Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Cysteine-silver sol at different pH: the influence of the chemical nature of silver salts

D.V. Vishnevetskii1, E.E. Polyakova1, D.V. Averkin2

1 Tver State University
2 All-Russian Scientific Research Institute of Physical-Technical and Radiotechnical Measurements

DOI: 10.26456/pcascnn/2026.18.823

Original article

Abstract: The effect of the chemical nature of silver salts (silver nitrate, silver nitrite, silver acetate) used as a precursor in the synthesis of cysteine-silver sols on their behavior at different medium acidities has been investigated. It has been shown that all sols, regardless of the chemical nature of the precursor, have an isoelectric point, the value of which depends on the history of sample preparation — the chemical nature of the silver salt. This behavior is associated with the presence of amino and carboxyl groups located on the surface of cysteine-silver sol nanoparticles. Based on previous results and the data obtained in this work, a structure of the nanoparticles forming the corresponding sol has been proposed.

Keywords: cysteine-silver sol, pH, isoelectric point, turbidity, zeta-potential

  • Dmitry V. Vishnevetskii – Ph. D., Docent, Physical Chemistry Department, Tver State University, ORCID: 0000-0003-1382-9451
  • Elizaveta E. Polyakova – 1st year graduate student, Leading Engineer, Physical Chemistry Department, Tver State University
  • Dmitry V. Averkin – Researcher, Laboratory of Metrological Support for Measurements of Dispersed Parameters of Aerosols, Suspensions and Powdery Materials, All-Russian Scientific Research Institute of Physical-Technical and Radiotechnical Measurements, ORCID: 0000-0002-8653-3267

For citation:

Vishnevetskii D.V., Polyakova E.E., Averkin D.V. Tsistein-serebryanyj zol pri razlichnykh pH: vliyanie khimicheskoj prirody solej serebra [Cysteine-silver sol at different pH: the influence of the chemical nature of silver salts], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 823-831. DOI: 10.26456/pcascnn/2026.18.823. ⎘

Full article (in Russian): download PDF file

References:

1. Smith D.K. Supramolecular gels – a panorama of low-molecular-weight gelators from ancient origins to next-generation technologies, Soft Matter, 2024, vol. 20, issue 1, pp. 10-70. DOI: 10.1039/D3SM01301D.
2. Adams D.J. Personal perspective on understanding low molecular weight gels, Journal of the American Chemical Society, 2022, vol. 144, issue 25, pp. 11047–11053. DOI: 10.1021/jacs.2c02096.
3. Du X., Zhou J., Shi J., Xu B. Supramolecular hydrogelators and hydrogels: From soft matter to molecular biomaterials, Chemical Reviews, 2015, vol. 115, issue 24, pp. 13165–13307. DOI: 10.1021/acs.chemrev.5b00299.
4. Bhattacharya S., Krishnan‑Ghosh Y. First report of phase selective gelation of oil from oil/water mixtures. Possible implications toward containing oil spills, Chemical Communications, 2001, issue 2, pp. 185-186. DOI: 10.1039/B007848O.
5. Gao P., Zhan C.L., Liu L.Z. et al. et al. Inter and intra‑molecular H‑bonds induced different nanostructures from a multi‑H‑bonding (MHB) amphiphile: nanofibers and nanodisks, Chemical Communications, 2004, issue 10, pp. 1174-1175. DOI: 10.1039/B402956A.
6. Khatua D., Dey J. Spontaneous formation of gel emulsions in organic solvents and commercial fuels induced by a novel class of amino acid derivatized surfactants, Langmuir, 2005, vol. 21, issue 1, pp. 109-114. DOI: 10.1021/la0481896.
7. Pal A., Dey J. Water‑induced physical gelation of organic solvents by N‑(N‑alkylcarbamoyl)‑L‑alanine amphiphiles, Langmuir, 2011, vol. 27, issue 7, pp. 3401–3408. DOI: 10.1021/la105027b.
8. Patra T., Pal A., Dey J. A smart supramolecular hydrogel of Nα‑(4‑N‑alkyloxybenzoyl)‑L‑histidine exhibiting pH‑modulated properties, Langmuir, 2010, vol. 26, issue 11, pp. 7761-7767. DOI: 10.1021/la904540x.
9. Minakuchi N., Hoe K., Yamaki D. et al. Versatile supramolecular gelators that can harden water, organic solvents and ionic liquids, Langmuir, 2012, vol. 28, issue 25, pp. 9259–9266. DOI: 10.1021/la301442f.
10. Yu Q., Fan M., Li D. et al. Thermoreversible gel lubricants through universal supramolecular assembly of a nonionic surfactant in a variety of base lubricating liquids, ACS Applied Materials & Interfaces, 2014, vol. 6, issue 18, pp. 15783-15794. DOI: 10.1021/am502832z.
11. Yu Q., Li D., Cai M. et al. Supramolecular gel lubricants based on amino acid derivative gelators, Tribology Letters, 2016, vol. 61, issue 2, pp. 1-16. DOI: 10.1007/s11249‑015‑0634‑y.
12. Odriozola I., Loinaz I., Pomposo J.A. et al. Gold–glutathione supramolecular hydrogels, Journal of Materials Chemistry, 2007, vol. 17, issue 46, pp. 4843-4845. DOI: 10.1039/B713542D.
13. Casuso P., Carrasco P., Loinaz I. et al. Converting drugs into gelators: supramolecular hydrogels from N‑acetyl‑L‑cysteine and coinage‑metal salts, Organic & Biomolecular Chemistry, 2010, vol. 8, issue 23, pp. 5455-5458. DOI: 10.1039/C0OB00311E.
14. Casuso P., Carrasco P., Loinaz I. et al. Argentophilic hydrogels: elucidating the structure of neutral versus acidic system, Soft Matter, 2011, vol. 7, issue 7, pp. 3627-3633. DOI: 10.1039/C0SM01217C.
15. Casuso P., Vicente A.P.-S., Iribar H. et al. Aurophilically cross‑linked «dynamic» hydrogels mimicking healthy synovial fluid properties, Chemical Communications, 2014, vol. 50, issue 96, pp. 15199-15201. DOI: 10.1039/C4CC05735J.
16. Khizhnyak S.D., Komarov P.V., Ovchinnikov M.M. et al. Mechanism of gelation in low-concentration aqueous solutions of silver nitrate with L-cysteine and its derivatives, Soft Matter, 2017, vol. 13, issue 30, pp. 5168-5184. DOI: 10.1039/C7SM00772H.
17. Vishnevetskii D.V., Adamyan A.N., Laguseva V.S. et al. Self-organization processes in aqueous solution of polyvinyl alcohol, L-cysteine, and silver nitrate, Polymer Science, Series A, 2019, vol. 61, issue 1, pp. 96-104. DOI: 10.1134/S0965545X19010103.
18. Vishnevetskii D.V., Averkin D.V., Efimov A.A. et al. L-cysteine and N-acetyl-L-cysteine mediated synthesis of nanosilver-based sols and hydrogels with antibacterial and antibiofilm properties, Journal of Materials Chemistry B, 2023, vol. 11, issue 25, pp. 5794-5804. DOI: 10.1039/D3TB00261F.
19. Vishnevetskii D.V., Mekhtiev A.R., Averkin D.V., Polyakova E.E. Cysteine–silver–polymer systems for the preparation of hydrogels and films with potential applications in regenerative medicine, Gels, 2023, vol. 9, issue 12, art. no 924, 13 p. DOI: 10.3390/gels9120924.
20. Vishnevetskii D.V., Andrianova Y.V., Polyakova E.E. et al. Fluoride-ion-responsive sol–gel transition in an L-cysteine/AgNO3 system: self-assembly peculiarities and anticancer activity, Gels, 2024, vol. 10, issue 5, art. no. 332, 14 p. DOI: 10.3390/gels10050332.
21. Vishnevetskii D.V., Metlin F.A., Andrianova Y.V. et al. Preparation of composite hydrogels based on cysteine–silver sol and methylene blue as promising systems for anticancer photodynamic therapy, Gels, 2024, vol. 10, issue 9, art. no. 577, 17 p. DOI: 10.3390/gels10090577.
22. Vishnevetskii D.V., Polyakova E.E., Andrianova Y.V. et al. L-cysteine/silver nitrate/iodate anions system: peculiarities of supramolecular gel formation with and without visible-light exposure, Gels, 2024, vol. 10, issue 12, art. no. 809, 16 p. DOI: 10.3390/gels10120809.
23. Malyshev M.D., Khizhnyak S.D., Zherenkova L.V. et al. Self-assembly in systems based on L-cysteine–silver-nitrate aqueous solution: multiscale computer simulation, Soft Matter, 2022, vol. 18, issue 39, pp. 7524-7536. DOI: 10.1039/D2SM00846G.
24. Vishnevetskii D.V., Semenova E.M., Averkin D.V., Mekhtiev A.R. Behavior and bioactive properties of aqueous L-cysteine–AgNO3 solution at different pH, Mendeleev Communications, 2023, vol. 33, issue 3, pp. 431-432. DOI: 10.1016/j.mencom.2023.04.042.
25. Vishnevetskii D.V., Mekhtiev A.R., Perevozova T.V. et al. L-cysteine/AgNO2 low molecular weight gelators: self-assembly and suppression of MCF-7 breast cancer cells, Soft Matter, 2020, vol. 16, issue 42, pp. 9669-9673. DOI: 10.1039/D0SM01431A.

Content |