Formation of the porous structure of the NiTi intermetallic compound during vacuum sintering of mechanically milled powder
S.S. Volodko1, G.V. Markova2, A.V. Kasimtsev1, D.V. Permyakova2, A.D. Gusev2
1 METSINTEZ LLC
2 Tula State University
DOI: 10.26456/pcascnn/2026.18.031
Original article
Abstract: A study explores the feasibility of controlling the morphology and pore size of a NiTi intermetallic compound by mechanical processing the starting powder. The powder was pre-hydrogenated to induce embrittlement, processed in a planetary mill, and then vacuum sintered. It was found that intense shrinkage of the starting powder begins at temperatures of approximately 0,9 melting temperature, significantly narrowing the temperature range for porosity control. Mechanical processing reduces the average particle size from approximately 90 to 10 μm, while maintaining the powder’s phase composition and not significantly increasing crystal lattice microstrain. The use of milled powder promotes the formation of smaller, more uniformly distributed pores and enhances sintering compared to the starting powder. With comparable overall porosity, the specific length of pore-matrix boundaries increases by almost an order of magnitude for the milled powder. These results demonstrate the feasibility of controlling geometric characteristics of the NiTi pore space by varying the dispersion of the starting powder without the use of some additional pore-forming agents. The proposed approach can be used in the development of porous functional materials for which a developed pore-matrix interface and controlled pore morphology are essential.
Keywords: NiTi, porous materials, pore structure, mechanical milling, planetary mill, vacuum sintering
- Sergey S. Volodko – Ph. D., Leading Engineer, METSINTEZ LLC, ORCID: 0000-0001-6309-8218
- Galina V. Markova – Dr. Sc., Professor, Department of Mechanical Engineering and Materials Science, Tula State University, ORCID: 0000-0002-2575-4605
- Anatoly V. Kasimtsev – Dr. Sc., Director, METSINTEZ LLC
- Dariya V. Permyakova – Laboratory Assistant, Department of Mechanical Engineering and Materials Science, Tula State University, ORCID: 0009-0001-4489-278X
- Andrej D. Gusev – Laboratory Assistant, Department of Mechanical Engineering and Materials Science, Tula State University, ORCID: 0009-0008-6120-9437
For citation:
Volodko S.S., Markova G.V., Kasimtsev A.V., Permyakova D.V., Gusev A.D. Formirovanie porovoj struktury intermetallida NiTi pri vakuumnom spekanii mekhanicheski izmelchennogo poroshka [Formation of the porous structure of the NiTi intermetallic compound during vacuum sintering of mechanically milled powder], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 31-43. DOI: 10.26456/pcascnn/2026.18.031. ⎘
Full article (in Russian): download PDF file
References:
1. Jani J.M., Leary M., Subic A., Gibson M.A. A review of shape memory alloy research, applications and opportunities, Materials & Design, 2014, vol. 56, pp. 1078-1113. DOI: 10.1016/j.matdes.2013.11.084.
2. Parvizi S., Hashemi S.M., Asgarinia F. et al. Effective parameters on the final properties of NiTi-based alloys manufactured by powder metallurgy methods: a review, Progress in Materials Science, 2021, vol. 117, art. no. 100739, 43 p. DOI: 10.1016/j.pmatsci.2020.100739.
3. Köhl M., Bram M., Moser A. et al. Characterization of porous, net-shaped NiTi alloy regarding its damping and energy-absorbing capacity, Materials Science and Engineering A, 2011, vol. 528, issue 6, pp. 2454-2462. DOI: 10.1016/j.msea.2010.11.055.
4. Zhang X.X., Hou H.W., Wei L.S. et al. High damping capacity in porous NiTi alloy with bimodal pore architecture, Journal of Alloys and Compounds, 2013, vol. 550, pp. 297-301. DOI: 10.1016/j.jallcom.2012.09.145.
5. Zhao M., Shao Y., Zheng W. et al. Tailoring the damping and mechanical properties of porous NiTi by a phase leaching process, Journal of Alloys and Compounds, 2021, vol. 855, part 1, art. no. 157471, 7 p. DOI: 10.1016/j.jallcom.2020.157471.
6. Bansiddhi A., Sargeant T.D., Stupp S.I., Dunand D.C. Porous NiTi for bone implants: a review, Acta Biomaterialia, 2008, vol. 4, issue 4, pp. 773-782. DOI: 10.1016/j.actbio.2008.02.009.
7. Peng W., Liu K., Shah B.A. et al. Enhanced internal friction and specific strength of porous TiNi shape memory alloy composite by the synergistic effect of pore and Ti₂Ni, Journal of Alloys and Compounds, 2020, vol. 816, art. no. 152578, 7 p. DOI: 10.1016/j.jallcom.2019.152578.
8. Sadrnezhaad S.K., Arami H., Keivan H., Khalifezadeh R. Powder metallurgical fabrication and characterization of nanostructured porous NiTi shape-memory alloy, Materials and Manufacturing Processes, 2006, vol. 21, issue 8, pp. 727-735. DOI: 10.1080/10426910600727882.
9. Li B.-Y., Rong L.-J., Li Y.-Y. Porous NiTi alloy prepared from elemental powder sintering, Journal of Materials Research, 1998, vol. 13, issue 10, pp. 2847-2851. DOI: 10.1557/JMR.1998.0389.
10. Miao T., Zhan S., Chen X., Hu L. Effect of sintering temperature on microstructure characteristics of porous NiTi alloy fabricated via elemental powder sintering, Materials, 2024, vol. 17, issue 3, art. no. 743, 10 p. DOI: 10.3390/ma17030743.
11. Chen G., Liss K.-D., Cao P. An in situ study of NiTi powder sintering using neutron diffraction, Metals, 2015, vol. 5, issue 2, pp. 530-546. DOI: 10.3390/met5020530.
12. Yuan B., Zhang X.P., Zhu M. et al. A comparative study of the porous TiNi shape-memory alloys fabricated by three different processes, Metallurgical and Materials Transactions A, 2006, vol. 37, issue 3, pp. 755-761. DOI: 10.1007/s11661-006-0047-5.
13. GOST 18898-89. Izdeliya poroshkovye. Metody opredeleniya plotnosti, soderzhaniya masla i poristosti [Powder products. Methods for determination of density oil content and porosity]. Moscow, Publishing standards, 1990. 10 p. (In Russian).