Changes in the mass composition of alkali metal clusters caused by the geometry of the field source surface changes

D.P. Bernatskii, V.G. Pavlov

Ioffe Institute

DOI: 10.26456/pcascnn/2026.18.787

Original article

Abstract: The effect of the surface structure of a metallic crystal on the formation of clusters of alkali metal atoms adsorbed on the surface has been studied. The study was carried out using field electron microscopy, field desorption microscopy, and time-of-flight mass analysis of ions desorbed by an electric field. Crystals of tungsten and rhenium were used as substrates. The adsorbates were sodium, potassium, and cesium. Alkali metal atoms were deposited on the surface of a tungsten or rhenium field emitter from an external spray. The experiments were carried out in an ultrahigh vacuum (p < 10-9 Torr). To determine the masses, pulsed field desorption of clusters from the surface and measurement of the time of flight of ionized clusters from the sample surface to the detector were performed. As a result of the measurements, clusters containing up to seven atoms were detected. To determine the effect of the structure of metal crystals on the number of atoms in clusters, a metal crystal was heated in an electric field (thermal field treatment). As a result of this treatment, the shape of the tip and the structure of its surface changed. The number of crystal steps decreased until they completely disappeared, and the crystal shape gradually shifted from a rounded shape close to a hemisphere (annealing shape) to a polyhedron shape. The cluster composition was measured at different stages of the transition from a round crystal shape to a polyhedron, and, accordingly, with a different number of steps on the surface. As the number of steps decreased, so did the number of atoms in the cluster. Only monatomic clusters were formed on the surface of a sample completely faceted with densely packed crystal planes without steps. From the experimental results obtained, it can be concluded that the formation of clusters of alkali metal atoms on the metal surface requires the presence of crystalline steps on the surface.

Keywords: field desorption, cesium, potassium, sodium, tungsten, rhenium, electric field, ion clusters

  • Dmitrii P. Bernatskii – Ph. D., Docent, Senior Researcher, Ioffe Institute, ORCID: 0009-0003-2028-061X
  • Victor G. Pavlov – Dr. Sc., Senior Researcher, Ioffe Institute, ORCID: 0000-0002-3297-9255

For citation:

Bernatskii D.P., Pavlov V.G. Izmenenie massovogo sostava klasterov shchelochnykh metallov pri izmenenii geometrii poverkhnosti polevogo istochnika [Changes in the mass composition of alkali metal clusters caused by the geometry of the field source surface changes], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 787-799. DOI: 10.26456/pcascnn/2026.18.787. ⎘

Full article (in Russian): download PDF file

References:

1. Muller E.W., Tsong T.T. Field ion microscopy, field ionization and field evaporation, Progress in Surface Science, 1974, vol. 4, pp. 1-139. DOI: 10.1016/S0079-6816(74)80005-5.
2. Gross H. From the discovery of field ionization to field desorption and liquid injection field desorption/ionization-mass spectrometry-A journey from principles and applications to a glimpse into the future, European journal of Mass Spectrometry, 2020, vol. 26, issue 4, pp. 241-273 DOI: 10.1177/1469066720939399.
3. Nanofabrication using focused ion and electron beams: principles and applications, ed. by I. Utke, S. Moshkalev, P. Russell. Oxford, Oxford University Press, 2012, 840 p.
4. Avasthi D.K., Mehta G.K. Swift heavy ions for materials engineering and nanostructuring, Springer Series in Materials Science, vol. 145. Dordrecht, Springer, 2011, XII + 280 p. DOI: 10.1007/978-94-007-1229-4.
5. Isahanov Z.A., Kosimov I.O., Umirzakov B.E., Erkulov R.M. Modification of the surface properties of free Si–Cu films by implantation of active metal ions, Technical Physics, 2020, vol. 65, issue 1, pp. 114-117. DOI: 10.1134/S1063784220010090.
6. Nano tools and devices for enhanced renewable energy, ed. by S. Devasahayam, C.M. Hussein. Amsterdam, Elsevier, 2021, 620 p. DOI: 10.1016/C2019-0-03671-0.
7. Luminescent metal nanoclusters. synthesis, characterization, and applications, ed.by S. Thomas, K. Joseps, S. Appukuttan, M.S. Mathew. Amsterdam, Elsevier, 2022, 726 p. DOI: 10.1016/C2020-0-03396-7.
8. Bernatskii D.P., Pavlov V.G. Investigation of a solid surface using continuous-mode field-desorption microscopy, Bulletin of the Russian Academy of Sciences: Physics, 2009, vol. 73, issue 5, pp. 673-675. DOI: DOI: 10.3103/S1062873809050438.
9. Suchorski Y. Field ion and field desorption microscopy: principles and applications, Surface science tools for nanomaterials characterization, ed. by C.S.S.R. Kumar. Berlin, Heidelberg, Springer-Verlag, 2015, pp. 227-272. DOI: 10.1007/978-3-662-44551-8_7.
10. Morozov S.N., Rasulev U.Kh. Application of the surface ionization for the detection of secondary particles in the secondary-ion mass spectrometry (SIMS), Technical Physics, 2013, vol. 58, issue 6, pp. 821-826.DOI: 10.1134/S1063784213060224.
11. Bernackij D.P., Pavlov V.G. Identifikatsiya klasterov shchelochnykh metallov s pomoshch'yu polevoj desorbtsii [Identification of alkali metal clusters by field desorption], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 795-804. DOI: 10.26456/pcascnn/2025.17.795.
12. Bol’shov L.A., Napartovich A.P., Naumovets A.G.N., Fedoras A.G. Submonolayer films on the surface of metals, Soviet Physics Uspekhi, 1977, vol. 20, no. 5, pp. 432-451. DOI: 10.1070/PU1977v020n05ABEH005398.
13. Klimenko E.V., Naumovets A.G. Ob elektronnom sostoyanii adsorbirovannykh atomov tseziya, litiya i bariya na grani (110) vol'frama [On the electronic state of adsorbed cesium, lithium and barium atoms on the (110) facet of tungsten], Fizika tverdogo tela [Physics of the Solid State], 1971, vol. 13, issue 1, pp. 33-40. (In Russian).
14. Naumovets A.G. Collective surface diffusion: an experimentalist’s view, Physica A, 2005, vol. 357, issue 2, pp. 189-215. DOI: 10.1016/j.physa.2005.06.027.
15. Shrednik V.N., Snezhko E.V. Avtoelektronnaya mikroskopiya Na na W v usloviyakh migratsionnogo ravnovesiya [Autoelectronic microscopy of Na on W under conditions of migration equilibrium], Fizika tverdogo tela [Physics of the Solid State], 1964, vol. 6, issue 11, pp. 3409-3422. (In Russian).
16. Fu T.-Y., Wu H.-T., Tsong T.T. Energetics of surface atoms processes near a lattice step, Physical Review B, 1998, vol. 58, issue 4, pp. 2340-2346. DOI: 10.1103/PhysRevB.58.2340.
17. Fu T.-Y., Tsong T.T. Determination of atomic potential energy around step corner sites of the Ir(111) surface, Physical Review B, 2001, vol. 61, issue 7, pp. 4511-4513. DOI: 10.1103/PhysRevB.61.4511.
18. Bettler P.C., Charbonnier F.M. Activation energy for the surface migration of tungsten in the presence of a high-electric field, Physical Review B, 1960, vol. 119, issue 1, pp. 85-93. DOI: 10.1103/PhysRev.119.85.
19. Meng G., Li Y., Koitermaa R.A. et al. In situ observation of field-induced nanoprotrusion growth on a carbon-coated tungsten nanotip, Physical Review Letters, 2024, vol. 132, issue 17, pp. 176201-1-176201-6. DOI: 10.1103/PhysRevLett.132.176201.
20. Beach Th., Vanselow R. Adsorption studies of aluminum oxide on rhenium by means of field emission microscopy, Applied Physics, 1974, vol. 4, issue 3, pp. 265-270. DOI: 10.1007/BF00884238.
21. Dobretsov L.N., Gomoyunova M.V. Emission Electronics, trans. by I. Schechtman, ed. by Y. Freundlich, T. Korn. Jerusalem, Israel Program for Scientific Translations, 1971, x+433 p.
22. Panitz J.A. Imaging atom-probe mass spectroscopy, Progress in Surface Science, 1978, vol. 8, issue 6, pp. 219-262. DOI: 10.1016/0079-6816(78)90002-3.
23. Dalgarno A. Atomic polarizabilities and shielding factor. Advances in Physics, 1962, vol. 11, issue 44, pp. 281-315. DOI: 10.1080/00018736200101302.
24. Müller E.W. Avtoionizatsiya i avtoionnaya mikroskopiya [Field ionization and field ion microscopy], Uspekhi Physics, 1962, vol. 77, issue 3, pp. 481-552. 10.3367/UFNr.0077.196207c.0481. (In Russian).

Content |