Ferromagnetic nanoclusters in austenite: nature, role, characteristics, and controllability
V.N. Pustovoit, Yu.V. Dolgachev
Don State Technical University
DOI: 10.26456/pcascnn/2026.18.122
Original article
Abstract: This article examines the nature of magnetic inhomogeneities in austenite steels and their fundamental role in phase transformations. It is shown that austenite, being a paramagnetic phase, contains spontaneously emerging regions of short-range ferromagnetic order (ferromagnetic nanoclusters), the existence of which has been confirmed experimentally using neutron magnetic diffraction methods. The dependence of the magnetic susceptibility of austenite is described by the Langevin function for superparamagnets, which reflects the fluctuation nature of these magnetic inhomogeneities localized in nanometer-sized regions. The magnetic state of the initial phase crucially determines the nature of the γ→α transformation. Using computer simulation based on the Ising model, the effect of an external magnetic field on the characteristics of nanoclusters over a wide temperature range was studied. It has been established that a magnetic field of up to 2,4 MA/m can increase the average cluster size, their total number by two orders of magnitude (most effectively at low temperatures, where the increase reaches 1,4 nm), and increase the proportion of large clusters, as well as extend their stable existence by up to 25%. Experiments with quenching in a constant magnetic field for a range of steels demonstrated a significant reduction in the volume fraction of retained austenite, comparable to cold treatment, and an acceleration of the bainitic transformation kinetics by 1,5-1,8 times. The magnetic field enhances the magnetic heterogeneity of austenite, activates new nucleation centers, and stimulates the multiplicative mechanism of α-phase formation, providing a practical tool for targeted phase transition control during heat treatment of steels in a magnetic field.
Keywords: austenite, magnetic state, nanocluster, steel, hardening, external magnetic field
- Victor N. Pustovoit – Dr. Sc., Professor, Department of Materials Science and Metal Technologies, Don State Technical University, ORCID: 0000-0001-6999-3520
- Yuri V. Dolgachev – Dr. Sc., Professor, Department of Materials Science and Metal Technologies, Don State Technical University, ORCID: 0000-0002-8558-1136
For citation:
Pustovoit V.N., Dolgachev Yu.V. Ferromagnitnye nanoklastery v austenite: priroda, rol, kharakteristiki i vozmozhnost upravleniya [Ferromagnetic nanoclusters in austenite: nature, role, characteristics, and controllability], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 122-132. DOI: 10.26456/pcascnn/2026.18.122. ⎘
Full article (in Russian): download PDF file
References:
1. Sucksmith W., Pearce R.R. The paramagnetism of the ferromagnetic elements, Proceedings of the Royal Society of London. Series A. Mathematical and Physical Sciences, 1938, vol. 167, isuue 929, pp. 189-204. DOI: 10.1098/rspa.1938.0126.
2. Vonsovsky S.V. Ferromagnetizm kak problema uporyadocheniya [Ferromagnetism as a problem of ordering], Izvestiya AN SSSR, Seriya Fizicheskaya [Bulletin of the Academy of Sciences of the USSR. Physical Series], 1947, vol. 11, issue 5, pp. 485-486. (In Russian).
3. Brown P.J., Capellmann H., Déportes J. et al. Observations of ferromagnetic correlations at high temperatures in paramagnetic iron, Journal of Magnetism and Magnetic Materials, 1982, vol. 30, issue 2. pp. 243-248. DOI: 10.1016/0304-8853(82)90204-9.
4. Korenman V. Consequences of short range magnetic order above TC in iron and nickel, Journal of Magnetism and Magnetic Materials, 1983, vol. 31-34, part 1, pp. 301-304. DOI: 10.1016/0304-8853(83)90258-5.
5. Ignatenko A.N., Katanin A.A., Irkhin V.Yu. Strong short-range magnetic order in a frustrated FCC lattice and its possible role in the iron structural transformation, Journal of Experimental and Theoretical Physics Letters, 2008, vol. 87, issue 10, pp. 555-559. DOI: 10.1134/S0021364008100093.
6. Voronchikhin L.D., Romashev L.N., Fakidov I.G. Anomalous superparamagnetism of the gamma phase of Fe-Cr-Ni alloy, Soviet Physics-Solid State, 1975, vol. 16, issue 9. pp. 1708-1711.
7. Shull C.G., Yamada Y. Magnetic electron configuration in iron, Journal of the Physical Society of Japan, 1962, vol. 17, supplement B-III, pp. 1-6.
8. Snezhnoj G.V., Snezhnoj V.L., Menyajlo V.I. Klasternyi kharakter zarozhdeniya martensita s izotermicheskoi i atermicheskoi mikrovkinetikami [Clustered character of martensite nucleation with isothermic and athermic microkinetics], Lit'e i metallurgiya [Foundry production and metallurgy], 2008, no. 4(49), pp. 63-66. DOI: 10.21122/1683-6065-2008-4-63-66. (In Russian).
9. Spooner S., Averbach B.L. Spin correlations in iron, Physical Review, 1966, vol. 142, issue 2. pp. 291-299. DOI: 10.1103/PhysRev.142.291.
10. Bozorth R.M. Magnetic properties of metals and alloys. Cleveland, American Society for Metals, 1959, vi, 349 p.
11. Kaufman L., Clougherty E.V., Weiss R.J. The lattice stability of metals – III. Iron, Acta Metallurgica, 1963, vol. 11, issue 5, pp. 323-335. DOI: 10.1016/0001-6160(63)90157-3.
12. Hasegawa H., Pettifor D.G. Microscopic theory of the temperature-pressure phase diagram of iron, Physical Review Letters, 1983, vol. 50, issue 2. pp. 130-133. DOI: 10.1103/PhysRevLett.50.130.
13. Sedov V.L. Antiferromagnetizm gamma-zheleza: problema invara [Antiferromagnetism of gamma-phase iron: invar problem]. Moskva, Nauka Publ., 1987, 287 p. (In Russian).
14. Zener C. Impact of magnetism upon metallurgy, Journal of The Minerals, Metals & Materials Society, 1955, vol. 7, issue 5. pp. 619-630. DOI: 10.1007/BF03377550.
15. Zener C. Interaction between the d shells in the transition metals, Physical Review, 1951, vol. 81, issue 3, pp. 440-444. DOI: 10.1103/PhysRev.81.440.
16. Zener C., Heikes R.R. Exchange interactions, Reviews of Modern Physics, 1953, vol. 25, issue 1, pp. 191-198. DOI: 10.1103/RevModPhys.25.191.2.
17. Weiss R.J., Tauer K.J. Components of the thermodynamic functions of iron, Physical Review, 1956, vol. 102, issue 6. pp. 1490-1495. DOI: 10.1103/PhysRev.102.1490.
18. Razumov I.K., Gornostyrev Y.N., Katsnelson M.I. Effect of magnetism on kinetics of γ-α transformation and pattern formation in iron, Journal of Physics: Condensed Matter, 2013, vol. 25, no. 13, art. no 135401, 9 p. DOI: 10.1088/0953-8984/25/13/135401.
19. Razumov I.K., Boukhvalov D.V., Petrik M.V. et al. Role of magnetic degrees of freedom in a scenario of phase transformations in steel, Physical Review B: Condensed Matter and Materials Physics, 2014, vol. 90, issue9, pp. 094101-1-094101-8. DOI: 10.1103/PhysRevB.90.094101.
20. Razumov I.K., Gornostyrev Y.N., Katsnelson M.I Towards the ab initio based theory of phase transformations in iron and steel, Physics of Metals and Metallography, 2017, vol. 118, issue 4, pp. 362-388. DOI: 10.1134/S0031918X16130032.
21. Landau L.D., Lifshitz E.M. Statistical Physics. Oxford: Elsevier, 2013, 544 p.
22. García-Hernández L.A., Guzmán-Hernández C.B., Oza G. Magnetic properties of CoFe₂O₄ nanoparticles: experimental characterization and numerical analysis using the Ising model, Journal of Nanoparticle Research, 2025, vol. 27, issue 1, art. no 281, 9 p. DOI: 10.1007/s11051-025-06476-y.
23. Pustovoit V.N., Dolgachev Yu.V. Magnitnaya geterogennost' austenita i prevrashcheniya v stalyakh [Magnetic heterogeneity of austenite and transformations in steels]. Rostov-on-Don, Don State Technical University Publ., 2021, 198 p. (In Russian).
24. Dolgachev Yu.V., Pustovoit V.N. Komp'yuternoe modelirovanie magnitnogo sostoyaniya austenita [Computer simulation of the magnetic state of austenite]. Certificate RF, no. 2021664709, 2021. (In Russian).
25. Pustovoit V.N., Dolgachev Yu.V. K voprosu o mestakh zarozhdeniya martensita [On the issue of the places of origin of martensite], Izvestiya Volgogradskogo gosudarstvennogo tekhnicheskogo universiteta [Bulletin of the Volgograd State Technical University], 2014, no. 23 (150), pp. 110-114. (In Russian).
26. Pustovoit V.N., Dolgachev Yu.V. O prirode mest zarozhdeniya martensita pri zakalke stali [Revisiting the nature of sites of martensite nucleation during steel hardening], Izvestiya vysshikh uchebnykh zavedeniy. Chernaya metallurgiya [Izvestiya. Ferrous Metallurgy], 2019, vol. 62, no. 2, pp. 109-114. DOI: 10.17073/0368-0797-2019-2-109-114. (In Russian).
27. Dolgachev Yu.V., Pustovoit V.N., Vernigorov Yu.M. Stress martensite nucleation in a state of premartensitic lattice instability, Advanced Engineering Research, 2024, vol. 24, issue 1, pp. 58-65. DOI: 10.23947/2687-1653-2024-24-1-58-65.
28. Pustovoit V.N., Dolgachev Yu.V. Interaction of ferromagnetically ordered clusters with dislocations in austenite and twinning, Materials Science Forum, 2022, vol. 1052, pp. 134-139. DOI: 10.4028/p-a8jty9.
29. Dolgachev Yu.V., Pustovoit V.N., Nefedov D.V. Stimulation of the bainite transformation scenario by an external magnetic field, Safety of Technogenic and Natural Systems, 2024, vol. 1, no. 11, pp. 88-96. DOI: 10.23947/2541-9129-2024-8-1-88-96.