The effect of NiO doping on the phase composition and ferroelectric properties of lead-free ceramics based on sodium and potassium niobate
S.V. Torianik1, T.S. Ilina1, E.A. Skryleva1, B.R. Senatulin1, M.I. Voronova1, A.V. Pavlenko2, D.A. Kiselev1, Yu.N. Parkhomenko1
1 University of Science and Technology MISIS
2 Federal Research Centre The Southern Scientific Centre of the RAS
DOI: 10.26456/pcascnn/2026.18.185
Original article
Abstract: The development of lead-free piezoelectric materials capable of replacing toxic lead zirconate titanate is a priority in modern materials science due to stricter environmental regulations and growing demand for environmentally friendly high-temperature transducers. Potassium sodium niobate based ceramics offer potential as promising candidates due to their high Curie temperature; however, their practical application is limited by the difficulty of obtaining dense samples and insufficiently high electrophysical characteristics, which makes it relevant to study the influence of both substitutions in the A- and B-positions of the perovskite structure (ABO3) and additives that can improve sinterability and modify local ferroelectric properties. In this work, three compositions 0,94(Na0,54K0,46)(Nb0,9Ta0,1)O3 – 0,06LiSbO3 – xNiO (KNNT‑LS‑xNiO), where x = 0, 0,01 and 0,02, were investigated. A comprehensive characterization of the samples was carried out using complementary methods – X-ray phase analysis with Rietveld structure refinement, X-ray photoelectron spectroscopy, atomic force microscopy and piezoresponse force microscopy. It was established that in samples with x = 0 and x = 0,01 nonpolar secondary phases are present, whereas at x = 0,02 these phases are completely suppressed and coexistence of polar phases P1m1 and P4mm is observed. The highest content of ferroactive phases and the maximum relaxation time of the induced domain structure were recorded for the sample with the highest NiO content, which indicates a significant increase in the stability of residual polarization upon optimal doping. The obtained results demonstrate that a targeted combination of substitutions in the crystal lattice and NiO additive makes it possible to control the phase composition and relaxation functions of the induced domain structure, opening the way to the creation of lead-free ceramics with improved and reproducible ferroelectric phenomena.
Keywords: potassium-sodium niobate, lead-free ceramics, atomic force microscopy, X-ray photoelectron spectroscopy, X-ray phase analysis
- Sofia V. Torianik – 1st year postgraduate student, Department of Materials Science of Semiconductors and Dielectrics, University of Science and Technology MISIS, ORCID: 0009-0001-7753-9907
- Tatiana S. Ilina – Ph. D., Senior Researcher, Laboratory of Physics of Oxide Ferroelectrics, University of Science and Technology MISIS, ORCID: 0000-0002-1641-1731
- Elena A. Skryleva – Engineer of the scientific project, Laboratory of Physics of Oxide Ferroelectrics, University of Science and Technology MISIS, ORCID: 0000-0002-9588-4456
- Boris R. Senatulin – Expert in the scientific project, Laboratory of Physics of Oxide Ferroelectrics, University of Science and Technology MISIS, ORCID: 0000-0001-8293-6221
- Marina I. Voronova – Expert in the scientific project, Laboratory of Physics of Oxide Ferroelectrics, University of Science and Technology MISIS, ORCID: 0000-0003-0233-7902
- Anatoliy V. Pavlenko – Dr. Sc., Head of the Laboratory of Nanoscale Active Media and Materials, Federal Research Centre The Southern Scientific Centre of the RAS, ORCID: 0000-0002-4257-2950
- Dmitry A. Kiselev – Ph. D., Head of the Department of Materials Science of Semiconductors and Dielectrics, University of Science and Technology MISIS, ORCID: 0000-0003-1047-3007
- Yurii N. Parkhomenko – Dr. Sc., Scientific supervisor, Professor, Department of Semiconductor and Dielectric Materials Science, University of Science and Technology MISIS, ORCID: 0000-0002-1970-9867
For citation:
Torianik S.V., Ilina T.S., Skryleva E.A., Senatulin B.R., Voronova M.I., Pavlenko A.V., Kiselev D.A., Parkhomenko Yu.N. Vliyanie dobavki NiO na fazovyj sostav i segnetoelektricheskie svojstva bessvintsovykh keramik na osnove niobata kaliya natriya [The effect of NiO doping on the phase composition and ferroelectric properties of lead-free ceramics based on sodium and potassium niobate], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 185-196. DOI: 10.26456/pcascnn/2026.18.185. ⎘
Full article (in Russian): download PDF file
References:
1 Lv X., Zhu J., Xiao D. et al. Emerging new phase boundary in potassium sodium niobate based ceramics, Chemical Society Reviews, 2020, vol. 49, issue 3, pp. 671-707. DOI: 10.1039/c9cs00432g.
2. Zhang N., Zheng T., Wu J. Lead-free (K,Na)NbO3-based materials: preparation techniques and piezoelectricity, ACS Omega, 2020, vol. 5, issue 7, pp. 3099-3107. DOI: 10.1021/acsomega.9b03658.
3. Chi W., Zhou X., Zou J. et al. Significantly enhanced mechanical quality factor with favorable piezoelectricity in K0.5Na0.5NbO3-based ceramics, Journal of Materials Science, 2022, vol. 57, issue 43, pp. 20285-20298. DOI: 10.1007/s10853-022-07901-6.
4. Serrazina R., Tkach A., Pereira L. et al. Flash sintered potassium sodium niobate: high performance piezoelectric ceramics at low thermal budget processing, Materials, 2022, vol. 15, issue 19, art. no. 6603, 8 p. DOI: 10.3390/ma15196603.
5. Wei N., Karaki T., Fujii T. Low temperature sintering of (K,Na,Li)NbO3-BaZrO3-(Bi,Na)TiO3 ceramics with enhanced dielectric and piezoelectric properties, Japanese Journal of Applied Physics, 2020, vol. 59, no. SP, art. no. SPPD02, 6 p. DOI: 10.35848/1347-4065/aba73b.
6. Piah H.M.A., Rashid M.W.A., Azlan U.A.-A., Hatta M.A.M. Potassium sodium niobate (KNN) lead-free piezoceramics: A review of phase boundary engineering based on KNN materials, AIMS Materials Science, 2023, vol. 10, issue 5, pp. 835-861. DOI: 10.3934/matersci.2023045.
7. Montero-Tavera C., Durruthy-Rodríguez M.D., Cortés-Vega F.D., Yáñez-Limón J.M. Study of the structural, ferroelectric, dielectric, and pyroelectric properties of the K0.5Na0.5NbO3 system doped with Li+, La3+, and Ti4+, Journal of Advanced Ceramics, 2020, vol. 9, issue 3, pp. 329-338. DOI: 10.1007/s40145-020-0372-y.
8. Yu Y., Zheng T., Zhang N., Wu J. Review of sintering aids in lead-free (K,Na)NbO3-based ceramics, IEEE Transactions on Ultrasonics, Ferroelectrics, and Frequency Control, 2022, vol. 69, issue 11, pp. 3003-3012. DOI: 10.1109/TUFFC.2022.3152412.
9. Delshad Chermahini M. Effect of NiO sintering aid on the electrical properties of KNN-LST lead-free piezoceramics, Advanced Ceramics Progress, 2024, vol. 10, issue 1, pp. 44-48. DOI: 10.30501/acp.2023.414402.1130.
10. Iacomini A., Tamayo-Ramos J.A., Rumbo C. et al. processing optimization and toxicological evaluation of «lead-free» piezoceramics: a KNN-based case study, Materials, 2021, vol. 14, issue 15, art. no. 4337, 13 p. DOI: 10.3390/ma14154337.
11. Panda P.K., Sahoo B., Thejas T.S. High strain lead-free piezo ceramics for sensor and actuator applications: a review, Sensors International, 2020, vol. 4, art. no. 100226, 11 p. DOI: 10.1016/j.sintl.2022.100226.
12. Zhang M.H., Hu C., Zhou Z. et al. Determination of polarization states in (K,Na)NbO3 lead-free piezoelectric crystal, Journal of Advanced Ceramics, 2020, vol. 9, issue 2, pp. 204-209. DOI: 10.1007/s40145-020-0360-2.
13. Xing J., Jiang L., Zhao C. et al. Potassium sodium niobate based lead-free ceramic for high-frequency ultrasound transducer applications, Journal of Materiomics, 2020, vol. 6, issue 3, pp. 513-522. DOI: 10.1016/j.jmat.2020.03.007.
14. FullProf Suite. Crystallographic tools for diffraction. Available at: https://www.ill.eu/sites/fullprof. (accessed 22.07.2026).
15. Ilina T.S., Skryleva E.A., Ermakov A.Yu. et al. Structural and compositional indicators of ferroelectric properties of KNN ceramics, Ceramics International, 2023, vol. 49, issue 22, part B, pp. 36206-36217. DOI: 10.1016/j.ceramint.2023.08.301.
16. Ilina T.S., Skryleva E.A., Kiselev D.A. et al. Study of the structure and ferroelectric properties of 1% barium doped KNN-based ceramics using combined analytical methods, Journal of Physics and Chemistry of Solids, 2025, vol. 205, art. no. 112802, 10 p. DOI: 10.1016/j.jpcs.2025.112802.
17. Skryleva E.A., Senatulin B.R., Ilina T.S.et al. Origin of chemical shifts in K 2p x-ray photoelectron spectra, Journal of Vacuum Science & Technology A, 2026, vol. 44, issue 1, art no. 013201, 10 p. DOI: 10.1116/6.0004936.