Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Production of a titanium-containing composite material with a wide spectrum of action based on ultradisperse hydroxyapatite

N.S. Kozhevnikova1, E.A. Bogdanova2, V.M. Skachkov1, A.Yu. Chufarov1, A.A. Yushkov3, I.V. Baklanova1, Y.A. Avdeeva1

1 Institute of Solid State Chemistry of the Ural Branch of RAS
2 JSC «Giredmet»
3 Ural Federal University named after the first President of Russia B.N. Yeltsin

DOI: 10.26456/pcascnn/2026.18.857

Original article

Abstract: The aim of this work was the sol-gel synthesis of promising titanium-containing composite materials based on nanosized hydroxyapatite (the titanium content in the final product, calculated as TiO2, is 10-40 wt.%). A comprehensive study of the composition and structure of the obtained materials was carried out using modern physicochemical analytical methods: X-ray diffraction and energy-dispersive X-ray analysis, Raman spectroscopy, scanning and transmission electron microscopy. The surface characteristics of the studied samples were evaluated using the Brunauer-Emmett-Teller method. Based on the specific surface area and pycnometric density data, the average surface diameter of the particles was calculated. A correlation was revealed between the amount of introduced titanium and the crystal lattice parameters of the sample, the band gap, the surface characteristics, the density and morphology of the obtained materials, demonstrating the promise of their further research for the purpose of practical application both as ceramic materials for medical purposes and as photocatalysts.

Keywords: hydroxyapatite, titanium-containing hydroxyapatite, synthesis, precipitation from solution, sol-gel method, titanium oxide, functional materials

  • Natal'ya S. Kozhevnikova – Ph. D., Senior Researcher, Laboratory of non-stoichiometric compounds, Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0001-9122-9078
  • Ekaterina A. Bogdanova – Ph. D., Leading Researcher, Laboratory of Materials and Technologies of the Fourth Energy Transition, JSC «Giredmet», ORCID: 0000-0002-6947-5368
  • Vladimir M. Skachkov – Ph. D., Senior Researcher, Laboratory of heterogeneous processes chemistry, Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0003-2551-3235
  • Alexsandr Yu. Chufarov – Researcher, Laboratory of structural and phase analysis, Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0003-3667-144X
  • Anton A. Yushkov – Ph. D., Researcher at the Department of Magnetism of Solids at the Institute of Natural Sciences and Mathematics, Ural Federal University named after the first President of Russia B.N. Yeltsin, ORCID: 0000-0001-9792-2324
  • Inna V. Baklanova – Ph. D., Senior Researcher, Laboratory of quantum chemistry and spectroscopy named after A.L. Ivanovsky, Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0002-5643-7004
  • Yulia A. Avdeeva – Researcher, Laboratory of structural and phase analysis, Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0002-1470-0476

For citation:

Kozhevnikova N.S., Bogdanova E.A., Skachkov V.M., Chufarov A.Yu., Yushkov A.A., Baklanova I.V., Avdeeva Y.A. Poluchenie titansoderzhashchego kompozitsionnogo materiala shirokogo spektra dejstviya na osnove ultradispersnogo gidroksiapatita [Production of a titanium-containing composite material with a wide spectrum of action based on ultradisperse hydroxyapatite], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 857-867. DOI: 10.26456/pcascnn/2026.18.857. ⎘

Full article (in Russian): download PDF file

References:

1. Adhikara G., Maharani A.P., Puspitasari A. et al. Bovine hydroxyapatite for bone tissue engineering: Preparation, characterization, challenges, and future perspectives, European Polymer Journal, 2024, vol. 214, art. no. 113171, 12 p. DOI: 10.1016/j.eurpolymj.2024.113171.
2. Barinov S.M., Komlev V.S. Biokeramika na osnove fosfatov kal'tsiya [Calcium phosphate bioceramics]. Moscow, Nauka Publ., 2006, 204 p. (In Russian).
3. Mondal S., Park S., Choi J. et al. Hydroxyapatite: a journey from biomaterials to advanced functional materials, Advances in Colloid and Interface Science, 2023, vol. 321, art. no. 103013, 27 p. DOI: 10.1016/j.cis.2023.103013.
4. Anmin H., Tong L., Ming L. et al. Preparation of nanocrystals hydroxyapatite/TiO2 compound by hydrothermal treatment, Applied Catalysis B: Environmental, 2006, vol. 63, issue 1-2, pp. 41-44. DOI: 10.1016/j.apcatb.2005.08.003.
5. Iwamoto T., Kogai Y. Influence of titanium ion doping on structural changes in porous hydroxyapatite ceramics, Solid State Sciences, 2023, vol. 142, art. no. 107222, 7 p. DOI: 10.1016/j.solidstatesciences.2023.107222.
6. Ribeiro C.C., Gibson I., Barbosa M.A. The uptake of titanium ions by hydroxyapatite particles–structural changes and possible mechanisms, Biomaterials, 2006, vol. 27, issue 9, pp. 1749-1761. DOI: 10.1016/j.biomaterials.2005.09.043.
7. Nath S., Tripathi R., Basu B. Understanding phase stability, microstructure development and biocompatibility in calcium phosphate–titania composites, synthesized from hydroxyapatite and titanium powder mix, Materials Science and Engineering: C, 2009, vol. 29, issue 1, pp. 97-107. DOI: 10.1016/j.msec.2008.05.019.
8. Tsukada M., Wakamura M., Yoshida N., Watanabe T. Band gap and photocatalytic properties of Ti-substituted hydroxyapatite: Comparison with anatase-TiO2, Journal of Molecular Catalysis A: Chemical, 2011, vol. 338, issue 1-2, pp 18-23. DOI: 10.1016/j.molcata.2011.01.017.
9. Iwamoto T., Hieda Y., Kogai Y. Effects of molecular weight on macropore sizes and characterization of porous hydroxyapatite ceramics fabricated using polyethylene glycol: mechanisms to generate macropores and tune their sizes, Materials Today Chemistry, 2021, vol. 20, art. no. 100421, 11 p. DOI: 10.1016/j.mtchem.2021.100421.
10. Huang J., Best S.M., Bonfield W., Buckland T. Development and characterization of titanium-containing hydroxyapatite for medical applications, Acta Biomaterialia, 2010, vol. 6, issue 1, pp. 241-249, DOI: 10.1016/j.actbio.2009.06.032.
11. Tanaka H., Ohnishi A. Synthesis of Ti(IV)-substituted calcium hydroxyapatite microparticles by hydrolysis of phenyl phosphates, Advanced Powder Technology, 2013, vol. 24, issue 6, pp. 1028-1033. DOI: 10.1016/j.apt.2013.02.012.
12. Sabirzyanov N.A., Bogdanova E.A., Khonina T.G. Sposob polucheniya suspenzii gidroksiapatita [A method of obtaining a suspension of hydroxyapatite]. Patent RF, no. 2406693, 2010. (In Russian).
13. Bogdanova E.A., Sabirzyanov N.A., Skachkov V.M. Sposob polucheniya suspenzii apatita [A method of obtaining a suspension of apatite]. Patent RF, no. 2652193, 2018. (In Russian).
14. Bogdanova E.A., Skachkov V.М., Medyankina I.S. et al. Formation of nanodimensional structures in precipitated hydroxyapatite by fluorine substitution, SN Applied Sciences, 2020, vol. 2, issue 9, art. no. 1565, 7 p. DOI: 10.1007/s42452-020-03388-5.
15. Powder Diffraction File JCPDS-ICDD PDF-2 (Set 1-47). (Release, 2016). – Режим доступа: www.url: https://www.icdd.com/pdf-2/. – 15.05.2026.
16. Petrakova N.V., Barinov S.M., Evstratov E.V. et al. Compaction of hydroxyapatite nanopowders by hydrostatic pressing, Inorganic Materials: Applied Research, 2017, vol. 8, issue 4, pp. 528-534. DOI: 10.1134/S2075113317040190.
17. Yu J., Yu J.C., Ho W. et al. Effects of alcohol content and calcination temperature on the textural properties of bimodally mesoporous titania, Applied Catalysis A: General, 2003, vol. 255, issue 2, pp. 309-320. DOI: 10.1016/S0926-860X(03)00570-2.

Content |