Dynamics of thermally induced structural transformations in a ternary Pd4@Ni2@Pt2 nanocube
V.M. Samsonov, N.Yu. Sdobnyakov, D.V. Zhigunov, E.S. Mitinev, I.P. Sinitsa, A.Yu. Kolosov, D.N. Sokolov
Tver State University
DOI: 10.26456/pcascnn/2026.18.504
Original article
Abstract: Using isothermal molecular dynamics and LAMMPS software, we studied the dynamics of chemical and structural segregation upon heating Pd4@Ni2@Pt2 nanocubes from 300 to 2000 K (the subscripts indicate the number of atomic monolayers). The embedded atom method was used for simulations. The system was preliminarily subjected to relaxation for 1 ns at a temperature of 300 K. Particular attention was paid to analyzing the temperature dependence of the specific potential energy and its relationship with structural transformations at temperatures near which some jumps in this dependence occur. Several types of transitions were identified: fcc/hcp structural transitions, order/disorder transitions associated with competition between identified and unidentified crystalline phases, sphere-to-polyhedron and vice versa transitions corresponding to shape changes, and a complex melting phase transition with an atypical behavior of the temperature dependence of the specific potential energy. Two alternative approaches were used for the first time to identify the local environment: the polyhedral template method and the Ackland-Jones method. The identification results using both methods are generally in good agreement, but the Ackland-Jones method sometimes identifies as bcc instead of the hcp local environment (when the polyhedral template method was employed), and this seems apparently be due to a feature of the Ackland-Jones method based on an analysis of the distribution of bond angles between the central atom and its nearest neighbors.
Keywords: nanocube Pd4@Ni2@Pt2, Ackland-Jones method, polyhedral template matching, LAMMPS, molecular dynamics, embedded atom potential, structure transformations
- Vladimir M. Samsonov – Dr. Sc., Full Professor, General Physics Department, Tver State University, ORCID: 0000-0003-2929-8069
- Nickolay Yu. Sdobnyakov – Dr. Sc., Docent, Professor, General Physics Department, Tver State University, ORCID: 0000-0003-1749-0336
- Dmitrii V. Zhigunov – Junior Researcher, General Physics Department, Tver State University, ORCID: 0009-0007-4745-0366
- Egor S. Mitinev – 2nd year postgraduate student, General Physics Department, Tver State University
- Ilia P. Sinitsa – 4th year student, General Physics Department, Tver State University
- Andrei Yu. Kolosov – Ph. D., Researcher, General Physics Department, Tver State University, ORCID: 0000-0003-3805-0567
- Denis N. Sokolov – Ph. D., Researcher, General Physics Department, Tver State University, ORCID: 0000-0003-2411-0143
For citation:
Samsonov V.M., Sdobnyakov N.Yu., Zhigunov D.V., Mitinev E.S., Sinitsa I.P., Kolosov A.Yu., Sokolov D.N. Dinamika termoindutsirovannykh strukturnykh prevrashchenij v ternarnom nanokube Pd4@Ni2@Pt2 [Dynamics of thermally induced structural transformations in a ternary Pd4@Ni2@Pt2 nanocube], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 504-514. DOI: 10.26456/pcascnn/2026.18.504. ⎘
Full article (in Russian): download PDF file
References:
1. Sdobnyakov N.Yu. [Modelirovanie strukturnykh prevrashchenij v odnokomponentnykh i mnogokomponentnykh metallicheskikh nanosistemakh: uchebnik] Simulation of structural transformations in single-component and multi-component metallic nanosystems: a textbook. Tver, Tver State University Publ., 2025, 408 p. DOI:10.26456/sny.2025.408. (In Russian).
2. Eom N. Messing M.E., Johansson J., Deppert K. General trends in core-shell preferences for bimetallic nanoparticles, ACS Nano, 2021, vol. 15, issue 5, pp. 8883-8895. DOI: 10.1021/acsnano.1c01500.
3. Ferrando R., Jellinek J., Johnston R.L. Nanoalloys: from theory to applications of alloy clusters and nanoparticles, Chemical Reviews, 2008, vol. 108, issue 3, pp. 845-910. DOI: 10.1021/cr040090g.
4. Bogdanov S., Samsonov V., Sdobnyakov N. et al. Molecular dynamics simulation of the formation of bimetallic core-shell nanostructures with binary Ni–Al nanoparticle quenching, Journal of Materials Science, 2022, vol. 57, issue 28, pp. 13467-13480. DOI: 10.1007/s10853-022-07476-2.
5. Li Y., Wu R., Liu Y. et al. High-quality and deeply excavated PtPdNi nanocubes as efficient catalysts toward oxygen reduction reaction, Chinese Journal of Catalysis, 2021, vol. 42, issue 5, pp. 772-780. DOI: 10.1016/S1872-2067(20)63703-2.
6. Zhao X., Chen S., Fang Z. et al Octahedral Pd@Pt1.8Ni core–shell nanocrystals with ultrathin PtNi alloy shells as active catalysts for oxygen reduction reaction, Journal of the American Chemical Society, 2015, vol. 137, issue 8, pp. 2804-2807. DOI: 10.1021/ja511596c.
7. Sneed B.T., Young A.P., Jalalpoor D. et al. Shaped Pd–Ni–Pt core-sandwich-shell nanoparticles: influence of ni sandwich layers on catalytic electrooxidations, ACS Nano, 2014, vol. 8, issue 7, pp. 7239-7250. DOI: 10.1021/nn502259g.
8. Sdobnyakov N., Samsonov V., Sokolov D. et al. Thermally induced structural transformations in Pd@Ni@Pt three-shell nanostructures: molecular dynamics simulation, Chemical Physics Letters, 2026.
9. Samsonov V., Nepsha N., Sdobnyakov N. et al., Chemical and structural segregation in Pt-Pd-Ni ternary nanosystems: molecular dynamics simulation, Materials Chemistry and Physics, 2025. vol. 340, art. № 130827, 11 p. DOI: 10.1016/j.matchemphys.2025.130827.
10. Samsonov V.M., Talyzin I.V., Romanov A.A. et al. On the relation between spontaneous segregation of components in ternary Pt–Pd–Ni nanoparticles and stability of core–shell nanostructures: molecular dynamics study, Colloid Journal, 2025, vol. 87, issue 4, pp. 547-559. DOI: 10.1134/S1061933X25600605.
11. Sdobnyakov N.Y., Samsonov V.M., Kolosov A.Yu. et al. Molecular dynamics simulation of segregation in ternary Pt–Pd–Cu nanoalloys using alternative force fields, Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques, 2026, vol. 20, issue 3, pp. 693-703. DOI: 10.1134/S1027451026701259.
12. LAMMPS Molecular Dynamics Simulator. Available at: www.url: http://lammps.sandia.gov. (accessed 02.05.2026).
13. Stukowski A. Visualization and analysis of atomistic simulation data with OVITO – the open visualization tool, Modelling and Simulation in Materials Science and Engineering, 2010, vol. 18, issue 1, pp. 015012-1-015012-7. DOI: 10.1088/0965-0393/18/1/015012.
14. Zhou X.W., Johnson R.A., Wadley H.N.G. Misfit-energy-increasing dislocations in vapor-deposited CoFe/NiFe multilayers, Physical Review B, 2004, vol. 69, issue 14, pp. 113-114. DOI: 10.1103/PhysRevB.69.144113.
15. Larsen P.M., Schmidt S., Schiøtz J. Robust structural identification via polyhedral template matching modelling, Modelling and Simulation in Materials Science and Engineering, 2016, vol. 24, no. 5, art. № 055007, 18 p. DOI: 10.1088/0965-0393/24/5/055007.
16. Polak W.Z. Efficiency in identification of internal structure in simulated monoatomic clusters: Comparison between common neighbor analysis and coordination polyhedron method, Computational Materials Science, 2022, vol. 201, art. № 110882, 8 p. DOI: 10.1016/j.commatsci.2021.110882.
17. Tsuzuki H., Branicio P.S., Rino J.P. Structural characterization of deformed crystals by analysis of common atomic neighborhood, Computer Physics Communications, 2007, vol. 177, issue 6, pp. 518-523. DOI: 10.1016/j.cpc.2007.05.018.
18. Ackland G.J., Jones A.P. Applications of local crystal structure measures in experiment and simulation, Physical Review B, 2006, vol. 73, issue 5, pp. 054101-1-054104-7. DOI: 10.1103/PhysRevB.73.054104.