molecular dynamics method. The aim of the study was to determine the influence of the mutual crystallographic orientation of atoms, as well as the magnitude of the interatomic interaction on the unification process. Coalescence of Pt and Pb nanoparticles of different diameters was studied, the distance between the particles varied from 1,5 to 0,5 ns, and the simulation time corresponded to 500 ps. The actual appearance and structure of the studied nanoparticles were determined using OVITO and XMakemol visualizers. Analysis of the results shows that various coalescence mechanisms are determined by thermally activated diffusion of surface atoms.

Keywords: coalescence, platinum, lead, nanoparticles, structure, computer simulations, molecular dynamics, tight-binding

  • Arina A. Cherepovskaya – assistant of the Department of Mathematics, Physics and Information Technology, Katanov Khakass State University, 1st year postgraduate student Polzunov Altai State Technical University
  • Daria A. Ryzhkova – Ph. D., Docent of the Department of Mathematics, Physics and Information Technology, Katanov Khakass State University
  • Yury Ya. Gafner – Dr. Sc., Professor, Chief of the Department of Mathematics, Physics and Information Technology, Katanov Khakass State University
  • Mikhail D. Starostenkov – Dr. Sc., Professor, Chief Researcher, Polzunov Altai State Technical University

For citation:

Cherepovskaya A.A., Ryzhkova D.A., Gafner Y.Ya., Starostenkov M.D. Izuchenie mekhanizmov koalestsentsii nanochastits na primere Pt i Pb [Study of nanoparticle coalescence mechanisms using Pt and Pb as an example], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 515-521. DOI: 10.26456/pcascnn/2026.18.515. ⎘

Full article (in Russian): download PDF file

References:

1. Theissmann R., Fendrich M., Zinetullin R. et.al. Crystallographic reorientation and nanoparticle coalescence, Physical Review B, 2008, vol. 78, issue 20, pp. 205413-1-205413-10. DOI: 10.1103/PhysRevB.78.205413.
2. Ingham B., Lim T.H., Dotzler C.J. et.al. How nanoparticles coalesce: an in situ study of Au nanoparticle aggregation and grain growth, Chemistry of Materials, 2011, vol. 23, issue 14, pp. 3312-3317. DOI: 10.1021/cm200354d.
3. Palasantzas G., Vystavel T., Koch S. A. et.al. Coalescence aspects of cobalt nanoparticles during in situ high-temperature annealing, Journal of Applied Physics, 2006, vol. 99, issue 2, pp. 024307-1-024307-5. DOI: 10.1063/1.2163983.
4. Esparza R., Gutiérrez-Wing C., Pérez R., José-Yacamán M. Coalescence of Au nanoparticles: an in-situ Cs-corrected stem study at low voltage, Acta Microscopica, 2018, vol. 28, no. 2, pp. 48-57.
5. Kolosov A.Yu., Sdobnyakov N.Yu., Komarov P.V. et al. Modelirovanie protsessa koalestsentsii nanochastits zolota metodom Monte-Karlo [Simulation of the coalescence process of gold nanoparticles by Monte-Carlo method], Nanotekhnika [Nanotechnics], 2013, vol. 2, issue 34, pp. 65-71. (In Russian).
6. Kolosov A.Yu., Sokolov D.N., Sdobnyakov N.Yu. et al. Ob otsenke dvugrannogo ugla mezhdu nanochastitsami metallov v protsesse koalestsentsii [About assessment of dihedral angle between metal nanoparticles in the coalescence process], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 172-179. DOI: 10.26456/pcascnn/2016.8.172. (In Russian).
7. Kolosov A.Yu., Myasnichenko V.S., Bogdanov S.S. et al. O zakonomernostyakh formirovaniya mono- i bimetallicheskikh nanochastits v protsesse koalestsentsii [On the regularities of formation of mono- and bimetallic nanoparticles in the coalescence process], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2018, issue 10, pp. 359-367. DOI: 10.26456/pcascnn/2018.10.359. (In Russian).
8. Sdobnyakov N.Yu., Kolosov A.Yu., Bogdanov S.S. Modelirovanie protsessov koalestsentsii i spekaniya v mono- i bimetallicheskikh nanosistemakh: monografiya [Simulation of the processes of coalescence and sintering in mono- and bimetallic nanosystems: monograph]. Tver, Tver State University Publ., 2021, 168 p. DOI: 10.26456/skb.2021.168. (In Russian).
9. Grammatikopoulos P., Sowwan M., Kioseoglou J. Computational modeling of nanoparticle coalescence, Advanced Theory and Simulations, 2019, vol. 2, art.no. 1900013, 26p. DOI: 10.1002/adts.201900013.
10. Wan N., Shuang-ying L., Jun X., Martini M. A 'jump-to-coalescence' mechanism during nanoparticle growth revealed by in situ aberration-corrected transmission electron microscopy observations, Nanotechnology, 2016, vol. 27, no. 20, art. no. 205605, 8 p. DOI: 10.1088/0957-4484/27/20/205605.
11. Shengnan Y., Wenjuan Y., Ziliang D. et.al. In situ tem observation of the atomic transport process during the coalescence of Au nanoparticles, Nano Letters, 2023, vol. 22, issue 20, pp. 8115-8121. DOI: 10.1021/acs.nanolett.2c02491.
12. Cherepovskaya A.A., Ryzhkova D.A. Nachal’naya stadiya protsessa koalestsentsii na primere nanochastits Ag [Initial stage of the coalescence process exemplifying on Ag nanoparticles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 17, pp. 506-513. DOI: 10.26456/pcascnn/2025.17.506. (In Russian).
13. Gafner Yu.Ya., Gromov D.G., Volkov R.L. et. al. Mechanisms of Au and Ag nanoparticle array evolution studied by in-situ TEM and molecular dynamics simulation, Surface and Interface, 2024, vol. 54, art. no. 105165, 11 p. DOI: 10.1016/j.surfin.2024.105165.
14. Rapallo A., Rossi G., Ferrando R. et al. Global optimization of bimetallic cluster structures. I. Size-mismatched Ag-Cu, Ag-Ni, and Au-Cu systems, The Journal of Chemical Physics, 2005, vol. 122, issue 19, pp. 194308-1-194308-13. DOI: 10.1063/1.1898223.
15. XMakemol - A program for visualizing atomic and molecular systems. Available at: www.url: https://manpages.ubuntu.com/manpages/bionic/man1/xmakemol.1.html. (accessed 10.06.2026).
16. Stukowski A. Visualization and analysis of atomistic simulation data with OVITO – the open visualization tool, Modelling and Simulation in Materials Science and Engineering, 2010, vol. 18, no. 1, art. no. 015012, 7 p. DOI: 10.1088/0965-0393/18/1/015012.
17. Kim J., Kang D., Kang S.et. al. Coalescence dynamics of platinum group metal nanoparticles revealed by liquid-phase transmission electron microscopy, iScience, 2022, vol. 25, issue 8, art. no. 104699, 12 p. DOI: 10.1016/j.isci.2022.104699.
18. Yun K., Lee J., Nam H.-S. Effect of temperature on coalescence behavior of unsupported gold nanoparticles, Electronic Materials Letters, 2018, vol. 15, issue 1, pp. 133-139. DOI: 10.1007/s13391-018-0090-6.

Content |